GB/T 714 Q420qNHE weathering bridge steel stacked at SHH STEEL warehouse

GB/T 714 Q420qNHE Weathering Bridge Steel Supplier

GB/T 714 Q420qNHE (Q420qENH) is weathering bridge steel plate with 420 MPa minimum yield, 120 J Charpy at −40°C (12–100 mm), Cu-Cr-Ni chemistry and a weathering index I ≥6.0 for unpainted bridges. SHH STEEL supplies it mill-direct with Z15–Z35, UT and full heat and product analysis.
Keywords
Q420qNHE, Q420qNHE weathering steel, GB/T 714 Q420qNHE, Q420qENH, Q420qENH steel plate, Q420qNH, Q420qNHE weathering bridge steel, Q420qENHZ15, Q420qENHZ25, Q420qENHZ35, bridge steel plate, Q420qNHE supplier
Equivalent Grades:
No direct equivalent in Annex B / closest: ASTM A709 HPS 70W (higher) / EN 10025-4 S420ML (not weathering) — Material Specification: GB/T 714-2025 (supersedes GB/T 714-2015) — Delivery: TMCP / TMCP+T
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Q420qNH Quality Grades
GB/T 714-2025 vs 2015
Q420qNHE vs ASTM A709 / EN 10025
Weathering Index and Unpainted Use
Welding and Fatigue
Z15 / Z25 / Z35
Equivalent Material Grades
Testing and Inspection
Dimensions
Tolerances
Price and Ordering
Applications
Supply Capability
Why Choose SHH STEEL
FAQ
Conclusion

What is GB/T 714 Q420qNHE Weathering Bridge Steel?

Q420qNHE is weathering bridge structural steel to GB/T 714. In the standard’s own notation it is written Q420qENH: Q for yield, 420 for the minimum yield in MPa, q for qiao (bridge), the quality letter, and NH for nai hou, weathering. The letter E means Charpy V-notch testing at −40°C.

Q420qNH is high-strength weathering plate for unpainted long-span girders and trusses. Q420qNH keeps the Q345qNH weathering chemistry and adds strength through TMCP and microalloying. Pcm is capped at 0.23% to 50 mm, and the grade is tested in D, E or F.

Q420qNHE (Q420qENH) combines 420 MPa yield, 120 J at −40°C and a weathering index of at least 6.0. The Zangmu Yarlung Tsangpo River Bridge in Tibet used Q420qENH for its unpainted 430 m-span arch ribs.

GB/T 714-2025, in force since 1 May 2026, fully replaces GB/T 714-2015; the changes for weathering grades are listed below.

SHH STEEL (Shanghai Shenghonghe Import & Export Co., Ltd.) is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. We ship Q420qNHE cut to size with an EN 10204 3.1 or 3.2 certificate. Sister grades are listed under GB/T 714; other unpainted options are under weathering steel plates and EN 10025-5.

Material Specification

Specification element Requirement SHH STEEL compliance
Standard GB/T 714-2025 Q420qENH Confirmed
Product Single-rolled plate ≤150 mm; hot-rolled strip and cut plate ≤25.4 mm Plate
Thickness with tensile values Up to 130 mm for Q420qNH Confirmed
Minimum yield ReL 420 MPa ≤50 mm; 410 MPa >50–100 mm Confirmed
Minimum tensile Rm 540 MPa ≤100 mm (no upper limit in the standard) Confirmed
Elongation A ≥ 19% Confirmed
Charpy V-notch −40°C, 120 J (12–100 mm), longitudinal Confirmed
Weathering index I ≥ 6.0 (Table 5, footnote c) Calculated on MTC
Delivery condition TMCP or TMCP + tempering As ordered
Weldability index Pcm (Table 8) Printed on MTC
Ultrasonic testing Plate >20 mm: GB/T 2970, Class II or better Every plate
Through-thickness Z15, Z25 or Z35 to GB/T 5313, when ordered As ordered
Dimensions GB/T 709 Confirmed
Certificate GB/T 247; EN 10204 3.1 or 3.2 As ordered

Grades often compared with Q420qNHE are ASTM A709 HPS 50W, ASTM A709 HPS 70W and EN 10025-4 S420ML; the comparison below shows where they differ.

Chemical Composition: Heat Analysis and Product Analysis

Read the Q420qNHE certificate with two tables in mind: heat limits from GB/T 714 and product limits from GB/T 222. A plate can pass one and be argued over in the other if the basis is not written into the contract.

Table 1 below is the heat (ladle) analysis for Q420qNHE from GB/T 714-2025 Tables 1, 5.

Element Q420qNHE heat analysis (%) Note
C, max 0.11
Si 0.15 – 0.50 Counts in I
Mn 1.10 – 1.50 Min 0.50% for coil only
P, max 0.020 Letter E
S, max 0.010 Letter E
Cu 0.25 – 0.50 Main weathering element
Cr 0.40 – 0.70 Weathering element
Ni 0.30 – 0.40 Weathering element
Mo, max 0.20
Nb 0.010 – 0.100 Microalloy (see note)
V 0.010 – 0.100 Microalloy (see note)
Ti 0.006 – 0.030 Microalloy (see note)
Als 0.015 – 0.050 Alt 0.020–0.055% if total Al is used
N, max 0.0080
B, max (residual) 0.0005 ≤0.0014% if C ≤0.06%
H, max (residual) 0.0002
Weathering index I ≥ 6.0 Calculated from heat analysis

Nb, V, Ti and Al may be added singly or together. Added singly, each must meet the range above; added together, at least one must reach its minimum and Nb + V + Ti ≤ 0.22%. Calcium treatment is required to control sulfide shape.

Table 2 is the product analysis: the limits a check analysis on finished plate is judged against. GB/T 714-2025 clause 7.1.3 calls up GB/T 222 for the permitted deviations.

Element Heat limit (%) Deviation, GB/T 222-2025 Table 1 Q420qNHE product analysis (%)
C ≤ 0.11 +0.02 ≤ 0.13
Si 0.15 – 0.50 ±0.05 0.10 – 0.55
Mn 1.10 – 1.50 ±0.06 1.04 – 1.56
P ≤ 0.020 +0.005 ≤ 0.025
S ≤ 0.010 +0.005 ≤ 0.015
V 0.010 – 0.100 +0.02 / −0.01 ≤ 0.120
Ti 0.006 – 0.030 +0.02 / −0.01 ≤ 0.050
Nb 0.010 – 0.100 ±0.005 (listed for 0.015–0.060%) Above 0.060%: agree in contract
Cu 0.25 – 0.50 ±0.05 0.20 – 0.55
Cr 0.40 – 0.70 ±0.05 0.35 – 0.75
Ni 0.30 – 0.40 ±0.05 0.25 – 0.45
Als 0.015 – 0.050 ±0.003 Lower limit −0.003 (Table 1 row is for Al ≥0.015%; confirm)
Mo ≤ 0.20 Not listed in Table 1 Agree in contract
N ≤ 0.0080 Listed only for 0.010–0.020% Agree in contract

How to read Table 2. Weathering bridge steel is normally classed as low-alloy steel, so Table 1 of GB/T 222 applies. Where the heat limit is a range, the deviation applies to both ends; for one heat, an element may deviate in one direction only.

Mechanical Properties

Tensile values follow Table 9 of GB/T 714-2025 for Q420qNH. Tensile specimens are transverse; round specimens are used above 40 mm. Where yield is not distinct, Rp0.2 replaces ReL.

Nominal thickness ReL min (MPa) Rm min (MPa) A min
≤ 50 mm 420 540 19%
> 50 – 100 mm 410 540 19%
> 100 – 130 mm 365 460 19%

Impact values follow Table 10, on longitudinal specimens, average of three:

Letter / test temperature KV2 ≤12 mm KV2 >12 – 100 mm KV2 >100 – 150 mm
E / −40°C 80 J 120 J 31 J

One single value may fall below the required average, but not below 70% of it. Plate over 8 mm and under 12 mm is tested with 7.5 mm specimens (75% of the value); 6–8 mm plate with 5 mm specimens (50%). Plate under 6 mm is not impact tested.

180° bend test, transverse: mandrel D = 2a up to 16 mm and 3a above 16 mm; may be omitted when the mill guarantees it. Yield ratio is not mandatory. If the contract asks for it, Annex C recommends ReL/Rm ≤ 0.88 up to 12 mm and ≤ 0.86 above 12 mm for TMCP plate.

Q420qNHD / Q420qNHE / Q420qNHF: Which Quality Grade?

Q420qNHE is tested at −40°C. It suits bridges in north-east China, Inner Mongolia, Xinjiang, Russia, Kazakhstan, Canada and high-altitude sites, and for thick, restrained members anywhere. E is tested at −40°C, with P ≤0.020% and S ≤0.010%. Many long-span bridges specify E even in mild climates, because thick plate and heavy welding raise the risk of brittle fracture.

Grade Test temp. KV2 ≤12 mm KV2 12–100 mm KV2 >100 mm P / S max (%)
Q420qNHD −20°C 80 J 120 J 47 J 0.025 / 0.015
Q420qNHE −40°C 80 J 120 J 31 J 0.020 / 0.010
Q420qNHF −60°C By agreement 47 J — 0.015 / 0.006

Over-specifying the letter costs money; under-specifying it costs safety. Choose from the lowest service or erection temperature, then step up one letter for thick, restrained or fracture-critical members.

Q420qNHE: What Changed from GB/T 714-2015 to GB/T 714-2025

For Q420qNHE buyers the 2025 edition changes more than the year on the certificate. The points below come from the foreword of GB/T 714-2025 and its tables.

  • The weathering requirement changed: Table 5 now requires a corrosion index I ≥ 6.0, and the 2015 Annex C guide for assessing weathering resistance was deleted.
  • A Pcm table for weathering steel (Table 8) was added.
  • Annex A now gives reference bridge-site environments for unpainted use (chloride, SO₂ and time-of-wetness limits).
  • Yield values above 100 mm were added for Q420qNH (365 MPa for >100–130 mm).
  • Tensile strength is now banded by thickness (e.g. lower minimum Rm above 100 mm) instead of one value.
  • Impact energy is set by thickness band (≤12 mm, 12–100 mm, >100 mm) in Table 10.
  • Yield ratio is no longer a clause value; it is agreed in the contract, with recommendations in informative Annex C.

If a drawing cites 2015 and the plate is made to 2025, get the designer’s written acceptance; tensile strength above 100 mm and the yield-ratio basis differ.

Q420qNHE vs ASTM A709 and EN 10025: Which Grade Matches?

Can Q420qNHE replace a US or European bridge grade, or the other way round? Strength can match; toughness rules differ in kind, not only in number.

Property Q420qNHE ASTM A709 HPS 50W ASTM A709 HPS 70W EN 10025-4 S420ML
Min. yield (MPa) 420 (≤50 mm) 345 485 420 (≤16 mm)
Tensile (MPa) 540 min 485 min 585 – 760 520 – 680
Charpy 120 J at −40°C (12–100 mm) CVN by temperature zone; fracture-critical (F) levels CVN by temperature zone; fracture-critical (F) levels 27 J at −50°C
Weathering chemistry Yes, I ≥ 6.0 Yes Yes No

ASTM A709 sets Charpy requirements by temperature zone (1, 2, 3) and by member type: non-fracture-critical (T) or fracture-critical (F). GB/T 714 sets one value per letter, so compare the A709 zone with the GB/T 714 test temperature, not grade with grade.

EN 10025-5 weathering grades are general structural steels without a bridge-specific toughness level of 120 J; they suit many bridges but are not a one-to-one match.

The 120 J requirement for 12–100 mm plate is several times the 27–40 J typical of general weathering grades such as ASTM A588 or Corten A/B plate, which is why bridge owners specify Q420qNHE.

Q420qNHE Atmospheric Corrosion Index I and Unpainted Bridges

GB/T 714-2025 Table 5, footnote c, requires every Q420qNHE heat to reach an atmospheric corrosion index I of at least 6.0, calculated from the heat analysis:

I = 26.01(%Cu) + 3.88(%Ni) + 1.20(%Cr) + 1.49(%Si) + 17.28(%P) − 7.29(%Cu)(%Ni) − 9.10(%Ni)(%P) − 33.39(%Cu)²

This is the same predictive formula used with ASTM G101 for ASTM A709 Grade 50W and ASTM A709 HPS 70W, which makes Chinese and US ASTM A709 weathering steel plates easy to compare with Q420qNHE.

Worked example (our calculation) Cu Ni Cr Si P I
All weathering elements at their Table 5 minimum 0.25 0.30 0.40 0.15 0.010 5.88
Illustrative mid-range heat 0.32 0.36 0.55 0.30 0.012 6.74

Note the first row: a heat that only just meets every Table 5 minimum can still fall short of I = 6.0. That is why we ask the mill to print I on every Q420qNHE certificate, not just the chemistry.

Where can the steel be left unpainted? Annex A of GB/T 714-2025 gives reference bridge-site conditions:

  • Rural or urban atmosphere with annual chloride deposition ≤ 3 mg/(m²·d)
  • Annual SO₂ deposition ≤ 24 mg/(m²·d)
  • Time of wetness ≤ 5,256 h per year (temperature above 0°C and relative humidity above 80%)
  • Coastal sites only if they meet the same limits; for marine atmospheres Annex D points to T/CISA 073

Owners choose Q420qNHE to avoid repainting for decades. That only works if the site matches Annex A and the details shed water. Where the site is borderline, paint the girder ends and leave the rest bare.

Welding Q420qNHE and Fatigue in Bridge Girders

GB/T 714-2025 clause 7.1.2 uses CEV for normalized, QT and TMCP steel with C >0.12%, and Pcm for weathering steel and TMCP steel with C ≤0.12%, both from the heat analysis:

CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15

Pcm = C + Si/30 + Mn/20 + Cu/20 + Ni/60 + Cr/20 + Mo/15 + V/10 + 5B

Index ≤50 mm >50–100 mm >100–130 mm
Pcm, Q420qNH (Table 8) ≤ 0.23 ≤ 0.25 By agreement

The index caps in GB/T 714 are maximums. Real Q420qNHE heats often sit well below them, and preheat should be set from the actual value, not the cap. At −40°C, HAZ toughness often becomes the limit. Fabricators usually cap heat input and qualify the procedure at −40°C on plate from the same route.

Typical consumables for Q420qNHE: weathering-matched Ni-Cu consumables (AWS E8018-W2 type for 345–420 MPa), with higher-strength weathering wires for 460–500 MPa.

Fatigue. Welded details govern fatigue life in a bridge, and their fatigue strength is set by detail category, not by yield strength. Higher-strength plate can carry higher stress ranges only if detailing improves too.

Fatigue design follows JTG D64 (highway) and TB 10091 (railway) in China, EN 1993-1-9 in Europe and AASHTO LRFD in the US; fabrication commonly follows TB 10212, JTG/T 3650 or AWS D1.5.

Q420qENHZ15, Z25 and Z35: Through-Thickness Plate for Bridges

Bridge node plates, anchor boxes and pylon walls take weld shrinkage through their thickness. If the plate holds sulfide stringers, it can tear in steps under the weld. Z grades prove through-thickness ductility.

GB/T 714 adds the Z level to the end of the designation, for example Q420qENHZ25. The test and acceptance follow GB/T 5313 and apply to plate 15 mm and thicker.

Z grade Heat sulfur, max (%) Reduction of area, avg / single (%)
Z15 0.010 15 / 10
Z25 0.007 25 / 15
Z35 0.005 35 / 25

E chemistry already limits S to 0.010%, the Z15 sulfur cap. Z25 (S ≤0.007%) and Z35 (S ≤0.005%) still need a cleaner heat.

Ask your designer which Q420qNHE plates are loaded through the thickness. Ordering Z35 on everything costs money and time without adding safety. Z options apply across the GB/T 714 bridge steel range.

Equivalent Material Grades

Annex B of GB/T 714-2025 lists foreign grades against each strength level. It is informative: it tells you which families are close, not that the plates are interchangeable.

Standard Grade(s) Fit for Q420qNHE
ASTM A709 ASTM A709 HPS 70W Higher strength; weathering
EN 10025-4 EN 10025-4 S420ML Strength match, not weathering
ASTM A588 ASTM A588 Grade K Weathering, lower strength
GB/T 714 (painted twin) Q420qE Same strength, no weathering elements

For weathering grades also compare the corrosion index basis. Q420qNHE requires I ≥ 6.0 by the formula above; check that the substitute is assessed on the same basis.

Q420qNHE Testing, UT and Certificate

A batch of Q420qNHE is one grade, one heat, one thickness, one rolling schedule and one heat-treatment condition, up to 60 t. Table 12 of GB/T 714-2025 sets the tests:

Test Frequency Method
Heat analysis 1 per heat GB/T 20066; GB/T 4336 / GB/T 223
Weathering index I Calculated per heat Table 5 formula
Tensile 1 per batch GB/T 2975 / GB/T 228.1
Bend 180° 1 per batch (may be waived if guaranteed) GB/T 232
Charpy V at −40°C 3 specimens per batch GB/T 229
Through-thickness (Z) 3 specimens per batch, when ordered GB/T 5313
Ultrasonic Every plate >20 mm, Class II or better GB/T 2970
Surface and dimensions Every plate Visual and gauges

Impact retest: if a set fails, three more specimens are taken from the same batch. The average of all six must meet the requirement; two values may be below it, but only one below 70%. At −40°C, retest risk rises on heavy plate; we build a margin for retests into the delivery schedule.

Dimensions

Q420qNHE sizes we supply from mill and stock:

  • Thickness: 6 mm – 130 mm under GB/T 714 tensile tables; most orders 10 – 80 mm
  • Width: 1500 – 4000 mm, depending on mill and thickness
  • Length: 6000 – 18000 mm; longer by enquiry
  • Edge: mill edge or cut edge
  • Weight: theoretical, 7.85 g/cm³

Deck plate, webs, flanges, diaphragms and stiffeners are cut to drawing. For U-ribs and rolled sections on the same bridge, see steel beam profiles and steel structural profiles.

Tolerances

GB/T 709 governs Q420qNHE thickness, width, length and flatness. Under Class B, plate may be up to 0.30 mm thin; the plus side grows with thickness and width.

Nominal thickness (mm) Width ≤ 1500 mm Width > 1500 – 2500 mm
> 8 – 15 −0.30 / +0.80 −0.30 / +1.00
> 15 – 25 −0.30 / +1.00 −0.30 / +1.20
> 25 – 40 −0.30 / +1.10 −0.30 / +1.30
> 40 – 60 −0.30 / +1.30 −0.30 / +1.50
> 60 – 100 −0.30 / +1.50 −0.30 / +1.80
> 100 – 150 −0.30 / +2.10 −0.30 / +2.50

Bridge fabricators often ask for Class C (zero minus) on deck and flange plate so section properties are never under the design value. Wider plates follow the heavier GB/T 709 rows; we state them on the offer.

Q420qNHE Price Factors and How to Order

Price questions on Q420qNHE usually come down to the extras in the table below.

Cost driver Effect on price
Strength level Q420q Higher levels need more alloy and tighter rolling control
Quality letter Higher extra: −40°C testing, S ≤0.010%, more retest risk
Weathering alloys Cu, Cr, Ni additions and I-index control add a weathering extra
Delivery route TMCP / TMCP+T
Thickness Over 60 mm and under 10 mm carry size extras
Z15 / Z25 / Z35 Low-sulfur heat, Z test, UT; Z35 costs most
Width and length Over 3000 mm wide or 15 m long needs mill confirmation
Quantity per size Mill minimums per heat and size
Inspection and processing 3.2 witness, profile cutting, blasting, priming quoted per item

To get a firm quote in one round, send:

  • Grade, edition and Z level, e.g. Q420qENHZ25 to GB/T 714-2025
  • Thickness × width × length and pieces or tonnes
  • Delivery route and UT class if beyond Class II
  • Certificate type and inspector
  • Destination port and Incoterm

We quote plate price, extras and freight line by line. Need another letter? See Q420qNHD, Q420qNHF.

Applications

Sector Typical Q420qNHE components
Unpainted highway bridges Plate girders and box girders in rural and urban atmospheres
Railway bridges Truss members, plate girders, bracing
Remote and mountain sites Bridges where repainting access is difficult or costly
Urban viaducts Exposed girders with architectural rust finish
Pedestrian bridges Unpainted box sections

The letter E suits bridges in north-east China, Inner Mongolia, Xinjiang, Russia, Kazakhstan, Canada and high-altitude sites, and for thick, restrained members anywhere.

Q420qNHE is the wrong plate for marine splash zones, tunnels, sites with heavy de-icing salt spray, or members that stay wet. There, use painted Q420qE or look at marine-atmosphere grades under T/CISA 073.

Supply Capability and Global Delivery

SHH STEEL sources Q420qNHE from first-line bridge-plate mills, including drafters of GB/T 714-2025 such as Ansteel, Valin Xiangtan, Jiangyin Xingcheng, Wuyang, Shougang and Xinyu.

  • Certificates: EN 10204 3.1 standard; 3.2 with third-party witness (SGS, BV, TÜV or owner’s inspector)
  • Tests: tensile, −40°C Charpy, bend, Z test, UT, product analysis, weathering index
  • Processing: CNC plasma and flame cutting, bevelling, drilling, shot blasting and priming (or blasting only, for unpainted weathering steel)
  • Terms: FOB Shanghai, CFR, CIF; TT, LC or TT + LC
  • Marking: steel-stamped and paint-marked with grade, heat, size and mill, per GB/T 247

Our Q420qNHE exports follow Chinese bridge design abroad: railway and highway bridges built by EPC contractors in Asia, Africa and Latin America.

Lead time: about 45–60 days from mill rolling; Z35, F letter or 3.2 inspection adds about 1–2 weeks. Sea time from Shanghai is about 7–12 days to Southeast Asia and 28–35 days to North Europe.

Why Choose SHH STEEL

SHH STEEL is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. For Q420qNHE that means bridge plate from bridge-plate mills, not relabelled structural plate.

Before shipment we check four lines on every Q420qNHE certificate: yield and tensile for the actual thickness band, Charpy at −40°C, the Pcm and weathering index, and UT results. If one fails, the plate does not ship as Q420qNHE.

Plan the patina: shot blast the whole girder to a uniform surface before erection, or the rust layer will form unevenly and stain piers.

We also tell buyers when another grade fits better. Neighbouring levels are Q390qNH and Q460qNHE. The painted counterpart is Q420qE. Browse more structural steel plates and high strength low alloy plates.

FAQ

What is Q420qNHE steel?
Q420qNHE (Q420qENH) is weathering bridge steel plate to GB/T 714-2025. It has 420 MPa minimum yield up to 50 mm, 540 MPa minimum tensile, Charpy impact of 120 J at −40°C for 12–100 mm plate, and Cu-Cr-Ni chemistry with a corrosion index I of at least 6.0 for unpainted bridges.
What is the difference between Q420qNHE and Q420qNHD?
Strength and chemistry box are the same. Q420qNHE is Charpy tested at −40°C, Q420qNHD at −20°C, both needing 120 J for 12–100 mm plate. P/S caps are 0.020/0.010% for E and 0.025/0.015% for D. Choose by the lowest service or erection temperature.
What is the yield strength of Q420qNHE?
Q420qNHE has a minimum lower yield strength of 420 MPa up to 50 mm and 410 MPa from 50 to 100 mm, and 365 MPa from 100 to 130 mm (GB/T 714-2025 Table 9). Minimum tensile is 540 MPa up to 100 mm. There is no upper tensile limit in the standard.
What is the ASTM or EN equivalent of Q420qNHE?
Close grades for Q420qNHE: No direct equivalent in Annex B / closest: ASTM A709 HPS 70W (higher) / EN 10025-4 S420ML (not weathering). These are close families, not drop-in substitutes; compare yield at thickness, impact temperature and energy, and the weldability index before substituting.
Does GB/T 714 require ultrasonic testing?
Yes. GB/T 714-2025 clause 7.5 requires every single-rolled plate over 20 mm to be ultrasonically tested to GB/T 2970, with acceptance Class II or better. Thinner plate is tested only by agreement.
What welding consumables are used for Q420qNHE?
Use low-hydrogen consumables that match both strength and weathering behaviour, typically Ni-Cu bearing electrodes and wires (AWS E8018-W2 type at 345–420 MPa). Exposed weld metal must weather like the plate, or it will corrode faster.

Conclusion

Q420qNHE to GB/T 714 is weathering bridge steel with 420 MPa minimum yield, Cu-Cr-Ni chemistry, a weathering index of at least 6.0 and 120 J Charpy at −40°C for 12–100 mm plate.

It sits between Q390qNH and Q460qNHE in the weathering range, with Q420qNHD and Q420qNHF as sister letters. The most common ordering mistake with Q420qNHE is leaving the Z level, UT class or impact position off the order; add them at enquiry stage, not after rolling.

Every Q420qNHE plate from SHH STEEL ships with heat analysis, the weldability index, tensile and Charpy results on an EN 10204 3.1 or 3.2 certificate. Product analysis, Z15–Z35, extra UT and cut-to-size are options.

We ship from Shanghai to bridge builders worldwide. Browse the full GB/T 714 range or other weathering steel plates.

Tell us the sizes, tonnage and any Z, UT or inspection needs. We check the request against GB/T 714 first, then confirm mill, route, lead time and price. Contact SHH STEEL today for Q420qNHE weathering bridge steel.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X