GB/T 714 Q345qNHE Weathering Bridge Steel Supplier
What is GB/T 714 Q345qNHE Weathering Bridge Steel?
Q345qNHE is weathering bridge structural steel to GB/T 714. In the standard’s own notation it is written Q345qENH: Q for yield, 345 for the minimum yield in MPa, q for qiao (bridge), the quality letter, and NH for nai hou, weathering. The letter E means Charpy V-notch testing at −40°C.
Q345qNH is the most widely used weathering bridge steel in China, for unpainted plate girders and box girders in rural and urban atmospheres. Q345qNH carries the same 345 MPa tensile table as Q345q, but adds Cu, Cr and Ni (Cu 0.25–0.50%, Cr 0.40–0.70%, Ni 0.30–0.40%) so a dense patina forms and paint can be left off. GB/T 714-2025 lists ASTM A709 50W and HPS 50W against Q345q.
Q345qNHE (Q345qENH) is the unpainted bridge plate for cold regions: −40°C Charpy, 120 J from 12 to 100 mm, and the Cu-Cr-Ni weathering chemistry. On the Zangmu Yarlung Tsangpo River Bridge (Lhasa–Nyingchi railway, 430 m arch span, 3,300–3,500 m altitude), Q345qENH was used for web members, bracing and cross beams, with Q420qENH arch ribs, all unpainted.
GB/T 714-2025, in force since 1 May 2026, fully replaces GB/T 714-2015; the changes for weathering grades are listed below.
SHH STEEL (Shanghai Shenghonghe Import & Export Co., Ltd.) is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. We ship Q345qNHE cut to size with an EN 10204 3.1 or 3.2 certificate. Sister grades are listed under GB/T 714; other unpainted options are under weathering steel plates and EN 10025-5.
Material Specification
| Specification element | Requirement | SHH STEEL compliance |
|---|---|---|
| Standard | GB/T 714-2025 Q345qENH | Confirmed |
| Product | Single-rolled plate ≤150 mm; hot-rolled strip and cut plate ≤25.4 mm | Plate |
| Thickness with tensile values | Up to 150 mm for Q345qNH | Confirmed |
| Minimum yield ReL | 345 MPa ≤50 mm; 335 MPa >50–100 mm | Confirmed |
| Minimum tensile Rm | 490 MPa ≤100 mm (no upper limit in the standard) | Confirmed |
| Elongation A | ≥ 20% | Confirmed |
| Charpy V-notch | −40°C, 120 J (12–100 mm), longitudinal | Confirmed |
| Weathering index | I ≥ 6.0 (Table 5, footnote c) | Calculated on MTC |
| Delivery condition | TMCP or TMCP + tempering | As ordered |
| Weldability index | Pcm (Table 8) | Printed on MTC |
| Ultrasonic testing | Plate >20 mm: GB/T 2970, Class II or better | Every plate |
| Through-thickness | Z15, Z25 or Z35 to GB/T 5313, when ordered | As ordered |
| Dimensions | GB/T 709 | Confirmed |
| Certificate | GB/T 247; EN 10204 3.1 or 3.2 | As ordered |
Grades often compared with Q345qNHE are ASTM A709 Grade 50W, ASTM A709 HPS 50W and EN 10025-5 S355J2W; the comparison below shows where they differ.
Chemical Composition: Heat Analysis and Product Analysis
Bridge owners increasingly order a product analysis on finished plate. For Q345qNHE that check is judged against GB/T 714 heat limits plus the deviations in GB/T 222, not against the heat limits alone.
Table 1 below is the heat (ladle) analysis for Q345qNHE from GB/T 714-2025 Tables 1, 5.
| Element | Q345qNHE heat analysis (%) | Note |
|---|---|---|
| C, max | 0.11 | |
| Si | 0.15 – 0.50 | Counts in I |
| Mn | 1.10 – 1.50 | Min 0.50% for coil only |
| P, max | 0.020 | Letter E |
| S, max | 0.010 | Letter E |
| Cu | 0.25 – 0.50 | Main weathering element |
| Cr | 0.40 – 0.70 | Weathering element |
| Ni | 0.30 – 0.40 | Weathering element |
| Mo, max | 0.20 | Changed in 2025 |
| Nb | 0.010 – 0.100 | Microalloy (see note) |
| V | 0.010 – 0.100 | Microalloy (see note) |
| Ti | 0.006 – 0.030 | Microalloy (see note) |
| Als | 0.015 – 0.050 | Alt 0.020–0.055% if total Al is used |
| N, max | 0.0080 | |
| B, max (residual) | 0.0005 | ≤0.0014% if C ≤0.06% |
| H, max (residual) | 0.0002 | |
| Weathering index I | ≥ 6.0 | Calculated from heat analysis |
Nb, V, Ti and Al may be added singly or together. Added singly, each must meet the range above; added together, at least one must reach its minimum and Nb + V + Ti ≤ 0.22%. Calcium treatment is required to control sulfide shape.
Table 2 is the product analysis: the limits a check analysis on finished plate is judged against. GB/T 714-2025 clause 7.1.3 calls up GB/T 222 for the permitted deviations.
| Element | Heat limit (%) | Deviation, GB/T 222-2025 Table 1 | Q345qNHE product analysis (%) |
|---|---|---|---|
| C | ≤ 0.11 | +0.02 | ≤ 0.13 |
| Si | 0.15 – 0.50 | ±0.05 | 0.10 – 0.55 |
| Mn | 1.10 – 1.50 | ±0.06 | 1.04 – 1.56 |
| P | ≤ 0.020 | +0.005 | ≤ 0.025 |
| S | ≤ 0.010 | +0.005 | ≤ 0.015 |
| V | 0.010 – 0.100 | +0.02 / −0.01 | ≤ 0.120 |
| Ti | 0.006 – 0.030 | +0.02 / −0.01 | ≤ 0.050 |
| Nb | 0.010 – 0.100 | ±0.005 (listed for 0.015–0.060%) | Above 0.060%: agree in contract |
| Cu | 0.25 – 0.50 | ±0.05 | 0.20 – 0.55 |
| Cr | 0.40 – 0.70 | ±0.05 | 0.35 – 0.75 |
| Ni | 0.30 – 0.40 | ±0.05 | 0.25 – 0.45 |
| Als | 0.015 – 0.050 | ±0.003 | Lower limit −0.003 (Table 1 row is for Al ≥0.015%; confirm) |
| Mo | ≤ 0.20 | Not listed in Table 1 | Agree in contract |
| N | ≤ 0.0080 | Listed only for 0.010–0.020% | Agree in contract |
How to read Table 2. Weathering bridge steel is normally classed as low-alloy steel, so Table 1 of GB/T 222 applies. Where the heat limit is a range, the deviation applies to both ends; for one heat, an element may deviate in one direction only.
Mechanical Properties
Tensile values follow Table 9 of GB/T 714-2025 for Q345qNH. Tensile specimens are transverse; round specimens are used above 40 mm. Where yield is not distinct, Rp0.2 replaces ReL.
| Nominal thickness | ReL min (MPa) | Rm min (MPa) | A min |
|---|---|---|---|
| ≤ 50 mm | 345 | 490 | 20% |
| > 50 – 100 mm | 335 | 490 | 20% |
| > 100 – 130 mm | 305 | 430 | 20% |
| > 130 – 150 mm | 305 | 430 | 20% |
Impact values follow Table 10, on longitudinal specimens, average of three:
| Letter / test temperature | KV2 ≤12 mm | KV2 >12 – 100 mm | KV2 >100 – 150 mm |
|---|---|---|---|
| E / −40°C | 80 J | 120 J | 31 J |
One single value may fall below the required average, but not below 70% of it. Plate over 8 mm and under 12 mm is tested with 7.5 mm specimens (75% of the value); 6–8 mm plate with 5 mm specimens (50%). Plate under 6 mm is not impact tested.
180° bend test, transverse: mandrel D = 2a up to 16 mm and 3a above 16 mm; may be omitted when the mill guarantees it. Yield ratio is not mandatory. If the contract asks for it, Annex C recommends ReL/Rm ≤ 0.88 up to 12 mm and ≤ 0.85 above 12 mm for TMCP plate.
Q345qNHC / Q345qNHD / Q345qNHE: Which Quality Grade?
Q345qNHE was tested at −60°C under GB/T 714-2015. In the 2025 tables the Q345qNH level stops at E (−40°C); the table shows what is listed today.
| Grade | Test temp. | KV2 ≤12 mm | KV2 12–100 mm | KV2 >100 mm | P / S max (%) |
|---|---|---|---|---|---|
| Q345qNHC | 0°C | 80 J | 120 J | 55 J | 0.030 / 0.025 |
| Q345qNHD | −20°C | 80 J | 120 J | 47 J | 0.025 / 0.015 |
| Q345qNHE | −40°C | 80 J | 120 J | 31 J | 0.020 / 0.010 |
| Q345qNHF | −60°C | 2015 edition only | 2015 edition only | — | 0.015 / 0.006 (2025 Table 1, F) |
For Q345qNHE the 2025 table stops at E. A −60°C requirement can still be met: by certifying to the 2015 edition where the contract allows, or by ordering Q345qENH with a supplementary −60°C test and an agreed energy. Where higher strength is acceptable, Q420qNHF is a listed −60°C weathering grade.
Q345qNHE: What Changed from GB/T 714-2015 to GB/T 714-2025
For Q345qNHE buyers the 2025 edition changes more than the year on the certificate. The points below come from the foreword of GB/T 714-2025 and its tables.
- The weathering requirement changed: Table 5 now requires a corrosion index I ≥ 6.0, and the 2015 Annex C guide for assessing weathering resistance was deleted.
- A Pcm table for weathering steel (Table 8) was added.
- Annex A now gives reference bridge-site environments for unpainted use (chloride, SO₂ and time-of-wetness limits).
- Mo maximum for Q345qNH was changed (now ≤0.20%; 2015-based sources quote ≤0.10%).
- Q345qNH is now listed in letters C, D and E. The 2015 edition listed it in D, E and F.
- Tensile strength is now banded by thickness (e.g. lower minimum Rm above 100 mm) instead of one value.
- Impact energy is set by thickness band (≤12 mm, 12–100 mm, >100 mm) in Table 10.
- Yield ratio is no longer a clause value; it is agreed in the contract, with recommendations in informative Annex C.
If a drawing cites 2015 and the plate is made to 2025, get the designer’s written acceptance; tensile strength above 100 mm and the yield-ratio basis differ.
Q345qNHE vs ASTM A709 and EN 10025: Which Grade Matches?
Can Q345qNHE replace a US or European bridge grade, or the other way round? Strength can match; toughness rules differ in kind, not only in number.
| Property | Q345qNHE | ASTM A709 Grade 50W | ASTM A709 HPS 50W | EN 10025-5 S355J2W |
|---|---|---|---|---|
| Min. yield (MPa) | 345 (≤50 mm) | 345 | 345 | 355 (≤16 mm) |
| Tensile (MPa) | 490 min | 485 min | 485 min | 470 – 630 |
| Charpy | 120 J at −40°C (12–100 mm) | CVN by temperature zone and member type (T / F) | CVN by temperature zone; fracture-critical (F) levels | 27 J at −20°C |
| Weathering chemistry | Yes, I ≥ 6.0 | Yes | Yes | Yes |
ASTM A709 sets Charpy requirements by temperature zone (1, 2, 3) and by member type: non-fracture-critical (T) or fracture-critical (F). GB/T 714 sets one value per letter, so compare the A709 zone with the GB/T 714 test temperature, not grade with grade.
EN 10025-5 weathering grades are general structural steels without a bridge-specific toughness level of 120 J; they suit many bridges but are not a one-to-one match.
The 120 J requirement for 12–100 mm plate is several times the 27–40 J typical of general weathering grades such as ASTM A588 or Corten A/B plate, which is why bridge owners specify Q345qNHE.
Q345qNHE Atmospheric Corrosion Index I and Unpainted Bridges
GB/T 714-2025 Table 5, footnote c, requires every Q345qNHE heat to reach an atmospheric corrosion index I of at least 6.0, calculated from the heat analysis:
I = 26.01(%Cu) + 3.88(%Ni) + 1.20(%Cr) + 1.49(%Si) + 17.28(%P) − 7.29(%Cu)(%Ni) − 9.10(%Ni)(%P) − 33.39(%Cu)²
This is the same predictive formula used with ASTM G101 for ASTM A709 Grade 50W and ASTM A709 HPS 70W, which makes Chinese and US ASTM A709 weathering steel plates easy to compare with Q345qNHE.
| Worked example (our calculation) | Cu | Ni | Cr | Si | P | I |
|---|---|---|---|---|---|---|
| All weathering elements at their Table 5 minimum | 0.25 | 0.30 | 0.40 | 0.15 | 0.010 | 5.88 |
| Illustrative mid-range heat | 0.32 | 0.36 | 0.55 | 0.30 | 0.012 | 6.74 |
Note the first row: a heat that only just meets every Table 5 minimum can still fall short of I = 6.0. That is why we ask the mill to print I on every Q345qNHE certificate, not just the chemistry.
Where can the steel be left unpainted? Annex A of GB/T 714-2025 gives reference bridge-site conditions:
- Rural or urban atmosphere with annual chloride deposition ≤ 3 mg/(m²·d)
- Annual SO₂ deposition ≤ 24 mg/(m²·d)
- Time of wetness ≤ 5,256 h per year (temperature above 0°C and relative humidity above 80%)
- Coastal sites only if they meet the same limits; for marine atmospheres Annex D points to T/CISA 073
Detailing decides whether unpainted Q345qNHE works. Avoid ledges that hold water, seal box girders or ventilate them, keep deck joints watertight, and protect piers from rust run-off in the first years while the patina forms.
Welding Q345qNHE and Fatigue in Bridge Girders
GB/T 714-2025 clause 7.1.2 uses CEV for normalized, QT and TMCP steel with C >0.12%, and Pcm for weathering steel and TMCP steel with C ≤0.12%, both from the heat analysis:
CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15
Pcm = C + Si/30 + Mn/20 + Cu/20 + Ni/60 + Cr/20 + Mo/15 + V/10 + 5B
| Index | ≤50 mm | >50–100 mm | >100–130 mm |
|---|---|---|---|
| Pcm, Q345qNH (Table 8) | ≤ 0.22 | ≤ 0.24 | By agreement |
Preheat for Q345qNHE is set by the qualified welding procedure, from the actual index on the certificate, plate thickness, restraint and hydrogen level. Lower actual values than the table caps save preheat time on large girders. At −40°C, HAZ toughness often becomes the limit. Fabricators usually cap heat input and qualify the procedure at −40°C on plate from the same route.
Typical consumables for Q345qNHE: weathering-matched Ni-Cu consumables (AWS E8018-W2 type for 345–420 MPa), with higher-strength weathering wires for 460–500 MPa.
Fatigue. Welded details govern fatigue life in a bridge, and their fatigue strength is set by detail category, not by yield strength. Higher-strength plate can carry higher stress ranges only if detailing improves too.
Fatigue design follows JTG D64 (highway) and TB 10091 (railway) in China, EN 1993-1-9 in Europe and AASHTO LRFD in the US; fabrication commonly follows TB 10212, JTG/T 3650 or AWS D1.5.
Q345qENHZ15, Z25 and Z35: Through-Thickness Plate for Bridges
A Z grade is cheap insurance for heavily restrained joints. It caps sulfur and proves reduction of area in the thickness direction with a short-transverse tensile test.
GB/T 714 adds the Z level to the end of the designation, for example Q345qENHZ25. The test and acceptance follow GB/T 5313 and apply to plate 15 mm and thicker.
| Z grade | Heat sulfur, max (%) | Reduction of area, avg / single (%) |
|---|---|---|
| Z15 | 0.010 | 15 / 10 |
| Z25 | 0.007 | 25 / 15 |
| Z35 | 0.005 | 35 / 25 |
E chemistry already limits S to 0.010%, the Z15 sulfur cap. Z25 (S ≤0.007%) and Z35 (S ≤0.005%) still need a cleaner heat.
A Z level on Q345qNHE does not change strength or impact rules. It adds a sulfur cap and a short-transverse tensile test. Z options apply across the GB/T 714 bridge steel range.
Equivalent Material Grades
Annex B of GB/T 714-2025 lists foreign grades against each strength level. It is informative: it tells you which families are close, not that the plates are interchangeable.
| Standard | Grade(s) | Fit for Q345qNHE |
|---|---|---|
| ASTM A709 | ASTM A709 Grade 50W, ASTM A709 HPS 50W | Listed in Annex B |
| EN 10025-5 | EN 10025-5 S355J2W, EN 10025-5 S355K2W | Closest weathering grades |
| ASTM A588 | ASTM A588 Grade A, ASTM A588 Grade B | Similar chemistry family |
| Trade name | Corten B | Similar weathering concept, not a bridge standard |
| GB/T 714 (painted twin) | Q345qE | Same strength, no weathering elements |
For weathering grades also compare the corrosion index basis. Q345qNHE requires I ≥ 6.0 by the formula above; check that the substitute is assessed on the same basis.
Q345qNHE Testing, UT and Certificate
A batch of Q345qNHE is one grade, one heat, one thickness, one rolling schedule and one heat-treatment condition, up to 60 t. Table 12 of GB/T 714-2025 sets the tests:
| Test | Frequency | Method |
|---|---|---|
| Heat analysis | 1 per heat | GB/T 20066; GB/T 4336 / GB/T 223 |
| Weathering index I | Calculated per heat | Table 5 formula |
| Tensile | 1 per batch | GB/T 2975 / GB/T 228.1 |
| Bend 180° | 1 per batch (may be waived if guaranteed) | GB/T 232 |
| Charpy V at −40°C | 3 specimens per batch | GB/T 229 |
| Through-thickness (Z) | 3 specimens per batch, when ordered | GB/T 5313 |
| Ultrasonic | Every plate >20 mm, Class II or better | GB/T 2970 |
| Surface and dimensions | Every plate | Visual and gauges |
Impact retest: if a set fails, three more specimens are taken from the same batch. The average of all six must meet the requirement; two values may be below it, but only one below 70%. At −40°C, retest risk rises on heavy plate; we build a margin for retests into the delivery schedule.
Dimensions
Typical Q345qNHE dimensions on our offers:
- Thickness: 6 mm – 150 mm under GB/T 714 tensile tables; most orders 8 – 60 mm
- Width: 1500 – 4000 mm, depending on mill and thickness
- Length: 6000 – 18000 mm; longer by enquiry
- Edge: mill edge or cut edge
- Weight: theoretical, 7.85 g/cm³
Deck plate, webs, flanges, diaphragms and stiffeners are cut to drawing. For U-ribs and rolled sections on the same bridge, see steel beam profiles and steel structural profiles.
Tolerances
Dimensional tolerances for Q345qNHE follow GB/T 709, as GB/T 714 directs. The default is Class B, which fixes the minus side at 0.30 mm.
| Nominal thickness (mm) | Width ≤ 1500 mm | Width > 1500 – 2500 mm |
|---|---|---|
| > 8 – 15 | −0.30 / +0.80 | −0.30 / +1.00 |
| > 15 – 25 | −0.30 / +1.00 | −0.30 / +1.20 |
| > 25 – 40 | −0.30 / +1.10 | −0.30 / +1.30 |
| > 40 – 60 | −0.30 / +1.30 | −0.30 / +1.50 |
| > 60 – 100 | −0.30 / +1.50 | −0.30 / +1.80 |
| > 100 – 150 | −0.30 / +2.10 | −0.30 / +2.50 |
Bridge fabricators often ask for Class C (zero minus) on deck and flange plate so section properties are never under the design value. Wider plates follow the heavier GB/T 709 rows; we state them on the offer.
Q345qNHE Price Factors and How to Order
Bridge plate prices move with the steel market, but for Q345qNHE the order details often matter more.
| Cost driver | Effect on price |
|---|---|
| Strength level Q345q | Higher levels need more alloy and tighter rolling control |
| Quality letter | Higher extra: −40°C testing, S ≤0.010%, more retest risk |
| Weathering alloys | Cu, Cr, Ni additions and I-index control add a weathering extra |
| Delivery route | TMCP / TMCP+T |
| Thickness | Over 60 mm and under 10 mm carry size extras |
| Z15 / Z25 / Z35 | Low-sulfur heat, Z test, UT; Z35 costs most |
| Width and length | Over 3000 mm wide or 15 m long needs mill confirmation |
| Quantity per size | Mill minimums per heat and size |
| Inspection and processing | 3.2 witness, profile cutting, blasting, priming quoted per item |
To get a firm quote in one round, send:
- Grade, edition and Z level, e.g. Q345qENHZ25 to GB/T 714-2025
- Thickness × width × length and pieces or tonnes
- Delivery route and UT class if beyond Class II
- Certificate type and inspector
- Destination port and Incoterm
We quote plate price, extras and freight line by line. Need another letter? See Q345qNHD.
Applications
| Sector | Typical Q345qNHE components |
|---|---|
| Unpainted highway bridges | Plate girders and box girders in rural and urban atmospheres |
| Railway bridges | Truss members, plate girders, bracing |
| Remote and mountain sites | Bridges where repainting access is difficult or costly |
| Urban viaducts | Exposed girders with architectural rust finish |
| Pedestrian bridges | Unpainted box sections |
The letter E suits bridges in north-east China, Inner Mongolia, Xinjiang, Russia, Kazakhstan, Canada and high-altitude sites, and for thick, restrained members anywhere.
Q345qNHE is the wrong plate for marine splash zones, tunnels, sites with heavy de-icing salt spray, or members that stay wet. There, use painted Q345qE or look at marine-atmosphere grades under T/CISA 073.
Supply Capability and Global Delivery
SHH STEEL sources Q345qNHE from first-line bridge-plate mills, including drafters of GB/T 714-2025 such as Ansteel, Valin Xiangtan, Jiangyin Xingcheng, Wuyang, Shougang and Xinyu.
- Certificates: EN 10204 3.1 standard; 3.2 with third-party witness (SGS, BV, TÜV or owner’s inspector)
- Tests: tensile, −40°C Charpy, bend, Z test, UT, product analysis, weathering index
- Processing: CNC plasma and flame cutting, bevelling, drilling, shot blasting and priming (or blasting only, for unpainted weathering steel)
- Terms: FOB Shanghai, CFR, CIF; TT, LC or TT + LC
- Marking: steel-stamped and paint-marked with grade, heat, size and mill, per GB/T 247
We ship GB, ASTM, EN and JIS plate to the Americas, Europe, the Middle East, Southeast Asia and Africa. Q345qNHE mostly goes to EPC contractors building bridges to Chinese codes abroad.
Lead time: about 45–60 days from mill rolling; Z35, F letter or 3.2 inspection adds about 1–2 weeks. Sea time from Shanghai is about 7–12 days to Southeast Asia and 28–35 days to North Europe.
Why Choose SHH STEEL
SHH STEEL is mill-direct: steel manufacturer and exporter and global steel mill sourcing partner, China origin. Every Q345qNHE plate we ship carries the original mill heat number.
Before shipment we check four lines on every Q345qNHE certificate: yield and tensile for the actual thickness band, Charpy at −40°C, the Pcm and weathering index, and UT results. If one fails, the plate does not ship as Q345qNHE.
In cold regions with de-icing salt, check chloride exposure at the bridge site against Annex A of GB/T 714-2025 before leaving the steel unpainted.
We also tell buyers when another grade fits better. Neighbouring levels are Q370qNHE. The painted counterpart is Q345qE. Browse more structural steel plates and high strength low alloy plates.
FAQ
-
What is Q345qNHE steel?
- Q345qNHE (Q345qENH) is weathering bridge steel plate to GB/T 714-2025. It has 345 MPa minimum yield up to 50 mm, 490 MPa minimum tensile, Charpy impact of 120 J at −40°C for 12–100 mm plate, and Cu-Cr-Ni chemistry with a corrosion index I of at least 6.0 for unpainted bridges.
-
What is the difference between Q345qNHE and Q345qNHD?
- Strength and chemistry box are the same. Q345qNHE is Charpy tested at −40°C, Q345qNHD at −20°C, both needing 120 J for 12–100 mm plate. P/S caps are 0.020/0.010% for E and 0.025/0.015% for D. Choose by the lowest service or erection temperature.
-
Is Q345qNHE the same as Q345E?
- No. Q345E is general structural steel (now Q355 under GB/T 1591-2018), while Q345qNHE is bridge steel to GB/T 714 with lower P and S, controlled weldability index, mandatory UT above 20 mm and 120 J impact for 12–100 mm plate. Bridge plate can replace general plate, not the reverse.
-
What is the ASTM or EN equivalent of Q345qNHE?
- Close grades for Q345qNHE: ASTM A709 50W / HPS 50W (Annex B) / EN 10025-5 S355J2W, S355K2W (closest) / ASTM A588 (closest). These are close families, not drop-in substitutes; compare yield at thickness, impact temperature and energy, and the weldability index before substituting.
-
Does GB/T 714 require ultrasonic testing?
- Yes. GB/T 714-2025 clause 7.5 requires every single-rolled plate over 20 mm to be ultrasonically tested to GB/T 2970, with acceptance Class II or better. Thinner plate is tested only by agreement.
-
Does Q345qNHE weathering steel need painting?
- Not if the bridge site and details suit it. GB/T 714-2025 Annex A gives reference conditions for unpainted use: annual chloride deposition ≤3 mg/(m²·d), SO₂ ≤24 mg/(m²·d) and time of wetness ≤5,256 h per year. Marine splash zones and salt-sprayed members still need protection.
Conclusion
Q345qNHE to GB/T 714 is weathering bridge steel with 345 MPa minimum yield, Cu-Cr-Ni chemistry, a weathering index of at least 6.0 and 120 J Charpy at −40°C for 12–100 mm plate.
The next strength level is Q370qNHE, with Q345qNHD as sister letters. We check every Q345qNHE order against GB/T 714-2025 before quoting, so the offer, the test plan and the certificate all match the drawing.
With SHH STEEL the Q345qNHE certificate is complete: heat chemistry, weldability index, yield, tensile, elongation and Charpy, to EN 10204 3.1 or 3.2. Add product analysis, a Z level or a stricter UT class as needed.
We ship from Shanghai to bridge builders worldwide. Browse the full GB/T 714 range or other weathering steel plates.
Share your size list, Z level and edition, and we reply with mill, route, lead time, test plan and price in one message. Contact SHH STEEL for a mill-direct Q345qNHE weathering bridge steel quotation.