GB/T 19879

Product Showcase

GB/T 19879 Carbon Steel Plates

SHH STEEL offers GB/T 19879-compliant high-performance steel plates for building structures. GB/T 19879 specifies hot-rolled plates with excellent toughness and weldability for seismic-resistant architecture. Reliable, cost-effective, certified quality, competitive prices, customizable. Trust SHH STEEL!

Q690GJE building steel plate stacks GB/T 19879 inside SHH STEEL warehouse

GB/T 19879 Q690GJE Building Steel Plate Supplier

GB/T 19879 Q690GJE is high-strength building steel plate, quenched and tempered or TMCP, 12–50 mm, with 690 – 860 MPa yield above 20 mm, 770 – 940 MPa tensile, CEV ≤0.60% and 47 J at −40°C. SHH STEEL supplies Q690GJE mill-direct with Z15–Z35 options and full heat and product analysis.
View More
Tall pile of GB/T 19879 Q690GJD building steel plates at SHH STEEL stockyard

GB/T 19879 Q690GJD Building Steel Plate Supplier

GB/T 19879 Q690GJD is high-strength building steel plate, quenched and tempered or TMCP, 12–50 mm, with 690 – 860 MPa yield above 20 mm, 770 – 940 MPa tensile, CEV ≤0.60% and 47 J at −20°C. SHH STEEL supplies Q690GJD mill-direct with Z15–Z35 options and full heat and product analysis.
View More
Q690GJC building steel plate stacks GB/T 19879 lined up at SHH STEEL yard

GB/T 19879 Q690GJC Building Steel Plate Supplier

GB/T 19879 Q690GJC is high-strength building steel plate, quenched and tempered or TMCP, 12–50 mm, with 690 – 860 MPa yield above 20 mm, 770 – 940 MPa tensile, CEV ≤0.60% and 55 J at 0°C. SHH STEEL supplies Q690GJC mill-direct with Z15–Z35 options and full heat and product analysis.
View More
GB/T 19879 Q620GJE building steel plates spread across SHH STEEL stockyard

GB/T 19879 Q620GJE Building Steel Plate Supplier

GB/T 19879 Q620GJE is high-strength building steel plate, quenched and tempered or TMCP, 12–50 mm, with 620 – 770 MPa yield above 20 mm, 730 – 900 MPa tensile, CEV ≤0.58% and 47 J at −40°C. SHH STEEL supplies Q620GJE mill-direct with Z15–Z35 options and full heat and product analysis.
View More
Q620GJD building steel plate stack GB/T 19879 on gravel at SHH STEEL yard

GB/T 19879 Q620GJD Building Steel Plate Supplier

GB/T 19879 Q620GJD is high-strength building steel plate, quenched and tempered or TMCP, 12–50 mm, with 620 – 770 MPa yield above 20 mm, 730 – 900 MPa tensile, CEV ≤0.58% and 47 J at −20°C. SHH STEEL supplies Q620GJD mill-direct with Z15–Z35 options and full heat and product analysis.
View More
GB/T 19879 Q620GJC building steel plate stacks in SHH STEEL open yard

GB/T 19879 Q620GJC Building Steel Plate Supplier

GB/T 19879 Q620GJC is high-strength building steel plate, quenched and tempered or TMCP, 12–50 mm, with 620 – 770 MPa yield above 20 mm, 730 – 900 MPa tensile, CEV ≤0.58% and 55 J at 0°C. SHH STEEL supplies Q620GJC mill-direct with Z15–Z35 options and full heat and product analysis.
View More
Stacked Q550GJE building steel plates GB/T 19879 ready for dispatch at SHH STEEL

GB/T 19879 Q550GJE Building Steel Plate Supplier

GB/T 19879 Q550GJE is high-strength building steel plate, quenched and tempered or TMCP, 12–50 mm, with 550 – 690 MPa yield above 20 mm, 670 – 830 MPa tensile, CEV ≤0.54% and 47 J at −40°C. SHH STEEL supplies Q550GJE mill-direct with Z15–Z35 options and full heat and product analysis.
View More
GB/T 19879 Q550GJD building steel plates laid out in SHH STEEL stockyard

GB/T 19879 Q550GJD Building Steel Plate Supplier

GB/T 19879 Q550GJD is high-strength building steel plate, quenched and tempered or TMCP, 12–50 mm, with 550 – 690 MPa yield above 20 mm, 670 – 830 MPa tensile, CEV ≤0.54% and 47 J at −20°C. SHH STEEL supplies Q550GJD mill-direct with Z15–Z35 options and full heat and product analysis.
View More
Q550GJC building steel plate stack GB/T 19879 in SHH STEEL storage yard

GB/T 19879 Q550GJC Building Steel Plate Supplier

GB/T 19879 Q550GJC is high-strength building steel plate, quenched and tempered or TMCP, 12–50 mm, with 550 – 690 MPa yield above 20 mm, 670 – 830 MPa tensile, CEV ≤0.54% and 55 J at 0°C. SHH STEEL supplies Q550GJC mill-direct with Z15–Z35 options and full heat and product analysis.
View More
Tall stacks of GB/T 19879 Q500GJE building steel plates under SHH STEEL cranes

GB/T 19879 Q500GJE Building Steel Plate Supplier

GB/T 19879 Q500GJE is high-strength building steel plate, quenched and tempered or TMCP, 12–50 mm, with 500 – 640 MPa yield above 20 mm, 610 – 770 MPa tensile, CEV ≤0.52% and 47 J at −40°C. SHH STEEL supplies Q500GJE mill-direct with Z15–Z35 options and full heat and product analysis.
View More
Q500GJD building steel plate stacks GB/T 19879 stored outdoors at SHH STEEL

GB/T 19879 Q500GJD Building Steel Plate Supplier

GB/T 19879 Q500GJD is high-strength building steel plate, quenched and tempered or TMCP, 12–50 mm, with 500 – 640 MPa yield above 20 mm, 610 – 770 MPa tensile, CEV ≤0.52% and 47 J at −20°C. SHH STEEL supplies Q500GJD mill-direct with Z15–Z35 options and full heat and product analysis.
View More
Close view of GB/T 19879 Q500GJC building steel plate pile at SHH STEEL

GB/T 19879 Q500GJC Building Steel Plate Supplier

GB/T 19879 Q500GJC is high-strength building steel plate, quenched and tempered or TMCP, 12–50 mm, with 500 – 640 MPa yield above 20 mm, 610 – 770 MPa tensile, CEV ≤0.52% and 55 J at 0°C. SHH STEEL supplies Q500GJC mill-direct with Z15–Z35 options and full heat and product analysis.
View More

GB/T 19879 Carbon Steel Plates

GB/T 19879 Q690GJE Building Steel Plate Supplier GB/T 19879 Q690GJD Building Steel Plate Supplier GB/T 19879 Q690GJC Building Steel Plate Supplier GB/T 19879 Q620GJE Building Steel Plate Supplier
GB/T 19879 Q620GJD Building Steel Plate Supplier GB/T 19879 Q620GJC Building Steel Plate Supplier GB/T 19879 Q550GJE Building Steel Plate Supplier GB/T 19879 Q550GJD Building Steel Plate Supplier
GB/T 19879 Q550GJC Building Steel Plate Supplier GB/T 19879 Q500GJE Building Steel Plate Supplier GB/T 19879 Q500GJD Building Steel Plate Supplier GB/T 19879 Q500GJC Building Steel Plate Supplier
GB/T 19879 Q460GJE Building Steel Plate Supplier GB/T 19879 Q460GJD Building Steel Plate Supplier GB/T 19879 Q460GJC Building Steel Plate Supplier GB/T 19879 Q460GJB Building Steel Plate Supplier
GB/T 19879 Q420GJE Building Steel Plate Supplier GB/T 19879 Q420GJD Building Steel Plate Supplier GB/T 19879 Q420GJC Building Steel Plate Supplier GB/T 19879 Q420GJB Building Steel Plate Supplier
GB/T 19879 Q390GJE Building Steel Plate Supplier GB/T 19879 Q390GJD Building Steel Plate Supplier GB/T 19879 Q390GJC Building Steel Plate Supplier GB/T 19879 Q390GJB Building Steel Plate Supplier
GB/T 19879 Q345GJE Building Steel Plate Supplier GB/T 19879 Q345GJD Building Steel Plate Supplier GB/T 19879 Q345GJC Building Steel Plate Supplier GB/T 19879 Q345GJB Building Steel Plate Supplier
GB/T 19879 Q235GJE Building Steel Plate Supplier GB/T 19879 Q235GJD Building Steel Plate Supplier GB/T 19879 Q235GJC Building Steel Plate Supplier Q235GJB Building Steel Plate GB/T 19879 Supplier
High-Strength Low Alloy Plates supplier- shh steel China mill

High-Strength Low Alloy Plates

SHH STEEL, a leading High-Strength Low Alloy Plates exporter, produces and exports HSLA steel plates for construction, bridges, and automotive applications. Our plates, like ASTM A572 Grade 50, offer superior strength-to-weight ratios and excellent weldability, meeting global standards. With a 5,000-ton inventory, we ensure 3–5 day delivery for in-stock items, supported by SGS/TUV inspections and mill certificates. Trust SHH STEEL for durable high-strength low alloy plates and custom solutions for structural projects.

High-Strength Low Alloy Plates

SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

    *

    *

    *

    *


    X