GB/T 714 Q460qE bridge steel plate stacked at SHH STEEL warehouse

GB/T 714 Q460qE Bridge Steel Plate Supplier

GB/T 714 Q460qE is bridge structural steel plate with 460 MPa minimum yield, 570 MPa minimum tensile and Charpy V-notch impact of 120 J at −40°C for 12–100 mm plate. SHH STEEL supplies Q460qE mill-direct, TMCP / TMCP+T, up to 130 mm, with Z15–Z35, UT and heat and product analysis.
Keywords
Q460qE, Q460qE steel plate, GB/T 714 Q460qE, Q460q-E, Q460q E, Q460qE bridge steel, Q460qEZ15, Q460qEZ25, Q460qEZ35, bridge steel plate, Q460qE supplier
Equivalent Grades:
ASTM A709 HPS 70W / EN 10025-4 S460M, S460ML / EN 10025-6 S460Q, S460QL, S460QL1 (Annex B) — Material Specification: GB/T 714-2025 (supersedes GB/T 714-2015) — Delivery: TMCP / TMCP+T
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Q460q Quality Grades
GB/T 714-2025 vs 2015
Q460qE vs ASTM A709 / EN 10025
TMCP vs Normalized vs QT
Welding and Fatigue
Z15 / Z25 / Z35
Equivalent Material Grades
Testing and Inspection
Dimensions
Tolerances
Price and Ordering
Applications
Supply Capability
Why Choose SHH STEEL
FAQ
Conclusion

What is GB/T 714 Q460qE Bridge Steel Plate?

Q460qE is bridge structural steel plate to GB/T 714. Q stands for yield, 460 is the minimum yield in MPa for plate up to 50 mm, q stands for qiao (bridge) and E is the quality grade: Charpy V-notch at −40°C on longitudinal specimens.

Q460q is high-strength TMCP plate for main load paths on long-span bridges, where 460 MPa yield cuts flange thickness and weld volume. Annex B of GB/T 714-2025 lists ASTM A709 HPS 70W against Q460q. In practice, Q460q is chosen where Q420q flanges would exceed about 50–60 mm and welding cost starts to dominate.

Q460qE is widely used on long-span road-rail bridges for main truss chords and node plates: 460 MPa yield and 120 J at −40°C from 12 to 100 mm, with 31 J required above 100 mm.

Since 1 May 2026, the valid edition is GB/T 714-2025, which fully replaced GB/T 714-2015. The changes matter for buyers: tensile strength now drops by thickness band, impact energy is set by thickness, and the yield ratio moved to an informative annex.

SHH STEEL (Shanghai Shenghonghe Import & Export Co., Ltd.) is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. We ship Q460qE cut to size with an EN 10204 3.1 or 3.2 certificate. Sister grades are listed under GB/T 714.

Material Specification

Specification element Requirement SHH STEEL compliance
Standard GB/T 714-2025 Q460qE Confirmed
Product Single-rolled plate ≤150 mm; hot-rolled strip and cut plate ≤25.4 mm Plate
Thickness with tensile values Up to 130 mm for Q460q Confirmed
Minimum yield ReL 460 MPa ≤50 mm; 450 MPa >50–100 mm Confirmed
Minimum tensile Rm 570 MPa ≤100 mm (no upper limit in the standard) Confirmed
Elongation A ≥ 18% Confirmed
Charpy V-notch −40°C, 120 J (12–100 mm), longitudinal Confirmed
Delivery condition TMCP or TMCP + tempering As ordered
Weldability index Pcm (Table 7) Printed on MTC
Ultrasonic testing Plate >20 mm: GB/T 2970, Class II or better Every plate
Through-thickness Z15, Z25 or Z35 to GB/T 5313, when ordered As ordered
Dimensions GB/T 709 Confirmed
Certificate GB/T 247; EN 10204 3.1 or 3.2 As ordered

Grades often compared with Q460qE are ASTM A709 HPS 70W, EN 10025-4 S460M and EN 10025-4 S460ML; the comparison below shows where they differ.

Chemical Composition: Heat Analysis and Product Analysis

Read the Q460qE certificate with two tables in mind: heat limits from GB/T 714 and product limits from GB/T 222. A plate can pass one and be argued over in the other if the basis is not written into the contract.

Table 1 below is the heat (ladle) analysis for Q460qE from GB/T 714-2025 Tables 1, 3.

Element Q460qE TMCP (%)
C, max 0.11
Si, max 0.55
Mn 0.80 – 1.70
P, max 0.020
S, max 0.010
Nb 0.010 – 0.090
V 0.010 – 0.080
Ti 0.006 – 0.030
Als 0.010 – 0.045
Cr, max 0.50
Ni, max 0.30
Cu, max 0.30
Mo, max 0.25
N, max 0.0080
B, max 0.0005 residual (≤0.0014 if C ≤0.10%)
H, max 0.0002

Nb, V, Ti and Al may be added singly or together. Added singly, each must meet the range above; added together, at least one must reach its minimum and Nb + V + Ti ≤ 0.22%.

Table 2 is the product analysis: the limits a check analysis on finished plate is judged against. GB/T 714-2025 clause 7.1.3 calls up GB/T 222 for the permitted deviations.

Element Heat limit (%) Deviation, GB/T 222-2025 Table 1 Q460qE product analysis (%)
C ≤ 0.11 +0.02 ≤ 0.13
Si ≤ 0.55 +0.05 ≤ 0.60
Mn 0.80 – 1.70 ±0.06 0.74 – 1.76
P ≤ 0.020 +0.005 ≤ 0.025
S ≤ 0.010 +0.005 ≤ 0.015
V 0.010 – 0.080 +0.02 / −0.01 ≤ 0.100
Ti 0.006 – 0.030 +0.02 / −0.01 ≤ 0.050
Nb 0.010 – 0.090 ±0.005 (listed for 0.015–0.060%) Above 0.060%: agree in contract
Cr ≤ 0.50 +0.05 ≤ 0.55
Ni ≤ 0.30 +0.05 ≤ 0.35
Cu ≤ 0.30 +0.05 ≤ 0.35
Als 0.010 – 0.045 ±0.003 Lower limit −0.003 (Table 1 row is for Al ≥0.015%; confirm)
Mo ≤ 0.25 Not listed in Table 1 Agree in contract
N ≤ 0.0080 Listed only for 0.010–0.020% Agree in contract

How to read Table 2. Q460q TMCP heats are low-alloy steel, so Table 1 of GB/T 222 applies. Si ≤0.55% is above 0.37%, so +0.05% applies; Mn falls in the 0.80–1.70% band, so ±0.06%. For one heat, an element may deviate in one direction only.

Mechanical Properties

Tensile values follow Table 9 of GB/T 714-2025 for Q460q. Tensile specimens are transverse; round specimens are used above 40 mm. Where yield is not distinct, Rp0.2 replaces ReL.

Nominal thickness ReL min (MPa) Rm min (MPa) A min
≤ 50 mm 460 570 18%
> 50 – 100 mm 450 570 18%
> 100 – 130 mm 385 490 18%

Impact values follow Table 10, on longitudinal specimens, average of three:

Letter / test temperature KV2 ≤12 mm KV2 >12 – 100 mm KV2 >100 – 150 mm
E / −40°C 80 J 120 J 31 J

One single value may fall below the required average, but not below 70% of it. Plate over 8 mm and under 12 mm is tested with 7.5 mm specimens (75% of the value); 6–8 mm plate with 5 mm specimens (50%). Plate under 6 mm is not impact tested.

180° bend test, transverse: mandrel D = 2a up to 16 mm and 3a above 16 mm; may be omitted when the mill guarantees it. Yield ratio is not mandatory. If the contract asks for it, Annex C recommends ReL/Rm ≤ 0.88 up to 12 mm and ≤ 0.86 above 12 mm for TMCP plate.

Q460qD / Q460qE / Q460qF: Which Quality Grade?

Q460qE is tested at −40°C. It suits bridges in north-east China, Inner Mongolia, Xinjiang, Russia, Kazakhstan, Canada and high-altitude sites, and for thick, restrained members anywhere. E is tested at −40°C, with P ≤0.020% and S ≤0.010%. Many long-span bridges specify E even in mild climates, because thick plate and heavy welding raise the risk of brittle fracture.

Grade Test temp. KV2 ≤12 mm KV2 12–100 mm KV2 >100 mm P / S max (%)
Q460qD −20°C 80 J 120 J 47 J 0.025 / 0.015
Q460qE −40°C 80 J 120 J 31 J 0.020 / 0.010
Q460qF −60°C By agreement 47 J — 0.015 / 0.006

Over-specifying the letter costs money; under-specifying it costs safety. Choose from the lowest service or erection temperature, then step up one letter for thick, restrained or fracture-critical members.

Q460qE: What Changed from GB/T 714-2015 to GB/T 714-2025

For Q460qE buyers the 2025 edition changes more than the year on the certificate. The points below come from the foreword of GB/T 714-2025 and its tables.

  • Yield values above 100 mm were added (385 MPa for >100–130 mm).
  • The Mn range for TMCP steel was revised: the minimum is now 0.80%, and the maximum may be raised to 2.00% by agreement.
  • CEV and Pcm limits were revised (Tables 6 and 7).
  • Tensile strength is now banded by thickness (e.g. lower minimum Rm above 100 mm) instead of one value.
  • Impact energy is set by thickness band (≤12 mm, 12–100 mm, >100 mm) in Table 10.
  • Yield ratio is no longer a clause value; it is agreed in the contract, with recommendations in informative Annex C.
  • Section products were removed; the standard now covers plate and strip only.
  • Delivery is TMCP, TMCP + tempering or QT; normalizing is kept only for Q345q/Q370q plate over 100 mm by agreement.

If a drawing cites 2015 and the plate is made to 2025, get the designer’s written acceptance; tensile strength above 100 mm and the yield-ratio basis differ.

Q460qE vs ASTM A709 and EN 10025: Which Grade Matches?

Can Q460qE replace a US or European bridge grade, or the other way round? Strength can match; toughness rules differ in kind, not only in number.

Property Q460qE ASTM A709 HPS 70W EN 10025-4 S460M EN 10025-4 S460ML
Min. yield (MPa) 460 (≤50 mm) 485 460 (≤16 mm) 460 (≤16 mm)
Tensile (MPa) 570 min 585 – 760 540 – 720 540 – 720
Charpy 120 J at −40°C (12–100 mm) CVN by temperature zone; fracture-critical (F) levels 40 J at −20°C 27 J at −50°C
Weathering chemistry No Yes No No

ASTM A709 sets Charpy requirements by temperature zone (1, 2, 3) and by member type: non-fracture-critical (T) or fracture-critical (F). GB/T 714 sets one value per letter, so compare the A709 zone with the GB/T 714 test temperature, not grade with grade.

EN 10025-3/-4/-6 grades show yield at the thinnest band; their values fall with thickness. GB/T 714 keeps 460 MPa to 50 mm. EN tensile ranges have upper limits; GB/T 714 gives minimums only.

The 120 J requirement in GB/T 714 for 12–100 mm plate is several times the 27–40 J typical of general structural grades. That margin is the main reason bridge owners specify Q460qE rather than GB/T 1591 plate.

Q460qE Delivery Condition: TMCP vs Normalized vs Quenched and Tempered

GB/T 714-2025 clause 3.2 defines TMCP as rolling with the final deformation in a controlled temperature range, including accelerated cooling with or without tempering (self-tempering included) but excluding direct quenching and quench-and-temper. The delivery route must be stated on the certificate.

Route Available for Q460qE Weldability index Notes
TMCP Yes, standard Pcm (C ≤0.11%) Up to 130 mm
TMCP + tempering Yes Same as TMCP Common on thick or E/F plate
Normalized No — Dropped in 2025 for this level
Quenched and tempered Not listed — Use GB/T 16270 if QT is required

Q460q is TMCP or TMCP + tempering. If a project insists on QT, GB/T 16270 Q460 grades are the alternative, with different toughness rules. For E-letter plate over about 50 mm, many mills add tempering after TMCP to reduce toughness scatter through the thickness.

Ask for the route on the purchase order. It changes the weldability index, the welding procedure and, for heavy plate, the price of Q460qE.

Welding Q460qE and Fatigue in Bridge Girders

GB/T 714-2025 clause 7.1.2 uses CEV for normalized, QT and TMCP steel with C >0.12%, and Pcm for weathering steel and TMCP steel with C ≤0.12%, both from the heat analysis:

CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15

Pcm = C + Si/30 + Mn/20 + Cu/20 + Ni/60 + Cr/20 + Mo/15 + V/10 + 5B

Index ≤50 mm >50–100 mm >100–130 mm
Pcm, TMCP (Table 7) ≤ 0.22 ≤ 0.23 ≤ 0.23

Preheat for Q460qE is set by the qualified welding procedure, from the actual index on the certificate, plate thickness, restraint and hydrogen level. Lower actual values than the table caps save preheat time on large girders. At −40°C, HAZ toughness often becomes the limit. Fabricators usually cap heat input and qualify the procedure at −40°C on plate from the same route.

Typical consumables for Q460qE: E55/E62-class consumables (AWS E8018 / E9018 type).

Fatigue. Welded details govern fatigue life in a bridge, and their fatigue strength is set by detail category, not by yield strength. Higher-strength plate can carry higher stress ranges only if detailing improves too.

Fatigue design follows JTG D64 (highway) and TB 10091 (railway) in China, EN 1993-1-9 in Europe and AASHTO LRFD in the US; fabrication commonly follows TB 10212, JTG/T 3650 or AWS D1.5.

Q460qEZ15, Z25 and Z35: Through-Thickness Plate for Bridges

Lamellar tearing appears in thick plate loaded across its thickness, typically at cruciform joints and anchor plates. A Z grade adds a short-transverse tensile test and a lower sulfur cap.

GB/T 714 adds the Z level to the end of the designation, for example Q460qEZ25. The test and acceptance follow GB/T 5313 and apply to plate 15 mm and thicker.

Z grade Heat sulfur, max (%) Reduction of area, avg / single (%)
Z15 0.010 15 / 10
Z25 0.007 25 / 15
Z35 0.005 35 / 25

E chemistry already limits S to 0.010%, the Z15 sulfur cap. Z25 (S ≤0.007%) and Z35 (S ≤0.005%) still need a cleaner heat.

For Q460qE, we test Z per GB/T 5313 batch rules and print the three reduction-of-area values on the certificate. Z options apply across the GB/T 714 bridge steel range.

Equivalent Material Grades

Annex B of GB/T 714-2025 lists foreign grades against each strength level. It is informative: it tells you which families are close, not that the plates are interchangeable.

Standard Grade(s) Fit for Q460qE
ASTM A709 ASTM A709 HPS 70W Listed in Annex B
EN 10025-4 EN 10025-4 S460M, EN 10025-4 S460ML Listed in Annex B
EN 10025-6 EN 10025-6 S460Q, EN 10025-6 S460QL, EN 10025-6 S460QL1 Listed in Annex B
GB/T 16270 GB/T 16270 Q460E QT alternative
GB/T 1591 GB/T 1591 Q460ME General structural
GB/T 714 (weathering twin) Q460qNHE Same strength, weathering chemistry

Before substituting, compare three things line by line: minimum yield at the actual thickness, the impact test temperature and energy, and the weldability index. For Q460qE, the 120 J impact level and the Pcm/CEV caps are usually the hardest to match.

Q460qE Testing, UT and Certificate

A batch of Q460qE is one grade, one heat, one thickness, one rolling schedule and one heat-treatment condition, up to 60 t. Table 12 of GB/T 714-2025 sets the tests:

Test Frequency Method
Heat analysis 1 per heat GB/T 20066; GB/T 4336 / GB/T 223
Tensile 1 per batch GB/T 2975 / GB/T 228.1
Bend 180° 1 per batch (may be waived if guaranteed) GB/T 232
Charpy V at −40°C 3 specimens per batch GB/T 229
Through-thickness (Z) 3 specimens per batch, when ordered GB/T 5313
Ultrasonic Every plate >20 mm, Class II or better GB/T 2970
Surface and dimensions Every plate Visual and gauges

Impact retest: if a set fails, three more specimens are taken from the same batch. The average of all six must meet the requirement; two values may be below it, but only one below 70%. At −40°C, retest risk rises on heavy plate; we build a margin for retests into the delivery schedule.

Dimensions

What we roll and cut in Q460qE:

  • Thickness: 6 mm – 130 mm under GB/T 714 tensile tables; most orders 10 – 80 mm
  • Width: 1500 – 4000 mm, depending on mill and thickness
  • Length: 6000 – 18000 mm; longer by enquiry
  • Edge: mill edge or cut edge
  • Weight: theoretical, 7.85 g/cm³

Deck plate, webs, flanges, diaphragms and stiffeners are cut to drawing. For U-ribs and rolled sections on the same bridge, see steel beam profiles and steel structural profiles.

Tolerances

Thickness, width, length, flatness and camber of Q460qE follow GB/T 709. The table shows Class B thickness limits for common sizes.

Nominal thickness (mm) Width ≤ 1500 mm Width > 1500 – 2500 mm
> 8 – 15 −0.30 / +0.80 −0.30 / +1.00
> 15 – 25 −0.30 / +1.00 −0.30 / +1.20
> 25 – 40 −0.30 / +1.10 −0.30 / +1.30
> 40 – 60 −0.30 / +1.30 −0.30 / +1.50
> 60 – 100 −0.30 / +1.50 −0.30 / +1.80
> 100 – 150 −0.30 / +2.10 −0.30 / +2.50

Bridge fabricators often ask for Class C (zero minus) on deck and flange plate so section properties are never under the design value. Wider plates follow the heavier GB/T 709 rows; we state them on the offer.

Q460qE Price Factors and How to Order

Price questions on Q460qE usually come down to the extras in the table below.

Cost driver Effect on price
Strength level Q460q Higher levels need more alloy and tighter rolling control
Quality letter Higher extra: −40°C testing, S ≤0.010%, more retest risk
Delivery route TMCP / TMCP+T
Thickness Over 60 mm and under 10 mm carry size extras
Z15 / Z25 / Z35 Low-sulfur heat, Z test, UT; Z35 costs most
Width and length Over 3000 mm wide or 15 m long needs mill confirmation
Quantity per size Mill minimums per heat and size
Inspection and processing 3.2 witness, profile cutting, blasting, priming quoted per item

To get a firm quote in one round, send:

  • Grade, edition and Z level, e.g. Q460qEZ25 to GB/T 714-2025
  • Thickness × width × length and pieces or tonnes
  • Delivery route and UT class if beyond Class II
  • Certificate type and inspector
  • Destination port and Incoterm

We quote plate price, extras and freight line by line. Need another letter? See Q460qD, Q460qF.

Applications

Sector Typical Q460qE components
Long-span truss bridges Highly stressed chords and node plates
Cable-stayed bridges Pylon steel anchor boxes, main girder flanges
Suspension bridges Stiffening truss chords
Railway bridges Heavy-haul truss members
Arch bridges Arch rib plate

The letter E suits bridges in north-east China, Inner Mongolia, Xinjiang, Russia, Kazakhstan, Canada and high-altitude sites, and for thick, restrained members anywhere.

It is the wrong plate for pressure equipment (pressure vessel steel plates), unpainted exposure (weathering steel plates) or ship hulls (shipbuilding steel plates).

Supply Capability and Global Delivery

SHH STEEL sources Q460qE from first-line bridge-plate mills, including drafters of GB/T 714-2025 such as Ansteel, Valin Xiangtan, Jiangyin Xingcheng, Wuyang, Shougang and Xinyu.

  • Certificates: EN 10204 3.1 standard; 3.2 with third-party witness (SGS, BV, TÜV or owner’s inspector)
  • Tests: tensile, −40°C Charpy, bend, Z test, UT, product analysis
  • Processing: CNC plasma and flame cutting, bevelling, drilling, shot blasting and priming
  • Terms: FOB Shanghai, CFR, CIF; TT, LC or TT + LC
  • Marking: steel-stamped and paint-marked with grade, heat, size and mill, per GB/T 247

We ship GB, ASTM, EN and JIS plate to the Americas, Europe, the Middle East, Southeast Asia and Africa. Q460qE mostly goes to EPC contractors building bridges to Chinese codes abroad.

Lead time: about 45–60 days from mill rolling; Z35, F letter or 3.2 inspection adds about 1–2 weeks. Sea time from Shanghai is about 7–12 days to Southeast Asia and 28–35 days to North Europe.

Why Choose SHH STEEL

SHH STEEL works mill-direct as a steel manufacturer and exporter and global steel mill sourcing partner, China origin. Every Q460qE plate is traced to its heat.

Before shipment we check four lines on every Q460qE certificate: yield and tensile for the actual thickness band, Charpy at −40°C, the CEV or Pcm for the delivery route, and UT results. If one fails, the plate does not ship as Q460qE.

For Q460qE plate over 80 mm, agree the impact test position (surface or quarter thickness) with the owner before rolling.

We also tell buyers when another grade fits better. Neighbouring levels are Q420qE and Q500qE. The weathering counterpart is Q460qNHE. Browse more structural steel plates and high strength low alloy plates.

FAQ

What is Q460qE steel?
Q460qE is bridge structural steel plate to GB/T 714-2025. It has 460 MPa minimum yield up to 50 mm, 570 MPa minimum tensile, 18% elongation and Charpy V-notch impact of 120 J at −40°C for 12–100 mm plate. It is delivered TMCP or TMCP + tempering.
What is the difference between Q460qE and Q460qD?
Strength and chemistry box are the same. Q460qE is Charpy tested at −40°C, Q460qD at −20°C, both needing 120 J for 12–100 mm plate. P/S caps are 0.020/0.010% for E and 0.025/0.015% for D. Choose by the lowest service or erection temperature.
Is Q460qE the same as Q460E?
No. Q460E is general structural steel (GB/T 1591), while Q460qE is bridge steel to GB/T 714 with lower P and S, controlled weldability index, mandatory UT above 20 mm and 120 J impact for 12–100 mm plate. Bridge plate can replace general plate, not the reverse.
What is the ASTM or EN equivalent of Q460qE?
Close grades for Q460qE: ASTM A709 HPS 70W / EN 10025-4 S460M, S460ML / EN 10025-6 S460Q, S460QL, S460QL1 (Annex B). These are close families, not drop-in substitutes; compare yield at thickness, impact temperature and energy, and the weldability index before substituting.
How is Q460qE marked?
Plates are marked per GB/T 247 with grade, heat number, size and mill, and the Z level if ordered, for example Q460qEZ25. The certificate must state the delivery condition (TMCP, TMCP + tempering or QT).
What is the carbon equivalent of Q460qE?
It depends on the route. For Q460qE up to 50 mm, GB/T 714-2025 sets Pcm ≤0.22%. CEV applies to normalized, QT and TMCP steel with C >0.12%; Pcm to TMCP steel with C ≤0.12%.

Conclusion

Q460qE to GB/T 714-2025 is bridge plate with 460 MPa minimum yield, 570 MPa minimum tensile and 120 J Charpy at −40°C for 12–100 mm plate.

It sits between Q420qE and Q500qE in the bridge range, with Q460qD and Q460qF as sister letters. Before ordering Q460qE, confirm the edition on the drawing, the delivery route and any Z level; those three choices drive cost, lead time and welding.

SHH STEEL delivers Q460qE with the full GB/T 714 data set on an EN 10204 3.1 or 3.2 certificate. On request we add product analysis to GB/T 222, Z15–Z35, a tighter UT class, Class C tolerance, cutting and blasting.

We ship from Shanghai to bridge builders worldwide. Browse the full GB/T 714 range or other high strength low alloy plates.

Send your enquiry with grade, edition, sizes and inspection needs, and we will answer within one working day. Contact SHH STEEL for Q460qE bridge steel plate.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X