GB/T 714 Q620qE bridge steel plate stacked at SHH STEEL warehouse

GB/T 714 Q620qE Bridge Steel Plate Supplier

GB/T 714 Q620qE is bridge structural steel plate with 620 MPa minimum yield, 720 MPa minimum tensile and Charpy V-notch impact of 120 J at −40°C for 12–100 mm plate. SHH STEEL supplies Q620qE mill-direct, TMCP / TMCP+T / QT, up to 100 mm, with Z15–Z35, UT and heat and product analysis.
Keywords
Q620qE, Q620qE steel plate, GB/T 714 Q620qE, Q620q-E, Q620q E, Q620qE bridge steel, Q620qEZ15, Q620qEZ25, Q620qEZ35, bridge steel plate, Q620qE supplier
Equivalent Grades:
EN 10025-6 S620Q, S620QL, S620QL1 (Annex B) — Material Specification: GB/T 714-2025 (supersedes GB/T 714-2015) — Delivery: TMCP / TMCP+T / QT
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Q620q Quality Grades
GB/T 714-2025 vs 2015
Q620qE vs ASTM A709 / EN 10025
TMCP vs Normalized vs QT
Welding and Fatigue
Z15 / Z25 / Z35
Equivalent Material Grades
Testing and Inspection
Dimensions
Tolerances
Price and Ordering
Applications
Supply Capability
Why Choose SHH STEEL
FAQ
Conclusion

What is GB/T 714 Q620qE Bridge Steel Plate?

Q620qE is bridge structural steel plate to GB/T 714. Q stands for yield, 620 is the minimum yield in MPa for plate up to 50 mm, q stands for qiao (bridge) and E is the quality grade: Charpy V-notch at −40°C on longitudinal specimens.

Q620q is ultra-high-strength bridge plate for members where weight and depth are the design limits. Q620q bridges the gap between Q550q and Q690q. Like Q550q it gained a TMCP route in 2025; in QT form it carries Cr, Ni, Cu and Mo minimums (Cr 0.40–0.80%, Mo 0.20–0.50%) for hardenability.

Q620qE adds −40°C proof to 620 MPa yield. It is used on long-span bridges in cold regions where highly stressed members must stay thin.

GB/T 714-2025 is the current edition. It was issued on 31 October 2025, took effect on 1 May 2026 and fully supersedes GB/T 714-2015, the fourth revision since the standard was first issued in 1965. We certify to the edition written on the purchase order.

SHH STEEL (Shanghai Shenghonghe Import & Export Co., Ltd.) is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. We ship Q620qE cut to size with an EN 10204 3.1 or 3.2 certificate. Sister grades are listed under GB/T 714.

Material Specification

Specification element Requirement SHH STEEL compliance
Standard GB/T 714-2025 Q620qE Confirmed
Product Single-rolled plate ≤150 mm; hot-rolled strip and cut plate ≤25.4 mm Plate
Thickness with tensile values Up to 100 mm for Q620q Confirmed
Minimum yield ReL 620 MPa ≤50 mm; 580 MPa >50–100 mm Confirmed
Minimum tensile Rm 720 MPa ≤100 mm (no upper limit in the standard) Confirmed
Elongation A ≥ 15% Confirmed
Charpy V-notch −40°C, 120 J (12–100 mm), longitudinal Confirmed
Delivery condition TMCP, TMCP + tempering, or quenched and tempered (QT) As ordered
Weldability index Pcm (Table 7) for TMCP; CEV (Table 6) for QT Printed on MTC
Ultrasonic testing Plate >20 mm: GB/T 2970, Class II or better Every plate
Through-thickness Z15, Z25 or Z35 to GB/T 5313, when ordered As ordered
Dimensions GB/T 709 Confirmed
Certificate GB/T 247; EN 10204 3.1 or 3.2 As ordered

Grades often compared with Q620qE are EN 10025-6 S460Q and ASTM A514 Grade Q; the comparison below shows where they differ.

Chemical Composition: Heat Analysis and Product Analysis

For Q620qE we report heat analysis on every certificate and add a product analysis when the buyer asks for it. The two use different limits: heat values follow GB/T 714, product values add the GB/T 222 deviations.

Table 1 below is the heat (ladle) analysis for Q620qE from GB/T 714-2025 Tables 1, 2, 3 and 4.

Element Q620qE TMCP (%) Q620q quenched and tempered (%)
C, max 0.11 0.14
Si, max 0.50 0.55
Mn 0.80 – 1.70 0.80 – 1.70
P, max 0.020 0.020
S, max 0.010 0.010
Nb 0.005 – 0.090 0.005 – 0.090
V 0.010 – 0.080 0.010 – 0.080
Ti 0.006 – 0.030 0.006 – 0.030
Als 0.010 – 0.045 0.010 – 0.045
Cr, max 1.00 0.40 – 0.80
Ni, max 1.20 0.25 – 1.00
Cu, max 0.55 0.15 – 0.55
Mo, max 0.60 0.20 – 0.50
N, max 0.0080 0.0080
B, max 0.0005 residual (≤0.0014 if C ≤0.10%) 0.0005–0.0030 may be added
H, max 0.0002 0.0002

Nb, V, Ti and Al may be added singly or together. Added singly, each must meet the range above; added together, at least one must reach its minimum and Nb + V + Ti ≤ 0.22%.

Table 2 is the product analysis: the limits a check analysis on finished plate is judged against. GB/T 714-2025 clause 7.1.3 calls up GB/T 222 for the permitted deviations.

Element Heat limit (%) Deviation, GB/T 222-2025 Table 2 (alloy) Q620qE product analysis (%)
C ≤ 0.11 +0.01 ≤ 0.12
Si ≤ 0.50 +0.04 ≤ 0.54
Mn 0.80 – 1.70 ±0.04 0.76 – 1.74
P ≤ 0.020 +0.005 (see note) ≤ 0.025
S ≤ 0.010 +0.005 (see note) ≤ 0.015
Cr ≤ 1.00 +0.05 (0.90–2.10% band) ≤ 1.05
Ni ≤ 1.20 +0.05 (1.00–2.00% band) ≤ 1.25
Cu ≤ 0.55 +0.03 ≤ 0.58
Mo ≤ 0.60 +0.02 (0.30–0.60% band) ≤ 0.62
V 0.010 – 0.080 +0.01 (≤0.10% band) ≤ 0.090
Ti 0.006 – 0.030 +0.02 ≤ 0.050
Nb, B, N See heat table Not read in our copy of Table 2 Agree in contract

How to read Table 2. With Ni up to 1.20% and Mo up to 0.60%, Q620q heats are normally classed as alloy steel under GB/T 13304, so the alloy-steel table of GB/T 222 applies. One steel uses one table only; the certificate should say which.

Mechanical Properties

Tensile values follow Table 9 of GB/T 714-2025 for Q620q. Tensile specimens are transverse; round specimens are used above 40 mm. Where yield is not distinct, Rp0.2 replaces ReL.

Nominal thickness ReL min (MPa) Rm min (MPa) A min
≤ 50 mm 620 720 15%
> 50 – 100 mm 580 720 15%

Impact values follow Table 10, on longitudinal specimens, average of three:

Letter / test temperature KV2 ≤12 mm KV2 >12 – 100 mm KV2 >100 – 150 mm
E / −40°C 80 J 120 J Not applicable

One single value may fall below the required average, but not below 70% of it. Plate over 8 mm and under 12 mm is tested with 7.5 mm specimens (75% of the value); 6–8 mm plate with 5 mm specimens (50%). Plate under 6 mm is not impact tested.

180° bend test, transverse: mandrel D = 2a up to 16 mm and 3a above 16 mm; may be omitted when the mill guarantees it. Yield ratio is not mandatory and Annex C gives no recommended value at this level; agree a limit in the contract if the design needs one.

Q620qD / Q620qE / Q620qF: Which Quality Grade?

Q620qE is tested at −40°C. It suits bridges in north-east China, Inner Mongolia, Xinjiang, Russia, Kazakhstan, Canada and high-altitude sites, and for thick, restrained members anywhere. E is tested at −40°C, with P ≤0.020% and S ≤0.010%. Many long-span bridges specify E even in mild climates, because thick plate and heavy welding raise the risk of brittle fracture.

Grade Test temp. KV2 ≤12 mm KV2 12–100 mm KV2 >100 mm P / S max (%)
Q620qD −20°C 80 J 120 J — 0.025 / 0.015
Q620qE −40°C 80 J 120 J — 0.020 / 0.010
Q620qF −60°C By agreement 69 J — 0.015 / 0.006

Over-specifying the letter costs money; under-specifying it costs safety. Choose from the lowest service or erection temperature, then step up one letter for thick, restrained or fracture-critical members.

Q620qE: What Changed from GB/T 714-2015 to GB/T 714-2025

For Q620qE buyers the 2025 edition changes more than the year on the certificate. The points below come from the foreword of GB/T 714-2025 and its tables.

  • A TMCP route was added for Q620q (C ≤0.11%, Pcm ≤0.24% to 50 mm). In 2015 it was QT only.
  • CEV and Pcm limits were revised (Tables 6 and 7).
  • Tensile strength is now banded by thickness (e.g. lower minimum Rm above 100 mm) instead of one value.
  • Impact energy is set by thickness band (≤12 mm, 12–100 mm, >100 mm) in Table 10.
  • Yield ratio is no longer a clause value; it is agreed in the contract, with recommendations in informative Annex C.
  • Section products were removed; the standard now covers plate and strip only.
  • Delivery is TMCP, TMCP + tempering or QT; normalizing is kept only for Q345q/Q370q plate over 100 mm by agreement.

If a drawing cites 2015 and the plate is made to 2025, get the designer’s written acceptance; tensile strength above 100 mm and the yield-ratio basis differ.

Q620qE vs ASTM A709 and EN 10025: Which Grade Matches?

Can Q620qE replace a US or European bridge grade, or the other way round? Strength can match; toughness rules differ in kind, not only in number.

Property Q620qE EN 10025-6 S460Q ASTM A514 Grade Q EN 10025-6 S620Q
Min. yield (MPa) 620 (≤50 mm) 460 (≤50 mm) 690 (≤65 mm) 620 (≤50 mm)
Tensile (MPa) 720 min 550 – 720 760 – 895 700 – 890
Charpy 120 J at −40°C (12–100 mm) Q: −20°C, QL: −40°C, QL1: −60°C Supplementary only Q / QL / QL1: −20 / −40 / −60°C
Weathering chemistry No No No No

ASTM A709 sets Charpy requirements by temperature zone (1, 2, 3) and by member type: non-fracture-critical (T) or fracture-critical (F). GB/T 714 sets one value per letter, so compare the A709 zone with the GB/T 714 test temperature, not grade with grade.

EN 10025-3/-4/-6 grades show yield at the thinnest band; their values fall with thickness. GB/T 714 keeps 620 MPa to 50 mm. EN tensile ranges have upper limits; GB/T 714 gives minimums only.

The 120 J requirement in GB/T 714 for 12–100 mm plate is several times the 27–40 J typical of general structural grades. That margin is the main reason bridge owners specify Q620qE rather than GB/T 1591 plate.

Q620qE Delivery Condition: TMCP vs Normalized vs Quenched and Tempered

GB/T 714-2025 clause 3.2 defines TMCP as rolling with the final deformation in a controlled temperature range, including accelerated cooling with or without tempering (self-tempering included) but excluding direct quenching and quench-and-temper. The delivery route must be stated on the certificate.

Route Available for Q620qE Weldability index Notes
TMCP Yes Pcm ≤0.24% (≤50 mm) C ≤0.11%; up to 100 mm
TMCP + tempering Yes Pcm Improves toughness uniformity
Quenched and tempered Yes CEV ≤0.55% (≤50 mm) C ≤0.14%; B 0.0005–0.0030% may be added
Normalized No — Not listed

Q620q can be TMCP or QT. QT chemistry has minimum Cr (0.40%), Ni (0.25%), Cu (0.15%) and Mo (0.20%) for hardenability; TMCP chemistry has only maximums. For E-letter plate over about 50 mm, many mills add tempering after TMCP to reduce toughness scatter through the thickness.

Ask for the route on the purchase order. It changes the weldability index, the welding procedure and, for heavy plate, the price of Q620qE.

Welding Q620qE and Fatigue in Bridge Girders

GB/T 714-2025 clause 7.1.2 uses CEV for normalized, QT and TMCP steel with C >0.12%, and Pcm for weathering steel and TMCP steel with C ≤0.12%, both from the heat analysis:

CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15

Pcm = C + Si/30 + Mn/20 + Cu/20 + Ni/60 + Cr/20 + Mo/15 + V/10 + 5B

Index ≤50 mm >50–100 mm >100–130 mm
Pcm, TMCP (Table 7) ≤ 0.24 ≤ 0.25 —
CEV, QT (Table 6) ≤ 0.55 ≤ 0.60 —

On thick Q620qE flanges, preheat, interpass control and low-hydrogen practice matter more than the grade itself. The certificate gives the data to set them. At −40°C, HAZ toughness often becomes the limit. Fabricators usually cap heat input and qualify the procedure at −40°C on plate from the same route.

Typical consumables for Q620qE: E69-class consumables (AWS E10018M type).

Fatigue. Welded details govern fatigue life in a bridge, and their fatigue strength is set by detail category, not by yield strength. Higher-strength plate can carry higher stress ranges only if detailing improves too.

Fatigue design follows JTG D64 (highway) and TB 10091 (railway) in China, EN 1993-1-9 in Europe and AASHTO LRFD in the US; fabrication commonly follows TB 10212, JTG/T 3650 or AWS D1.5.

Q620qEZ15, Z25 and Z35: Through-Thickness Plate for Bridges

Bridge node plates, anchor boxes and pylon walls take weld shrinkage through their thickness. If the plate holds sulfide stringers, it can tear in steps under the weld. Z grades prove through-thickness ductility.

GB/T 714 adds the Z level to the end of the designation, for example Q620qEZ25. The test and acceptance follow GB/T 5313 and apply to plate 15 mm and thicker.

Z grade Heat sulfur, max (%) Reduction of area, avg / single (%)
Z15 0.010 15 / 10
Z25 0.007 25 / 15
Z35 0.005 35 / 25

E chemistry already limits S to 0.010%, the Z15 sulfur cap. Z25 (S ≤0.007%) and Z35 (S ≤0.005%) still need a cleaner heat.

For Q620qE, we test Z per GB/T 5313 batch rules and print the three reduction-of-area values on the certificate. Z options apply across the GB/T 714 bridge steel range.

Equivalent Material Grades

Annex B of GB/T 714-2025 lists foreign grades against each strength level. It is informative: it tells you which families are close, not that the plates are interchangeable.

Standard Grade(s) Fit for Q620qE
EN 10025-6 EN 10025-6 S620Q, EN 10025-6 S620QL, EN 10025-6 S620QL1 Listed in Annex B
GB/T 16270 GB/T 16270 Q620E QT alternative, different toughness rules
GB/T 1591 GB/T 1591 Q620ME TMCP general structural

Before substituting, compare three things line by line: minimum yield at the actual thickness, the impact test temperature and energy, and the weldability index. For Q620qE, the 120 J impact level and the Pcm/CEV caps are usually the hardest to match.

Q620qE Testing, UT and Certificate

A batch of Q620qE is one grade, one heat, one thickness, one rolling schedule and one heat-treatment condition, up to 60 t. Table 12 of GB/T 714-2025 sets the tests:

Test Frequency Method
Heat analysis 1 per heat GB/T 20066; GB/T 4336 / GB/T 223
Tensile 1 per batch GB/T 2975 / GB/T 228.1
Bend 180° 1 per batch (may be waived if guaranteed) GB/T 232
Charpy V at −40°C 3 specimens per batch GB/T 229
Through-thickness (Z) 3 specimens per batch, when ordered GB/T 5313
Ultrasonic Every plate >20 mm, Class II or better GB/T 2970
Surface and dimensions Every plate Visual and gauges

Impact retest: if a set fails, three more specimens are taken from the same batch. The average of all six must meet the requirement; two values may be below it, but only one below 70%. At −40°C, retest risk rises on heavy plate; we build a margin for retests into the delivery schedule.

Dimensions

Size range for Q620qE plate:

  • Thickness: 6 mm – 100 mm under GB/T 714 tensile tables; most orders 10 – 60 mm
  • Width: 1500 – 4000 mm, depending on mill and thickness
  • Length: 6000 – 18000 mm; longer by enquiry
  • Edge: mill edge or cut edge
  • Weight: theoretical, 7.85 g/cm³

Deck plate, webs, flanges, diaphragms and stiffeners are cut to drawing. For U-ribs and rolled sections on the same bridge, see steel beam profiles and steel structural profiles.

Tolerances

Dimensional tolerances for Q620qE follow GB/T 709, as GB/T 714 directs. The default is Class B, which fixes the minus side at 0.30 mm.

Nominal thickness (mm) Width ≤ 1500 mm Width > 1500 – 2500 mm
> 8 – 15 −0.30 / +0.80 −0.30 / +1.00
> 15 – 25 −0.30 / +1.00 −0.30 / +1.20
> 25 – 40 −0.30 / +1.10 −0.30 / +1.30
> 40 – 60 −0.30 / +1.30 −0.30 / +1.50
> 60 – 100 −0.30 / +1.50 −0.30 / +1.80
> 100 – 150 −0.30 / +2.10 −0.30 / +2.50

Bridge fabricators often ask for Class C (zero minus) on deck and flange plate so section properties are never under the design value. Wider plates follow the heavier GB/T 709 rows; we state them on the offer.

Q620qE Price Factors and How to Order

When you compare Q620qE offers, compare extras line by line. These are the items that move the price.

Cost driver Effect on price
Strength level Q620q Higher levels need more alloy and tighter rolling control
Quality letter Higher extra: −40°C testing, S ≤0.010%, more retest risk
Delivery route TMCP / TMCP+T / QT; QT costs more than TMCP
Thickness Over 60 mm and under 10 mm carry size extras
Z15 / Z25 / Z35 Low-sulfur heat, Z test, UT; Z35 costs most
Width and length Over 3000 mm wide or 15 m long needs mill confirmation
Quantity per size Mill minimums per heat and size
Inspection and processing 3.2 witness, profile cutting, blasting, priming quoted per item

To get a firm quote in one round, send:

  • Grade, edition and Z level, e.g. Q620qEZ25 to GB/T 714-2025
  • Thickness × width × length and pieces or tonnes
  • Delivery route and UT class if beyond Class II
  • Certificate type and inspector
  • Destination port and Incoterm

We quote plate price, extras and freight line by line. Need another letter? See Q620qD, Q620qF.

Applications

Sector Typical Q620qE components
Ultra-long-span bridges Highly stressed truss chords
Cable anchorages Anchor boxes and anchor plates
Steel pylons Pylon shells
Movable bridges Lightweight girders
Special structures Members where depth is limited

The letter E suits bridges in north-east China, Inner Mongolia, Xinjiang, Russia, Kazakhstan, Canada and high-altitude sites, and for thick, restrained members anywhere.

It is the wrong plate for pressure equipment (pressure vessel steel plates), unpainted exposure (weathering steel plates) or ship hulls (shipbuilding steel plates).

Supply Capability and Global Delivery

SHH STEEL sources Q620qE from first-line bridge-plate mills, including drafters of GB/T 714-2025 such as Ansteel, Valin Xiangtan, Jiangyin Xingcheng, Wuyang, Shougang and Xinyu.

  • Certificates: EN 10204 3.1 standard; 3.2 with third-party witness (SGS, BV, TÜV or owner’s inspector)
  • Tests: tensile, −40°C Charpy, bend, Z test, UT, product analysis
  • Processing: CNC plasma and flame cutting, bevelling, drilling, shot blasting and priming
  • Terms: FOB Shanghai, CFR, CIF; TT, LC or TT + LC
  • Marking: steel-stamped and paint-marked with grade, heat, size and mill, per GB/T 247

Q620qE goes from Shanghai to bridge sites and fabrication yards worldwide, usually as break-bulk for long plates.

Lead time: about 45–60 days from mill rolling; Z35, F letter or 3.2 inspection adds about 1–2 weeks. Sea time from Shanghai is about 7–12 days to Southeast Asia and 28–35 days to North Europe.

Why Choose SHH STEEL

SHH STEEL is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. For Q620qE that means bridge plate from bridge-plate mills, not relabelled structural plate.

Before shipment we check four lines on every Q620qE certificate: yield and tensile for the actual thickness band, Charpy at −40°C, the CEV or Pcm for the delivery route, and UT results. If one fails, the plate does not ship as Q620qE.

Elongation drops to 15% at this level. Bending and forming rules in the fabrication specification should be checked for Q620qE before cutting starts.

We also tell buyers when another grade fits better. Neighbouring levels are Q550qE and Q690qE. Browse more structural steel plates and high strength low alloy plates.

FAQ

What is Q620qE steel?
Q620qE is bridge structural steel plate to GB/T 714-2025. It has 620 MPa minimum yield up to 50 mm, 720 MPa minimum tensile, 15% elongation and Charpy V-notch impact of 120 J at −40°C for 12–100 mm plate. It is delivered TMCP, TMCP + tempering, or quenched and tempered.
What is the difference between Q620qE and Q620qD?
Strength and chemistry box are the same. Q620qE is Charpy tested at −40°C, Q620qD at −20°C, both needing 120 J for 12–100 mm plate. P/S caps are 0.020/0.010% for E and 0.025/0.015% for D. Choose by the lowest service or erection temperature.
What is the yield strength of Q620qE?
Q620qE has a minimum lower yield strength of 620 MPa up to 50 mm and 580 MPa from 50 to 100 mm (GB/T 714-2025 Table 9). Minimum tensile is 720 MPa up to 100 mm. There is no upper tensile limit in the standard.
What is the ASTM or EN equivalent of Q620qE?
Close grades for Q620qE: EN 10025-6 S620Q, S620QL, S620QL1 (Annex B). These are close families, not drop-in substitutes; compare yield at thickness, impact temperature and energy, and the weldability index before substituting.
Can GB/T 714 bridge plate be normalized?
Only in one case. GB/T 714-2025 clause 6.2 requires TMCP, TMCP + tempering or quenched and tempered delivery, but Q345q and Q370q plate over 100 mm and up to 150 mm may be normalized by agreement.
What is the carbon equivalent of Q620qE?
It depends on the route. For Q620qE up to 50 mm, GB/T 714-2025 sets Pcm ≤0.24% (TMCP) or CEV ≤0.55% (QT). CEV applies to normalized, QT and TMCP steel with C >0.12%; Pcm to TMCP steel with C ≤0.12%.

Conclusion

Q620qE to GB/T 714-2025 is bridge plate with 620 MPa minimum yield, 720 MPa minimum tensile and 120 J Charpy at −40°C for 12–100 mm plate.

It sits between Q550qE and Q690qE in the bridge range, with Q620qD and Q620qF as sister letters. Before ordering Q620qE, confirm the edition on the drawing, the delivery route and any Z level; those three choices drive cost, lead time and welding.

From SHH STEEL, Q620qE arrives with traceable heat numbers, a complete EN 10204 3.1 or 3.2 certificate and, if ordered, third-party witness, product analysis and Z testing.

We ship from Shanghai to bridge builders worldwide. Browse the full GB/T 714 range or other high strength low alloy plates.

Share your size list, Z level and edition, and we reply with mill, route, lead time, test plan and price in one message. Contact SHH STEEL for a mill-direct Q620qE bridge steel plate quotation.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *