GB/T 714 Q620qD bridge steel plate stacked at SHH STEEL warehouse

GB/T 714 Q620qD Bridge Steel Plate Supplier

GB/T 714 Q620qD is bridge structural steel plate with 620 MPa minimum yield, 720 MPa minimum tensile and Charpy V-notch impact of 120 J at −20°C for 12–100 mm plate. SHH STEEL supplies Q620qD mill-direct, TMCP / TMCP+T / QT, up to 100 mm, with Z15–Z35, UT and heat and product analysis.
Keywords
Q620qD, Q620qD steel plate, GB/T 714 Q620qD, Q620q-D, Q620q D, Q620qD bridge steel, Q620qDZ15, Q620qDZ25, Q620qDZ35, bridge steel plate, Q620qD supplier
Equivalent Grades:
EN 10025-6 S620Q, S620QL, S620QL1 (Annex B) — Material Specification: GB/T 714-2025 (supersedes GB/T 714-2015) — Delivery: TMCP / TMCP+T / QT
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Q620q Quality Grades
GB/T 714-2025 vs 2015
Q620qD vs ASTM A709 / EN 10025
TMCP vs Normalized vs QT
Welding and Fatigue
Z15 / Z25 / Z35
Equivalent Material Grades
Testing and Inspection
Dimensions
Tolerances
Price and Ordering
Applications
Supply Capability
Why Choose SHH STEEL
FAQ
Conclusion

What is GB/T 714 Q620qD Bridge Steel Plate?

Q620qD is bridge structural steel plate to GB/T 714. Q stands for yield, 620 is the minimum yield in MPa for plate up to 50 mm, q stands for qiao (bridge) and D is the quality grade: Charpy V-notch at −20°C on longitudinal specimens.

Q620q is ultra-high-strength bridge plate for members where weight and depth are the design limits. Q620q bridges the gap between Q550q and Q690q. Like Q550q it gained a TMCP route in 2025; in QT form it carries Cr, Ni, Cu and Mo minimums (Cr 0.40–0.80%, Mo 0.20–0.50%) for hardenability.

Q620qD gives 620 MPa yield up to 50 mm with a −20°C Charpy. It is a specialist grade for members where depth and weight are restricted, such as cable anchorages and pylon walls.

Edition status: GB/T 714-2025 was published on 31 October 2025 and has applied since 1 May 2026. It fully replaces GB/T 714-2015. Orders signed under the 2015 edition can still be certified to it if the contract says so; new orders default to 2025.

SHH STEEL (Shanghai Shenghonghe Import & Export Co., Ltd.) is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. We ship Q620qD cut to size with an EN 10204 3.1 or 3.2 certificate. Sister grades are listed under GB/T 714.

Material Specification

Specification element Requirement SHH STEEL compliance
Standard GB/T 714-2025 Q620qD Confirmed
Product Single-rolled plate ≤150 mm; hot-rolled strip and cut plate ≤25.4 mm Plate
Thickness with tensile values Up to 100 mm for Q620q Confirmed
Minimum yield ReL 620 MPa ≤50 mm; 580 MPa >50–100 mm Confirmed
Minimum tensile Rm 720 MPa ≤100 mm (no upper limit in the standard) Confirmed
Elongation A ≥ 15% Confirmed
Charpy V-notch −20°C, 120 J (12–100 mm), longitudinal Confirmed
Delivery condition TMCP, TMCP + tempering, or quenched and tempered (QT) As ordered
Weldability index Pcm (Table 7) for TMCP; CEV (Table 6) for QT Printed on MTC
Ultrasonic testing Plate >20 mm: GB/T 2970, Class II or better Every plate
Through-thickness Z15, Z25 or Z35 to GB/T 5313, when ordered As ordered
Dimensions GB/T 709 Confirmed
Certificate GB/T 247; EN 10204 3.1 or 3.2 As ordered

Grades often compared with Q620qD are EN 10025-6 S460Q and ASTM A514 Grade Q; the comparison below shows where they differ.

Chemical Composition: Heat Analysis and Product Analysis

Third-party labs test plate, not ladles. So when an inspector checks Q620qD, the result is a product analysis and must be compared with product limits, not with the heat limits on the certificate.

Table 1 below is the heat (ladle) analysis for Q620qD from GB/T 714-2025 Tables 1, 2, 3 and 4.

Element Q620qD TMCP (%) Q620q quenched and tempered (%)
C, max 0.11 0.14
Si, max 0.50 0.55
Mn 0.80 – 1.70 0.80 – 1.70
P, max 0.025 0.025
S, max 0.015 0.015
Nb 0.005 – 0.090 0.005 – 0.090
V 0.010 – 0.080 0.010 – 0.080
Ti 0.006 – 0.030 0.006 – 0.030
Als 0.010 – 0.045 0.010 – 0.045
Cr, max 1.00 0.40 – 0.80
Ni, max 1.20 0.25 – 1.00
Cu, max 0.55 0.15 – 0.55
Mo, max 0.60 0.20 – 0.50
N, max 0.0080 0.0080
B, max 0.0005 residual (≤0.0014 if C ≤0.10%) 0.0005–0.0030 may be added
H, max 0.0002 0.0002

Nb, V, Ti and Al may be added singly or together. Added singly, each must meet the range above; added together, at least one must reach its minimum and Nb + V + Ti ≤ 0.22%.

Table 2 is the product analysis: the limits a check analysis on finished plate is judged against. GB/T 714-2025 clause 7.1.3 calls up GB/T 222 for the permitted deviations.

Element Heat limit (%) Deviation, GB/T 222-2025 Table 2 (alloy) Q620qD product analysis (%)
C ≤ 0.11 +0.01 ≤ 0.12
Si ≤ 0.50 +0.04 ≤ 0.54
Mn 0.80 – 1.70 ±0.04 0.76 – 1.74
P ≤ 0.025 +0.005 (see note) ≤ 0.030
S ≤ 0.015 +0.005 (see note) ≤ 0.020
Cr ≤ 1.00 +0.05 (0.90–2.10% band) ≤ 1.05
Ni ≤ 1.20 +0.05 (1.00–2.00% band) ≤ 1.25
Cu ≤ 0.55 +0.03 ≤ 0.58
Mo ≤ 0.60 +0.02 (0.30–0.60% band) ≤ 0.62
V 0.010 – 0.080 +0.01 (≤0.10% band) ≤ 0.090
Ti 0.006 – 0.030 +0.02 ≤ 0.050
Nb, B, N See heat table Not read in our copy of Table 2 Agree in contract

How to read Table 2. With Ni up to 1.20% and Mo up to 0.60%, Q620q heats are normally classed as alloy steel under GB/T 13304, so the alloy-steel table of GB/T 222 applies. One steel uses one table only; the certificate should say which.

Mechanical Properties

Tensile values follow Table 9 of GB/T 714-2025 for Q620q. Tensile specimens are transverse; round specimens are used above 40 mm. Where yield is not distinct, Rp0.2 replaces ReL.

Nominal thickness ReL min (MPa) Rm min (MPa) A min
≤ 50 mm 620 720 15%
> 50 – 100 mm 580 720 15%

Impact values follow Table 10, on longitudinal specimens, average of three:

Letter / test temperature KV2 ≤12 mm KV2 >12 – 100 mm KV2 >100 – 150 mm
D / −20°C 80 J 120 J Not applicable

One single value may fall below the required average, but not below 70% of it. Plate over 8 mm and under 12 mm is tested with 7.5 mm specimens (75% of the value); 6–8 mm plate with 5 mm specimens (50%). Plate under 6 mm is not impact tested.

180° bend test, transverse: mandrel D = 2a up to 16 mm and 3a above 16 mm; may be omitted when the mill guarantees it. Yield ratio is not mandatory and Annex C gives no recommended value at this level; agree a limit in the contract if the design needs one.

Q620qD / Q620qE / Q620qF: Which Quality Grade?

Q620qD is tested at −20°C. It suits most highway and railway bridges in central and northern China, Europe and North America, where winter lows reach about −20°C. D is the most specified letter on Chinese bridge drawings. It is tested at −20°C and the melt is tighter than C: P ≤0.025%, S ≤0.015%.

Grade Test temp. KV2 ≤12 mm KV2 12–100 mm KV2 >100 mm P / S max (%)
Q620qD −20°C 80 J 120 J — 0.025 / 0.015
Q620qE −40°C 80 J 120 J — 0.020 / 0.010
Q620qF −60°C By agreement 69 J — 0.015 / 0.006

Over-specifying the letter costs money; under-specifying it costs safety. Choose from the lowest service or erection temperature, then step up one letter for thick, restrained or fracture-critical members.

Q620qD: What Changed from GB/T 714-2015 to GB/T 714-2025

For Q620qD buyers the 2025 edition changes more than the year on the certificate. The points below come from the foreword of GB/T 714-2025 and its tables.

  • A TMCP route was added for Q620q (C ≤0.11%, Pcm ≤0.24% to 50 mm). In 2015 it was QT only.
  • CEV and Pcm limits were revised (Tables 6 and 7).
  • Tensile strength is now banded by thickness (e.g. lower minimum Rm above 100 mm) instead of one value.
  • Impact energy is set by thickness band (≤12 mm, 12–100 mm, >100 mm) in Table 10.
  • Yield ratio is no longer a clause value; it is agreed in the contract, with recommendations in informative Annex C.
  • Section products were removed; the standard now covers plate and strip only.
  • Delivery is TMCP, TMCP + tempering or QT; normalizing is kept only for Q345q/Q370q plate over 100 mm by agreement.

If a drawing cites 2015 and the plate is made to 2025, get the designer’s written acceptance; tensile strength above 100 mm and the yield-ratio basis differ.

Q620qD vs ASTM A709 and EN 10025: Which Grade Matches?

Can Q620qD replace a US or European bridge grade, or the other way round? Strength can match; toughness rules differ in kind, not only in number.

Property Q620qD EN 10025-6 S460Q ASTM A514 Grade Q EN 10025-6 S620Q
Min. yield (MPa) 620 (≤50 mm) 460 (≤50 mm) 690 (≤65 mm) 620 (≤50 mm)
Tensile (MPa) 720 min 550 – 720 760 – 895 700 – 890
Charpy 120 J at −20°C (12–100 mm) Q: −20°C, QL: −40°C, QL1: −60°C Supplementary only Q / QL / QL1: −20 / −40 / −60°C
Weathering chemistry No No No No

ASTM A709 sets Charpy requirements by temperature zone (1, 2, 3) and by member type: non-fracture-critical (T) or fracture-critical (F). GB/T 714 sets one value per letter, so compare the A709 zone with the GB/T 714 test temperature, not grade with grade.

EN 10025-3/-4/-6 grades show yield at the thinnest band; their values fall with thickness. GB/T 714 keeps 620 MPa to 50 mm. EN tensile ranges have upper limits; GB/T 714 gives minimums only.

The 120 J requirement in GB/T 714 for 12–100 mm plate is several times the 27–40 J typical of general structural grades. That margin is the main reason bridge owners specify Q620qD rather than GB/T 1591 plate.

Q620qD Delivery Condition: TMCP vs Normalized vs Quenched and Tempered

GB/T 714-2025 clause 3.2 defines TMCP as rolling with the final deformation in a controlled temperature range, including accelerated cooling with or without tempering (self-tempering included) but excluding direct quenching and quench-and-temper. The delivery route must be stated on the certificate.

Route Available for Q620qD Weldability index Notes
TMCP Yes Pcm ≤0.24% (≤50 mm) C ≤0.11%; up to 100 mm
TMCP + tempering Yes Pcm Improves toughness uniformity
Quenched and tempered Yes CEV ≤0.55% (≤50 mm) C ≤0.14%; B 0.0005–0.0030% may be added
Normalized No — Not listed

Q620q can be TMCP or QT. QT chemistry has minimum Cr (0.40%), Ni (0.25%), Cu (0.15%) and Mo (0.20%) for hardenability; TMCP chemistry has only maximums. D-letter plate is usually plain TMCP; tempering is added mainly for heavy plate or tight yield-ratio limits.

Ask for the route on the purchase order. It changes the weldability index, the welding procedure and, for heavy plate, the price of Q620qD.

Welding Q620qD and Fatigue in Bridge Girders

GB/T 714-2025 clause 7.1.2 uses CEV for normalized, QT and TMCP steel with C >0.12%, and Pcm for weathering steel and TMCP steel with C ≤0.12%, both from the heat analysis:

CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15

Pcm = C + Si/30 + Mn/20 + Cu/20 + Ni/60 + Cr/20 + Mo/15 + V/10 + 5B

Index ≤50 mm >50–100 mm >100–130 mm
Pcm, TMCP (Table 7) ≤ 0.24 ≤ 0.25 —
CEV, QT (Table 6) ≤ 0.55 ≤ 0.60 —

For Q620qD, ask the fabricator which index the WPS was qualified on. Where the WPS uses CEV and the standard uses Pcm, we print both on the certificate. At −20°C, most procedures qualified on TMCP plate pass HAZ impact without special measures; keep multi-wire SAW heat input inside the qualified band.

Typical consumables for Q620qD: E69-class consumables (AWS E10018M type).

Fatigue. Welded details govern fatigue life in a bridge, and their fatigue strength is set by detail category, not by yield strength. Higher-strength plate can carry higher stress ranges only if detailing improves too.

Fatigue design follows JTG D64 (highway) and TB 10091 (railway) in China, EN 1993-1-9 in Europe and AASHTO LRFD in the US; fabrication commonly follows TB 10212, JTG/T 3650 or AWS D1.5.

Q620qDZ15, Z25 and Z35: Through-Thickness Plate for Bridges

Z15, Z25 and Z35 tell the mill how much through-thickness ductility a plate must prove. The higher the number, the lower the sulfur and the higher the cost.

GB/T 714 adds the Z level to the end of the designation, for example Q620qDZ25. The test and acceptance follow GB/T 5313 and apply to plate 15 mm and thicker.

Z grade Heat sulfur, max (%) Reduction of area, avg / single (%)
Z15 0.010 15 / 10
Z25 0.007 25 / 15
Z35 0.005 35 / 25

D chemistry allows S up to 0.015%. Z15 needs S ≤0.010% and Z25 needs ≤0.007%, so Z plate is still made from a dedicated low-sulfur heat.

Most bridges need Z on a small share of the tonnage. Mark it item by item on the cutting list rather than on the whole Q620qD order. Z options apply across the GB/T 714 bridge steel range.

Equivalent Material Grades

Annex B of GB/T 714-2025 lists foreign grades against each strength level. It is informative: it tells you which families are close, not that the plates are interchangeable.

Standard Grade(s) Fit for Q620qD
EN 10025-6 EN 10025-6 S620Q, EN 10025-6 S620QL, EN 10025-6 S620QL1 Listed in Annex B
GB/T 16270 GB/T 16270 Q620D QT alternative, different toughness rules
GB/T 1591 GB/T 1591 Q620MD TMCP general structural

Before substituting, compare three things line by line: minimum yield at the actual thickness, the impact test temperature and energy, and the weldability index. For Q620qD, the 120 J impact level and the Pcm/CEV caps are usually the hardest to match.

Q620qD Testing, UT and Certificate

A batch of Q620qD is one grade, one heat, one thickness, one rolling schedule and one heat-treatment condition, up to 60 t. Table 12 of GB/T 714-2025 sets the tests:

Test Frequency Method
Heat analysis 1 per heat GB/T 20066; GB/T 4336 / GB/T 223
Tensile 1 per batch GB/T 2975 / GB/T 228.1
Bend 180° 1 per batch (may be waived if guaranteed) GB/T 232
Charpy V at −20°C 3 specimens per batch GB/T 229
Through-thickness (Z) 3 specimens per batch, when ordered GB/T 5313
Ultrasonic Every plate >20 mm, Class II or better GB/T 2970
Surface and dimensions Every plate Visual and gauges

Impact retest: if a set fails, three more specimens are taken from the same batch. The average of all six must meet the requirement; two values may be below it, but only one below 70%. At −20°C the 120 J level is comfortable for well-made TMCP plate, but we still check each batch value, not just the average.

Dimensions

What we roll and cut in Q620qD:

  • Thickness: 6 mm – 100 mm under GB/T 714 tensile tables; most orders 10 – 60 mm
  • Width: 1500 – 4000 mm, depending on mill and thickness
  • Length: 6000 – 18000 mm; longer by enquiry
  • Edge: mill edge or cut edge
  • Weight: theoretical, 7.85 g/cm³

Deck plate, webs, flanges, diaphragms and stiffeners are cut to drawing. For U-ribs and rolled sections on the same bridge, see steel beam profiles and steel structural profiles.

Tolerances

GB/T 714-2025 clause 7.6 sends dimensions and shape to GB/T 709. Thickness tolerance is Class B by default: −0.30 mm fixed, plus side by thickness and width.

Nominal thickness (mm) Width ≤ 1500 mm Width > 1500 – 2500 mm
> 8 – 15 −0.30 / +0.80 −0.30 / +1.00
> 15 – 25 −0.30 / +1.00 −0.30 / +1.20
> 25 – 40 −0.30 / +1.10 −0.30 / +1.30
> 40 – 60 −0.30 / +1.30 −0.30 / +1.50
> 60 – 100 −0.30 / +1.50 −0.30 / +1.80
> 100 – 150 −0.30 / +2.10 −0.30 / +2.50

Bridge fabricators often ask for Class C (zero minus) on deck and flange plate so section properties are never under the design value. Wider plates follow the heavier GB/T 709 rows; we state them on the offer.

Q620qD Price Factors and How to Order

There is no single Q620qD price. Mills price bridge plate as base plus extras, and the order sets the extras.

Cost driver Effect on price
Strength level Q620q Higher levels need more alloy and tighter rolling control
Quality letter Small extra for −20°C testing and cleaner melt
Delivery route TMCP / TMCP+T / QT; QT costs more than TMCP
Thickness Over 60 mm and under 10 mm carry size extras
Z15 / Z25 / Z35 Low-sulfur heat, Z test, UT; Z35 costs most
Width and length Over 3000 mm wide or 15 m long needs mill confirmation
Quantity per size Mill minimums per heat and size
Inspection and processing 3.2 witness, profile cutting, blasting, priming quoted per item

To get a firm quote in one round, send:

  • Grade, edition and Z level, e.g. Q620qDZ25 to GB/T 714-2025
  • Thickness × width × length and pieces or tonnes
  • Delivery route and UT class if beyond Class II
  • Certificate type and inspector
  • Destination port and Incoterm

We quote plate price, extras and freight line by line. Need another letter? See Q620qE, Q620qF.

Applications

Sector Typical Q620qD components
Ultra-long-span bridges Highly stressed truss chords
Cable anchorages Anchor boxes and anchor plates
Steel pylons Pylon shells
Movable bridges Lightweight girders
Special structures Members where depth is limited

The letter D suits most highway and railway bridges in central and northern China, Europe and North America, where winter lows reach about −20°C.

It is the wrong plate for pressure equipment (pressure vessel steel plates), unpainted exposure (weathering steel plates) or ship hulls (shipbuilding steel plates).

Supply Capability and Global Delivery

SHH STEEL sources Q620qD from first-line bridge-plate mills, including drafters of GB/T 714-2025 such as Ansteel, Valin Xiangtan, Jiangyin Xingcheng, Wuyang, Shougang and Xinyu.

  • Certificates: EN 10204 3.1 standard; 3.2 with third-party witness (SGS, BV, TÜV or owner’s inspector)
  • Tests: tensile, −20°C Charpy, bend, Z test, UT, product analysis
  • Processing: CNC plasma and flame cutting, bevelling, drilling, shot blasting and priming
  • Terms: FOB Shanghai, CFR, CIF; TT, LC or TT + LC
  • Marking: steel-stamped and paint-marked with grade, heat, size and mill, per GB/T 247

We ship Q620qD to fabricators in Asia, Africa, the Middle East, Europe and the Americas, by break-bulk or container.

Lead time: about 45–60 days from mill rolling; Z35, F letter or 3.2 inspection adds about 1–2 weeks. Sea time from Shanghai is about 7–12 days to Southeast Asia and 28–35 days to North Europe.

Why Choose SHH STEEL

Mill-direct, China origin: SHH STEEL is a steel manufacturer and exporter and global steel mill sourcing partner, and Q620qD is one of the bridge grades we handle regularly.

Before shipment we check four lines on every Q620qD certificate: yield and tensile for the actual thickness band, Charpy at −20°C, the CEV or Pcm for the delivery route, and UT results. If one fails, the plate does not ship as Q620qD.

Q620q QT chemistry has minimum Cr, Ni, Cu and Mo contents. If you compare offers, check that the certificate shows those minimums are met.

We also tell buyers when another grade fits better. Neighbouring levels are Q550qD and Q690qD. Browse more structural steel plates and high strength low alloy plates.

FAQ

What is Q620qD steel?
Q620qD is bridge structural steel plate to GB/T 714-2025. It has 620 MPa minimum yield up to 50 mm, 720 MPa minimum tensile, 15% elongation and Charpy V-notch impact of 120 J at −20°C for 12–100 mm plate. It is delivered TMCP, TMCP + tempering, or quenched and tempered.
What is the difference between Q620qD and Q620qE?
Strength and chemistry box are the same. Q620qD is Charpy tested at −20°C, Q620qE at −40°C, both needing 120 J for 12–100 mm plate. P/S caps are 0.025/0.015% for D and 0.020/0.010% for E. Choose by the lowest service or erection temperature.
Can Q620qD be supplied TMCP?
Yes, since GB/T 714-2025. The 2015 edition listed Q620q as quenched and tempered only. The 2025 edition adds a TMCP route with C ≤0.11% and Pcm ≤0.24% up to 50 mm; QT plate is still available with CEV ≤0.55% up to 50 mm.
What is the ASTM or EN equivalent of Q620qD?
Close grades for Q620qD: EN 10025-6 S620Q, S620QL, S620QL1 (Annex B). These are close families, not drop-in substitutes; compare yield at thickness, impact temperature and energy, and the weldability index before substituting.
Does GB/T 714 require ultrasonic testing?
Yes. GB/T 714-2025 clause 7.5 requires every single-rolled plate over 20 mm to be ultrasonically tested to GB/T 2970, with acceptance Class II or better. Thinner plate is tested only by agreement.
Is Q620qD weldable?
Yes. GB/T 714-2025 caps the weldability index for Q620qD up to 50 mm at Pcm ≤0.24% (TMCP) or CEV ≤0.55% (QT). Preheat depends on actual chemistry, thickness and restraint, and is fixed by the qualified welding procedure.

Conclusion

Q620qD to GB/T 714-2025 is bridge plate with 620 MPa minimum yield, 720 MPa minimum tensile and 120 J Charpy at −20°C for 12–100 mm plate.

It sits between Q550qD and Q690qD in the bridge range, with Q620qE and Q620qF as sister letters. For Q620qD, the deciding numbers on the certificate are yield at the actual thickness, Charpy at −20°C and the weldability index for the delivery route.

SHH STEEL delivers Q620qD with the full GB/T 714 data set on an EN 10204 3.1 or 3.2 certificate. On request we add product analysis to GB/T 222, Z15–Z35, a tighter UT class, Class C tolerance, cutting and blasting.

We ship from Shanghai to bridge builders worldwide. Browse the full GB/T 714 range or other high strength low alloy plates.

Send the edition, quality letter, Z level and size list; we confirm mill, delivery route, lead time and price in one reply. Contact SHH STEEL for a mill-direct quotation on Q620qD bridge steel plate.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X