GB/T 714 Q420qNHF Weathering Bridge Steel Supplier
What is GB/T 714 Q420qNHF Weathering Bridge Steel?
Q420qNHF is weathering bridge structural steel to GB/T 714. In the standard’s own notation it is written Q420qFNH: Q for yield, 420 for the minimum yield in MPa, q for qiao (bridge), the quality letter, and NH for nai hou, weathering. The letter F means Charpy V-notch testing at −60°C.
Q420qNH is high-strength weathering plate for unpainted long-span girders and trusses. Q420qNH keeps the Q345qNH weathering chemistry and adds strength through TMCP and microalloying. Pcm is capped at 0.23% to 50 mm, and the grade is tested in D, E or F.
Q420qNHF (Q420qFNH) is the lowest weathering grade that offers the F letter in GB/T 714-2025: −60°C Charpy, 47 J over 12 mm. It suits unpainted bridges in Arctic and sub-Arctic climates.
GB/T 714-2025, in force since 1 May 2026, fully replaces GB/T 714-2015; the changes for weathering grades are listed below.
SHH STEEL (Shanghai Shenghonghe Import & Export Co., Ltd.) is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. We ship Q420qNHF cut to size with an EN 10204 3.1 or 3.2 certificate. Sister grades are listed under GB/T 714; other unpainted options are under weathering steel plates and EN 10025-5.
Material Specification
| Specification element | Requirement | SHH STEEL compliance |
|---|---|---|
| Standard | GB/T 714-2025 Q420qFNH | Confirmed |
| Product | Single-rolled plate ≤150 mm; hot-rolled strip and cut plate ≤25.4 mm | Plate |
| Thickness with tensile values | Up to 130 mm for Q420qNH | Confirmed |
| Minimum yield ReL | 420 MPa ≤50 mm; 410 MPa >50–100 mm | Confirmed |
| Minimum tensile Rm | 540 MPa ≤100 mm (no upper limit in the standard) | Confirmed |
| Elongation A | ≥ 19% | Confirmed |
| Charpy V-notch | −60°C, 47 J (12–100 mm), longitudinal | Confirmed |
| Weathering index | I ≥ 6.0 (Table 5, footnote c) | Calculated on MTC |
| Delivery condition | TMCP or TMCP + tempering | As ordered |
| Weldability index | Pcm (Table 8) | Printed on MTC |
| Ultrasonic testing | Plate >20 mm: GB/T 2970, Class II or better | Every plate |
| Through-thickness | Z15, Z25 or Z35 to GB/T 5313, when ordered | As ordered |
| Dimensions | GB/T 709 | Confirmed |
| Certificate | GB/T 247; EN 10204 3.1 or 3.2 | As ordered |
Grades often compared with Q420qNHF are ASTM A709 HPS 50W, ASTM A709 HPS 70W and EN 10025-4 S420ML; the comparison below shows where they differ.
Chemical Composition: Heat Analysis and Product Analysis
A check analysis on finished plate often reads a few hundredths higher than the mill certificate. That is not automatically a failure. The certificate shows the heat (ladle) analysis; plate drilled after rolling is judged as product analysis, with the tolerances of GB/T 222.
Table 1 below is the heat (ladle) analysis for Q420qNHF from GB/T 714-2025 Tables 1, 5.
| Element | Q420qNHF heat analysis (%) | Note |
|---|---|---|
| C, max | 0.11 | |
| Si | 0.15 – 0.50 | Counts in I |
| Mn | 1.10 – 1.50 | Min 0.50% for coil only |
| P, max | 0.015 | Letter F |
| S, max | 0.006 | Letter F |
| Cu | 0.25 – 0.50 | Main weathering element |
| Cr | 0.40 – 0.70 | Weathering element |
| Ni | 0.30 – 0.40 | Weathering element |
| Mo, max | 0.20 | |
| Nb | 0.010 – 0.100 | Microalloy (see note) |
| V | 0.010 – 0.100 | Microalloy (see note) |
| Ti | 0.006 – 0.030 | Microalloy (see note) |
| Als | 0.015 – 0.050 | Alt 0.020–0.055% if total Al is used |
| N, max | 0.0080 | |
| B, max (residual) | 0.0005 | ≤0.0014% if C ≤0.06% |
| H, max (residual) | 0.0002 | |
| Weathering index I | ≥ 6.0 | Calculated from heat analysis |
Nb, V, Ti and Al may be added singly or together. Added singly, each must meet the range above; added together, at least one must reach its minimum and Nb + V + Ti ≤ 0.22%. Calcium treatment is required to control sulfide shape.
Table 2 is the product analysis: the limits a check analysis on finished plate is judged against. GB/T 714-2025 clause 7.1.3 calls up GB/T 222 for the permitted deviations.
| Element | Heat limit (%) | Deviation, GB/T 222-2025 Table 1 | Q420qNHF product analysis (%) |
|---|---|---|---|
| C | ≤ 0.11 | +0.02 | ≤ 0.13 |
| Si | 0.15 – 0.50 | ±0.05 | 0.10 – 0.55 |
| Mn | 1.10 – 1.50 | ±0.06 | 1.04 – 1.56 |
| P | ≤ 0.015 | +0.005 | ≤ 0.020 |
| S | ≤ 0.006 | +0.005 | ≤ 0.011 |
| V | 0.010 – 0.100 | +0.02 / −0.01 | ≤ 0.120 |
| Ti | 0.006 – 0.030 | +0.02 / −0.01 | ≤ 0.050 |
| Nb | 0.010 – 0.100 | ±0.005 (listed for 0.015–0.060%) | Above 0.060%: agree in contract |
| Cu | 0.25 – 0.50 | ±0.05 | 0.20 – 0.55 |
| Cr | 0.40 – 0.70 | ±0.05 | 0.35 – 0.75 |
| Ni | 0.30 – 0.40 | ±0.05 | 0.25 – 0.45 |
| Als | 0.015 – 0.050 | ±0.003 | Lower limit −0.003 (Table 1 row is for Al ≥0.015%; confirm) |
| Mo | ≤ 0.20 | Not listed in Table 1 | Agree in contract |
| N | ≤ 0.0080 | Listed only for 0.010–0.020% | Agree in contract |
How to read Table 2. Weathering bridge steel is normally classed as low-alloy steel, so Table 1 of GB/T 222 applies. Where the heat limit is a range, the deviation applies to both ends; for one heat, an element may deviate in one direction only.
Mechanical Properties
Tensile values follow Table 9 of GB/T 714-2025 for Q420qNH. Tensile specimens are transverse; round specimens are used above 40 mm. Where yield is not distinct, Rp0.2 replaces ReL.
| Nominal thickness | ReL min (MPa) | Rm min (MPa) | A min |
|---|---|---|---|
| ≤ 50 mm | 420 | 540 | 19% |
| > 50 – 100 mm | 410 | 540 | 19% |
| > 100 – 130 mm | 365 | 460 | 19% |
Impact values follow Table 10, on longitudinal specimens, average of three:
| Letter / test temperature | KV2 ≤12 mm | KV2 >12 – 100 mm | KV2 >100 – 150 mm |
|---|---|---|---|
| F / −60°C | By agreement | 47 J | Not applicable |
One single value may fall below the required average, but not below 70% of it. Plate over 8 mm and under 12 mm is tested with 7.5 mm specimens (75% of the value); 6–8 mm plate with 5 mm specimens (50%). Plate under 6 mm is not impact tested.
180° bend test, transverse: mandrel D = 2a up to 16 mm and 3a above 16 mm; may be omitted when the mill guarantees it. Yield ratio is not mandatory. If the contract asks for it, Annex C recommends ReL/Rm ≤ 0.88 up to 12 mm and ≤ 0.86 above 12 mm for TMCP plate.
Q420qNHD / Q420qNHE / Q420qNHF: Which Quality Grade?
Q420qNHF is tested at −60°C. It suits Arctic and sub-Arctic bridges, high-latitude rail lines and owners who want the largest toughness margin for fracture-critical members. F is the coldest letter in GB/T 714: Charpy at −60°C, P ≤0.015% and S ≤0.006%. It exists only for Q420q and above (and their NH versions), and its energy rises with strength.
| Grade | Test temp. | KV2 ≤12 mm | KV2 12–100 mm | KV2 >100 mm | P / S max (%) |
|---|---|---|---|---|---|
| Q420qNHD | −20°C | 80 J | 120 J | 47 J | 0.025 / 0.015 |
| Q420qNHE | −40°C | 80 J | 120 J | 31 J | 0.020 / 0.010 |
| Q420qNHF | −60°C | By agreement | 47 J | — | 0.015 / 0.006 |
Note that F energy at Q420q is 47 J, not 120 J: the colder test uses a lower energy that GB/T 714-2025 raises with strength, from 47 J at Q420q/Q460q to 77 J at Q690q. Plate up to 12 mm needs an agreed value.
Q420qNHF: What Changed from GB/T 714-2015 to GB/T 714-2025
For Q420qNHF buyers the 2025 edition changes more than the year on the certificate. The points below come from the foreword of GB/T 714-2025 and its tables.
- The weathering requirement changed: Table 5 now requires a corrosion index I ≥ 6.0, and the 2015 Annex C guide for assessing weathering resistance was deleted.
- A Pcm table for weathering steel (Table 8) was added.
- Annex A now gives reference bridge-site environments for unpainted use (chloride, SO₂ and time-of-wetness limits).
- Yield values above 100 mm were added for Q420qNH (365 MPa for >100–130 mm).
- Tensile strength is now banded by thickness (e.g. lower minimum Rm above 100 mm) instead of one value.
- Impact energy is set by thickness band (≤12 mm, 12–100 mm, >100 mm) in Table 10.
- Yield ratio is no longer a clause value; it is agreed in the contract, with recommendations in informative Annex C.
If a drawing cites 2015 and the plate is made to 2025, get the designer’s written acceptance; tensile strength above 100 mm and the yield-ratio basis differ.
Q420qNHF vs ASTM A709 and EN 10025: Which Grade Matches?
Can Q420qNHF replace a US or European bridge grade, or the other way round? Strength can match; toughness rules differ in kind, not only in number.
| Property | Q420qNHF | ASTM A709 HPS 50W | ASTM A709 HPS 70W | EN 10025-4 S420ML |
|---|---|---|---|---|
| Min. yield (MPa) | 420 (≤50 mm) | 345 | 485 | 420 (≤16 mm) |
| Tensile (MPa) | 540 min | 485 min | 585 – 760 | 520 – 680 |
| Charpy | 47 J at −60°C (12–100 mm) | CVN by temperature zone; fracture-critical (F) levels | CVN by temperature zone; fracture-critical (F) levels | 27 J at −50°C |
| Weathering chemistry | Yes, I ≥ 6.0 | Yes | Yes | No |
ASTM A709 sets Charpy requirements by temperature zone (1, 2, 3) and by member type: non-fracture-critical (T) or fracture-critical (F). GB/T 714 sets one value per letter, so compare the A709 zone with the GB/T 714 test temperature, not grade with grade.
EN 10025-5 weathering grades are general structural steels without a bridge-specific toughness level of 120 J; they suit many bridges but are not a one-to-one match.
At −60°C, the 47 J required for Q420qNHF is a demanding figure; general structural grades rarely prove any toughness that cold. For the C, D and E letters GB/T 714 asks 120 J, several times the 27–40 J typical of GB/T 1591 plate.
Q420qNHF Atmospheric Corrosion Index I and Unpainted Bridges
GB/T 714-2025 Table 5, footnote c, requires every Q420qNHF heat to reach an atmospheric corrosion index I of at least 6.0, calculated from the heat analysis:
I = 26.01(%Cu) + 3.88(%Ni) + 1.20(%Cr) + 1.49(%Si) + 17.28(%P) − 7.29(%Cu)(%Ni) − 9.10(%Ni)(%P) − 33.39(%Cu)²
This is the same predictive formula used with ASTM G101 for ASTM A709 Grade 50W and ASTM A709 HPS 70W, which makes Chinese and US ASTM A709 weathering steel plates easy to compare with Q420qNHF.
| Worked example (our calculation) | Cu | Ni | Cr | Si | P | I |
|---|---|---|---|---|---|---|
| All weathering elements at their Table 5 minimum | 0.25 | 0.30 | 0.40 | 0.15 | 0.010 | 5.88 |
| Illustrative mid-range heat | 0.32 | 0.36 | 0.55 | 0.30 | 0.012 | 6.74 |
Note the first row: a heat that only just meets every Table 5 minimum can still fall short of I = 6.0. That is why we ask the mill to print I on every Q420qNHF certificate, not just the chemistry.
Where can the steel be left unpainted? Annex A of GB/T 714-2025 gives reference bridge-site conditions:
- Rural or urban atmosphere with annual chloride deposition ≤ 3 mg/(m²·d)
- Annual SO₂ deposition ≤ 24 mg/(m²·d)
- Time of wetness ≤ 5,256 h per year (temperature above 0°C and relative humidity above 80%)
- Coastal sites only if they meet the same limits; for marine atmospheres Annex D points to T/CISA 073
The patina on Q420qNHF needs wet-dry cycles. Members that stay damp, such as those under leaking joints or close to vegetation, rust like ordinary steel. Plan inspection access in the first five years.
Welding Q420qNHF and Fatigue in Bridge Girders
GB/T 714-2025 clause 7.1.2 uses CEV for normalized, QT and TMCP steel with C >0.12%, and Pcm for weathering steel and TMCP steel with C ≤0.12%, both from the heat analysis:
CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15
Pcm = C + Si/30 + Mn/20 + Cu/20 + Ni/60 + Cr/20 + Mo/15 + V/10 + 5B
| Index | ≤50 mm | >50–100 mm | >100–130 mm |
|---|---|---|---|
| Pcm, Q420qNH (Table 8) | ≤ 0.23 | ≤ 0.25 | By agreement |
For Q420qNHF, ask the fabricator which index the WPS was qualified on. Where the WPS uses CEV and the standard uses Pcm, we print both on the certificate. At −60°C, both weld metal and HAZ must prove toughness. Expect lower heat input, more passes and consumables qualified at −60°C.
Typical consumables for Q420qNHF: weathering-matched Ni-Cu consumables (AWS E8018-W2 type for 345–420 MPa), with higher-strength weathering wires for 460–500 MPa.
Fatigue. Welded details govern fatigue life in a bridge, and their fatigue strength is set by detail category, not by yield strength. Higher-strength plate can carry higher stress ranges only if detailing improves too.
Fatigue design follows JTG D64 (highway) and TB 10091 (railway) in China, EN 1993-1-9 in Europe and AASHTO LRFD in the US; fabrication commonly follows TB 10212, JTG/T 3650 or AWS D1.5.
Q420qFNHZ15, Z25 and Z35: Through-Thickness Plate for Bridges
Lamellar tearing appears in thick plate loaded across its thickness, typically at cruciform joints and anchor plates. A Z grade adds a short-transverse tensile test and a lower sulfur cap.
GB/T 714 adds the Z level to the end of the designation, for example Q420qFNHZ25. The test and acceptance follow GB/T 5313 and apply to plate 15 mm and thicker.
| Z grade | Heat sulfur, max (%) | Reduction of area, avg / single (%) |
|---|---|---|
| Z15 | 0.010 | 15 / 10 |
| Z25 | 0.007 | 25 / 15 |
| Z35 | 0.005 | 35 / 25 |
F chemistry limits S to 0.006%, which already meets the Z25 sulfur cap (0.007%). Only Z35 (S ≤0.005%) needs a further step.
Z-grade Q420qNHF carries a longer lead time because the heat must be planned as low-sulfur from the start. Tell us early. Z options apply across the GB/T 714 bridge steel range.
Equivalent Material Grades
Annex B of GB/T 714-2025 lists foreign grades against each strength level. It is informative: it tells you which families are close, not that the plates are interchangeable.
| Standard | Grade(s) | Fit for Q420qNHF |
|---|---|---|
| ASTM A709 | ASTM A709 HPS 70W | Higher strength; weathering |
| EN 10025-4 | EN 10025-4 S420ML | Strength match, not weathering |
| ASTM A588 | ASTM A588 Grade K | Weathering, lower strength |
| GB/T 714 (painted twin) | Q420qF | Same strength, no weathering elements |
For weathering grades also compare the corrosion index basis. Q420qNHF requires I ≥ 6.0 by the formula above; check that the substitute is assessed on the same basis.
Q420qNHF Testing, UT and Certificate
A batch of Q420qNHF is one grade, one heat, one thickness, one rolling schedule and one heat-treatment condition, up to 60 t. Table 12 of GB/T 714-2025 sets the tests:
| Test | Frequency | Method |
|---|---|---|
| Heat analysis | 1 per heat | GB/T 20066; GB/T 4336 / GB/T 223 |
| Weathering index I | Calculated per heat | Table 5 formula |
| Tensile | 1 per batch | GB/T 2975 / GB/T 228.1 |
| Bend 180° | 1 per batch (may be waived if guaranteed) | GB/T 232 |
| Charpy V at −60°C | 3 specimens per batch | GB/T 229 |
| Through-thickness (Z) | 3 specimens per batch, when ordered | GB/T 5313 |
| Ultrasonic | Every plate >20 mm, Class II or better | GB/T 2970 |
| Surface and dimensions | Every plate | Visual and gauges |
Impact retest: if a set fails, three more specimens are taken from the same batch. The average of all six must meet the requirement; two values may be below it, but only one below 70%. At −60°C, mills may need trial heats before the production run; we agree the test plan before accepting the order.
Dimensions
Typical Q420qNHF dimensions on our offers:
- Thickness: 6 mm – 130 mm under GB/T 714 tensile tables; most orders 10 – 80 mm
- Width: 1500 – 4000 mm, depending on mill and thickness
- Length: 6000 – 18000 mm; longer by enquiry
- Edge: mill edge or cut edge
- Weight: theoretical, 7.85 g/cm³
Deck plate, webs, flanges, diaphragms and stiffeners are cut to drawing. For U-ribs and rolled sections on the same bridge, see steel beam profiles and steel structural profiles.
Tolerances
For Q420qNHF, thickness tolerance follows GB/T 709 Class B unless the order says otherwise: −0.30 mm at every thickness, with the plus side shown below.
| Nominal thickness (mm) | Width ≤ 1500 mm | Width > 1500 – 2500 mm |
|---|---|---|
| > 8 – 15 | −0.30 / +0.80 | −0.30 / +1.00 |
| > 15 – 25 | −0.30 / +1.00 | −0.30 / +1.20 |
| > 25 – 40 | −0.30 / +1.10 | −0.30 / +1.30 |
| > 40 – 60 | −0.30 / +1.30 | −0.30 / +1.50 |
| > 60 – 100 | −0.30 / +1.50 | −0.30 / +1.80 |
| > 100 – 150 | −0.30 / +2.10 | −0.30 / +2.50 |
Bridge fabricators often ask for Class C (zero minus) on deck and flange plate so section properties are never under the design value. Wider plates follow the heavier GB/T 709 rows; we state them on the offer.
Q420qNHF Price Factors and How to Order
A Q420qNHF price per ton is a base price plus extras. The extras explain most gaps between quotes.
| Cost driver | Effect on price |
|---|---|
| Strength level Q420q | Higher levels need more alloy and tighter rolling control |
| Quality letter | Highest extra: −60°C testing, S ≤0.006%, limited mills |
| Weathering alloys | Cu, Cr, Ni additions and I-index control add a weathering extra |
| Delivery route | TMCP / TMCP+T |
| Thickness | Over 60 mm and under 10 mm carry size extras |
| Z15 / Z25 / Z35 | Low-sulfur heat, Z test, UT; Z35 costs most |
| Width and length | Over 3000 mm wide or 15 m long needs mill confirmation |
| Quantity per size | Mill minimums per heat and size |
| Inspection and processing | 3.2 witness, profile cutting, blasting, priming quoted per item |
To get a firm quote in one round, send:
- Grade, edition and Z level, e.g. Q420qFNHZ25 to GB/T 714-2025
- Thickness × width × length and pieces or tonnes
- Delivery route and UT class if beyond Class II
- Certificate type and inspector
- Destination port and Incoterm
We quote plate price, extras and freight line by line. Need another letter? See Q420qNHD, Q420qNHE.
Applications
| Sector | Typical Q420qNHF components |
|---|---|
| Unpainted highway bridges | Plate girders and box girders in rural and urban atmospheres |
| Railway bridges | Truss members, plate girders, bracing |
| Remote and mountain sites | Bridges where repainting access is difficult or costly |
| Urban viaducts | Exposed girders with architectural rust finish |
| Pedestrian bridges | Unpainted box sections |
The letter F suits Arctic and sub-Arctic bridges, high-latitude rail lines and owners who want the largest toughness margin for fracture-critical members.
Q420qNHF is the wrong plate for marine splash zones, tunnels, sites with heavy de-icing salt spray, or members that stay wet. There, use painted Q420qF or look at marine-atmosphere grades under T/CISA 073.
Supply Capability and Global Delivery
SHH STEEL sources Q420qNHF from first-line bridge-plate mills, including drafters of GB/T 714-2025 such as Ansteel, Valin Xiangtan, Jiangyin Xingcheng, Wuyang, Shougang and Xinyu.
- Certificates: EN 10204 3.1 standard; 3.2 with third-party witness (SGS, BV, TÜV or owner’s inspector)
- Tests: tensile, −60°C Charpy, bend, Z test, UT, product analysis, weathering index
- Processing: CNC plasma and flame cutting, bevelling, drilling, shot blasting and priming (or blasting only, for unpainted weathering steel)
- Terms: FOB Shanghai, CFR, CIF; TT, LC or TT + LC
- Marking: steel-stamped and paint-marked with grade, heat, size and mill, per GB/T 247
We ship Q420qNHF to fabricators in Asia, Africa, the Middle East, Europe and the Americas, by break-bulk or container.
Lead time: about 45–60 days from mill rolling; Z35, F letter or 3.2 inspection adds about 1–2 weeks. Sea time from Shanghai is about 7–12 days to Southeast Asia and 28–35 days to North Europe.
Why Choose SHH STEEL
SHH STEEL works mill-direct as a steel manufacturer and exporter and global steel mill sourcing partner, China origin. Every Q420qNHF plate is traced to its heat.
Before shipment we check four lines on every Q420qNHF certificate: yield and tensile for the actual thickness band, Charpy at −60°C, the Pcm and weathering index, and UT results. If one fails, the plate does not ship as Q420qNHF.
Arctic sites often have long wet periods under snow. Check time of wetness against the 5,256 h/year limit in Annex A before omitting paint.
We also tell buyers when another grade fits better. Neighbouring levels are Q390qNH and Q460qNHF. The painted counterpart is Q420qF. Browse more structural steel plates and high strength low alloy plates.
FAQ
-
What is Q420qNHF steel?
- Q420qNHF (Q420qFNH) is weathering bridge steel plate to GB/T 714-2025. It has 420 MPa minimum yield up to 50 mm, 540 MPa minimum tensile, Charpy impact of 47 J at −60°C for 12–100 mm plate, and Cu-Cr-Ni chemistry with a corrosion index I of at least 6.0 for unpainted bridges.
-
What impact energy does Q420qNHF need at −60°C?
- GB/T 714-2025 requires at least 47 J at −60°C on longitudinal specimens for Q420qNHF plate over 12 mm and up to 100 mm. For plate 12 mm and thinner the value is by agreement. F energy rises with strength: 47 J for Q420q and Q460q, 54 J for Q500q, 60 J for Q550q, 69 J for Q620q and 77 J for Q690q.
-
What is the maximum thickness of Q420qNHF?
- GB/T 714-2025 covers bridge plate up to 150 mm, but tensile values for Q420qNH stop at 130 mm. Above that there is no table value, so Q420qNHF cannot be certified thicker than 130 mm without a special agreement.
-
What is the ASTM or EN equivalent of Q420qNHF?
- Close grades for Q420qNHF: No direct equivalent in Annex B / closest: ASTM A709 HPS 70W (higher) / EN 10025-4 S420ML (not weathering). These are close families, not drop-in substitutes; compare yield at thickness, impact temperature and energy, and the weldability index before substituting.
-
Can GB/T 714 bridge plate be normalized?
- Only in one case. GB/T 714-2025 clause 6.2 requires TMCP, TMCP + tempering or quenched and tempered delivery, but Q345q and Q370q plate over 100 mm and up to 150 mm may be normalized by agreement.
-
Does Q420qNHF weathering steel need painting?
- Not if the bridge site and details suit it. GB/T 714-2025 Annex A gives reference conditions for unpainted use: annual chloride deposition ≤3 mg/(m²·d), SO₂ ≤24 mg/(m²·d) and time of wetness ≤5,256 h per year. Marine splash zones and salt-sprayed members still need protection.
Conclusion
Q420qNHF to GB/T 714 is weathering bridge steel with 420 MPa minimum yield, Cu-Cr-Ni chemistry, a weathering index of at least 6.0 and 47 J Charpy at −60°C for 12–100 mm plate.
It sits between Q390qNH and Q460qNHF in the weathering range, with Q420qNHD and Q420qNHE as sister letters. For Q420qNHF, a product analysis on finished plate is judged against GB/T 222 deviations, not the heat limits, so put the basis in the contract.
With SHH STEEL the Q420qNHF certificate is complete: heat chemistry, weldability index, yield, tensile, elongation and Charpy, to EN 10204 3.1 or 3.2. Add product analysis, a Z level or a stricter UT class as needed.
We ship from Shanghai to bridge builders worldwide. Browse the full GB/T 714 range or other weathering steel plates.