GB/T 714 Q500qNHE Weathering Bridge Steel Supplier
What is GB/T 714 Q500qNHE Weathering Bridge Steel?
Q500qNHE is weathering bridge structural steel to GB/T 714. In the standard’s own notation it is written Q500qENH: Q for yield, 500 for the minimum yield in MPa, q for qiao (bridge), the quality letter, and NH for nai hou, weathering. The letter E means Charpy V-notch testing at −40°C.
Q500qNH is the strongest weathering bridge grade on our list, with a richer Cr-Ni-Cu band for heavy unpainted members. Q500qNH moves to Cr 0.45–0.70%, Ni 0.30–0.45%, Cu 0.25–0.55% and Mo ≤0.25%, which supports both strength and the weathering index. Pcm is capped at 0.24% to 50 mm.
Q500qNHE (Q500qENH) gives 500 MPa yield, 120 J at −40°C and weathering chemistry. It is used for heavily loaded unpainted members on long-span bridges in cold regions.
GB/T 714-2025, in force since 1 May 2026, fully replaces GB/T 714-2015; the changes for weathering grades are listed below.
SHH STEEL (Shanghai Shenghonghe Import & Export Co., Ltd.) is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. We ship Q500qNHE cut to size with an EN 10204 3.1 or 3.2 certificate. Sister grades are listed under GB/T 714; other unpainted options are under weathering steel plates and EN 10025-5.
Material Specification
| Specification element | Requirement | SHH STEEL compliance |
|---|---|---|
| Standard | GB/T 714-2025 Q500qENH | Confirmed |
| Product | Single-rolled plate ≤150 mm; hot-rolled strip and cut plate ≤25.4 mm | Plate |
| Thickness with tensile values | Up to 130 mm for Q500qNH | Confirmed |
| Minimum yield ReL | 500 MPa ≤50 mm; 480 MPa >50–100 mm | Confirmed |
| Minimum tensile Rm | 630 MPa ≤100 mm (no upper limit in the standard) | Confirmed |
| Elongation A | ≥ 18% | Confirmed |
| Charpy V-notch | −40°C, 120 J (12–100 mm), longitudinal | Confirmed |
| Weathering index | I ≥ 6.0 (Table 5, footnote c) | Calculated on MTC |
| Delivery condition | TMCP or TMCP + tempering | As ordered |
| Weldability index | Pcm (Table 8) | Printed on MTC |
| Ultrasonic testing | Plate >20 mm: GB/T 2970, Class II or better | Every plate |
| Through-thickness | Z15, Z25 or Z35 to GB/T 5313, when ordered | As ordered |
| Dimensions | GB/T 709 | Confirmed |
| Certificate | GB/T 247; EN 10204 3.1 or 3.2 | As ordered |
Grades often compared with Q500qNHE are ASTM A709 HPS 70W and EN 10025-4 S460ML; the comparison below shows where they differ.
Chemical Composition: Heat Analysis and Product Analysis
A check analysis on finished plate often reads a few hundredths higher than the mill certificate. That is not automatically a failure. The certificate shows the heat (ladle) analysis; plate drilled after rolling is judged as product analysis, with the tolerances of GB/T 222.
Table 1 below is the heat (ladle) analysis for Q500qNHE from GB/T 714-2025 Tables 1, 5.
| Element | Q500qNHE heat analysis (%) | Note |
|---|---|---|
| C, max | 0.11 | |
| Si | 0.15 – 0.50 | Counts in I |
| Mn | 1.10 – 1.50 | Min 0.50% for coil only |
| P, max | 0.020 | Letter E |
| S, max | 0.010 | Letter E |
| Cu | 0.25 – 0.55 | Main weathering element |
| Cr | 0.45 – 0.70 | Weathering element |
| Ni | 0.30 – 0.45 | Weathering element |
| Mo, max | 0.25 | |
| Nb | 0.010 – 0.100 | Microalloy (see note) |
| V | 0.010 – 0.100 | Microalloy (see note) |
| Ti | 0.006 – 0.030 | Microalloy (see note) |
| Als | 0.015 – 0.050 | Alt 0.020–0.055% if total Al is used |
| N, max | 0.0080 | |
| B, max (residual) | 0.0005 | ≤0.0014% if C ≤0.06% |
| H, max (residual) | 0.0002 | |
| Weathering index I | ≥ 6.0 | Calculated from heat analysis |
Nb, V, Ti and Al may be added singly or together. Added singly, each must meet the range above; added together, at least one must reach its minimum and Nb + V + Ti ≤ 0.22%. Calcium treatment is required to control sulfide shape.
Table 2 is the product analysis: the limits a check analysis on finished plate is judged against. GB/T 714-2025 clause 7.1.3 calls up GB/T 222 for the permitted deviations.
| Element | Heat limit (%) | Deviation, GB/T 222-2025 Table 1 | Q500qNHE product analysis (%) |
|---|---|---|---|
| C | ≤ 0.11 | +0.02 | ≤ 0.13 |
| Si | 0.15 – 0.50 | ±0.05 | 0.10 – 0.55 |
| Mn | 1.10 – 1.50 | ±0.06 | 1.04 – 1.56 |
| P | ≤ 0.020 | +0.005 | ≤ 0.025 |
| S | ≤ 0.010 | +0.005 | ≤ 0.015 |
| V | 0.010 – 0.100 | +0.02 / −0.01 | ≤ 0.120 |
| Ti | 0.006 – 0.030 | +0.02 / −0.01 | ≤ 0.050 |
| Nb | 0.010 – 0.100 | ±0.005 (listed for 0.015–0.060%) | Above 0.060%: agree in contract |
| Cu | 0.25 – 0.55 | ±0.05 | 0.20 – 0.60 |
| Cr | 0.45 – 0.70 | ±0.05 | 0.40 – 0.75 |
| Ni | 0.30 – 0.45 | ±0.05 | 0.25 – 0.50 |
| Als | 0.015 – 0.050 | ±0.003 | Lower limit −0.003 (Table 1 row is for Al ≥0.015%; confirm) |
| Mo | ≤ 0.25 | Not listed in Table 1 | Agree in contract |
| N | ≤ 0.0080 | Listed only for 0.010–0.020% | Agree in contract |
How to read Table 2. Weathering bridge steel is normally classed as low-alloy steel, so Table 1 of GB/T 222 applies. Where the heat limit is a range, the deviation applies to both ends; for one heat, an element may deviate in one direction only.
Mechanical Properties
Tensile values follow Table 9 of GB/T 714-2025 for Q500qNH. Tensile specimens are transverse; round specimens are used above 40 mm. Where yield is not distinct, Rp0.2 replaces ReL.
| Nominal thickness | ReL min (MPa) | Rm min (MPa) | A min |
|---|---|---|---|
| ≤ 50 mm | 500 | 630 | 18% |
| > 50 – 100 mm | 480 | 630 | 18% |
| > 100 – 130 mm | 450 | 560 | 18% |
Impact values follow Table 10, on longitudinal specimens, average of three:
| Letter / test temperature | KV2 ≤12 mm | KV2 >12 – 100 mm | KV2 >100 – 150 mm |
|---|---|---|---|
| E / −40°C | 80 J | 120 J | 31 J |
One single value may fall below the required average, but not below 70% of it. Plate over 8 mm and under 12 mm is tested with 7.5 mm specimens (75% of the value); 6–8 mm plate with 5 mm specimens (50%). Plate under 6 mm is not impact tested.
180° bend test, transverse: mandrel D = 2a up to 16 mm and 3a above 16 mm; may be omitted when the mill guarantees it. Yield ratio is not mandatory. If the contract asks for it, Annex C recommends ReL/Rm ≤ 0.88 up to 12 mm and ≤ 0.86 above 12 mm for TMCP plate.
Q500qNHD / Q500qNHE / Q500qNHF: Which Quality Grade?
Q500qNHE is tested at −40°C. It suits bridges in north-east China, Inner Mongolia, Xinjiang, Russia, Kazakhstan, Canada and high-altitude sites, and for thick, restrained members anywhere. E is tested at −40°C, with P ≤0.020% and S ≤0.010%. Many long-span bridges specify E even in mild climates, because thick plate and heavy welding raise the risk of brittle fracture.
| Grade | Test temp. | KV2 ≤12 mm | KV2 12–100 mm | KV2 >100 mm | P / S max (%) |
|---|---|---|---|---|---|
| Q500qNHD | −20°C | 80 J | 120 J | 47 J | 0.025 / 0.015 |
| Q500qNHE | −40°C | 80 J | 120 J | 31 J | 0.020 / 0.010 |
| Q500qNHF | −60°C | By agreement | 54 J | — | 0.015 / 0.006 |
Over-specifying the letter costs money; under-specifying it costs safety. Choose from the lowest service or erection temperature, then step up one letter for thick, restrained or fracture-critical members.
Q500qNHE: What Changed from GB/T 714-2015 to GB/T 714-2025
For Q500qNHE buyers the 2025 edition changes more than the year on the certificate. The points below come from the foreword of GB/T 714-2025 and its tables.
- The weathering requirement changed: Table 5 now requires a corrosion index I ≥ 6.0, and the 2015 Annex C guide for assessing weathering resistance was deleted.
- A Pcm table for weathering steel (Table 8) was added.
- Annex A now gives reference bridge-site environments for unpainted use (chloride, SO₂ and time-of-wetness limits).
- Yield values above 100 mm were added for Q500qNH (450 MPa for >100–130 mm).
- Tensile strength is now banded by thickness (e.g. lower minimum Rm above 100 mm) instead of one value.
- Impact energy is set by thickness band (≤12 mm, 12–100 mm, >100 mm) in Table 10.
- Yield ratio is no longer a clause value; it is agreed in the contract, with recommendations in informative Annex C.
If a drawing cites 2015 and the plate is made to 2025, get the designer’s written acceptance; tensile strength above 100 mm and the yield-ratio basis differ.
Q500qNHE vs ASTM A709 and EN 10025: Which Grade Matches?
Can Q500qNHE replace a US or European bridge grade, or the other way round? Strength can match; toughness rules differ in kind, not only in number.
| Property | Q500qNHE | ASTM A709 HPS 70W | EN 10025-4 S460ML |
|---|---|---|---|
| Min. yield (MPa) | 500 (≤50 mm) | 485 | 460 (≤16 mm) |
| Tensile (MPa) | 630 min | 585 – 760 | 540 – 720 |
| Charpy | 120 J at −40°C (12–100 mm) | CVN by temperature zone; fracture-critical (F) levels | 27 J at −50°C |
| Weathering chemistry | Yes, I ≥ 6.0 | Yes | No |
ASTM A709 sets Charpy requirements by temperature zone (1, 2, 3) and by member type: non-fracture-critical (T) or fracture-critical (F). GB/T 714 sets one value per letter, so compare the A709 zone with the GB/T 714 test temperature, not grade with grade.
EN 10025-5 weathering grades are general structural steels without a bridge-specific toughness level of 120 J; they suit many bridges but are not a one-to-one match.
The 120 J requirement for 12–100 mm plate is several times the 27–40 J typical of general weathering grades such as ASTM A588 or Corten A/B plate, which is why bridge owners specify Q500qNHE.
Q500qNHE Atmospheric Corrosion Index I and Unpainted Bridges
GB/T 714-2025 Table 5, footnote c, requires every Q500qNHE heat to reach an atmospheric corrosion index I of at least 6.0, calculated from the heat analysis:
I = 26.01(%Cu) + 3.88(%Ni) + 1.20(%Cr) + 1.49(%Si) + 17.28(%P) − 7.29(%Cu)(%Ni) − 9.10(%Ni)(%P) − 33.39(%Cu)²
This is the same predictive formula used with ASTM G101 for ASTM A709 Grade 50W and ASTM A709 HPS 70W, which makes Chinese and US ASTM A709 weathering steel plates easy to compare with Q500qNHE.
| Worked example (our calculation) | Cu | Ni | Cr | Si | P | I |
|---|---|---|---|---|---|---|
| All weathering elements at their Table 5 minimum | 0.25 | 0.30 | 0.45 | 0.15 | 0.010 | 5.94 |
| Illustrative mid-range heat | 0.32 | 0.36 | 0.55 | 0.30 | 0.012 | 6.74 |
Note the first row: a heat that only just meets every Table 5 minimum can still fall short of I = 6.0. That is why we ask the mill to print I on every Q500qNHE certificate, not just the chemistry.
Where can the steel be left unpainted? Annex A of GB/T 714-2025 gives reference bridge-site conditions:
- Rural or urban atmosphere with annual chloride deposition ≤ 3 mg/(m²·d)
- Annual SO₂ deposition ≤ 24 mg/(m²·d)
- Time of wetness ≤ 5,256 h per year (temperature above 0°C and relative humidity above 80%)
- Coastal sites only if they meet the same limits; for marine atmospheres Annex D points to T/CISA 073
Before omitting paint on Q500qNHE, measure or estimate chloride and SO₂ deposition at the site. One year of monitoring is a small cost against a bridge life of 100 years.
Welding Q500qNHE and Fatigue in Bridge Girders
GB/T 714-2025 clause 7.1.2 uses CEV for normalized, QT and TMCP steel with C >0.12%, and Pcm for weathering steel and TMCP steel with C ≤0.12%, both from the heat analysis:
CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15
Pcm = C + Si/30 + Mn/20 + Cu/20 + Ni/60 + Cr/20 + Mo/15 + V/10 + 5B
| Index | ≤50 mm | >50–100 mm | >100–130 mm |
|---|---|---|---|
| Pcm, Q500qNH (Table 8) | ≤ 0.24 | ≤ 0.26 | By agreement |
On thick Q500qNHE flanges, preheat, interpass control and low-hydrogen practice matter more than the grade itself. The certificate gives the data to set them. At −40°C, HAZ toughness often becomes the limit. Fabricators usually cap heat input and qualify the procedure at −40°C on plate from the same route.
Typical consumables for Q500qNHE: weathering-matched Ni-Cu consumables (AWS E8018-W2 type for 345–420 MPa), with higher-strength weathering wires for 460–500 MPa.
Fatigue. Welded details govern fatigue life in a bridge, and their fatigue strength is set by detail category, not by yield strength. Higher-strength plate can carry higher stress ranges only if detailing improves too.
Fatigue design follows JTG D64 (highway) and TB 10091 (railway) in China, EN 1993-1-9 in Europe and AASHTO LRFD in the US; fabrication commonly follows TB 10212, JTG/T 3650 or AWS D1.5.
Q500qENHZ15, Z25 and Z35: Through-Thickness Plate for Bridges
A Z grade is cheap insurance for heavily restrained joints. It caps sulfur and proves reduction of area in the thickness direction with a short-transverse tensile test.
GB/T 714 adds the Z level to the end of the designation, for example Q500qENHZ25. The test and acceptance follow GB/T 5313 and apply to plate 15 mm and thicker.
| Z grade | Heat sulfur, max (%) | Reduction of area, avg / single (%) |
|---|---|---|
| Z15 | 0.010 | 15 / 10 |
| Z25 | 0.007 | 25 / 15 |
| Z35 | 0.005 | 35 / 25 |
E chemistry already limits S to 0.010%, the Z15 sulfur cap. Z25 (S ≤0.007%) and Z35 (S ≤0.005%) still need a cleaner heat.
Most bridges need Z on a small share of the tonnage. Mark it item by item on the cutting list rather than on the whole Q500qNHE order. Z options apply across the GB/T 714 bridge steel range.
Equivalent Material Grades
Annex B of GB/T 714-2025 lists foreign grades against each strength level. It is informative: it tells you which families are close, not that the plates are interchangeable.
| Standard | Grade(s) | Fit for Q500qNHE |
|---|---|---|
| ASTM A709 | ASTM A709 HPS 70W | Listed against Q460q in Annex B |
| EN 10025-4 | EN 10025-4 S460ML | Strength match, not weathering |
| EN 10025-6 | EN 10025-6 S460QL | QT, not weathering |
| GB/T 714 (painted twin) | Q500qE | Same strength, no weathering elements |
For weathering grades also compare the corrosion index basis. Q500qNHE requires I ≥ 6.0 by the formula above; check that the substitute is assessed on the same basis.
Q500qNHE Testing, UT and Certificate
A batch of Q500qNHE is one grade, one heat, one thickness, one rolling schedule and one heat-treatment condition, up to 60 t. Table 12 of GB/T 714-2025 sets the tests:
| Test | Frequency | Method |
|---|---|---|
| Heat analysis | 1 per heat | GB/T 20066; GB/T 4336 / GB/T 223 |
| Weathering index I | Calculated per heat | Table 5 formula |
| Tensile | 1 per batch | GB/T 2975 / GB/T 228.1 |
| Bend 180° | 1 per batch (may be waived if guaranteed) | GB/T 232 |
| Charpy V at −40°C | 3 specimens per batch | GB/T 229 |
| Through-thickness (Z) | 3 specimens per batch, when ordered | GB/T 5313 |
| Ultrasonic | Every plate >20 mm, Class II or better | GB/T 2970 |
| Surface and dimensions | Every plate | Visual and gauges |
Impact retest: if a set fails, three more specimens are taken from the same batch. The average of all six must meet the requirement; two values may be below it, but only one below 70%. At −40°C, retest risk rises on heavy plate; we build a margin for retests into the delivery schedule.
Dimensions
Common Q500qNHE sizes:
- Thickness: 6 mm – 130 mm under GB/T 714 tensile tables; most orders 10 – 80 mm
- Width: 1500 – 4000 mm, depending on mill and thickness
- Length: 6000 – 18000 mm; longer by enquiry
- Edge: mill edge or cut edge
- Weight: theoretical, 7.85 g/cm³
Deck plate, webs, flanges, diaphragms and stiffeners are cut to drawing. For U-ribs and rolled sections on the same bridge, see steel beam profiles and steel structural profiles.
Tolerances
GB/T 709 governs Q500qNHE thickness, width, length and flatness. Under Class B, plate may be up to 0.30 mm thin; the plus side grows with thickness and width.
| Nominal thickness (mm) | Width ≤ 1500 mm | Width > 1500 – 2500 mm |
|---|---|---|
| > 8 – 15 | −0.30 / +0.80 | −0.30 / +1.00 |
| > 15 – 25 | −0.30 / +1.00 | −0.30 / +1.20 |
| > 25 – 40 | −0.30 / +1.10 | −0.30 / +1.30 |
| > 40 – 60 | −0.30 / +1.30 | −0.30 / +1.50 |
| > 60 – 100 | −0.30 / +1.50 | −0.30 / +1.80 |
| > 100 – 150 | −0.30 / +2.10 | −0.30 / +2.50 |
Bridge fabricators often ask for Class C (zero minus) on deck and flange plate so section properties are never under the design value. Wider plates follow the heavier GB/T 709 rows; we state them on the offer.
Q500qNHE Price Factors and How to Order
A Q500qNHE price per ton is a base price plus extras. The extras explain most gaps between quotes.
| Cost driver | Effect on price |
|---|---|
| Strength level Q500q | Higher levels need more alloy and tighter rolling control |
| Quality letter | Higher extra: −40°C testing, S ≤0.010%, more retest risk |
| Weathering alloys | Cu, Cr, Ni additions and I-index control add a weathering extra |
| Delivery route | TMCP / TMCP+T |
| Thickness | Over 60 mm and under 10 mm carry size extras |
| Z15 / Z25 / Z35 | Low-sulfur heat, Z test, UT; Z35 costs most |
| Width and length | Over 3000 mm wide or 15 m long needs mill confirmation |
| Quantity per size | Mill minimums per heat and size |
| Inspection and processing | 3.2 witness, profile cutting, blasting, priming quoted per item |
To get a firm quote in one round, send:
- Grade, edition and Z level, e.g. Q500qENHZ25 to GB/T 714-2025
- Thickness × width × length and pieces or tonnes
- Delivery route and UT class if beyond Class II
- Certificate type and inspector
- Destination port and Incoterm
We quote plate price, extras and freight line by line. Need another letter? See Q500qNHD, Q500qNHF.
Applications
| Sector | Typical Q500qNHE components |
|---|---|
| Unpainted highway bridges | Plate girders and box girders in rural and urban atmospheres |
| Railway bridges | Truss members, plate girders, bracing |
| Remote and mountain sites | Bridges where repainting access is difficult or costly |
| Urban viaducts | Exposed girders with architectural rust finish |
| Pedestrian bridges | Unpainted box sections |
The letter E suits bridges in north-east China, Inner Mongolia, Xinjiang, Russia, Kazakhstan, Canada and high-altitude sites, and for thick, restrained members anywhere.
Q500qNHE is the wrong plate for marine splash zones, tunnels, sites with heavy de-icing salt spray, or members that stay wet. There, use painted Q500qE or look at marine-atmosphere grades under T/CISA 073.
Supply Capability and Global Delivery
SHH STEEL sources Q500qNHE from first-line bridge-plate mills, including drafters of GB/T 714-2025 such as Ansteel, Valin Xiangtan, Jiangyin Xingcheng, Wuyang, Shougang and Xinyu.
- Certificates: EN 10204 3.1 standard; 3.2 with third-party witness (SGS, BV, TÜV or owner’s inspector)
- Tests: tensile, −40°C Charpy, bend, Z test, UT, product analysis, weathering index
- Processing: CNC plasma and flame cutting, bevelling, drilling, shot blasting and priming (or blasting only, for unpainted weathering steel)
- Terms: FOB Shanghai, CFR, CIF; TT, LC or TT + LC
- Marking: steel-stamped and paint-marked with grade, heat, size and mill, per GB/T 247
Q500qNHE goes from Shanghai to bridge sites and fabrication yards worldwide, usually as break-bulk for long plates.
Lead time: about 45–60 days from mill rolling; Z35, F letter or 3.2 inspection adds about 1–2 weeks. Sea time from Shanghai is about 7–12 days to Southeast Asia and 28–35 days to North Europe.
Why Choose SHH STEEL
SHH STEEL is mill-direct: steel manufacturer and exporter and global steel mill sourcing partner, China origin. Every Q500qNHE plate we ship carries the original mill heat number.
Before shipment we check four lines on every Q500qNHE certificate: yield and tensile for the actual thickness band, Charpy at −40°C, the Pcm and weathering index, and UT results. If one fails, the plate does not ship as Q500qNHE.
For Q500qNHE we recommend a weld procedure test at the lowest design temperature, not just at the impact letter.
We also tell buyers when another grade fits better. Neighbouring levels are Q460qNHE. The painted counterpart is Q500qE. Browse more structural steel plates and high strength low alloy plates.
FAQ
-
What is Q500qNHE steel?
- Q500qNHE (Q500qENH) is weathering bridge steel plate to GB/T 714-2025. It has 500 MPa minimum yield up to 50 mm, 630 MPa minimum tensile, Charpy impact of 120 J at −40°C for 12–100 mm plate, and Cu-Cr-Ni chemistry with a corrosion index I of at least 6.0 for unpainted bridges.
-
What is the difference between Q500qNHE and Q500qNHD?
- Strength and chemistry box are the same. Q500qNHE is Charpy tested at −40°C, Q500qNHD at −20°C, both needing 120 J for 12–100 mm plate. P/S caps are 0.020/0.010% for E and 0.025/0.015% for D. Choose by the lowest service or erection temperature.
-
Is Q500q bridge steel TMCP or quenched and tempered?
- Both are allowed by GB/T 714-2025. TMCP Q500q has C ≤0.11% and is judged by Pcm (≤0.23% to 50 mm); QT Q500q is judged by CEV (≤0.50% to 50 mm, ≤0.55% to 100 mm). The route must be stated on the order and the certificate.
-
What is the ASTM or EN equivalent of Q500qNHE?
- Close grades for Q500qNHE: No direct equivalent in Annex B / closest: ASTM A709 HPS 70W (485 MPa). These are close families, not drop-in substitutes; compare yield at thickness, impact temperature and energy, and the weldability index before substituting.
-
How is Q500qNHE marked?
- Plates are marked per GB/T 247 with grade, heat number, size and mill, and the Z level if ordered, for example Q500qENHZ25. The certificate must state the delivery condition (TMCP, TMCP + tempering or QT).
-
What is the weathering index I in GB/T 714?
- It is a corrosion index calculated from the heat analysis: I = 26.01Cu + 3.88Ni + 1.20Cr + 1.49Si + 17.28P − 7.29Cu·Ni − 9.10Ni·P − 33.39Cu². GB/T 714-2025 requires I ≥6.0 for every weathering grade, the same basis ASTM G101 uses for A709 weathering steels.
Conclusion
Q500qNHE to GB/T 714 is weathering bridge steel with 500 MPa minimum yield, Cu-Cr-Ni chemistry, a weathering index of at least 6.0 and 120 J Charpy at −40°C for 12–100 mm plate.
The next strength level is Q460qNHE, with Q500qNHD and Q500qNHF as sister letters. For Q500qNHE, the deciding numbers on the certificate are yield at the actual thickness, Charpy at −40°C and the weldability index for the delivery route.
Our Q500qNHE certificates carry heat chemistry, weldability index, tensile and Charpy data to EN 10204 3.1 or 3.2. SHH STEEL can add product analysis, Z15–Z35 and witness inspection.
We ship from Shanghai to bridge builders worldwide. Browse the full GB/T 714 range or other weathering steel plates.
Tell us the sizes, tonnage and any Z, UT or inspection needs. We check the request against GB/T 714 first, then confirm mill, route, lead time and price. Contact SHH STEEL today for Q500qNHE weathering bridge steel.