GB/T 714 Q550qD bridge steel plate stacked at SHH STEEL warehouse

GB/T 714 Q550qD Bridge Steel Plate Supplier

GB/T 714 Q550qD is bridge structural steel plate with 550 MPa minimum yield, 660 MPa minimum tensile and Charpy V-notch impact of 120 J at −20°C for 12–100 mm plate. SHH STEEL supplies Q550qD mill-direct, TMCP / TMCP+T / QT, up to 100 mm, with Z15–Z35, UT and heat and product analysis.
Keywords
Q550qD, Q550qD steel plate, GB/T 714 Q550qD, Q550q-D, Q550q D, Q550qD bridge steel, Q550qDZ15, Q550qDZ25, Q550qDZ35, bridge steel plate, Q550qD supplier
Equivalent Grades:
EN 10025-6 S550Q, S550QL, S550QL1 (Annex B) — Material Specification: GB/T 714-2025 (supersedes GB/T 714-2015) — Delivery: TMCP / TMCP+T / QT
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Q550q Quality Grades
GB/T 714-2025 vs 2015
Q550qD vs ASTM A709 / EN 10025
TMCP vs Normalized vs QT
Welding and Fatigue
Z15 / Z25 / Z35
Equivalent Material Grades
Testing and Inspection
Dimensions
Tolerances
Price and Ordering
Applications
Supply Capability
Why Choose SHH STEEL
FAQ
Conclusion

What is GB/T 714 Q550qD Bridge Steel Plate?

Q550qD is bridge structural steel plate to GB/T 714. Q stands for yield, 550 is the minimum yield in MPa for plate up to 50 mm, q stands for qiao (bridge) and D is the quality grade: Charpy V-notch at −20°C on longitudinal specimens.

Q550q is ultra-high-strength bridge plate up to 100 mm, now available TMCP as well as QT under GB/T 714-2025. Q550q was a QT-only grade in the 2015 edition. The 2025 edition adds a TMCP route with C ≤0.11% and Pcm ≤0.23% to 50 mm, which makes thinner, easier-to-weld plate possible at 550 MPa.

Q550qD gives 550 MPa yield up to 50 mm and 530 MPa to 100 mm, with a −20°C Charpy. Under GB/T 714-2025 it can be supplied TMCP as well as QT, which was not possible in 2015.

GB/T 714-2015 is no longer current. Its replacement, GB/T 714-2025, was published on 31 October 2025 and became effective on 1 May 2026. Where a contract still names the 2015 edition, we certify to it and flag any difference from 2025.

SHH STEEL (Shanghai Shenghonghe Import & Export Co., Ltd.) is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. We ship Q550qD cut to size with an EN 10204 3.1 or 3.2 certificate. Sister grades are listed under GB/T 714.

Material Specification

Specification element Requirement SHH STEEL compliance
Standard GB/T 714-2025 Q550qD Confirmed
Product Single-rolled plate ≤150 mm; hot-rolled strip and cut plate ≤25.4 mm Plate
Thickness with tensile values Up to 100 mm for Q550q Confirmed
Minimum yield ReL 550 MPa ≤50 mm; 530 MPa >50–100 mm Confirmed
Minimum tensile Rm 660 MPa ≤100 mm (no upper limit in the standard) Confirmed
Elongation A ≥ 16% Confirmed
Charpy V-notch −20°C, 120 J (12–100 mm), longitudinal Confirmed
Delivery condition TMCP, TMCP + tempering, or quenched and tempered (QT) As ordered
Weldability index Pcm (Table 7) for TMCP; CEV (Table 6) for QT Printed on MTC
Ultrasonic testing Plate >20 mm: GB/T 2970, Class II or better Every plate
Through-thickness Z15, Z25 or Z35 to GB/T 5313, when ordered As ordered
Dimensions GB/T 709 Confirmed
Certificate GB/T 247; EN 10204 3.1 or 3.2 As ordered

Grades often compared with Q550qD are and EN 10025-6 S460Q; the comparison below shows where they differ.

Chemical Composition: Heat Analysis and Product Analysis

Read the Q550qD certificate with two tables in mind: heat limits from GB/T 714 and product limits from GB/T 222. A plate can pass one and be argued over in the other if the basis is not written into the contract.

Table 1 below is the heat (ladle) analysis for Q550qD from GB/T 714-2025 Tables 1, 2, 3 and 4.

Element Q550qD TMCP (%) Q550q quenched and tempered (%)
C, max 0.11 0.12
Si, max 0.50 0.55
Mn 0.80 – 1.70 0.80 – 1.70
P, max 0.025 0.025
S, max 0.015 0.015
Nb 0.005 – 0.090 0.005 – 0.060
V 0.010 – 0.080 0.010 – 0.080
Ti 0.006 – 0.030 0.006 – 0.030
Als 0.010 – 0.045 0.010 – 0.045
Cr, max 1.00 ≤ 0.80
Ni, max 1.20 ≤ 0.70
Cu, max 0.55 ≤ 0.30
Mo, max 0.60 ≤ 0.30
N, max 0.0080 0.0080
B, max 0.0005 residual (≤0.0014 if C ≤0.10%) 0.0005–0.0030 may be added
H, max 0.0002 0.0002

Nb, V, Ti and Al may be added singly or together. Added singly, each must meet the range above; added together, at least one must reach its minimum and Nb + V + Ti ≤ 0.22%.

Table 2 is the product analysis: the limits a check analysis on finished plate is judged against. GB/T 714-2025 clause 7.1.3 calls up GB/T 222 for the permitted deviations.

Element Heat limit (%) Deviation, GB/T 222-2025 Table 2 (alloy) Q550qD product analysis (%)
C ≤ 0.11 +0.01 ≤ 0.12
Si ≤ 0.50 +0.04 ≤ 0.54
Mn 0.80 – 1.70 ±0.04 0.76 – 1.74
P ≤ 0.025 +0.005 (see note) ≤ 0.030
S ≤ 0.015 +0.005 (see note) ≤ 0.020
Cr ≤ 1.00 +0.05 (0.90–2.10% band) ≤ 1.05
Ni ≤ 1.20 +0.05 (1.00–2.00% band) ≤ 1.25
Cu ≤ 0.55 +0.03 ≤ 0.58
Mo ≤ 0.60 +0.02 (0.30–0.60% band) ≤ 0.62
V 0.010 – 0.080 +0.01 (≤0.10% band) ≤ 0.090
Ti 0.006 – 0.030 +0.02 ≤ 0.050
Nb, B, N See heat table Not read in our copy of Table 2 Agree in contract

How to read Table 2. With Ni up to 1.20% and Mo up to 0.60%, Q550q heats are normally classed as alloy steel under GB/T 13304, so the alloy-steel table of GB/T 222 applies. One steel uses one table only; the certificate should say which.

Mechanical Properties

Tensile values follow Table 9 of GB/T 714-2025 for Q550q. Tensile specimens are transverse; round specimens are used above 40 mm. Where yield is not distinct, Rp0.2 replaces ReL.

Nominal thickness ReL min (MPa) Rm min (MPa) A min
≤ 50 mm 550 660 16%
> 50 – 100 mm 530 660 16%

Impact values follow Table 10, on longitudinal specimens, average of three:

Letter / test temperature KV2 ≤12 mm KV2 >12 – 100 mm KV2 >100 – 150 mm
D / −20°C 80 J 120 J Not applicable

One single value may fall below the required average, but not below 70% of it. Plate over 8 mm and under 12 mm is tested with 7.5 mm specimens (75% of the value); 6–8 mm plate with 5 mm specimens (50%). Plate under 6 mm is not impact tested.

180° bend test, transverse: mandrel D = 2a up to 16 mm and 3a above 16 mm; may be omitted when the mill guarantees it. Yield ratio is not mandatory and Annex C gives no recommended value at this level; agree a limit in the contract if the design needs one.

Q550qD / Q550qE / Q550qF: Which Quality Grade?

Q550qD is tested at −20°C. It suits most highway and railway bridges in central and northern China, Europe and North America, where winter lows reach about −20°C. D is the most specified letter on Chinese bridge drawings. It is tested at −20°C and the melt is tighter than C: P ≤0.025%, S ≤0.015%.

Grade Test temp. KV2 ≤12 mm KV2 12–100 mm KV2 >100 mm P / S max (%)
Q550qD −20°C 80 J 120 J — 0.025 / 0.015
Q550qE −40°C 80 J 120 J — 0.020 / 0.010
Q550qF −60°C By agreement 60 J — 0.015 / 0.006

Over-specifying the letter costs money; under-specifying it costs safety. Choose from the lowest service or erection temperature, then step up one letter for thick, restrained or fracture-critical members.

Q550qD: What Changed from GB/T 714-2015 to GB/T 714-2025

For Q550qD buyers the 2025 edition changes more than the year on the certificate. The points below come from the foreword of GB/T 714-2025 and its tables.

  • A TMCP route was added for Q550q (C ≤0.11%, Pcm ≤0.23% to 50 mm). In 2015 it was QT only.
  • CEV and Pcm limits were revised (Tables 6 and 7).
  • Tensile strength is now banded by thickness (e.g. lower minimum Rm above 100 mm) instead of one value.
  • Impact energy is set by thickness band (≤12 mm, 12–100 mm, >100 mm) in Table 10.
  • Yield ratio is no longer a clause value; it is agreed in the contract, with recommendations in informative Annex C.
  • Section products were removed; the standard now covers plate and strip only.
  • Delivery is TMCP, TMCP + tempering or QT; normalizing is kept only for Q345q/Q370q plate over 100 mm by agreement.

If a drawing cites 2015 and the plate is made to 2025, get the designer’s written acceptance; tensile strength above 100 mm and the yield-ratio basis differ.

Q550qD vs ASTM A709 and EN 10025: Which Grade Matches?

Can Q550qD replace a US or European bridge grade, or the other way round? Strength can match; toughness rules differ in kind, not only in number.

Property Q550qD EN 10025-6 S460Q EN 10025-6 S550Q
Min. yield (MPa) 550 (≤50 mm) 460 (≤50 mm) 550 (≤50 mm)
Tensile (MPa) 660 min 550 – 720 640 – 820
Charpy 120 J at −20°C (12–100 mm) Q: −20°C, QL: −40°C, QL1: −60°C Q / QL / QL1: −20 / −40 / −60°C
Weathering chemistry No No No

ASTM A709 sets Charpy requirements by temperature zone (1, 2, 3) and by member type: non-fracture-critical (T) or fracture-critical (F). GB/T 714 sets one value per letter, so compare the A709 zone with the GB/T 714 test temperature, not grade with grade.

EN 10025-3/-4/-6 grades show yield at the thinnest band; their values fall with thickness. GB/T 714 keeps 550 MPa to 50 mm. EN tensile ranges have upper limits; GB/T 714 gives minimums only.

The 120 J requirement in GB/T 714 for 12–100 mm plate is several times the 27–40 J typical of general structural grades. That margin is the main reason bridge owners specify Q550qD rather than GB/T 1591 plate.

Q550qD Delivery Condition: TMCP vs Normalized vs Quenched and Tempered

GB/T 714-2025 clause 3.2 defines TMCP as rolling with the final deformation in a controlled temperature range, including accelerated cooling with or without tempering (self-tempering included) but excluding direct quenching and quench-and-temper. The delivery route must be stated on the certificate.

Route Available for Q550qD Weldability index Notes
TMCP Yes Pcm ≤0.23% (≤50 mm) C ≤0.11%; up to 100 mm
TMCP + tempering Yes Pcm Improves toughness uniformity
Quenched and tempered Yes CEV ≤0.52% (≤50 mm) C ≤0.12%; B 0.0005–0.0030% may be added
Normalized No — Not listed

Before 2026, Q550q bridge plate was QT only. GB/T 714-2025 added TMCP, which allows leaner chemistry and easier welding on plate up to about 50 mm. D-letter plate is usually plain TMCP; tempering is added mainly for heavy plate or tight yield-ratio limits.

Ask for the route on the purchase order. It changes the weldability index, the welding procedure and, for heavy plate, the price of Q550qD.

Welding Q550qD and Fatigue in Bridge Girders

GB/T 714-2025 clause 7.1.2 uses CEV for normalized, QT and TMCP steel with C >0.12%, and Pcm for weathering steel and TMCP steel with C ≤0.12%, both from the heat analysis:

CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15

Pcm = C + Si/30 + Mn/20 + Cu/20 + Ni/60 + Cr/20 + Mo/15 + V/10 + 5B

Index ≤50 mm >50–100 mm >100–130 mm
Pcm, TMCP (Table 7) ≤ 0.23 ≤ 0.25 —
CEV, QT (Table 6) ≤ 0.52 ≤ 0.57 —

We send the actual heat analysis of Q550qD before shipment, so the fabricator can check preheat and interpass limits against the procedure qualification record. At −20°C, most procedures qualified on TMCP plate pass HAZ impact without special measures; keep multi-wire SAW heat input inside the qualified band.

Typical consumables for Q550qD: E62/E69-class consumables (AWS E9018M / E10018M type).

Fatigue. Welded details govern fatigue life in a bridge, and their fatigue strength is set by detail category, not by yield strength. Higher-strength plate can carry higher stress ranges only if detailing improves too.

Fatigue design follows JTG D64 (highway) and TB 10091 (railway) in China, EN 1993-1-9 in Europe and AASHTO LRFD in the US; fabrication commonly follows TB 10212, JTG/T 3650 or AWS D1.5.

Q550qDZ15, Z25 and Z35: Through-Thickness Plate for Bridges

A Z grade is cheap insurance for heavily restrained joints. It caps sulfur and proves reduction of area in the thickness direction with a short-transverse tensile test.

GB/T 714 adds the Z level to the end of the designation, for example Q550qDZ25. The test and acceptance follow GB/T 5313 and apply to plate 15 mm and thicker.

Z grade Heat sulfur, max (%) Reduction of area, avg / single (%)
Z15 0.010 15 / 10
Z25 0.007 25 / 15
Z35 0.005 35 / 25

D chemistry allows S up to 0.015%. Z15 needs S ≤0.010% and Z25 needs ≤0.007%, so Z plate is still made from a dedicated low-sulfur heat.

Z-grade Q550qD carries a longer lead time because the heat must be planned as low-sulfur from the start. Tell us early. Z options apply across the GB/T 714 bridge steel range.

Equivalent Material Grades

Annex B of GB/T 714-2025 lists foreign grades against each strength level. It is informative: it tells you which families are close, not that the plates are interchangeable.

Standard Grade(s) Fit for Q550qD
EN 10025-6 EN 10025-6 S550Q, EN 10025-6 S550QL, EN 10025-6 S550QL1 Listed in Annex B
GB/T 16270 GB/T 16270 Q550D QT alternative, different toughness rules
GB/T 1591 GB/T 1591 Q550MD TMCP general structural

Before substituting, compare three things line by line: minimum yield at the actual thickness, the impact test temperature and energy, and the weldability index. For Q550qD, the 120 J impact level and the Pcm/CEV caps are usually the hardest to match.

Q550qD Testing, UT and Certificate

A batch of Q550qD is one grade, one heat, one thickness, one rolling schedule and one heat-treatment condition, up to 60 t. Table 12 of GB/T 714-2025 sets the tests:

Test Frequency Method
Heat analysis 1 per heat GB/T 20066; GB/T 4336 / GB/T 223
Tensile 1 per batch GB/T 2975 / GB/T 228.1
Bend 180° 1 per batch (may be waived if guaranteed) GB/T 232
Charpy V at −20°C 3 specimens per batch GB/T 229
Through-thickness (Z) 3 specimens per batch, when ordered GB/T 5313
Ultrasonic Every plate >20 mm, Class II or better GB/T 2970
Surface and dimensions Every plate Visual and gauges

Impact retest: if a set fails, three more specimens are taken from the same batch. The average of all six must meet the requirement; two values may be below it, but only one below 70%. At −20°C the 120 J level is comfortable for well-made TMCP plate, but we still check each batch value, not just the average.

Dimensions

Usual Q550qD supply range from SHH STEEL:

  • Thickness: 6 mm – 100 mm under GB/T 714 tensile tables; most orders 10 – 60 mm
  • Width: 1500 – 4000 mm, depending on mill and thickness
  • Length: 6000 – 18000 mm; longer by enquiry
  • Edge: mill edge or cut edge
  • Weight: theoretical, 7.85 g/cm³

Deck plate, webs, flanges, diaphragms and stiffeners are cut to drawing. For U-ribs and rolled sections on the same bridge, see steel beam profiles and steel structural profiles.

Tolerances

Q550qD plate is rolled to GB/T 709 tolerances. Class B (−0.30 mm) is standard; Class C (zero minus) can be agreed.

Nominal thickness (mm) Width ≤ 1500 mm Width > 1500 – 2500 mm
> 8 – 15 −0.30 / +0.80 −0.30 / +1.00
> 15 – 25 −0.30 / +1.00 −0.30 / +1.20
> 25 – 40 −0.30 / +1.10 −0.30 / +1.30
> 40 – 60 −0.30 / +1.30 −0.30 / +1.50
> 60 – 100 −0.30 / +1.50 −0.30 / +1.80
> 100 – 150 −0.30 / +2.10 −0.30 / +2.50

Bridge fabricators often ask for Class C (zero minus) on deck and flange plate so section properties are never under the design value. Wider plates follow the heavier GB/T 709 rows; we state them on the offer.

Q550qD Price Factors and How to Order

Price questions on Q550qD usually come down to the extras in the table below.

Cost driver Effect on price
Strength level Q550q Higher levels need more alloy and tighter rolling control
Quality letter Small extra for −20°C testing and cleaner melt
Delivery route TMCP / TMCP+T / QT; QT costs more than TMCP
Thickness Over 60 mm and under 10 mm carry size extras
Z15 / Z25 / Z35 Low-sulfur heat, Z test, UT; Z35 costs most
Width and length Over 3000 mm wide or 15 m long needs mill confirmation
Quantity per size Mill minimums per heat and size
Inspection and processing 3.2 witness, profile cutting, blasting, priming quoted per item

To get a firm quote in one round, send:

  • Grade, edition and Z level, e.g. Q550qDZ25 to GB/T 714-2025
  • Thickness × width × length and pieces or tonnes
  • Delivery route and UT class if beyond Class II
  • Certificate type and inspector
  • Destination port and Incoterm

We quote plate price, extras and freight line by line. Need another letter? See Q550qE, Q550qF.

Applications

Sector Typical Q550qD components
Ultra-long-span bridges Main truss chords and anchor zones
Cable-stayed bridges Highly stressed box girder flanges
Steel pylons Pylon wall plate
Railway bridges Heavily loaded node plates
Weight-critical retrofits Replacement members with limited depth

The letter D suits most highway and railway bridges in central and northern China, Europe and North America, where winter lows reach about −20°C.

It is the wrong plate for pressure equipment (pressure vessel steel plates), unpainted exposure (weathering steel plates) or ship hulls (shipbuilding steel plates).

Supply Capability and Global Delivery

SHH STEEL sources Q550qD from first-line bridge-plate mills, including drafters of GB/T 714-2025 such as Ansteel, Valin Xiangtan, Jiangyin Xingcheng, Wuyang, Shougang and Xinyu.

  • Certificates: EN 10204 3.1 standard; 3.2 with third-party witness (SGS, BV, TÜV or owner’s inspector)
  • Tests: tensile, −20°C Charpy, bend, Z test, UT, product analysis
  • Processing: CNC plasma and flame cutting, bevelling, drilling, shot blasting and priming
  • Terms: FOB Shanghai, CFR, CIF; TT, LC or TT + LC
  • Marking: steel-stamped and paint-marked with grade, heat, size and mill, per GB/T 247

Q550qD leaves Shanghai for bridge projects designed to Chinese codes abroad, mainly through EPC contractors in Southeast Asia, Central Asia, the Middle East and Africa.

Lead time: about 45–60 days from mill rolling; Z35, F letter or 3.2 inspection adds about 1–2 weeks. Sea time from Shanghai is about 7–12 days to Southeast Asia and 28–35 days to North Europe.

Why Choose SHH STEEL

SHH STEEL is mill-direct: steel manufacturer and exporter and global steel mill sourcing partner, China origin. Every Q550qD plate we ship carries the original mill heat number.

Before shipment we check four lines on every Q550qD certificate: yield and tensile for the actual thickness band, Charpy at −20°C, the CEV or Pcm for the delivery route, and UT results. If one fails, the plate does not ship as Q550qD.

Q550q stops at 100 mm. If the design calls for thicker plate, the answer is a lower grade or a built-up section, not a thicker Q550q.

We also tell buyers when another grade fits better. Neighbouring levels are Q500qD and Q620qD. Browse more structural steel plates and high strength low alloy plates.

FAQ

What is Q550qD steel?
Q550qD is bridge structural steel plate to GB/T 714-2025. It has 550 MPa minimum yield up to 50 mm, 660 MPa minimum tensile, 16% elongation and Charpy V-notch impact of 120 J at −20°C for 12–100 mm plate. It is delivered TMCP, TMCP + tempering, or quenched and tempered.
What is the difference between Q550qD and Q550qE?
Strength and chemistry box are the same. Q550qD is Charpy tested at −20°C, Q550qE at −40°C, both needing 120 J for 12–100 mm plate. P/S caps are 0.025/0.015% for D and 0.020/0.010% for E. Choose by the lowest service or erection temperature.
What is the yield strength of Q550qD?
Q550qD has a minimum lower yield strength of 550 MPa up to 50 mm and 530 MPa from 50 to 100 mm (GB/T 714-2025 Table 9). Minimum tensile is 660 MPa up to 100 mm. There is no upper tensile limit in the standard.
What is the ASTM or EN equivalent of Q550qD?
Close grades for Q550qD: EN 10025-6 S550Q, S550QL, S550QL1 (Annex B). These are close families, not drop-in substitutes; compare yield at thickness, impact temperature and energy, and the weldability index before substituting.
What does the q mean in GB/T 714 bridge steel grades?
The lowercase q stands for qiao, Chinese for bridge. In a grade such as Q420qD, Q means yield, 420 is the minimum yield in MPa, q marks bridge steel to GB/T 714 and D is the quality letter (−20°C Charpy). NH after the letter, as in Q420qDNH, marks weathering steel.
Is Q550qD weldable?
Yes. GB/T 714-2025 caps the weldability index for Q550qD up to 50 mm at Pcm ≤0.23% (TMCP) or CEV ≤0.52% (QT). Preheat depends on actual chemistry, thickness and restraint, and is fixed by the qualified welding procedure.

Conclusion

Q550qD to GB/T 714-2025 is bridge plate with 550 MPa minimum yield, 660 MPa minimum tensile and 120 J Charpy at −20°C for 12–100 mm plate.

It sits between Q500qD and Q620qD in the bridge range, with Q550qE and Q550qF as sister letters. For Q550qD, a product analysis on finished plate is judged against GB/T 222 deviations, not the heat limits, so put the basis in the contract.

SHH STEEL supplies Q550qD with heat analysis, Pcm or CEV, tensile and Charpy results on an EN 10204 3.1 or 3.2 certificate, and adds product analysis to GB/T 222 when you need it.

We ship from Shanghai to bridge builders worldwide. Browse the full GB/T 714 range or other high strength low alloy plates.

Email the cutting list and the owner’s specification. We return a line-by-line offer with test plan and lead time. Contact SHH STEEL for Q550qD bridge steel plate.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X