GB/T 714 Q690qF bridge steel plate stacked at SHH STEEL warehouse

GB/T 714 Q690qF Bridge Steel Plate Supplier

GB/T 714 Q690qF is bridge structural steel plate with 690 MPa minimum yield, 770 MPa minimum tensile and Charpy V-notch impact of 77 J at −60°C for 12–100 mm plate. SHH STEEL supplies Q690qF mill-direct, TMCP / TMCP+T / QT, up to 100 mm, with Z15–Z35, UT and heat and product analysis.
Keywords
Q690qF, Q690qF steel plate, GB/T 714 Q690qF, Q690q-F, Q690q F, Q690qF bridge steel, Q690qFZ15, Q690qFZ25, Q690qFZ35, bridge steel plate, Q690qF supplier
Equivalent Grades:
ASTM A709 HPS 100W / EN 10025-6 S690Q, S690QL, S690QL1 (Annex B) — Material Specification: GB/T 714-2025 (supersedes GB/T 714-2015) — Delivery: TMCP / TMCP+T / QT
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Q690q Quality Grades
GB/T 714-2025 vs 2015
Q690qF vs ASTM A709 / EN 10025
TMCP vs Normalized vs QT
Welding and Fatigue
Z15 / Z25 / Z35
Equivalent Material Grades
Testing and Inspection
Dimensions
Tolerances
Price and Ordering
Applications
Supply Capability
Why Choose SHH STEEL
FAQ
Conclusion

What is GB/T 714 Q690qF Bridge Steel Plate?

Q690qF is bridge structural steel plate to GB/T 714. Q stands for yield, 690 is the minimum yield in MPa for plate up to 50 mm, q stands for qiao (bridge) and F is the quality grade: Charpy V-notch at −60°C on longitudinal specimens.

Q690q is the top strength level of GB/T 714, with 690 MPa yield up to 50 mm and 650 MPa to 100 mm. Annex B lists ASTM A709 HPS 100W against Q690q. It is a specialist plate: thin, highly stressed members on record spans, where every tonne of girder weight saved reduces cable, pylon and foundation size.

Q690qF is the most demanding plate in GB/T 714: 690 MPa yield and 77 J at −60°C for plate over 12 mm. Very few mills offer it, and only to order.

GB/T 714-2025 has been in force since 1 May 2026, replacing GB/T 714-2015 in full. If your specification was written earlier, check the edition before ordering: some table values changed, and a few grades were added or dropped.

SHH STEEL (Shanghai Shenghonghe Import & Export Co., Ltd.) is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. We ship Q690qF cut to size with an EN 10204 3.1 or 3.2 certificate. Sister grades are listed under GB/T 714.

Material Specification

Specification element Requirement SHH STEEL compliance
Standard GB/T 714-2025 Q690qF Confirmed
Product Single-rolled plate ≤150 mm; hot-rolled strip and cut plate ≤25.4 mm Plate
Thickness with tensile values Up to 100 mm for Q690q Confirmed
Minimum yield ReL 690 MPa ≤50 mm; 650 MPa >50–100 mm Confirmed
Minimum tensile Rm 770 MPa ≤100 mm (no upper limit in the standard) Confirmed
Elongation A ≥ 14% Confirmed
Charpy V-notch −60°C, 77 J (12–100 mm), longitudinal Confirmed
Delivery condition TMCP, TMCP + tempering, or quenched and tempered (QT) As ordered
Weldability index Pcm (Table 7) for TMCP; CEV (Table 6) for QT Printed on MTC
Ultrasonic testing Plate >20 mm: GB/T 2970, Class II or better Every plate
Through-thickness Z15, Z25 or Z35 to GB/T 5313, when ordered As ordered
Dimensions GB/T 709 Confirmed
Certificate GB/T 247; EN 10204 3.1 or 3.2 As ordered

Grades often compared with Q690qF are ASTM A709 HPS 100W and ASTM A514 Grade Q; the comparison below shows where they differ.

Chemical Composition: Heat Analysis and Product Analysis

Third-party labs test plate, not ladles. So when an inspector checks Q690qF, the result is a product analysis and must be compared with product limits, not with the heat limits on the certificate.

Table 1 below is the heat (ladle) analysis for Q690qF from GB/T 714-2025 Tables 1, 2, 3 and 4.

Element Q690qF TMCP (%) Q690q quenched and tempered (%)
C, max 0.11 0.15
Si, max 0.50 0.55
Mn 0.80 – 1.70 0.80 – 1.70
P, max 0.015 0.015
S, max 0.006 0.006
Nb 0.005 – 0.090 0.005 – 0.090
V 0.010 – 0.080 0.010 – 0.080
Ti 0.006 – 0.030 0.006 – 0.030
Als 0.010 – 0.045 0.010 – 0.045
Cr, max 1.00 0.40 – 1.00
Ni, max 1.20 0.25 – 1.20
Cu, max 0.55 0.15 – 0.55
Mo, max 0.60 0.20 – 0.60
N, max 0.0080 0.0080
B, max 0.0005 residual (≤0.0014 if C ≤0.10%) 0.0005–0.0030 may be added
H, max 0.0002 0.0002

Nb, V, Ti and Al may be added singly or together. Added singly, each must meet the range above; added together, at least one must reach its minimum and Nb + V + Ti ≤ 0.22%.

Table 2 is the product analysis: the limits a check analysis on finished plate is judged against. GB/T 714-2025 clause 7.1.3 calls up GB/T 222 for the permitted deviations.

Element Heat limit (%) Deviation, GB/T 222-2025 Table 2 (alloy) Q690qF product analysis (%)
C ≤ 0.11 +0.01 ≤ 0.12
Si ≤ 0.50 +0.04 ≤ 0.54
Mn 0.80 – 1.70 ±0.04 0.76 – 1.74
P ≤ 0.015 +0.005 (see note) ≤ 0.020
S ≤ 0.006 +0.005 (see note) ≤ 0.011
Cr ≤ 1.00 +0.05 (0.90–2.10% band) ≤ 1.05
Ni ≤ 1.20 +0.05 (1.00–2.00% band) ≤ 1.25
Cu ≤ 0.55 +0.03 ≤ 0.58
Mo ≤ 0.60 +0.02 (0.30–0.60% band) ≤ 0.62
V 0.010 – 0.080 +0.01 (≤0.10% band) ≤ 0.090
Ti 0.006 – 0.030 +0.02 ≤ 0.050
Nb, B, N See heat table Not read in our copy of Table 2 Agree in contract

How to read Table 2. With Ni up to 1.20% and Mo up to 0.60%, Q690q heats are normally classed as alloy steel under GB/T 13304, so the alloy-steel table of GB/T 222 applies. One steel uses one table only; the certificate should say which.

Mechanical Properties

Tensile values follow Table 9 of GB/T 714-2025 for Q690q. Tensile specimens are transverse; round specimens are used above 40 mm. Where yield is not distinct, Rp0.2 replaces ReL.

Nominal thickness ReL min (MPa) Rm min (MPa) A min
≤ 50 mm 690 770 14%
> 50 – 100 mm 650 770 14%

Impact values follow Table 10, on longitudinal specimens, average of three:

Letter / test temperature KV2 ≤12 mm KV2 >12 – 100 mm KV2 >100 – 150 mm
F / −60°C By agreement 77 J Not applicable

One single value may fall below the required average, but not below 70% of it. Plate over 8 mm and under 12 mm is tested with 7.5 mm specimens (75% of the value); 6–8 mm plate with 5 mm specimens (50%). Plate under 6 mm is not impact tested.

180° bend test, transverse: mandrel D = 2a up to 16 mm and 3a above 16 mm; may be omitted when the mill guarantees it. Yield ratio is not mandatory and Annex C gives no recommended value at this level; agree a limit in the contract if the design needs one.

Q690qD / Q690qE / Q690qF: Which Quality Grade?

Q690qF is tested at −60°C. It suits Arctic and sub-Arctic bridges, high-latitude rail lines and owners who want the largest toughness margin for fracture-critical members. F is the coldest letter in GB/T 714: Charpy at −60°C, P ≤0.015% and S ≤0.006%. It exists only for Q420q and above (and their NH versions), and its energy rises with strength.

Grade Test temp. KV2 ≤12 mm KV2 12–100 mm KV2 >100 mm P / S max (%)
Q690qD −20°C 80 J 120 J — 0.025 / 0.015
Q690qE −40°C 80 J 120 J — 0.020 / 0.010
Q690qF −60°C By agreement 77 J — 0.015 / 0.006

Note that F energy at Q690q is 77 J, not 120 J: the colder test uses a lower energy that GB/T 714-2025 raises with strength, from 47 J at Q420q/Q460q to 77 J at Q690q. Plate up to 12 mm needs an agreed value.

Q690qF: What Changed from GB/T 714-2015 to GB/T 714-2025

For Q690qF buyers the 2025 edition changes more than the year on the certificate. The points below come from the foreword of GB/T 714-2025 and its tables.

  • A TMCP route was added for Q690q (C ≤0.11%, Pcm ≤0.24% to 50 mm). In 2015 it was QT only.
  • CEV and Pcm limits were revised (Tables 6 and 7).
  • Tensile strength is now banded by thickness (e.g. lower minimum Rm above 100 mm) instead of one value.
  • Impact energy is set by thickness band (≤12 mm, 12–100 mm, >100 mm) in Table 10.
  • Yield ratio is no longer a clause value; it is agreed in the contract, with recommendations in informative Annex C.
  • Section products were removed; the standard now covers plate and strip only.
  • Delivery is TMCP, TMCP + tempering or QT; normalizing is kept only for Q345q/Q370q plate over 100 mm by agreement.

If a drawing cites 2015 and the plate is made to 2025, get the designer’s written acceptance; tensile strength above 100 mm and the yield-ratio basis differ.

Q690qF vs ASTM A709 and EN 10025: Which Grade Matches?

Can Q690qF replace a US or European bridge grade, or the other way round? Strength can match; toughness rules differ in kind, not only in number.

Property Q690qF ASTM A709 HPS 100W ASTM A514 Grade Q EN 10025-6 S690Q
Min. yield (MPa) 690 (≤50 mm) 690 (≤65 mm) 690 (≤65 mm) 690 (≤50 mm)
Tensile (MPa) 770 min 760 – 895 760 – 895 770 – 940
Charpy 77 J at −60°C (12–100 mm) CVN by temperature zone; fracture-critical (F) levels Supplementary only Q / QL / QL1: −20 / −40 / −60°C
Weathering chemistry No Yes No No

ASTM A709 sets Charpy requirements by temperature zone (1, 2, 3) and by member type: non-fracture-critical (T) or fracture-critical (F). GB/T 714 sets one value per letter, so compare the A709 zone with the GB/T 714 test temperature, not grade with grade.

EN 10025-3/-4/-6 grades show yield at the thinnest band; their values fall with thickness. GB/T 714 keeps 690 MPa to 50 mm. EN tensile ranges have upper limits; GB/T 714 gives minimums only.

At −60°C, the 77 J required for Q690qF is a demanding figure; general structural grades rarely prove any toughness that cold. For the C, D and E letters GB/T 714 asks 120 J, several times the 27–40 J typical of GB/T 1591 plate.

Q690qF Delivery Condition: TMCP vs Normalized vs Quenched and Tempered

GB/T 714-2025 clause 3.2 defines TMCP as rolling with the final deformation in a controlled temperature range, including accelerated cooling with or without tempering (self-tempering included) but excluding direct quenching and quench-and-temper. The delivery route must be stated on the certificate.

Route Available for Q690qF Weldability index Notes
TMCP Yes Pcm ≤0.24% (≤50 mm) C ≤0.11%; up to 100 mm
TMCP + tempering Yes Pcm Improves toughness uniformity
Quenched and tempered Yes CEV ≤0.60% (≤50 mm) C ≤0.15%; B 0.0005–0.0030% may be added
Normalized No — Not listed

Q690q can be TMCP or QT. A published study on 40 mm Q690qNH plate found QT plate more uniform in strength and toughness through the thickness than TMCP + tempered plate; we discuss route choice with the owner on every Q690q enquiry. F-letter plate is often TMCP + tempering or, at the top strength levels, QT; ask which route the mill has qualified for −60°C.

Ask for the route on the purchase order. It changes the weldability index, the welding procedure and, for heavy plate, the price of Q690qF.

Welding Q690qF and Fatigue in Bridge Girders

GB/T 714-2025 clause 7.1.2 uses CEV for normalized, QT and TMCP steel with C >0.12%, and Pcm for weathering steel and TMCP steel with C ≤0.12%, both from the heat analysis:

CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15

Pcm = C + Si/30 + Mn/20 + Cu/20 + Ni/60 + Cr/20 + Mo/15 + V/10 + 5B

Index ≤50 mm >50–100 mm >100–130 mm
Pcm, TMCP (Table 7) ≤ 0.24 ≤ 0.25 —
CEV, QT (Table 6) ≤ 0.60 ≤ 0.65 —

On thick Q690qF flanges, preheat, interpass control and low-hydrogen practice matter more than the grade itself. The certificate gives the data to set them. At −60°C, both weld metal and HAZ must prove toughness. Expect lower heat input, more passes and consumables qualified at −60°C.

Typical consumables for Q690qF: E76-class consumables (AWS E11018M type).

Fatigue. Welded details govern fatigue life in a bridge, and their fatigue strength is set by detail category, not by yield strength. Higher-strength plate can carry higher stress ranges only if detailing improves too.

Fatigue design follows JTG D64 (highway) and TB 10091 (railway) in China, EN 1993-1-9 in Europe and AASHTO LRFD in the US; fabrication commonly follows TB 10212, JTG/T 3650 or AWS D1.5.

Q690qFZ15, Z25 and Z35: Through-Thickness Plate for Bridges

Lamellar tearing appears in thick plate loaded across its thickness, typically at cruciform joints and anchor plates. A Z grade adds a short-transverse tensile test and a lower sulfur cap.

GB/T 714 adds the Z level to the end of the designation, for example Q690qFZ25. The test and acceptance follow GB/T 5313 and apply to plate 15 mm and thicker.

Z grade Heat sulfur, max (%) Reduction of area, avg / single (%)
Z15 0.010 15 / 10
Z25 0.007 25 / 15
Z35 0.005 35 / 25

F chemistry limits S to 0.006%, which already meets the Z25 sulfur cap (0.007%). Only Z35 (S ≤0.005%) needs a further step.

Ask your designer which Q690qF plates are loaded through the thickness. Ordering Z35 on everything costs money and time without adding safety. Z options apply across the GB/T 714 bridge steel range.

Equivalent Material Grades

Annex B of GB/T 714-2025 lists foreign grades against each strength level. It is informative: it tells you which families are close, not that the plates are interchangeable.

Standard Grade(s) Fit for Q690qF
ASTM A709 ASTM A709 HPS 100W Listed in Annex B
EN 10025-6 EN 10025-6 S690Q, EN 10025-6 S690QL, EN 10025-6 S690QL1 Listed in Annex B
ASTM A514 ASTM A514 Grade Q QT, strength only
GB/T 16270 GB/T 16270 Q690F QT alternative, different toughness rules
GB/T 1591 GB/T 1591 Q690MF TMCP general structural

Before substituting, compare three things line by line: minimum yield at the actual thickness, the impact test temperature and energy, and the weldability index. For Q690qF, the 120 J impact level and the Pcm/CEV caps are usually the hardest to match.

Q690qF Testing, UT and Certificate

A batch of Q690qF is one grade, one heat, one thickness, one rolling schedule and one heat-treatment condition, up to 60 t. Table 12 of GB/T 714-2025 sets the tests:

Test Frequency Method
Heat analysis 1 per heat GB/T 20066; GB/T 4336 / GB/T 223
Tensile 1 per batch GB/T 2975 / GB/T 228.1
Bend 180° 1 per batch (may be waived if guaranteed) GB/T 232
Charpy V at −60°C 3 specimens per batch GB/T 229
Through-thickness (Z) 3 specimens per batch, when ordered GB/T 5313
Ultrasonic Every plate >20 mm, Class II or better GB/T 2970
Surface and dimensions Every plate Visual and gauges

Impact retest: if a set fails, three more specimens are taken from the same batch. The average of all six must meet the requirement; two values may be below it, but only one below 70%. At −60°C, mills may need trial heats before the production run; we agree the test plan before accepting the order.

Dimensions

Usual Q690qF supply range from SHH STEEL:

  • Thickness: 6 mm – 100 mm under GB/T 714 tensile tables; most orders 10 – 60 mm
  • Width: 1500 – 4000 mm, depending on mill and thickness
  • Length: 6000 – 18000 mm; longer by enquiry
  • Edge: mill edge or cut edge
  • Weight: theoretical, 7.85 g/cm³

Deck plate, webs, flanges, diaphragms and stiffeners are cut to drawing. For U-ribs and rolled sections on the same bridge, see steel beam profiles and steel structural profiles.

Tolerances

GB/T 714 does not set its own size tolerances; Q690qF follows GB/T 709. Other tolerance standards can be agreed in the contract (clause 7.6.2).

Nominal thickness (mm) Width ≤ 1500 mm Width > 1500 – 2500 mm
> 8 – 15 −0.30 / +0.80 −0.30 / +1.00
> 15 – 25 −0.30 / +1.00 −0.30 / +1.20
> 25 – 40 −0.30 / +1.10 −0.30 / +1.30
> 40 – 60 −0.30 / +1.30 −0.30 / +1.50
> 60 – 100 −0.30 / +1.50 −0.30 / +1.80
> 100 – 150 −0.30 / +2.10 −0.30 / +2.50

Bridge fabricators often ask for Class C (zero minus) on deck and flange plate so section properties are never under the design value. Wider plates follow the heavier GB/T 709 rows; we state them on the offer.

Q690qF Price Factors and How to Order

There is no single Q690qF price. Mills price bridge plate as base plus extras, and the order sets the extras.

Cost driver Effect on price
Strength level Q690q Higher levels need more alloy and tighter rolling control
Quality letter Highest extra: −60°C testing, S ≤0.006%, limited mills
Delivery route TMCP / TMCP+T / QT; QT costs more than TMCP
Thickness Over 60 mm and under 10 mm carry size extras
Z15 / Z25 / Z35 Low-sulfur heat, Z test, UT; Z35 costs most
Width and length Over 3000 mm wide or 15 m long needs mill confirmation
Quantity per size Mill minimums per heat and size
Inspection and processing 3.2 witness, profile cutting, blasting, priming quoted per item

To get a firm quote in one round, send:

  • Grade, edition and Z level, e.g. Q690qFZ25 to GB/T 714-2025
  • Thickness × width × length and pieces or tonnes
  • Delivery route and UT class if beyond Class II
  • Certificate type and inspector
  • Destination port and Incoterm

We quote plate price, extras and freight line by line. Need another letter? See Q690qD, Q690qE.

Applications

Sector Typical Q690qF components
Record-span bridges Main truss chords and node plates
Cable anchorages Anchor boxes and anchor plates
Steel pylons Highly stressed pylon walls
Movable and military bridges Lightweight girders
Retrofit High-strength replacement members

The letter F suits Arctic and sub-Arctic bridges, high-latitude rail lines and owners who want the largest toughness margin for fracture-critical members.

It is the wrong plate for pressure equipment (pressure vessel steel plates), unpainted exposure (weathering steel plates) or ship hulls (shipbuilding steel plates).

Supply Capability and Global Delivery

SHH STEEL sources Q690qF from first-line bridge-plate mills, including drafters of GB/T 714-2025 such as Ansteel, Valin Xiangtan, Jiangyin Xingcheng, Wuyang, Shougang and Xinyu.

  • Certificates: EN 10204 3.1 standard; 3.2 with third-party witness (SGS, BV, TÜV or owner’s inspector)
  • Tests: tensile, −60°C Charpy, bend, Z test, UT, product analysis
  • Processing: CNC plasma and flame cutting, bevelling, drilling, shot blasting and priming
  • Terms: FOB Shanghai, CFR, CIF; TT, LC or TT + LC
  • Marking: steel-stamped and paint-marked with grade, heat, size and mill, per GB/T 247

Q690qF goes from Shanghai to bridge sites and fabrication yards worldwide, usually as break-bulk for long plates.

Lead time: about 45–60 days from mill rolling; Z35, F letter or 3.2 inspection adds about 1–2 weeks. Sea time from Shanghai is about 7–12 days to Southeast Asia and 28–35 days to North Europe.

Why Choose SHH STEEL

SHH STEEL works mill-direct as a steel manufacturer and exporter and global steel mill sourcing partner, China origin. Every Q690qF plate is traced to its heat.

Before shipment we check four lines on every Q690qF certificate: yield and tensile for the actual thickness band, Charpy at −60°C, the CEV or Pcm for the delivery route, and UT results. If one fails, the plate does not ship as Q690qF.

We quote Q690qF only after the mill confirms the test plan. Expect a longer lead time and a pre-production trial if the order is large.

We also tell buyers when another grade fits better. Neighbouring levels are Q620qF. Browse more structural steel plates and high strength low alloy plates.

FAQ

What is Q690qF steel?
Q690qF is bridge structural steel plate to GB/T 714-2025. It has 690 MPa minimum yield up to 50 mm, 770 MPa minimum tensile, 14% elongation and Charpy V-notch impact of 77 J at −60°C for 12–100 mm plate. It is delivered TMCP, TMCP + tempering, or quenched and tempered.
What impact energy does Q690qF need at −60°C?
GB/T 714-2025 requires at least 77 J at −60°C on longitudinal specimens for Q690qF plate over 12 mm and up to 100 mm. For plate 12 mm and thinner the value is by agreement. F energy rises with strength: 47 J for Q420q and Q460q, 54 J for Q500q, 60 J for Q550q, 69 J for Q620q and 77 J for Q690q.
What is the yield strength of Q690qF?
Q690qF has a minimum lower yield strength of 690 MPa up to 50 mm and 650 MPa from 50 to 100 mm (GB/T 714-2025 Table 9). Minimum tensile is 770 MPa up to 100 mm. There is no upper tensile limit in the standard.
What is the ASTM or EN equivalent of Q690qF?
Close grades for Q690qF: ASTM A709 HPS 100W / EN 10025-6 S690Q, S690QL, S690QL1 (Annex B). These are close families, not drop-in substitutes; compare yield at thickness, impact temperature and energy, and the weldability index before substituting.
What is the batch size for GB/T 714 bridge plate testing?
Up to 60 t of one grade, heat, thickness, rolling schedule and heat-treatment condition. Each batch gets one tensile test, one bend test and one set of three Charpy specimens; heat analysis is reported per heat.
Does steel grade affect fatigue life of a Q690qF bridge girder?
Very little. Fatigue life of welded bridge details is governed by the detail category and stress range, not by yield strength. Higher-strength plate raises working stress, so detailing and weld quality must improve to keep the same fatigue life.

Conclusion

Q690qF to GB/T 714-2025 is bridge plate with 690 MPa minimum yield, 770 MPa minimum tensile and 77 J Charpy at −60°C for 12–100 mm plate.

The next strength level is Q620qF, with Q690qD and Q690qE as sister letters. The most common ordering mistake with Q690qF is leaving the Z level, UT class or impact position off the order; add them at enquiry stage, not after rolling.

SHH STEEL supplies Q690qF with heat analysis, Pcm or CEV, tensile and Charpy results on an EN 10204 3.1 or 3.2 certificate, and adds product analysis to GB/T 222 when you need it.

We ship from Shanghai to bridge builders worldwide. Browse the full GB/T 714 range or other high strength low alloy plates.

Contact SHH STEEL with your Q690qF requirements. We confirm the mill, delivery route, testing and price before you commit.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X