GB/T 714 Q620qF bridge steel plate stacked at SHH STEEL warehouse

GB/T 714 Q620qF Bridge Steel Plate Supplier

GB/T 714 Q620qF is bridge structural steel plate with 620 MPa minimum yield, 720 MPa minimum tensile and Charpy V-notch impact of 69 J at −60°C for 12–100 mm plate. SHH STEEL supplies Q620qF mill-direct, TMCP / TMCP+T / QT, up to 100 mm, with Z15–Z35, UT and heat and product analysis.
Keywords
Q620qF, Q620qF steel plate, GB/T 714 Q620qF, Q620q-F, Q620q F, Q620qF bridge steel, Q620qFZ15, Q620qFZ25, Q620qFZ35, bridge steel plate, Q620qF supplier
Equivalent Grades:
EN 10025-6 S620Q, S620QL, S620QL1 (Annex B) — Material Specification: GB/T 714-2025 (supersedes GB/T 714-2015) — Delivery: TMCP / TMCP+T / QT
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Q620q Quality Grades
GB/T 714-2025 vs 2015
Q620qF vs ASTM A709 / EN 10025
TMCP vs Normalized vs QT
Welding and Fatigue
Z15 / Z25 / Z35
Equivalent Material Grades
Testing and Inspection
Dimensions
Tolerances
Price and Ordering
Applications
Supply Capability
Why Choose SHH STEEL
FAQ
Conclusion

What is GB/T 714 Q620qF Bridge Steel Plate?

Q620qF is bridge structural steel plate to GB/T 714. Q stands for yield, 620 is the minimum yield in MPa for plate up to 50 mm, q stands for qiao (bridge) and F is the quality grade: Charpy V-notch at −60°C on longitudinal specimens.

Q620q is ultra-high-strength bridge plate for members where weight and depth are the design limits. Q620q bridges the gap between Q550q and Q690q. Like Q550q it gained a TMCP route in 2025; in QT form it carries Cr, Ni, Cu and Mo minimums (Cr 0.40–0.80%, Mo 0.20–0.50%) for hardenability.

Q620qF is tested at −60°C with at least 69 J above 12 mm, the second-highest F energy in GB/T 714. It is for cold-climate, fracture-critical members at very high stress.

The current text is GB/T 714-2025 (published 31 October 2025, effective 1 May 2026). It replaced GB/T 714-2015 completely and was drafted by Ansteel, Valin Xiangtan, Wuyang, Shougang and other plate mills together with the main bridge fabricators.

SHH STEEL (Shanghai Shenghonghe Import & Export Co., Ltd.) is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. We ship Q620qF cut to size with an EN 10204 3.1 or 3.2 certificate. Sister grades are listed under GB/T 714.

Material Specification

Specification element Requirement SHH STEEL compliance
Standard GB/T 714-2025 Q620qF Confirmed
Product Single-rolled plate ≤150 mm; hot-rolled strip and cut plate ≤25.4 mm Plate
Thickness with tensile values Up to 100 mm for Q620q Confirmed
Minimum yield ReL 620 MPa ≤50 mm; 580 MPa >50–100 mm Confirmed
Minimum tensile Rm 720 MPa ≤100 mm (no upper limit in the standard) Confirmed
Elongation A ≥ 15% Confirmed
Charpy V-notch −60°C, 69 J (12–100 mm), longitudinal Confirmed
Delivery condition TMCP, TMCP + tempering, or quenched and tempered (QT) As ordered
Weldability index Pcm (Table 7) for TMCP; CEV (Table 6) for QT Printed on MTC
Ultrasonic testing Plate >20 mm: GB/T 2970, Class II or better Every plate
Through-thickness Z15, Z25 or Z35 to GB/T 5313, when ordered As ordered
Dimensions GB/T 709 Confirmed
Certificate GB/T 247; EN 10204 3.1 or 3.2 As ordered

Grades often compared with Q620qF are EN 10025-6 S460Q and ASTM A514 Grade Q; the comparison below shows where they differ.

Chemical Composition: Heat Analysis and Product Analysis

Read the Q620qF certificate with two tables in mind: heat limits from GB/T 714 and product limits from GB/T 222. A plate can pass one and be argued over in the other if the basis is not written into the contract.

Table 1 below is the heat (ladle) analysis for Q620qF from GB/T 714-2025 Tables 1, 2, 3 and 4.

Element Q620qF TMCP (%) Q620q quenched and tempered (%)
C, max 0.11 0.14
Si, max 0.50 0.55
Mn 0.80 – 1.70 0.80 – 1.70
P, max 0.015 0.015
S, max 0.006 0.006
Nb 0.005 – 0.090 0.005 – 0.090
V 0.010 – 0.080 0.010 – 0.080
Ti 0.006 – 0.030 0.006 – 0.030
Als 0.010 – 0.045 0.010 – 0.045
Cr, max 1.00 0.40 – 0.80
Ni, max 1.20 0.25 – 1.00
Cu, max 0.55 0.15 – 0.55
Mo, max 0.60 0.20 – 0.50
N, max 0.0080 0.0080
B, max 0.0005 residual (≤0.0014 if C ≤0.10%) 0.0005–0.0030 may be added
H, max 0.0002 0.0002

Nb, V, Ti and Al may be added singly or together. Added singly, each must meet the range above; added together, at least one must reach its minimum and Nb + V + Ti ≤ 0.22%.

Table 2 is the product analysis: the limits a check analysis on finished plate is judged against. GB/T 714-2025 clause 7.1.3 calls up GB/T 222 for the permitted deviations.

Element Heat limit (%) Deviation, GB/T 222-2025 Table 2 (alloy) Q620qF product analysis (%)
C ≤ 0.11 +0.01 ≤ 0.12
Si ≤ 0.50 +0.04 ≤ 0.54
Mn 0.80 – 1.70 ±0.04 0.76 – 1.74
P ≤ 0.015 +0.005 (see note) ≤ 0.020
S ≤ 0.006 +0.005 (see note) ≤ 0.011
Cr ≤ 1.00 +0.05 (0.90–2.10% band) ≤ 1.05
Ni ≤ 1.20 +0.05 (1.00–2.00% band) ≤ 1.25
Cu ≤ 0.55 +0.03 ≤ 0.58
Mo ≤ 0.60 +0.02 (0.30–0.60% band) ≤ 0.62
V 0.010 – 0.080 +0.01 (≤0.10% band) ≤ 0.090
Ti 0.006 – 0.030 +0.02 ≤ 0.050
Nb, B, N See heat table Not read in our copy of Table 2 Agree in contract

How to read Table 2. With Ni up to 1.20% and Mo up to 0.60%, Q620q heats are normally classed as alloy steel under GB/T 13304, so the alloy-steel table of GB/T 222 applies. One steel uses one table only; the certificate should say which.

Mechanical Properties

Tensile values follow Table 9 of GB/T 714-2025 for Q620q. Tensile specimens are transverse; round specimens are used above 40 mm. Where yield is not distinct, Rp0.2 replaces ReL.

Nominal thickness ReL min (MPa) Rm min (MPa) A min
≤ 50 mm 620 720 15%
> 50 – 100 mm 580 720 15%

Impact values follow Table 10, on longitudinal specimens, average of three:

Letter / test temperature KV2 ≤12 mm KV2 >12 – 100 mm KV2 >100 – 150 mm
F / −60°C By agreement 69 J Not applicable

One single value may fall below the required average, but not below 70% of it. Plate over 8 mm and under 12 mm is tested with 7.5 mm specimens (75% of the value); 6–8 mm plate with 5 mm specimens (50%). Plate under 6 mm is not impact tested.

180° bend test, transverse: mandrel D = 2a up to 16 mm and 3a above 16 mm; may be omitted when the mill guarantees it. Yield ratio is not mandatory and Annex C gives no recommended value at this level; agree a limit in the contract if the design needs one.

Q620qD / Q620qE / Q620qF: Which Quality Grade?

Q620qF is tested at −60°C. It suits Arctic and sub-Arctic bridges, high-latitude rail lines and owners who want the largest toughness margin for fracture-critical members. F is the coldest letter in GB/T 714: Charpy at −60°C, P ≤0.015% and S ≤0.006%. It exists only for Q420q and above (and their NH versions), and its energy rises with strength.

Grade Test temp. KV2 ≤12 mm KV2 12–100 mm KV2 >100 mm P / S max (%)
Q620qD −20°C 80 J 120 J — 0.025 / 0.015
Q620qE −40°C 80 J 120 J — 0.020 / 0.010
Q620qF −60°C By agreement 69 J — 0.015 / 0.006

Note that F energy at Q620q is 69 J, not 120 J: the colder test uses a lower energy that GB/T 714-2025 raises with strength, from 47 J at Q420q/Q460q to 77 J at Q690q. Plate up to 12 mm needs an agreed value.

Q620qF: What Changed from GB/T 714-2015 to GB/T 714-2025

For Q620qF buyers the 2025 edition changes more than the year on the certificate. The points below come from the foreword of GB/T 714-2025 and its tables.

  • A TMCP route was added for Q620q (C ≤0.11%, Pcm ≤0.24% to 50 mm). In 2015 it was QT only.
  • CEV and Pcm limits were revised (Tables 6 and 7).
  • Tensile strength is now banded by thickness (e.g. lower minimum Rm above 100 mm) instead of one value.
  • Impact energy is set by thickness band (≤12 mm, 12–100 mm, >100 mm) in Table 10.
  • Yield ratio is no longer a clause value; it is agreed in the contract, with recommendations in informative Annex C.
  • Section products were removed; the standard now covers plate and strip only.
  • Delivery is TMCP, TMCP + tempering or QT; normalizing is kept only for Q345q/Q370q plate over 100 mm by agreement.

If a drawing cites 2015 and the plate is made to 2025, get the designer’s written acceptance; tensile strength above 100 mm and the yield-ratio basis differ.

Q620qF vs ASTM A709 and EN 10025: Which Grade Matches?

Can Q620qF replace a US or European bridge grade, or the other way round? Strength can match; toughness rules differ in kind, not only in number.

Property Q620qF EN 10025-6 S460Q ASTM A514 Grade Q EN 10025-6 S620Q
Min. yield (MPa) 620 (≤50 mm) 460 (≤50 mm) 690 (≤65 mm) 620 (≤50 mm)
Tensile (MPa) 720 min 550 – 720 760 – 895 700 – 890
Charpy 69 J at −60°C (12–100 mm) Q: −20°C, QL: −40°C, QL1: −60°C Supplementary only Q / QL / QL1: −20 / −40 / −60°C
Weathering chemistry No No No No

ASTM A709 sets Charpy requirements by temperature zone (1, 2, 3) and by member type: non-fracture-critical (T) or fracture-critical (F). GB/T 714 sets one value per letter, so compare the A709 zone with the GB/T 714 test temperature, not grade with grade.

EN 10025-3/-4/-6 grades show yield at the thinnest band; their values fall with thickness. GB/T 714 keeps 620 MPa to 50 mm. EN tensile ranges have upper limits; GB/T 714 gives minimums only.

At −60°C, the 69 J required for Q620qF is a demanding figure; general structural grades rarely prove any toughness that cold. For the C, D and E letters GB/T 714 asks 120 J, several times the 27–40 J typical of GB/T 1591 plate.

Q620qF Delivery Condition: TMCP vs Normalized vs Quenched and Tempered

GB/T 714-2025 clause 3.2 defines TMCP as rolling with the final deformation in a controlled temperature range, including accelerated cooling with or without tempering (self-tempering included) but excluding direct quenching and quench-and-temper. The delivery route must be stated on the certificate.

Route Available for Q620qF Weldability index Notes
TMCP Yes Pcm ≤0.24% (≤50 mm) C ≤0.11%; up to 100 mm
TMCP + tempering Yes Pcm Improves toughness uniformity
Quenched and tempered Yes CEV ≤0.55% (≤50 mm) C ≤0.14%; B 0.0005–0.0030% may be added
Normalized No — Not listed

Q620q can be TMCP or QT. QT chemistry has minimum Cr (0.40%), Ni (0.25%), Cu (0.15%) and Mo (0.20%) for hardenability; TMCP chemistry has only maximums. F-letter plate is often TMCP + tempering or, at the top strength levels, QT; ask which route the mill has qualified for −60°C.

Ask for the route on the purchase order. It changes the weldability index, the welding procedure and, for heavy plate, the price of Q620qF.

Welding Q620qF and Fatigue in Bridge Girders

GB/T 714-2025 clause 7.1.2 uses CEV for normalized, QT and TMCP steel with C >0.12%, and Pcm for weathering steel and TMCP steel with C ≤0.12%, both from the heat analysis:

CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15

Pcm = C + Si/30 + Mn/20 + Cu/20 + Ni/60 + Cr/20 + Mo/15 + V/10 + 5B

Index ≤50 mm >50–100 mm >100–130 mm
Pcm, TMCP (Table 7) ≤ 0.24 ≤ 0.25 —
CEV, QT (Table 6) ≤ 0.55 ≤ 0.60 —

Most bridge fabricators qualify Q620qF procedures on plate from the same mill and route as the production order. Changing mill or route mid-project usually means re-qualifying. At −60°C, both weld metal and HAZ must prove toughness. Expect lower heat input, more passes and consumables qualified at −60°C.

Typical consumables for Q620qF: E69-class consumables (AWS E10018M type).

Fatigue. Welded details govern fatigue life in a bridge, and their fatigue strength is set by detail category, not by yield strength. Higher-strength plate can carry higher stress ranges only if detailing improves too.

Fatigue design follows JTG D64 (highway) and TB 10091 (railway) in China, EN 1993-1-9 in Europe and AASHTO LRFD in the US; fabrication commonly follows TB 10212, JTG/T 3650 or AWS D1.5.

Q620qFZ15, Z25 and Z35: Through-Thickness Plate for Bridges

When a bridge drawing marks a plate Z25, the mill must supply a low-sulfur heat and prove reduction of area through the thickness on every batch.

GB/T 714 adds the Z level to the end of the designation, for example Q620qFZ25. The test and acceptance follow GB/T 5313 and apply to plate 15 mm and thicker.

Z grade Heat sulfur, max (%) Reduction of area, avg / single (%)
Z15 0.010 15 / 10
Z25 0.007 25 / 15
Z35 0.005 35 / 25

F chemistry limits S to 0.006%, which already meets the Z25 sulfur cap (0.007%). Only Z35 (S ≤0.005%) needs a further step.

Most bridges need Z on a small share of the tonnage. Mark it item by item on the cutting list rather than on the whole Q620qF order. Z options apply across the GB/T 714 bridge steel range.

Equivalent Material Grades

Annex B of GB/T 714-2025 lists foreign grades against each strength level. It is informative: it tells you which families are close, not that the plates are interchangeable.

Standard Grade(s) Fit for Q620qF
EN 10025-6 EN 10025-6 S620Q, EN 10025-6 S620QL, EN 10025-6 S620QL1 Listed in Annex B
GB/T 16270 GB/T 16270 Q620F QT alternative, different toughness rules
GB/T 1591 GB/T 1591 Q620MF TMCP general structural

Before substituting, compare three things line by line: minimum yield at the actual thickness, the impact test temperature and energy, and the weldability index. For Q620qF, the 120 J impact level and the Pcm/CEV caps are usually the hardest to match.

Q620qF Testing, UT and Certificate

A batch of Q620qF is one grade, one heat, one thickness, one rolling schedule and one heat-treatment condition, up to 60 t. Table 12 of GB/T 714-2025 sets the tests:

Test Frequency Method
Heat analysis 1 per heat GB/T 20066; GB/T 4336 / GB/T 223
Tensile 1 per batch GB/T 2975 / GB/T 228.1
Bend 180° 1 per batch (may be waived if guaranteed) GB/T 232
Charpy V at −60°C 3 specimens per batch GB/T 229
Through-thickness (Z) 3 specimens per batch, when ordered GB/T 5313
Ultrasonic Every plate >20 mm, Class II or better GB/T 2970
Surface and dimensions Every plate Visual and gauges

Impact retest: if a set fails, three more specimens are taken from the same batch. The average of all six must meet the requirement; two values may be below it, but only one below 70%. At −60°C, mills may need trial heats before the production run; we agree the test plan before accepting the order.

Dimensions

Size range for Q620qF plate:

  • Thickness: 6 mm – 100 mm under GB/T 714 tensile tables; most orders 10 – 60 mm
  • Width: 1500 – 4000 mm, depending on mill and thickness
  • Length: 6000 – 18000 mm; longer by enquiry
  • Edge: mill edge or cut edge
  • Weight: theoretical, 7.85 g/cm³

Deck plate, webs, flanges, diaphragms and stiffeners are cut to drawing. For U-ribs and rolled sections on the same bridge, see steel beam profiles and steel structural profiles.

Tolerances

For Q620qF, thickness tolerance follows GB/T 709 Class B unless the order says otherwise: −0.30 mm at every thickness, with the plus side shown below.

Nominal thickness (mm) Width ≤ 1500 mm Width > 1500 – 2500 mm
> 8 – 15 −0.30 / +0.80 −0.30 / +1.00
> 15 – 25 −0.30 / +1.00 −0.30 / +1.20
> 25 – 40 −0.30 / +1.10 −0.30 / +1.30
> 40 – 60 −0.30 / +1.30 −0.30 / +1.50
> 60 – 100 −0.30 / +1.50 −0.30 / +1.80
> 100 – 150 −0.30 / +2.10 −0.30 / +2.50

Bridge fabricators often ask for Class C (zero minus) on deck and flange plate so section properties are never under the design value. Wider plates follow the heavier GB/T 709 rows; we state them on the offer.

Q620qF Price Factors and How to Order

Price questions on Q620qF usually come down to the extras in the table below.

Cost driver Effect on price
Strength level Q620q Higher levels need more alloy and tighter rolling control
Quality letter Highest extra: −60°C testing, S ≤0.006%, limited mills
Delivery route TMCP / TMCP+T / QT; QT costs more than TMCP
Thickness Over 60 mm and under 10 mm carry size extras
Z15 / Z25 / Z35 Low-sulfur heat, Z test, UT; Z35 costs most
Width and length Over 3000 mm wide or 15 m long needs mill confirmation
Quantity per size Mill minimums per heat and size
Inspection and processing 3.2 witness, profile cutting, blasting, priming quoted per item

To get a firm quote in one round, send:

  • Grade, edition and Z level, e.g. Q620qFZ25 to GB/T 714-2025
  • Thickness × width × length and pieces or tonnes
  • Delivery route and UT class if beyond Class II
  • Certificate type and inspector
  • Destination port and Incoterm

We quote plate price, extras and freight line by line. Need another letter? See Q620qD, Q620qE.

Applications

Sector Typical Q620qF components
Ultra-long-span bridges Highly stressed truss chords
Cable anchorages Anchor boxes and anchor plates
Steel pylons Pylon shells
Movable bridges Lightweight girders
Special structures Members where depth is limited

The letter F suits Arctic and sub-Arctic bridges, high-latitude rail lines and owners who want the largest toughness margin for fracture-critical members.

It is the wrong plate for pressure equipment (pressure vessel steel plates), unpainted exposure (weathering steel plates) or ship hulls (shipbuilding steel plates).

Supply Capability and Global Delivery

SHH STEEL sources Q620qF from first-line bridge-plate mills, including drafters of GB/T 714-2025 such as Ansteel, Valin Xiangtan, Jiangyin Xingcheng, Wuyang, Shougang and Xinyu.

  • Certificates: EN 10204 3.1 standard; 3.2 with third-party witness (SGS, BV, TÜV or owner’s inspector)
  • Tests: tensile, −60°C Charpy, bend, Z test, UT, product analysis
  • Processing: CNC plasma and flame cutting, bevelling, drilling, shot blasting and priming
  • Terms: FOB Shanghai, CFR, CIF; TT, LC or TT + LC
  • Marking: steel-stamped and paint-marked with grade, heat, size and mill, per GB/T 247

Buyers of Q620qF are usually bridge fabricators and EPC contractors working to Chinese drawings overseas. We ship worldwide.

Lead time: about 45–60 days from mill rolling; Z35, F letter or 3.2 inspection adds about 1–2 weeks. Sea time from Shanghai is about 7–12 days to Southeast Asia and 28–35 days to North Europe.

Why Choose SHH STEEL

SHH STEEL has supplied bridge plate as a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. Q620qF is ordered from mills that roll bridge steel every month.

Before shipment we check four lines on every Q620qF certificate: yield and tensile for the actual thickness band, Charpy at −60°C, the CEV or Pcm for the delivery route, and UT results. If one fails, the plate does not ship as Q620qF.

Q620qF needs careful planning: a dedicated heat, S ≤0.006%, and often QT. Allow extra time in the programme for testing and possible retests.

We also tell buyers when another grade fits better. Neighbouring levels are Q550qF and Q690qF. Browse more structural steel plates and high strength low alloy plates.

FAQ

What is Q620qF steel?
Q620qF is bridge structural steel plate to GB/T 714-2025. It has 620 MPa minimum yield up to 50 mm, 720 MPa minimum tensile, 15% elongation and Charpy V-notch impact of 69 J at −60°C for 12–100 mm plate. It is delivered TMCP, TMCP + tempering, or quenched and tempered.
What impact energy does Q620qF need at −60°C?
GB/T 714-2025 requires at least 69 J at −60°C on longitudinal specimens for Q620qF plate over 12 mm and up to 100 mm. For plate 12 mm and thinner the value is by agreement. F energy rises with strength: 47 J for Q420q and Q460q, 54 J for Q500q, 60 J for Q550q, 69 J for Q620q and 77 J for Q690q.
What is the maximum thickness of Q620qF?
GB/T 714-2025 covers bridge plate up to 150 mm, but tensile values for Q620q stop at 100 mm. Above that there is no table value, so Q620qF cannot be certified thicker than 100 mm without a special agreement.
What is the ASTM or EN equivalent of Q620qF?
Close grades for Q620qF: EN 10025-6 S620Q, S620QL, S620QL1 (Annex B). These are close families, not drop-in substitutes; compare yield at thickness, impact temperature and energy, and the weldability index before substituting.
Is GB/T 714-2015 still valid?
No. GB/T 714-2025 was published on 31 October 2025 and took effect on 1 May 2026, fully replacing GB/T 714-2015. Contracts that still cite the 2015 edition can be certified to it, but new orders default to the 2025 edition.
Does steel grade affect fatigue life of a Q620qF bridge girder?
Very little. Fatigue life of welded bridge details is governed by the detail category and stress range, not by yield strength. Higher-strength plate raises working stress, so detailing and weld quality must improve to keep the same fatigue life.

Conclusion

Q620qF to GB/T 714-2025 is bridge plate with 620 MPa minimum yield, 720 MPa minimum tensile and 69 J Charpy at −60°C for 12–100 mm plate.

It sits between Q550qF and Q690qF in the bridge range, with Q620qD and Q620qE as sister letters. For Q620qF, the deciding numbers on the certificate are yield at the actual thickness, Charpy at −60°C and the weldability index for the delivery route.

From SHH STEEL, Q620qF arrives with traceable heat numbers, a complete EN 10204 3.1 or 3.2 certificate and, if ordered, third-party witness, product analysis and Z testing.

We ship from Shanghai to bridge builders worldwide. Browse the full GB/T 714 range or other high strength low alloy plates.

Ready to order? Send the drawing or cutting list, the certificate type and the destination port. Contact SHH STEEL for a mill-direct quotation on Q620qF bridge steel plate.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X