GB/T 714 Q690qE bridge steel plate stacked at SHH STEEL warehouse

GB/T 714 Q690qE Bridge Steel Plate Supplier

GB/T 714 Q690qE is bridge structural steel plate with 690 MPa minimum yield, 770 MPa minimum tensile and Charpy V-notch impact of 120 J at −40°C for 12–100 mm plate. SHH STEEL supplies Q690qE mill-direct, TMCP / TMCP+T / QT, up to 100 mm, with Z15–Z35, UT and heat and product analysis.
Keywords
Q690qE, Q690qE steel plate, GB/T 714 Q690qE, Q690q-E, Q690q E, Q690qE bridge steel, Q690qEZ15, Q690qEZ25, Q690qEZ35, bridge steel plate, Q690qE supplier
Equivalent Grades:
ASTM A709 HPS 100W / EN 10025-6 S690Q, S690QL, S690QL1 (Annex B) — Material Specification: GB/T 714-2025 (supersedes GB/T 714-2015) — Delivery: TMCP / TMCP+T / QT
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Q690q Quality Grades
GB/T 714-2025 vs 2015
Q690qE vs ASTM A709 / EN 10025
TMCP vs Normalized vs QT
Welding and Fatigue
Z15 / Z25 / Z35
Equivalent Material Grades
Testing and Inspection
Dimensions
Tolerances
Price and Ordering
Applications
Supply Capability
Why Choose SHH STEEL
FAQ
Conclusion

What is GB/T 714 Q690qE Bridge Steel Plate?

Q690qE is bridge structural steel plate to GB/T 714. Q stands for yield, 690 is the minimum yield in MPa for plate up to 50 mm, q stands for qiao (bridge) and E is the quality grade: Charpy V-notch at −40°C on longitudinal specimens.

Q690q is the top strength level of GB/T 714, with 690 MPa yield up to 50 mm and 650 MPa to 100 mm. Annex B lists ASTM A709 HPS 100W against Q690q. It is a specialist plate: thin, highly stressed members on record spans, where every tonne of girder weight saved reduces cable, pylon and foundation size.

Q690qE combines 690 MPa yield with 120 J at −40°C. A published study on 40 mm Q690qNH plate found QT plate more uniform through the thickness than TMCP + tempered plate, a point worth weighing when choosing the route for Q690qE too.

Since 1 May 2026, the valid edition is GB/T 714-2025, which fully replaced GB/T 714-2015. The changes matter for buyers: tensile strength now drops by thickness band, impact energy is set by thickness, and the yield ratio moved to an informative annex.

SHH STEEL (Shanghai Shenghonghe Import & Export Co., Ltd.) is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. We ship Q690qE cut to size with an EN 10204 3.1 or 3.2 certificate. Sister grades are listed under GB/T 714.

Material Specification

Specification element Requirement SHH STEEL compliance
Standard GB/T 714-2025 Q690qE Confirmed
Product Single-rolled plate ≤150 mm; hot-rolled strip and cut plate ≤25.4 mm Plate
Thickness with tensile values Up to 100 mm for Q690q Confirmed
Minimum yield ReL 690 MPa ≤50 mm; 650 MPa >50–100 mm Confirmed
Minimum tensile Rm 770 MPa ≤100 mm (no upper limit in the standard) Confirmed
Elongation A ≥ 14% Confirmed
Charpy V-notch −40°C, 120 J (12–100 mm), longitudinal Confirmed
Delivery condition TMCP, TMCP + tempering, or quenched and tempered (QT) As ordered
Weldability index Pcm (Table 7) for TMCP; CEV (Table 6) for QT Printed on MTC
Ultrasonic testing Plate >20 mm: GB/T 2970, Class II or better Every plate
Through-thickness Z15, Z25 or Z35 to GB/T 5313, when ordered As ordered
Dimensions GB/T 709 Confirmed
Certificate GB/T 247; EN 10204 3.1 or 3.2 As ordered

Grades often compared with Q690qE are ASTM A709 HPS 100W and ASTM A514 Grade Q; the comparison below shows where they differ.

Chemical Composition: Heat Analysis and Product Analysis

Two analyses matter for Q690qE. The heat (ladle) analysis is taken during casting and printed on the certificate. The product analysis is taken from finished plate and judged with the wider GB/T 222 tolerances. Mixing the two is the most common reason for disputed rejections.

Table 1 below is the heat (ladle) analysis for Q690qE from GB/T 714-2025 Tables 1, 2, 3 and 4.

Element Q690qE TMCP (%) Q690q quenched and tempered (%)
C, max 0.11 0.15
Si, max 0.50 0.55
Mn 0.80 – 1.70 0.80 – 1.70
P, max 0.020 0.020
S, max 0.010 0.010
Nb 0.005 – 0.090 0.005 – 0.090
V 0.010 – 0.080 0.010 – 0.080
Ti 0.006 – 0.030 0.006 – 0.030
Als 0.010 – 0.045 0.010 – 0.045
Cr, max 1.00 0.40 – 1.00
Ni, max 1.20 0.25 – 1.20
Cu, max 0.55 0.15 – 0.55
Mo, max 0.60 0.20 – 0.60
N, max 0.0080 0.0080
B, max 0.0005 residual (≤0.0014 if C ≤0.10%) 0.0005–0.0030 may be added
H, max 0.0002 0.0002

Nb, V, Ti and Al may be added singly or together. Added singly, each must meet the range above; added together, at least one must reach its minimum and Nb + V + Ti ≤ 0.22%.

Table 2 is the product analysis: the limits a check analysis on finished plate is judged against. GB/T 714-2025 clause 7.1.3 calls up GB/T 222 for the permitted deviations.

Element Heat limit (%) Deviation, GB/T 222-2025 Table 2 (alloy) Q690qE product analysis (%)
C ≤ 0.11 +0.01 ≤ 0.12
Si ≤ 0.50 +0.04 ≤ 0.54
Mn 0.80 – 1.70 ±0.04 0.76 – 1.74
P ≤ 0.020 +0.005 (see note) ≤ 0.025
S ≤ 0.010 +0.005 (see note) ≤ 0.015
Cr ≤ 1.00 +0.05 (0.90–2.10% band) ≤ 1.05
Ni ≤ 1.20 +0.05 (1.00–2.00% band) ≤ 1.25
Cu ≤ 0.55 +0.03 ≤ 0.58
Mo ≤ 0.60 +0.02 (0.30–0.60% band) ≤ 0.62
V 0.010 – 0.080 +0.01 (≤0.10% band) ≤ 0.090
Ti 0.006 – 0.030 +0.02 ≤ 0.050
Nb, B, N See heat table Not read in our copy of Table 2 Agree in contract

How to read Table 2. With Ni up to 1.20% and Mo up to 0.60%, Q690q heats are normally classed as alloy steel under GB/T 13304, so the alloy-steel table of GB/T 222 applies. One steel uses one table only; the certificate should say which.

Mechanical Properties

Tensile values follow Table 9 of GB/T 714-2025 for Q690q. Tensile specimens are transverse; round specimens are used above 40 mm. Where yield is not distinct, Rp0.2 replaces ReL.

Nominal thickness ReL min (MPa) Rm min (MPa) A min
≤ 50 mm 690 770 14%
> 50 – 100 mm 650 770 14%

Impact values follow Table 10, on longitudinal specimens, average of three:

Letter / test temperature KV2 ≤12 mm KV2 >12 – 100 mm KV2 >100 – 150 mm
E / −40°C 80 J 120 J Not applicable

One single value may fall below the required average, but not below 70% of it. Plate over 8 mm and under 12 mm is tested with 7.5 mm specimens (75% of the value); 6–8 mm plate with 5 mm specimens (50%). Plate under 6 mm is not impact tested.

180° bend test, transverse: mandrel D = 2a up to 16 mm and 3a above 16 mm; may be omitted when the mill guarantees it. Yield ratio is not mandatory and Annex C gives no recommended value at this level; agree a limit in the contract if the design needs one.

Q690qD / Q690qE / Q690qF: Which Quality Grade?

Q690qE is tested at −40°C. It suits bridges in north-east China, Inner Mongolia, Xinjiang, Russia, Kazakhstan, Canada and high-altitude sites, and for thick, restrained members anywhere. E is tested at −40°C, with P ≤0.020% and S ≤0.010%. Many long-span bridges specify E even in mild climates, because thick plate and heavy welding raise the risk of brittle fracture.

Grade Test temp. KV2 ≤12 mm KV2 12–100 mm KV2 >100 mm P / S max (%)
Q690qD −20°C 80 J 120 J — 0.025 / 0.015
Q690qE −40°C 80 J 120 J — 0.020 / 0.010
Q690qF −60°C By agreement 77 J — 0.015 / 0.006

Over-specifying the letter costs money; under-specifying it costs safety. Choose from the lowest service or erection temperature, then step up one letter for thick, restrained or fracture-critical members.

Q690qE: What Changed from GB/T 714-2015 to GB/T 714-2025

For Q690qE buyers the 2025 edition changes more than the year on the certificate. The points below come from the foreword of GB/T 714-2025 and its tables.

  • A TMCP route was added for Q690q (C ≤0.11%, Pcm ≤0.24% to 50 mm). In 2015 it was QT only.
  • CEV and Pcm limits were revised (Tables 6 and 7).
  • Tensile strength is now banded by thickness (e.g. lower minimum Rm above 100 mm) instead of one value.
  • Impact energy is set by thickness band (≤12 mm, 12–100 mm, >100 mm) in Table 10.
  • Yield ratio is no longer a clause value; it is agreed in the contract, with recommendations in informative Annex C.
  • Section products were removed; the standard now covers plate and strip only.
  • Delivery is TMCP, TMCP + tempering or QT; normalizing is kept only for Q345q/Q370q plate over 100 mm by agreement.

If a drawing cites 2015 and the plate is made to 2025, get the designer’s written acceptance; tensile strength above 100 mm and the yield-ratio basis differ.

Q690qE vs ASTM A709 and EN 10025: Which Grade Matches?

Can Q690qE replace a US or European bridge grade, or the other way round? Strength can match; toughness rules differ in kind, not only in number.

Property Q690qE ASTM A709 HPS 100W ASTM A514 Grade Q EN 10025-6 S690Q
Min. yield (MPa) 690 (≤50 mm) 690 (≤65 mm) 690 (≤65 mm) 690 (≤50 mm)
Tensile (MPa) 770 min 760 – 895 760 – 895 770 – 940
Charpy 120 J at −40°C (12–100 mm) CVN by temperature zone; fracture-critical (F) levels Supplementary only Q / QL / QL1: −20 / −40 / −60°C
Weathering chemistry No Yes No No

ASTM A709 sets Charpy requirements by temperature zone (1, 2, 3) and by member type: non-fracture-critical (T) or fracture-critical (F). GB/T 714 sets one value per letter, so compare the A709 zone with the GB/T 714 test temperature, not grade with grade.

EN 10025-3/-4/-6 grades show yield at the thinnest band; their values fall with thickness. GB/T 714 keeps 690 MPa to 50 mm. EN tensile ranges have upper limits; GB/T 714 gives minimums only.

The 120 J requirement in GB/T 714 for 12–100 mm plate is several times the 27–40 J typical of general structural grades. That margin is the main reason bridge owners specify Q690qE rather than GB/T 1591 plate.

Q690qE Delivery Condition: TMCP vs Normalized vs Quenched and Tempered

GB/T 714-2025 clause 3.2 defines TMCP as rolling with the final deformation in a controlled temperature range, including accelerated cooling with or without tempering (self-tempering included) but excluding direct quenching and quench-and-temper. The delivery route must be stated on the certificate.

Route Available for Q690qE Weldability index Notes
TMCP Yes Pcm ≤0.24% (≤50 mm) C ≤0.11%; up to 100 mm
TMCP + tempering Yes Pcm Improves toughness uniformity
Quenched and tempered Yes CEV ≤0.60% (≤50 mm) C ≤0.15%; B 0.0005–0.0030% may be added
Normalized No — Not listed

Q690q can be TMCP or QT. A published study on 40 mm Q690qNH plate found QT plate more uniform in strength and toughness through the thickness than TMCP + tempered plate; we discuss route choice with the owner on every Q690q enquiry. For E-letter plate over about 50 mm, many mills add tempering after TMCP to reduce toughness scatter through the thickness.

Ask for the route on the purchase order. It changes the weldability index, the welding procedure and, for heavy plate, the price of Q690qE.

Welding Q690qE and Fatigue in Bridge Girders

GB/T 714-2025 clause 7.1.2 uses CEV for normalized, QT and TMCP steel with C >0.12%, and Pcm for weathering steel and TMCP steel with C ≤0.12%, both from the heat analysis:

CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15

Pcm = C + Si/30 + Mn/20 + Cu/20 + Ni/60 + Cr/20 + Mo/15 + V/10 + 5B

Index ≤50 mm >50–100 mm >100–130 mm
Pcm, TMCP (Table 7) ≤ 0.24 ≤ 0.25 —
CEV, QT (Table 6) ≤ 0.60 ≤ 0.65 —

For Q690qE, ask the fabricator which index the WPS was qualified on. Where the WPS uses CEV and the standard uses Pcm, we print both on the certificate. At −40°C, HAZ toughness often becomes the limit. Fabricators usually cap heat input and qualify the procedure at −40°C on plate from the same route.

Typical consumables for Q690qE: E76-class consumables (AWS E11018M type).

Fatigue. Welded details govern fatigue life in a bridge, and their fatigue strength is set by detail category, not by yield strength. Higher-strength plate can carry higher stress ranges only if detailing improves too.

Fatigue design follows JTG D64 (highway) and TB 10091 (railway) in China, EN 1993-1-9 in Europe and AASHTO LRFD in the US; fabrication commonly follows TB 10212, JTG/T 3650 or AWS D1.5.

Q690qEZ15, Z25 and Z35: Through-Thickness Plate for Bridges

Bridge node plates, anchor boxes and pylon walls take weld shrinkage through their thickness. If the plate holds sulfide stringers, it can tear in steps under the weld. Z grades prove through-thickness ductility.

GB/T 714 adds the Z level to the end of the designation, for example Q690qEZ25. The test and acceptance follow GB/T 5313 and apply to plate 15 mm and thicker.

Z grade Heat sulfur, max (%) Reduction of area, avg / single (%)
Z15 0.010 15 / 10
Z25 0.007 25 / 15
Z35 0.005 35 / 25

E chemistry already limits S to 0.010%, the Z15 sulfur cap. Z25 (S ≤0.007%) and Z35 (S ≤0.005%) still need a cleaner heat.

Z plate for Q690qE should also get ultrasonic testing beyond the Class II minimum if the joint is critical. Write the UT class next to the Z level. Z options apply across the GB/T 714 bridge steel range.

Equivalent Material Grades

Annex B of GB/T 714-2025 lists foreign grades against each strength level. It is informative: it tells you which families are close, not that the plates are interchangeable.

Standard Grade(s) Fit for Q690qE
ASTM A709 ASTM A709 HPS 100W Listed in Annex B
EN 10025-6 EN 10025-6 S690Q, EN 10025-6 S690QL, EN 10025-6 S690QL1 Listed in Annex B
ASTM A514 ASTM A514 Grade Q QT, strength only
GB/T 16270 GB/T 16270 Q690E QT alternative, different toughness rules
GB/T 1591 GB/T 1591 Q690ME TMCP general structural

Before substituting, compare three things line by line: minimum yield at the actual thickness, the impact test temperature and energy, and the weldability index. For Q690qE, the 120 J impact level and the Pcm/CEV caps are usually the hardest to match.

Q690qE Testing, UT and Certificate

A batch of Q690qE is one grade, one heat, one thickness, one rolling schedule and one heat-treatment condition, up to 60 t. Table 12 of GB/T 714-2025 sets the tests:

Test Frequency Method
Heat analysis 1 per heat GB/T 20066; GB/T 4336 / GB/T 223
Tensile 1 per batch GB/T 2975 / GB/T 228.1
Bend 180° 1 per batch (may be waived if guaranteed) GB/T 232
Charpy V at −40°C 3 specimens per batch GB/T 229
Through-thickness (Z) 3 specimens per batch, when ordered GB/T 5313
Ultrasonic Every plate >20 mm, Class II or better GB/T 2970
Surface and dimensions Every plate Visual and gauges

Impact retest: if a set fails, three more specimens are taken from the same batch. The average of all six must meet the requirement; two values may be below it, but only one below 70%. At −40°C, retest risk rises on heavy plate; we build a margin for retests into the delivery schedule.

Dimensions

Common Q690qE sizes:

  • Thickness: 6 mm – 100 mm under GB/T 714 tensile tables; most orders 10 – 60 mm
  • Width: 1500 – 4000 mm, depending on mill and thickness
  • Length: 6000 – 18000 mm; longer by enquiry
  • Edge: mill edge or cut edge
  • Weight: theoretical, 7.85 g/cm³

Deck plate, webs, flanges, diaphragms and stiffeners are cut to drawing. For U-ribs and rolled sections on the same bridge, see steel beam profiles and steel structural profiles.

Tolerances

Thickness, width, length, flatness and camber of Q690qE follow GB/T 709. The table shows Class B thickness limits for common sizes.

Nominal thickness (mm) Width ≤ 1500 mm Width > 1500 – 2500 mm
> 8 – 15 −0.30 / +0.80 −0.30 / +1.00
> 15 – 25 −0.30 / +1.00 −0.30 / +1.20
> 25 – 40 −0.30 / +1.10 −0.30 / +1.30
> 40 – 60 −0.30 / +1.30 −0.30 / +1.50
> 60 – 100 −0.30 / +1.50 −0.30 / +1.80
> 100 – 150 −0.30 / +2.10 −0.30 / +2.50

Bridge fabricators often ask for Class C (zero minus) on deck and flange plate so section properties are never under the design value. Wider plates follow the heavier GB/T 709 rows; we state them on the offer.

Q690qE Price Factors and How to Order

Two Q690qE quotes can differ a lot and both be fair. Base prices are similar; extras are where mills part.

Cost driver Effect on price
Strength level Q690q Higher levels need more alloy and tighter rolling control
Quality letter Higher extra: −40°C testing, S ≤0.010%, more retest risk
Delivery route TMCP / TMCP+T / QT; QT costs more than TMCP
Thickness Over 60 mm and under 10 mm carry size extras
Z15 / Z25 / Z35 Low-sulfur heat, Z test, UT; Z35 costs most
Width and length Over 3000 mm wide or 15 m long needs mill confirmation
Quantity per size Mill minimums per heat and size
Inspection and processing 3.2 witness, profile cutting, blasting, priming quoted per item

To get a firm quote in one round, send:

  • Grade, edition and Z level, e.g. Q690qEZ25 to GB/T 714-2025
  • Thickness × width × length and pieces or tonnes
  • Delivery route and UT class if beyond Class II
  • Certificate type and inspector
  • Destination port and Incoterm

We quote plate price, extras and freight line by line. Need another letter? See Q690qD, Q690qF.

Applications

Sector Typical Q690qE components
Record-span bridges Main truss chords and node plates
Cable anchorages Anchor boxes and anchor plates
Steel pylons Highly stressed pylon walls
Movable and military bridges Lightweight girders
Retrofit High-strength replacement members

The letter E suits bridges in north-east China, Inner Mongolia, Xinjiang, Russia, Kazakhstan, Canada and high-altitude sites, and for thick, restrained members anywhere.

It is the wrong plate for pressure equipment (pressure vessel steel plates), unpainted exposure (weathering steel plates) or ship hulls (shipbuilding steel plates).

Supply Capability and Global Delivery

SHH STEEL sources Q690qE from first-line bridge-plate mills, including drafters of GB/T 714-2025 such as Ansteel, Valin Xiangtan, Jiangyin Xingcheng, Wuyang, Shougang and Xinyu.

  • Certificates: EN 10204 3.1 standard; 3.2 with third-party witness (SGS, BV, TÜV or owner’s inspector)
  • Tests: tensile, −40°C Charpy, bend, Z test, UT, product analysis
  • Processing: CNC plasma and flame cutting, bevelling, drilling, shot blasting and priming
  • Terms: FOB Shanghai, CFR, CIF; TT, LC or TT + LC
  • Marking: steel-stamped and paint-marked with grade, heat, size and mill, per GB/T 247

We ship Q690qE to fabricators in Asia, Africa, the Middle East, Europe and the Americas, by break-bulk or container.

Lead time: about 45–60 days from mill rolling; Z35, F letter or 3.2 inspection adds about 1–2 weeks. Sea time from Shanghai is about 7–12 days to Southeast Asia and 28–35 days to North Europe.

Why Choose SHH STEEL

SHH STEEL is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. For Q690qE that means bridge plate from bridge-plate mills, not relabelled structural plate.

Before shipment we check four lines on every Q690qE certificate: yield and tensile for the actual thickness band, Charpy at −40°C, the CEV or Pcm for the delivery route, and UT results. If one fails, the plate does not ship as Q690qE.

For Q690qE, discuss impact test position and route (TMCP or QT) with the owner. They change both price and toughness margin.

We also tell buyers when another grade fits better. Neighbouring levels are Q620qE. Browse more structural steel plates and high strength low alloy plates.

FAQ

What is Q690qE steel?
Q690qE is bridge structural steel plate to GB/T 714-2025. It has 690 MPa minimum yield up to 50 mm, 770 MPa minimum tensile, 14% elongation and Charpy V-notch impact of 120 J at −40°C for 12–100 mm plate. It is delivered TMCP, TMCP + tempering, or quenched and tempered.
What is the difference between Q690qE and Q690qD?
Strength and chemistry box are the same. Q690qE is Charpy tested at −40°C, Q690qD at −20°C, both needing 120 J for 12–100 mm plate. P/S caps are 0.020/0.010% for E and 0.025/0.015% for D. Choose by the lowest service or erection temperature.
Can Q690qE be supplied TMCP?
Yes, since GB/T 714-2025. The 2015 edition listed Q690q as quenched and tempered only. The 2025 edition adds a TMCP route with C ≤0.11% and Pcm ≤0.24% up to 50 mm; QT plate is still available with CEV ≤0.60% up to 50 mm.
What is the ASTM or EN equivalent of Q690qE?
Close grades for Q690qE: ASTM A709 HPS 100W / EN 10025-6 S690Q, S690QL, S690QL1 (Annex B). These are close families, not drop-in substitutes; compare yield at thickness, impact temperature and energy, and the weldability index before substituting.
What does the q mean in GB/T 714 bridge steel grades?
The lowercase q stands for qiao, Chinese for bridge. In a grade such as Q420qD, Q means yield, 420 is the minimum yield in MPa, q marks bridge steel to GB/T 714 and D is the quality letter (−20°C Charpy). NH after the letter, as in Q420qDNH, marks weathering steel.
What is the carbon equivalent of Q690qE?
It depends on the route. For Q690qE up to 50 mm, GB/T 714-2025 sets Pcm ≤0.24% (TMCP) or CEV ≤0.60% (QT). CEV applies to normalized, QT and TMCP steel with C >0.12%; Pcm to TMCP steel with C ≤0.12%.

Conclusion

Q690qE to GB/T 714-2025 is bridge plate with 690 MPa minimum yield, 770 MPa minimum tensile and 120 J Charpy at −40°C for 12–100 mm plate.

The next strength level is Q620qE, with Q690qD and Q690qF as sister letters. If the drawing still cites GB/T 714-2015, we can certify Q690qE to it, but we recommend confirming with the designer that the 2025 values are accepted.

Our Q690qE certificates carry heat chemistry, weldability index, tensile and Charpy data to EN 10204 3.1 or 3.2. SHH STEEL can add product analysis, Z15–Z35 and witness inspection.

We ship from Shanghai to bridge builders worldwide. Browse the full GB/T 714 range or other high strength low alloy plates.

Send your enquiry with grade, edition, sizes and inspection needs, and we will answer within one working day. Contact SHH STEEL for Q690qE bridge steel plate.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X