GB/T 714 Q345qNHF weathering bridge steel stacked at SHH STEEL warehouse

GB/T 714 Q345qNHF Weathering Bridge Steel Supplier

Q345qNHF (standard notation Q345qFNH) is a GB/T 714-2015 weathering bridge steel with 345 MPa yield and −60°C Charpy. GB/T 714-2025 lists this level in C, D and E only, so SHH STEEL supplies it to the 2015 edition or as Q345qENH with an agreed −60°C test, mill-direct.
Keywords
Q345qNHF, Q345qNHF weathering steel, GB/T 714 Q345qNHF, Q345qFNH, Q345qFNH steel plate, Q345qNH, Q345qNHF weathering bridge steel, Q345qFNHZ15, Q345qFNHZ25, Q345qFNHZ35, bridge steel plate, Q345qNHF supplier, Q345qENH
Equivalent Grades:
ASTM A709 50W / HPS 50W (Annex B) / EN 10025-5 S355J2W, S355K2W (closest) / ASTM A588 (closest) — Material Specification: GB/T 714-2025 (supersedes GB/T 714-2015) — Delivery: TMCP / TMCP+T
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Q345qNH Quality Grades
GB/T 714-2025 vs 2015
Q345qNHF vs ASTM A709 / EN 10025
Weathering Index and Unpainted Use
Welding and Fatigue
Z15 / Z25 / Z35
Equivalent Material Grades
Testing and Inspection
Dimensions
Tolerances
Price and Ordering
Applications
Supply Capability
Why Choose SHH STEEL
FAQ
Conclusion

What is GB/T 714 Q345qNHF Weathering Bridge Steel?

Q345qNHF is weathering bridge structural steel to GB/T 714. In the standard’s own notation it is written Q345qFNH: Q for yield, 345 for the minimum yield in MPa, q for qiao (bridge), the quality letter, and NH for nai hou, weathering. The letter F means Charpy V-notch testing at −60°C.

Q345qNH is the most widely used weathering bridge steel in China, for unpainted plate girders and box girders in rural and urban atmospheres. Q345qNH carries the same 345 MPa tensile table as Q345q, but adds Cu, Cr and Ni (Cu 0.25–0.50%, Cr 0.40–0.70%, Ni 0.30–0.40%) so a dense patina forms and paint can be left off. GB/T 714-2025 lists ASTM A709 50W and HPS 50W against Q345q.

Q345qNHF (Q345qFNH) is a GB/T 714-2015 designation. In the 2025 edition, the Q345qNH level is listed in quality grades C, D and E only, so a new order for −60°C weathering plate at 345 MPa must be handled by agreement.

GB/T 714-2025 was published on 31 October 2025 and took effect on 1 May 2026. It replaces GB/T 714-2015 completely. The 2015 edition listed every weathering level in D, E and F; the 2025 edition lists Q345qNH, Q370qNH and Q390qNH in C, D and E, and keeps F only from Q420qNH upward.

SHH STEEL (Shanghai Shenghonghe Import & Export Co., Ltd.) is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. We ship Q345qNHF cut to size with an EN 10204 3.1 or 3.2 certificate. Sister grades are listed under GB/T 714; other unpainted options are under weathering steel plates and EN 10025-5.

Material Specification

Specification element Requirement SHH STEEL compliance
Standard GB/T 714-2015 Q345qFNH, or GB/T 714-2025 Q345qENH + agreed −60°C test Confirmed
Product Single-rolled plate ≤150 mm; hot-rolled strip and cut plate ≤25.4 mm Plate
Thickness with tensile values Up to 150 mm for Q345qNH Confirmed
Minimum yield ReL 345 MPa ≤50 mm; 335 MPa >50–100 mm Confirmed
Minimum tensile Rm 490 MPa ≤100 mm (no upper limit in the standard) Confirmed
Elongation A ≥ 20% Confirmed
Charpy V-notch −60°C, energy agreed in the order, longitudinal Confirmed
Weathering index I ≥ 6.0 (Table 5, footnote c) Calculated on MTC
Delivery condition TMCP or TMCP + tempering As ordered
Weldability index Pcm (Table 8) Printed on MTC
Ultrasonic testing Plate >20 mm: GB/T 2970, Class II or better Every plate
Through-thickness Z15, Z25 or Z35 to GB/T 5313, when ordered As ordered
Dimensions GB/T 709 Confirmed
Certificate GB/T 247; EN 10204 3.1 or 3.2 As ordered

Grades often compared with Q345qNHF are ASTM A709 Grade 50W, ASTM A709 HPS 50W and EN 10025-5 S355J2W; the comparison below shows where they differ.

Chemical Composition: Heat Analysis and Product Analysis

Chemistry for Q345qNHF is fixed at the ladle, but it is verified on plate. GB/T 714 sets the ladle (heat) limits; GB/T 222 sets how far a finished-plate analysis may stray from them.

Table 1 below is the heat (ladle) analysis for Q345qNHF from GB/T 714-2025 Tables 1, 5.

Element Q345qNHF heat analysis (%) Note
C, max 0.11
Si 0.15 – 0.50 Counts in I
Mn 1.10 – 1.50 Min 0.50% for coil only
P, max 0.015 Letter F
S, max 0.006 Letter F
Cu 0.25 – 0.50 Main weathering element
Cr 0.40 – 0.70 Weathering element
Ni 0.30 – 0.40 Weathering element
Mo, max 0.20 Changed in 2025
Nb 0.010 – 0.100 Microalloy (see note)
V 0.010 – 0.100 Microalloy (see note)
Ti 0.006 – 0.030 Microalloy (see note)
Als 0.015 – 0.050 Alt 0.020–0.055% if total Al is used
N, max 0.0080
B, max (residual) 0.0005 ≤0.0014% if C ≤0.06%
H, max (residual) 0.0002
Weathering index I ≥ 6.0 Calculated from heat analysis

Nb, V, Ti and Al may be added singly or together. Added singly, each must meet the range above; added together, at least one must reach its minimum and Nb + V + Ti ≤ 0.22%. Calcium treatment is required to control sulfide shape.

Table 2 is the product analysis: the limits a check analysis on finished plate is judged against. GB/T 714-2025 clause 7.1.3 calls up GB/T 222 for the permitted deviations.

Element Heat limit (%) Deviation, GB/T 222-2025 Table 1 Q345qNHF product analysis (%)
C ≤ 0.11 +0.02 ≤ 0.13
Si 0.15 – 0.50 ±0.05 0.10 – 0.55
Mn 1.10 – 1.50 ±0.06 1.04 – 1.56
P ≤ 0.015 +0.005 ≤ 0.020
S ≤ 0.006 +0.005 ≤ 0.011
V 0.010 – 0.100 +0.02 / −0.01 ≤ 0.120
Ti 0.006 – 0.030 +0.02 / −0.01 ≤ 0.050
Nb 0.010 – 0.100 ±0.005 (listed for 0.015–0.060%) Above 0.060%: agree in contract
Cu 0.25 – 0.50 ±0.05 0.20 – 0.55
Cr 0.40 – 0.70 ±0.05 0.35 – 0.75
Ni 0.30 – 0.40 ±0.05 0.25 – 0.45
Als 0.015 – 0.050 ±0.003 Lower limit −0.003 (Table 1 row is for Al ≥0.015%; confirm)
Mo ≤ 0.20 Not listed in Table 1 Agree in contract
N ≤ 0.0080 Listed only for 0.010–0.020% Agree in contract

How to read Table 2. Weathering bridge steel is normally classed as low-alloy steel, so Table 1 of GB/T 222 applies. Where the heat limit is a range, the deviation applies to both ends; for one heat, an element may deviate in one direction only.

Mechanical Properties

Tensile values follow Table 9 of GB/T 714-2025 for Q345qNH. Tensile specimens are transverse; round specimens are used above 40 mm. Where yield is not distinct, Rp0.2 replaces ReL.

Nominal thickness ReL min (MPa) Rm min (MPa) A min
≤ 50 mm 345 490 20%
> 50 – 100 mm 335 490 20%
> 100 – 130 mm 305 430 20%
> 130 – 150 mm 305 430 20%

Impact values follow Table 10, on longitudinal specimens, average of three:

Letter / test temperature KV2 ≤12 mm KV2 >12 – 100 mm KV2 >100 – 150 mm
F / −60°C By agreement by agreement Not applicable

One single value may fall below the required average, but not below 70% of it. Plate over 8 mm and under 12 mm is tested with 7.5 mm specimens (75% of the value); 6–8 mm plate with 5 mm specimens (50%). Plate under 6 mm is not impact tested.

180° bend test, transverse: mandrel D = 2a up to 16 mm and 3a above 16 mm; may be omitted when the mill guarantees it. Yield ratio is not mandatory. If the contract asks for it, Annex C recommends ReL/Rm ≤ 0.88 up to 12 mm and ≤ 0.85 above 12 mm for TMCP plate.

Q345qNHC / Q345qNHD / Q345qNHE: Which Quality Grade?

Q345qNHF was tested at −60°C under GB/T 714-2015. In the 2025 tables the Q345qNH level stops at E (−40°C); the table shows what is listed today.

Grade Test temp. KV2 ≤12 mm KV2 12–100 mm KV2 >100 mm P / S max (%)
Q345qNHC 0°C 80 J 120 J 55 J 0.030 / 0.025
Q345qNHD −20°C 80 J 120 J 47 J 0.025 / 0.015
Q345qNHE −40°C 80 J 120 J 31 J 0.020 / 0.010
Q345qNHF −60°C 2015 edition only 2015 edition only — 0.015 / 0.006 (2025 Table 1, F)

For Q345qNHF the 2025 table stops at E. A −60°C requirement can still be met: by certifying to the 2015 edition where the contract allows, or by ordering Q345qENH with a supplementary −60°C test and an agreed energy. Where higher strength is acceptable, Q420qNHF is a listed −60°C weathering grade.

Q345qNHF: What Changed from GB/T 714-2015 to GB/T 714-2025

Q345qNHF is the case where the edition matters most: the letter itself is not in the 2025 tables. The points below come from the foreword and tables of GB/T 714-2025.

  • The weathering requirement changed: Table 5 now requires a corrosion index I ≥ 6.0, and the 2015 Annex C guide for assessing weathering resistance was deleted.
  • A Pcm table for weathering steel (Table 8) was added.
  • Annex A now gives reference bridge-site environments for unpainted use (chloride, SO₂ and time-of-wetness limits).
  • Mo maximum for Q345qNH was changed (now ≤0.20%; 2015-based sources quote ≤0.10%).
  • Q345qNH is now listed in letters C, D and E. The 2015 edition listed it in D, E and F.
  • Tensile strength is now banded by thickness (e.g. lower minimum Rm above 100 mm) instead of one value.
  • Impact energy is set by thickness band (≤12 mm, 12–100 mm, >100 mm) in Table 10.
  • Yield ratio is no longer a clause value; it is agreed in the contract, with recommendations in informative Annex C.

If a drawing cites 2015 and the plate is made to 2025, get the designer’s written acceptance; tensile strength above 100 mm and the yield-ratio basis differ.

Q345qNHF vs ASTM A709 and EN 10025: Which Grade Matches?

Can Q345qNHF replace a US or European bridge grade, or the other way round? Strength can match; toughness rules differ in kind, not only in number.

Property Q345qNHF ASTM A709 Grade 50W ASTM A709 HPS 50W EN 10025-5 S355J2W
Min. yield (MPa) 345 (≤50 mm) 345 345 355 (≤16 mm)
Tensile (MPa) 490 min 485 min 485 min 470 – 630
Charpy by agreement at −60°C (12–100 mm) CVN by temperature zone and member type (T / F) CVN by temperature zone; fracture-critical (F) levels 27 J at −20°C
Weathering chemistry Yes, I ≥ 6.0 Yes Yes Yes

ASTM A709 sets Charpy requirements by temperature zone (1, 2, 3) and by member type: non-fracture-critical (T) or fracture-critical (F). GB/T 714 sets one value per letter, so compare the A709 zone with the GB/T 714 test temperature, not grade with grade.

EN 10025-5 weathering grades are general structural steels without a bridge-specific toughness level of 120 J; they suit many bridges but are not a one-to-one match.

At −60°C, the by agreement required for Q345qNHF is a demanding figure; general structural grades rarely prove any toughness that cold. For the C, D and E letters GB/T 714 asks 120 J, several times the 27–40 J typical of GB/T 1591 plate.

Q345qNHF Atmospheric Corrosion Index I and Unpainted Bridges

GB/T 714-2025 Table 5, footnote c, requires every Q345qNHF heat to reach an atmospheric corrosion index I of at least 6.0, calculated from the heat analysis:

I = 26.01(%Cu) + 3.88(%Ni) + 1.20(%Cr) + 1.49(%Si) + 17.28(%P) − 7.29(%Cu)(%Ni) − 9.10(%Ni)(%P) − 33.39(%Cu)²

This is the same predictive formula used with ASTM G101 for ASTM A709 Grade 50W and ASTM A709 HPS 70W, which makes Chinese and US ASTM A709 weathering steel plates easy to compare with Q345qNHF.

Worked example (our calculation) Cu Ni Cr Si P I
All weathering elements at their Table 5 minimum 0.25 0.30 0.40 0.15 0.010 5.88
Illustrative mid-range heat 0.32 0.36 0.55 0.30 0.012 6.74

Note the first row: a heat that only just meets every Table 5 minimum can still fall short of I = 6.0. That is why we ask the mill to print I on every Q345qNHF certificate, not just the chemistry.

Where can the steel be left unpainted? Annex A of GB/T 714-2025 gives reference bridge-site conditions:

  • Rural or urban atmosphere with annual chloride deposition ≤ 3 mg/(m²·d)
  • Annual SO₂ deposition ≤ 24 mg/(m²·d)
  • Time of wetness ≤ 5,256 h per year (temperature above 0°C and relative humidity above 80%)
  • Coastal sites only if they meet the same limits; for marine atmospheres Annex D points to T/CISA 073

Weathering steel is not stainless. Q345qNHF corrodes slowly once a stable patina forms, which takes a few years of wet-dry cycles. Designers usually add a corrosion allowance and design drainage so no surface stays wet.

Welding Q345qNHF and Fatigue in Bridge Girders

GB/T 714-2025 clause 7.1.2 uses CEV for normalized, QT and TMCP steel with C >0.12%, and Pcm for weathering steel and TMCP steel with C ≤0.12%, both from the heat analysis:

CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15

Pcm = C + Si/30 + Mn/20 + Cu/20 + Ni/60 + Cr/20 + Mo/15 + V/10 + 5B

Index ≤50 mm >50–100 mm >100–130 mm
Pcm, Q345qNH (Table 8) ≤ 0.22 ≤ 0.24 By agreement

We send the actual heat analysis of Q345qNHF before shipment, so the fabricator can check preheat and interpass limits against the procedure qualification record. At −60°C, both weld metal and HAZ must prove toughness. Expect lower heat input, more passes and consumables qualified at −60°C.

Typical consumables for Q345qNHF: weathering-matched Ni-Cu consumables (AWS E8018-W2 type for 345–420 MPa), with higher-strength weathering wires for 460–500 MPa.

Fatigue. Welded details govern fatigue life in a bridge, and their fatigue strength is set by detail category, not by yield strength. Higher-strength plate can carry higher stress ranges only if detailing improves too.

Fatigue design follows JTG D64 (highway) and TB 10091 (railway) in China, EN 1993-1-9 in Europe and AASHTO LRFD in the US; fabrication commonly follows TB 10212, JTG/T 3650 or AWS D1.5.

Q345qFNHZ15, Z25 and Z35: Through-Thickness Plate for Bridges

On long-span bridges, Z25 or Z35 is common on node plates and anchor zones. The extra cost is in desulfurization, testing and a higher reject rate.

GB/T 714 adds the Z level to the end of the designation, for example Q345qFNHZ25. The test and acceptance follow GB/T 5313 and apply to plate 15 mm and thicker.

Z grade Heat sulfur, max (%) Reduction of area, avg / single (%)
Z15 0.010 15 / 10
Z25 0.007 25 / 15
Z35 0.005 35 / 25

F chemistry limits S to 0.006%, which already meets the Z25 sulfur cap (0.007%). Only Z35 (S ≤0.005%) needs a further step.

Put Z only where the joint needs it, usually node plates, anchor boxes and diaphragm-to-flange joints over about 25 mm. Keep the rest standard Q345qNHF. Z options apply across the GB/T 714 bridge steel range.

Equivalent Material Grades

Annex B of GB/T 714-2025 lists foreign grades against each strength level. It is informative: it tells you which families are close, not that the plates are interchangeable.

Standard Grade(s) Fit for Q345qNHF
ASTM A709 ASTM A709 Grade 50W, ASTM A709 HPS 50W Listed in Annex B
EN 10025-5 EN 10025-5 S355J2W, EN 10025-5 S355K2W Closest weathering grades
ASTM A588 ASTM A588 Grade A, ASTM A588 Grade B Similar chemistry family
Trade name Corten B Similar weathering concept, not a bridge standard
GB/T 714 (painted twin) Q345qE Same strength, no weathering elements

For weathering grades also compare the corrosion index basis. Q345qNHF requires I ≥ 6.0 by the formula above; check that the substitute is assessed on the same basis.

Q345qNHF Testing, UT and Certificate

A batch of Q345qNHF is one grade, one heat, one thickness, one rolling schedule and one heat-treatment condition, up to 60 t. Table 12 of GB/T 714-2025 sets the tests:

Test Frequency Method
Heat analysis 1 per heat GB/T 20066; GB/T 4336 / GB/T 223
Weathering index I Calculated per heat Table 5 formula
Tensile 1 per batch GB/T 2975 / GB/T 228.1
Bend 180° 1 per batch (may be waived if guaranteed) GB/T 232
Charpy V at −60°C 3 specimens per batch GB/T 229
Through-thickness (Z) 3 specimens per batch, when ordered GB/T 5313
Ultrasonic Every plate >20 mm, Class II or better GB/T 2970
Surface and dimensions Every plate Visual and gauges

Impact retest: if a set fails, three more specimens are taken from the same batch. The average of all six must meet the requirement; two values may be below it, but only one below 70%. At −60°C, mills may need trial heats before the production run; we agree the test plan before accepting the order.

Dimensions

What we roll and cut in Q345qNHF:

  • Thickness: 6 mm – 150 mm under GB/T 714 tensile tables; most orders 8 – 60 mm
  • Width: 1500 – 4000 mm, depending on mill and thickness
  • Length: 6000 – 18000 mm; longer by enquiry
  • Edge: mill edge or cut edge
  • Weight: theoretical, 7.85 g/cm³

Deck plate, webs, flanges, diaphragms and stiffeners are cut to drawing. For U-ribs and rolled sections on the same bridge, see steel beam profiles and steel structural profiles.

Tolerances

GB/T 709 governs Q345qNHF thickness, width, length and flatness. Under Class B, plate may be up to 0.30 mm thin; the plus side grows with thickness and width.

Nominal thickness (mm) Width ≤ 1500 mm Width > 1500 – 2500 mm
> 8 – 15 −0.30 / +0.80 −0.30 / +1.00
> 15 – 25 −0.30 / +1.00 −0.30 / +1.20
> 25 – 40 −0.30 / +1.10 −0.30 / +1.30
> 40 – 60 −0.30 / +1.30 −0.30 / +1.50
> 60 – 100 −0.30 / +1.50 −0.30 / +1.80
> 100 – 150 −0.30 / +2.10 −0.30 / +2.50

Bridge fabricators often ask for Class C (zero minus) on deck and flange plate so section properties are never under the design value. Wider plates follow the heavier GB/T 709 rows; we state them on the offer.

Q345qNHF Price Factors and How to Order

For Q345qNHF, the base price follows the market; grade, letter, size and testing extras decide the rest.

Cost driver Effect on price
Strength level Q345q Higher levels need more alloy and tighter rolling control
Quality letter Highest extra: −60°C testing, S ≤0.006%, limited mills
Weathering alloys Cu, Cr, Ni additions and I-index control add a weathering extra
Delivery route TMCP / TMCP+T
Thickness Over 60 mm and under 10 mm carry size extras
Z15 / Z25 / Z35 Low-sulfur heat, Z test, UT; Z35 costs most
Width and length Over 3000 mm wide or 15 m long needs mill confirmation
Quantity per size Mill minimums per heat and size
Inspection and processing 3.2 witness, profile cutting, blasting, priming quoted per item

To get a firm quote in one round, send:

  • Grade, edition and Z level, e.g. Q345qFNHZ25 to GB/T 714-2025
  • Thickness × width × length and pieces or tonnes
  • Delivery route and UT class if beyond Class II
  • Certificate type and inspector
  • Destination port and Incoterm

We quote plate price, extras and freight line by line. Need another letter? See Q345qNHD, Q345qNHE.

Applications

Sector Typical Q345qNHF components
Unpainted highway bridges Plate girders and box girders in rural and urban atmospheres
Railway bridges Truss members, plate girders, bracing
Remote and mountain sites Bridges where repainting access is difficult or costly
Urban viaducts Exposed girders with architectural rust finish
Pedestrian bridges Unpainted box sections

The letter F suits Arctic and sub-Arctic bridges, high-latitude rail lines and owners who want the largest toughness margin for fracture-critical members.

Q345qNHF is the wrong plate for marine splash zones, tunnels, sites with heavy de-icing salt spray, or members that stay wet. There, use painted bridge steel or look at marine-atmosphere grades under T/CISA 073.

Supply Capability and Global Delivery

SHH STEEL sources Q345qNHF from first-line bridge-plate mills, including drafters of GB/T 714-2025 such as Ansteel, Valin Xiangtan, Jiangyin Xingcheng, Wuyang, Shougang and Xinyu.

  • Certificates: EN 10204 3.1 standard; 3.2 with third-party witness (SGS, BV, TÜV or owner’s inspector)
  • Tests: tensile, −60°C Charpy, bend, Z test, UT, product analysis, weathering index
  • Processing: CNC plasma and flame cutting, bevelling, drilling, shot blasting and priming (or blasting only, for unpainted weathering steel)
  • Terms: FOB Shanghai, CFR, CIF; TT, LC or TT + LC
  • Marking: steel-stamped and paint-marked with grade, heat, size and mill, per GB/T 247

Q345qNHF leaves Shanghai for bridge projects designed to Chinese codes abroad, mainly through EPC contractors in Southeast Asia, Central Asia, the Middle East and Africa.

Lead time: about 45–60 days from mill rolling; Z35, F letter or 3.2 inspection adds about 1–2 weeks. Sea time from Shanghai is about 7–12 days to Southeast Asia and 28–35 days to North Europe.

Why Choose SHH STEEL

SHH STEEL is a steel manufacturer and exporter and global steel mill sourcing partner. We buy Q345qNHF mill-direct, China origin, and check every certificate before shipment.

Before shipment we check four lines on every Q345qNHF certificate: yield and tensile for the actual thickness band, Charpy at −60°C, the Pcm and weathering index, and UT results. If one fails, the plate does not ship as Q345qNHF.

If your drawing still says Q345qNHF, we offer two routes: plate certified to GB/T 714-2015 Q345qFNH if the contract allows the old edition, or Q345qENH to GB/T 714-2025 with a supplementary −60°C impact test agreed in the order.

We also tell buyers when another grade fits better. Neighbouring levels are Q370qNHF. The painted counterpart is Q345qE. Browse more structural steel plates and high strength low alloy plates.

FAQ

What is Q345qNHF steel?
Q345qNHF, written Q345qFNH in the standard, is a weathering bridge steel from GB/T 714-2015 with 345 MPa minimum yield and Charpy testing at −60°C. GB/T 714-2025 lists Q345qNH only in grades C, D and E, so new orders are certified to the 2015 edition or supplied as Q345qENH with an agreed −60°C test.
Is Q345qNHF still available under GB/T 714-2025?
Not as a listed grade. GB/T 714-2025 Table 10 gives Q345qNH impact rows for C, D and E only. Plate meeting a −60°C requirement can still be made: either certified to GB/T 714-2015 where the contract allows, or as Q345qENH with a supplementary −60°C Charpy test and energy agreed in the order.
Is Q345q replaced by Q355q?
No. GB/T 1591 renamed Q345 to Q355 in 2018, but GB/T 714-2025 still uses Q345q for bridge steel. Q345qC, Q345qD and Q345qE remain current grades with 345 MPa minimum yield up to 50 mm.
What is the ASTM or EN equivalent of Q345qNHF?
Close grades for Q345qNHF: ASTM A709 50W / HPS 50W (Annex B) / EN 10025-5 S355J2W, S355K2W (closest) / ASTM A588 (closest). These are close families, not drop-in substitutes; compare yield at thickness, impact temperature and energy, and the weldability index before substituting.
Can GB/T 714 bridge plate be normalized?
Only in one case. GB/T 714-2025 clause 6.2 requires TMCP, TMCP + tempering or quenched and tempered delivery, but Q345q and Q370q plate over 100 mm and up to 150 mm may be normalized by agreement.
What is the weathering index I in GB/T 714?
It is a corrosion index calculated from the heat analysis: I = 26.01Cu + 3.88Ni + 1.20Cr + 1.49Si + 17.28P − 7.29Cu·Ni − 9.10Ni·P − 33.39Cu². GB/T 714-2025 requires I ≥6.0 for every weathering grade, the same basis ASTM G101 uses for A709 weathering steels.

Conclusion

Q345qNHF to GB/T 714 is weathering bridge steel with 345 MPa minimum yield, Cu-Cr-Ni chemistry, a weathering index of at least 6.0 and −60°C Charpy as a 2015-edition grade, now supplied by agreement under GB/T 714-2025.

The next strength level is Q370qNHF, with Q345qNHD and Q345qNHE as sister letters. Choose the letter from the lowest service or erection temperature, here −60°C, and step up a letter for thick, restrained or fracture-critical members.

SHH STEEL delivers Q345qNHF with the full GB/T 714 data set on an EN 10204 3.1 or 3.2 certificate. On request we add product analysis to GB/T 222, Z15–Z35, a tighter UT class, Class C tolerance, cutting and blasting.

We ship from Shanghai to bridge builders worldwide. Browse the full GB/T 714 range or other weathering steel plates.

Tell us the sizes, tonnage and any Z, UT or inspection needs. We check the request against GB/T 714 first, then confirm mill, route, lead time and price. Contact SHH STEEL today for Q345qNHF weathering bridge steel.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X