GB/T 714 Q550qF bridge steel plate stacked at SHH STEEL warehouse

GB/T 714 Q550qF Bridge Steel Plate Supplier

GB/T 714 Q550qF is bridge structural steel plate with 550 MPa minimum yield, 660 MPa minimum tensile and Charpy V-notch impact of 60 J at −60°C for 12–100 mm plate. SHH STEEL supplies Q550qF mill-direct, TMCP / TMCP+T / QT, up to 100 mm, with Z15–Z35, UT and heat and product analysis.
Keywords
Q550qF, Q550qF steel plate, GB/T 714 Q550qF, Q550q-F, Q550q F, Q550qF bridge steel, Q550qFZ15, Q550qFZ25, Q550qFZ35, bridge steel plate, Q550qF supplier
Equivalent Grades:
EN 10025-6 S550Q, S550QL, S550QL1 (Annex B) — Material Specification: GB/T 714-2025 (supersedes GB/T 714-2015) — Delivery: TMCP / TMCP+T / QT
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Q550q Quality Grades
GB/T 714-2025 vs 2015
Q550qF vs ASTM A709 / EN 10025
TMCP vs Normalized vs QT
Welding and Fatigue
Z15 / Z25 / Z35
Equivalent Material Grades
Testing and Inspection
Dimensions
Tolerances
Price and Ordering
Applications
Supply Capability
Why Choose SHH STEEL
FAQ
Conclusion

What is GB/T 714 Q550qF Bridge Steel Plate?

Q550qF is bridge structural steel plate to GB/T 714. Q stands for yield, 550 is the minimum yield in MPa for plate up to 50 mm, q stands for qiao (bridge) and F is the quality grade: Charpy V-notch at −60°C on longitudinal specimens.

Q550q is ultra-high-strength bridge plate up to 100 mm, now available TMCP as well as QT under GB/T 714-2025. Q550q was a QT-only grade in the 2015 edition. The 2025 edition adds a TMCP route with C ≤0.11% and Pcm ≤0.23% to 50 mm, which makes thinner, easier-to-weld plate possible at 550 MPa.

Q550qF is tested at −60°C with at least 60 J for plate over 12 mm. Few projects need it, but where they do, it is usually for fracture-critical members in Arctic or high-altitude climates.

GB/T 714-2025 has been in force since 1 May 2026, replacing GB/T 714-2015 in full. If your specification was written earlier, check the edition before ordering: some table values changed, and a few grades were added or dropped.

SHH STEEL (Shanghai Shenghonghe Import & Export Co., Ltd.) is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. We ship Q550qF cut to size with an EN 10204 3.1 or 3.2 certificate. Sister grades are listed under GB/T 714.

Material Specification

Specification element Requirement SHH STEEL compliance
Standard GB/T 714-2025 Q550qF Confirmed
Product Single-rolled plate ≤150 mm; hot-rolled strip and cut plate ≤25.4 mm Plate
Thickness with tensile values Up to 100 mm for Q550q Confirmed
Minimum yield ReL 550 MPa ≤50 mm; 530 MPa >50–100 mm Confirmed
Minimum tensile Rm 660 MPa ≤100 mm (no upper limit in the standard) Confirmed
Elongation A ≥ 16% Confirmed
Charpy V-notch −60°C, 60 J (12–100 mm), longitudinal Confirmed
Delivery condition TMCP, TMCP + tempering, or quenched and tempered (QT) As ordered
Weldability index Pcm (Table 7) for TMCP; CEV (Table 6) for QT Printed on MTC
Ultrasonic testing Plate >20 mm: GB/T 2970, Class II or better Every plate
Through-thickness Z15, Z25 or Z35 to GB/T 5313, when ordered As ordered
Dimensions GB/T 709 Confirmed
Certificate GB/T 247; EN 10204 3.1 or 3.2 As ordered

Grades often compared with Q550qF are and EN 10025-6 S460Q; the comparison below shows where they differ.

Chemical Composition: Heat Analysis and Product Analysis

Two analyses matter for Q550qF. The heat (ladle) analysis is taken during casting and printed on the certificate. The product analysis is taken from finished plate and judged with the wider GB/T 222 tolerances. Mixing the two is the most common reason for disputed rejections.

Table 1 below is the heat (ladle) analysis for Q550qF from GB/T 714-2025 Tables 1, 2, 3 and 4.

Element Q550qF TMCP (%) Q550q quenched and tempered (%)
C, max 0.11 0.12
Si, max 0.50 0.55
Mn 0.80 – 1.70 0.80 – 1.70
P, max 0.015 0.015
S, max 0.006 0.006
Nb 0.005 – 0.090 0.005 – 0.060
V 0.010 – 0.080 0.010 – 0.080
Ti 0.006 – 0.030 0.006 – 0.030
Als 0.010 – 0.045 0.010 – 0.045
Cr, max 1.00 ≤ 0.80
Ni, max 1.20 ≤ 0.70
Cu, max 0.55 ≤ 0.30
Mo, max 0.60 ≤ 0.30
N, max 0.0080 0.0080
B, max 0.0005 residual (≤0.0014 if C ≤0.10%) 0.0005–0.0030 may be added
H, max 0.0002 0.0002

Nb, V, Ti and Al may be added singly or together. Added singly, each must meet the range above; added together, at least one must reach its minimum and Nb + V + Ti ≤ 0.22%.

Table 2 is the product analysis: the limits a check analysis on finished plate is judged against. GB/T 714-2025 clause 7.1.3 calls up GB/T 222 for the permitted deviations.

Element Heat limit (%) Deviation, GB/T 222-2025 Table 2 (alloy) Q550qF product analysis (%)
C ≤ 0.11 +0.01 ≤ 0.12
Si ≤ 0.50 +0.04 ≤ 0.54
Mn 0.80 – 1.70 ±0.04 0.76 – 1.74
P ≤ 0.015 +0.005 (see note) ≤ 0.020
S ≤ 0.006 +0.005 (see note) ≤ 0.011
Cr ≤ 1.00 +0.05 (0.90–2.10% band) ≤ 1.05
Ni ≤ 1.20 +0.05 (1.00–2.00% band) ≤ 1.25
Cu ≤ 0.55 +0.03 ≤ 0.58
Mo ≤ 0.60 +0.02 (0.30–0.60% band) ≤ 0.62
V 0.010 – 0.080 +0.01 (≤0.10% band) ≤ 0.090
Ti 0.006 – 0.030 +0.02 ≤ 0.050
Nb, B, N See heat table Not read in our copy of Table 2 Agree in contract

How to read Table 2. With Ni up to 1.20% and Mo up to 0.60%, Q550q heats are normally classed as alloy steel under GB/T 13304, so the alloy-steel table of GB/T 222 applies. One steel uses one table only; the certificate should say which.

Mechanical Properties

Tensile values follow Table 9 of GB/T 714-2025 for Q550q. Tensile specimens are transverse; round specimens are used above 40 mm. Where yield is not distinct, Rp0.2 replaces ReL.

Nominal thickness ReL min (MPa) Rm min (MPa) A min
≤ 50 mm 550 660 16%
> 50 – 100 mm 530 660 16%

Impact values follow Table 10, on longitudinal specimens, average of three:

Letter / test temperature KV2 ≤12 mm KV2 >12 – 100 mm KV2 >100 – 150 mm
F / −60°C By agreement 60 J Not applicable

One single value may fall below the required average, but not below 70% of it. Plate over 8 mm and under 12 mm is tested with 7.5 mm specimens (75% of the value); 6–8 mm plate with 5 mm specimens (50%). Plate under 6 mm is not impact tested.

180° bend test, transverse: mandrel D = 2a up to 16 mm and 3a above 16 mm; may be omitted when the mill guarantees it. Yield ratio is not mandatory and Annex C gives no recommended value at this level; agree a limit in the contract if the design needs one.

Q550qD / Q550qE / Q550qF: Which Quality Grade?

Q550qF is tested at −60°C. It suits Arctic and sub-Arctic bridges, high-latitude rail lines and owners who want the largest toughness margin for fracture-critical members. F is the coldest letter in GB/T 714: Charpy at −60°C, P ≤0.015% and S ≤0.006%. It exists only for Q420q and above (and their NH versions), and its energy rises with strength.

Grade Test temp. KV2 ≤12 mm KV2 12–100 mm KV2 >100 mm P / S max (%)
Q550qD −20°C 80 J 120 J — 0.025 / 0.015
Q550qE −40°C 80 J 120 J — 0.020 / 0.010
Q550qF −60°C By agreement 60 J — 0.015 / 0.006

Note that F energy at Q550q is 60 J, not 120 J: the colder test uses a lower energy that GB/T 714-2025 raises with strength, from 47 J at Q420q/Q460q to 77 J at Q690q. Plate up to 12 mm needs an agreed value.

Q550qF: What Changed from GB/T 714-2015 to GB/T 714-2025

For Q550qF buyers the 2025 edition changes more than the year on the certificate. The points below come from the foreword of GB/T 714-2025 and its tables.

  • A TMCP route was added for Q550q (C ≤0.11%, Pcm ≤0.23% to 50 mm). In 2015 it was QT only.
  • CEV and Pcm limits were revised (Tables 6 and 7).
  • Tensile strength is now banded by thickness (e.g. lower minimum Rm above 100 mm) instead of one value.
  • Impact energy is set by thickness band (≤12 mm, 12–100 mm, >100 mm) in Table 10.
  • Yield ratio is no longer a clause value; it is agreed in the contract, with recommendations in informative Annex C.
  • Section products were removed; the standard now covers plate and strip only.
  • Delivery is TMCP, TMCP + tempering or QT; normalizing is kept only for Q345q/Q370q plate over 100 mm by agreement.

If a drawing cites 2015 and the plate is made to 2025, get the designer’s written acceptance; tensile strength above 100 mm and the yield-ratio basis differ.

Q550qF vs ASTM A709 and EN 10025: Which Grade Matches?

Can Q550qF replace a US or European bridge grade, or the other way round? Strength can match; toughness rules differ in kind, not only in number.

Property Q550qF EN 10025-6 S460Q EN 10025-6 S550Q
Min. yield (MPa) 550 (≤50 mm) 460 (≤50 mm) 550 (≤50 mm)
Tensile (MPa) 660 min 550 – 720 640 – 820
Charpy 60 J at −60°C (12–100 mm) Q: −20°C, QL: −40°C, QL1: −60°C Q / QL / QL1: −20 / −40 / −60°C
Weathering chemistry No No No

ASTM A709 sets Charpy requirements by temperature zone (1, 2, 3) and by member type: non-fracture-critical (T) or fracture-critical (F). GB/T 714 sets one value per letter, so compare the A709 zone with the GB/T 714 test temperature, not grade with grade.

EN 10025-3/-4/-6 grades show yield at the thinnest band; their values fall with thickness. GB/T 714 keeps 550 MPa to 50 mm. EN tensile ranges have upper limits; GB/T 714 gives minimums only.

At −60°C, the 60 J required for Q550qF is a demanding figure; general structural grades rarely prove any toughness that cold. For the C, D and E letters GB/T 714 asks 120 J, several times the 27–40 J typical of GB/T 1591 plate.

Q550qF Delivery Condition: TMCP vs Normalized vs Quenched and Tempered

GB/T 714-2025 clause 3.2 defines TMCP as rolling with the final deformation in a controlled temperature range, including accelerated cooling with or without tempering (self-tempering included) but excluding direct quenching and quench-and-temper. The delivery route must be stated on the certificate.

Route Available for Q550qF Weldability index Notes
TMCP Yes Pcm ≤0.23% (≤50 mm) C ≤0.11%; up to 100 mm
TMCP + tempering Yes Pcm Improves toughness uniformity
Quenched and tempered Yes CEV ≤0.52% (≤50 mm) C ≤0.12%; B 0.0005–0.0030% may be added
Normalized No — Not listed

Before 2026, Q550q bridge plate was QT only. GB/T 714-2025 added TMCP, which allows leaner chemistry and easier welding on plate up to about 50 mm. F-letter plate is often TMCP + tempering or, at the top strength levels, QT; ask which route the mill has qualified for −60°C.

Ask for the route on the purchase order. It changes the weldability index, the welding procedure and, for heavy plate, the price of Q550qF.

Welding Q550qF and Fatigue in Bridge Girders

GB/T 714-2025 clause 7.1.2 uses CEV for normalized, QT and TMCP steel with C >0.12%, and Pcm for weathering steel and TMCP steel with C ≤0.12%, both from the heat analysis:

CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15

Pcm = C + Si/30 + Mn/20 + Cu/20 + Ni/60 + Cr/20 + Mo/15 + V/10 + 5B

Index ≤50 mm >50–100 mm >100–130 mm
Pcm, TMCP (Table 7) ≤ 0.23 ≤ 0.25 —
CEV, QT (Table 6) ≤ 0.52 ≤ 0.57 —

The index caps in GB/T 714 are maximums. Real Q550qF heats often sit well below them, and preheat should be set from the actual value, not the cap. At −60°C, both weld metal and HAZ must prove toughness. Expect lower heat input, more passes and consumables qualified at −60°C.

Typical consumables for Q550qF: E62/E69-class consumables (AWS E9018M / E10018M type).

Fatigue. Welded details govern fatigue life in a bridge, and their fatigue strength is set by detail category, not by yield strength. Higher-strength plate can carry higher stress ranges only if detailing improves too.

Fatigue design follows JTG D64 (highway) and TB 10091 (railway) in China, EN 1993-1-9 in Europe and AASHTO LRFD in the US; fabrication commonly follows TB 10212, JTG/T 3650 or AWS D1.5.

Q550qFZ15, Z25 and Z35: Through-Thickness Plate for Bridges

When a bridge drawing marks a plate Z25, the mill must supply a low-sulfur heat and prove reduction of area through the thickness on every batch.

GB/T 714 adds the Z level to the end of the designation, for example Q550qFZ25. The test and acceptance follow GB/T 5313 and apply to plate 15 mm and thicker.

Z grade Heat sulfur, max (%) Reduction of area, avg / single (%)
Z15 0.010 15 / 10
Z25 0.007 25 / 15
Z35 0.005 35 / 25

F chemistry limits S to 0.006%, which already meets the Z25 sulfur cap (0.007%). Only Z35 (S ≤0.005%) needs a further step.

Put Z only where the joint needs it, usually node plates, anchor boxes and diaphragm-to-flange joints over about 25 mm. Keep the rest standard Q550qF. Z options apply across the GB/T 714 bridge steel range.

Equivalent Material Grades

Annex B of GB/T 714-2025 lists foreign grades against each strength level. It is informative: it tells you which families are close, not that the plates are interchangeable.

Standard Grade(s) Fit for Q550qF
EN 10025-6 EN 10025-6 S550Q, EN 10025-6 S550QL, EN 10025-6 S550QL1 Listed in Annex B
GB/T 16270 GB/T 16270 Q550F QT alternative, different toughness rules
GB/T 1591 GB/T 1591 Q550MF TMCP general structural

Before substituting, compare three things line by line: minimum yield at the actual thickness, the impact test temperature and energy, and the weldability index. For Q550qF, the 120 J impact level and the Pcm/CEV caps are usually the hardest to match.

Q550qF Testing, UT and Certificate

A batch of Q550qF is one grade, one heat, one thickness, one rolling schedule and one heat-treatment condition, up to 60 t. Table 12 of GB/T 714-2025 sets the tests:

Test Frequency Method
Heat analysis 1 per heat GB/T 20066; GB/T 4336 / GB/T 223
Tensile 1 per batch GB/T 2975 / GB/T 228.1
Bend 180° 1 per batch (may be waived if guaranteed) GB/T 232
Charpy V at −60°C 3 specimens per batch GB/T 229
Through-thickness (Z) 3 specimens per batch, when ordered GB/T 5313
Ultrasonic Every plate >20 mm, Class II or better GB/T 2970
Surface and dimensions Every plate Visual and gauges

Impact retest: if a set fails, three more specimens are taken from the same batch. The average of all six must meet the requirement; two values may be below it, but only one below 70%. At −60°C, mills may need trial heats before the production run; we agree the test plan before accepting the order.

Dimensions

Typical Q550qF dimensions on our offers:

  • Thickness: 6 mm – 100 mm under GB/T 714 tensile tables; most orders 10 – 60 mm
  • Width: 1500 – 4000 mm, depending on mill and thickness
  • Length: 6000 – 18000 mm; longer by enquiry
  • Edge: mill edge or cut edge
  • Weight: theoretical, 7.85 g/cm³

Deck plate, webs, flanges, diaphragms and stiffeners are cut to drawing. For U-ribs and rolled sections on the same bridge, see steel beam profiles and steel structural profiles.

Tolerances

GB/T 714 does not set its own size tolerances; Q550qF follows GB/T 709. Other tolerance standards can be agreed in the contract (clause 7.6.2).

Nominal thickness (mm) Width ≤ 1500 mm Width > 1500 – 2500 mm
> 8 – 15 −0.30 / +0.80 −0.30 / +1.00
> 15 – 25 −0.30 / +1.00 −0.30 / +1.20
> 25 – 40 −0.30 / +1.10 −0.30 / +1.30
> 40 – 60 −0.30 / +1.30 −0.30 / +1.50
> 60 – 100 −0.30 / +1.50 −0.30 / +1.80
> 100 – 150 −0.30 / +2.10 −0.30 / +2.50

Bridge fabricators often ask for Class C (zero minus) on deck and flange plate so section properties are never under the design value. Wider plates follow the heavier GB/T 709 rows; we state them on the offer.

Q550qF Price Factors and How to Order

Two Q550qF quotes can differ a lot and both be fair. Base prices are similar; extras are where mills part.

Cost driver Effect on price
Strength level Q550q Higher levels need more alloy and tighter rolling control
Quality letter Highest extra: −60°C testing, S ≤0.006%, limited mills
Delivery route TMCP / TMCP+T / QT; QT costs more than TMCP
Thickness Over 60 mm and under 10 mm carry size extras
Z15 / Z25 / Z35 Low-sulfur heat, Z test, UT; Z35 costs most
Width and length Over 3000 mm wide or 15 m long needs mill confirmation
Quantity per size Mill minimums per heat and size
Inspection and processing 3.2 witness, profile cutting, blasting, priming quoted per item

To get a firm quote in one round, send:

  • Grade, edition and Z level, e.g. Q550qFZ25 to GB/T 714-2025
  • Thickness × width × length and pieces or tonnes
  • Delivery route and UT class if beyond Class II
  • Certificate type and inspector
  • Destination port and Incoterm

We quote plate price, extras and freight line by line. Need another letter? See Q550qD, Q550qE.

Applications

Sector Typical Q550qF components
Ultra-long-span bridges Main truss chords and anchor zones
Cable-stayed bridges Highly stressed box girder flanges
Steel pylons Pylon wall plate
Railway bridges Heavily loaded node plates
Weight-critical retrofits Replacement members with limited depth

The letter F suits Arctic and sub-Arctic bridges, high-latitude rail lines and owners who want the largest toughness margin for fracture-critical members.

It is the wrong plate for pressure equipment (pressure vessel steel plates), unpainted exposure (weathering steel plates) or ship hulls (shipbuilding steel plates).

Supply Capability and Global Delivery

SHH STEEL sources Q550qF from first-line bridge-plate mills, including drafters of GB/T 714-2025 such as Ansteel, Valin Xiangtan, Jiangyin Xingcheng, Wuyang, Shougang and Xinyu.

  • Certificates: EN 10204 3.1 standard; 3.2 with third-party witness (SGS, BV, TÜV or owner’s inspector)
  • Tests: tensile, −60°C Charpy, bend, Z test, UT, product analysis
  • Processing: CNC plasma and flame cutting, bevelling, drilling, shot blasting and priming
  • Terms: FOB Shanghai, CFR, CIF; TT, LC or TT + LC
  • Marking: steel-stamped and paint-marked with grade, heat, size and mill, per GB/T 247

Our Q550qF exports follow Chinese bridge design abroad: railway and highway bridges built by EPC contractors in Asia, Africa and Latin America.

Lead time: about 45–60 days from mill rolling; Z35, F letter or 3.2 inspection adds about 1–2 weeks. Sea time from Shanghai is about 7–12 days to Southeast Asia and 28–35 days to North Europe.

Why Choose SHH STEEL

SHH STEEL has supplied bridge plate as a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. Q550qF is ordered from mills that roll bridge steel every month.

Before shipment we check four lines on every Q550qF certificate: yield and tensile for the actual thickness band, Charpy at −60°C, the CEV or Pcm for the delivery route, and UT results. If one fails, the plate does not ship as Q550qF.

Q550qF is a made-to-order item. We confirm mill capacity, test plan and retest risk in writing before accepting the order.

We also tell buyers when another grade fits better. Neighbouring levels are Q500qF and Q620qF. Browse more structural steel plates and high strength low alloy plates.

FAQ

What is Q550qF steel?
Q550qF is bridge structural steel plate to GB/T 714-2025. It has 550 MPa minimum yield up to 50 mm, 660 MPa minimum tensile, 16% elongation and Charpy V-notch impact of 60 J at −60°C for 12–100 mm plate. It is delivered TMCP, TMCP + tempering, or quenched and tempered.
What impact energy does Q550qF need at −60°C?
GB/T 714-2025 requires at least 60 J at −60°C on longitudinal specimens for Q550qF plate over 12 mm and up to 100 mm. For plate 12 mm and thinner the value is by agreement. F energy rises with strength: 47 J for Q420q and Q460q, 54 J for Q500q, 60 J for Q550q, 69 J for Q620q and 77 J for Q690q.
Is Q550qF the same as Q550F?
No. Q550F is general structural steel (GB/T 1591), while Q550qF is bridge steel to GB/T 714 with lower P and S, controlled weldability index, mandatory UT above 20 mm and 120 J impact for 12–100 mm plate. Bridge plate can replace general plate, not the reverse.
What is the ASTM or EN equivalent of Q550qF?
Close grades for Q550qF: EN 10025-6 S550Q, S550QL, S550QL1 (Annex B). These are close families, not drop-in substitutes; compare yield at thickness, impact temperature and energy, and the weldability index before substituting.
How is Q550qF marked?
Plates are marked per GB/T 247 with grade, heat number, size and mill, and the Z level if ordered, for example Q550qFZ25. The certificate must state the delivery condition (TMCP, TMCP + tempering or QT).
Does steel grade affect fatigue life of a Q550qF bridge girder?
Very little. Fatigue life of welded bridge details is governed by the detail category and stress range, not by yield strength. Higher-strength plate raises working stress, so detailing and weld quality must improve to keep the same fatigue life.

Conclusion

Q550qF to GB/T 714-2025 is bridge plate with 550 MPa minimum yield, 660 MPa minimum tensile and 60 J Charpy at −60°C for 12–100 mm plate.

It sits between Q500qF and Q620qF in the bridge range, with Q550qD and Q550qE as sister letters. Choose the letter from the lowest service or erection temperature, here −60°C, and step up a letter for thick, restrained or fracture-critical members.

With SHH STEEL the Q550qF certificate is complete: heat chemistry, weldability index, yield, tensile, elongation and Charpy, to EN 10204 3.1 or 3.2. Add product analysis, a Z level or a stricter UT class as needed.

We ship from Shanghai to bridge builders worldwide. Browse the full GB/T 714 range or other high strength low alloy plates.

Contact SHH STEEL with your Q550qF requirements. We confirm the mill, delivery route, testing and price before you commit.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X