GB/T 714 Q370qNHD Weathering Bridge Steel Supplier
What is GB/T 714 Q370qNHD Weathering Bridge Steel?
Q370qNHD is weathering bridge structural steel to GB/T 714. In the standard’s own notation it is written Q370qDNH: Q for yield, 370 for the minimum yield in MPa, q for qiao (bridge), the quality letter, and NH for nai hou, weathering. The letter D means Charpy V-notch testing at −20°C.
Q370qNH is weathering plate for unpainted railway and highway bridges that need 370 MPa yield. Q370qNH shares the Q345qNH chemistry box and Pcm cap (≤0.22% to 50 mm) but proves 370 MPa yield and 510 MPa tensile. Fabricators qualified on Q345qNH move across with no change of consumables.
Q370qNHD (Q370qDNH) is the unpainted bridge plate for railway and highway girders that need 370 MPa yield and −20°C toughness. Chemistry, Pcm cap and welding are the same as Q345qNH.
GB/T 714-2025, in force since 1 May 2026, fully replaces GB/T 714-2015; the changes for weathering grades are listed below.
SHH STEEL (Shanghai Shenghonghe Import & Export Co., Ltd.) is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. We ship Q370qNHD cut to size with an EN 10204 3.1 or 3.2 certificate. Sister grades are listed under GB/T 714; other unpainted options are under weathering steel plates and EN 10025-5.
Material Specification
| Specification element | Requirement | SHH STEEL compliance |
|---|---|---|
| Standard | GB/T 714-2025 Q370qDNH | Confirmed |
| Product | Single-rolled plate ≤150 mm; hot-rolled strip and cut plate ≤25.4 mm | Plate |
| Thickness with tensile values | Up to 150 mm for Q370qNH | Confirmed |
| Minimum yield ReL | 370 MPa ≤50 mm; 360 MPa >50–100 mm | Confirmed |
| Minimum tensile Rm | 510 MPa ≤100 mm (no upper limit in the standard) | Confirmed |
| Elongation A | ≥ 20% | Confirmed |
| Charpy V-notch | −20°C, 120 J (12–100 mm), longitudinal | Confirmed |
| Weathering index | I ≥ 6.0 (Table 5, footnote c) | Calculated on MTC |
| Delivery condition | TMCP or TMCP + tempering | As ordered |
| Weldability index | Pcm (Table 8) | Printed on MTC |
| Ultrasonic testing | Plate >20 mm: GB/T 2970, Class II or better | Every plate |
| Through-thickness | Z15, Z25 or Z35 to GB/T 5313, when ordered | As ordered |
| Dimensions | GB/T 709 | Confirmed |
| Certificate | GB/T 247; EN 10204 3.1 or 3.2 | As ordered |
Grades often compared with Q370qNHD are ASTM A709 Grade 50W, ASTM A709 HPS 50W and EN 10025-5 S355K2W; the comparison below shows where they differ.
Chemical Composition: Heat Analysis and Product Analysis
Two analyses matter for Q370qNHD. The heat (ladle) analysis is taken during casting and printed on the certificate. The product analysis is taken from finished plate and judged with the wider GB/T 222 tolerances. Mixing the two is the most common reason for disputed rejections.
Table 1 below is the heat (ladle) analysis for Q370qNHD from GB/T 714-2025 Tables 1, 5.
| Element | Q370qNHD heat analysis (%) | Note |
|---|---|---|
| C, max | 0.11 | |
| Si | 0.15 – 0.50 | Counts in I |
| Mn | 1.10 – 1.50 | Min 0.50% for coil only |
| P, max | 0.025 | Letter D |
| S, max | 0.015 | Letter D |
| Cu | 0.25 – 0.50 | Main weathering element |
| Cr | 0.40 – 0.70 | Weathering element |
| Ni | 0.30 – 0.40 | Weathering element |
| Mo, max | 0.20 | Changed in 2025 |
| Nb | 0.010 – 0.100 | Microalloy (see note) |
| V | 0.010 – 0.100 | Microalloy (see note) |
| Ti | 0.006 – 0.030 | Microalloy (see note) |
| Als | 0.015 – 0.050 | Alt 0.020–0.055% if total Al is used |
| N, max | 0.0080 | |
| B, max (residual) | 0.0005 | ≤0.0014% if C ≤0.06% |
| H, max (residual) | 0.0002 | |
| Weathering index I | ≥ 6.0 | Calculated from heat analysis |
Nb, V, Ti and Al may be added singly or together. Added singly, each must meet the range above; added together, at least one must reach its minimum and Nb + V + Ti ≤ 0.22%. Calcium treatment is required to control sulfide shape.
Table 2 is the product analysis: the limits a check analysis on finished plate is judged against. GB/T 714-2025 clause 7.1.3 calls up GB/T 222 for the permitted deviations.
| Element | Heat limit (%) | Deviation, GB/T 222-2025 Table 1 | Q370qNHD product analysis (%) |
|---|---|---|---|
| C | ≤ 0.11 | +0.02 | ≤ 0.13 |
| Si | 0.15 – 0.50 | ±0.05 | 0.10 – 0.55 |
| Mn | 1.10 – 1.50 | ±0.06 | 1.04 – 1.56 |
| P | ≤ 0.025 | +0.005 | ≤ 0.030 |
| S | ≤ 0.015 | +0.005 | ≤ 0.020 |
| V | 0.010 – 0.100 | +0.02 / −0.01 | ≤ 0.120 |
| Ti | 0.006 – 0.030 | +0.02 / −0.01 | ≤ 0.050 |
| Nb | 0.010 – 0.100 | ±0.005 (listed for 0.015–0.060%) | Above 0.060%: agree in contract |
| Cu | 0.25 – 0.50 | ±0.05 | 0.20 – 0.55 |
| Cr | 0.40 – 0.70 | ±0.05 | 0.35 – 0.75 |
| Ni | 0.30 – 0.40 | ±0.05 | 0.25 – 0.45 |
| Als | 0.015 – 0.050 | ±0.003 | Lower limit −0.003 (Table 1 row is for Al ≥0.015%; confirm) |
| Mo | ≤ 0.20 | Not listed in Table 1 | Agree in contract |
| N | ≤ 0.0080 | Listed only for 0.010–0.020% | Agree in contract |
How to read Table 2. Weathering bridge steel is normally classed as low-alloy steel, so Table 1 of GB/T 222 applies. Where the heat limit is a range, the deviation applies to both ends; for one heat, an element may deviate in one direction only.
Mechanical Properties
Tensile values follow Table 9 of GB/T 714-2025 for Q370qNH. Tensile specimens are transverse; round specimens are used above 40 mm. Where yield is not distinct, Rp0.2 replaces ReL.
| Nominal thickness | ReL min (MPa) | Rm min (MPa) | A min |
|---|---|---|---|
| ≤ 50 mm | 370 | 510 | 20% |
| > 50 – 100 mm | 360 | 510 | 20% |
| > 100 – 130 mm | 320 | 430 | 20% |
| > 130 – 150 mm | 320 | 430 | 20% |
Impact values follow Table 10, on longitudinal specimens, average of three:
| Letter / test temperature | KV2 ≤12 mm | KV2 >12 – 100 mm | KV2 >100 – 150 mm |
|---|---|---|---|
| D / −20°C | 80 J | 120 J | 47 J |
One single value may fall below the required average, but not below 70% of it. Plate over 8 mm and under 12 mm is tested with 7.5 mm specimens (75% of the value); 6–8 mm plate with 5 mm specimens (50%). Plate under 6 mm is not impact tested.
180° bend test, transverse: mandrel D = 2a up to 16 mm and 3a above 16 mm; may be omitted when the mill guarantees it. Yield ratio is not mandatory. If the contract asks for it, Annex C recommends ReL/Rm ≤ 0.88 up to 12 mm and ≤ 0.85 above 12 mm for TMCP plate.
Q370qNHC / Q370qNHD / Q370qNHE: Which Quality Grade?
Q370qNHD was tested at −60°C under GB/T 714-2015. In the 2025 tables the Q370qNH level stops at E (−40°C); the table shows what is listed today.
| Grade | Test temp. | KV2 ≤12 mm | KV2 12–100 mm | KV2 >100 mm | P / S max (%) |
|---|---|---|---|---|---|
| Q370qNHC | 0°C | 80 J | 120 J | 55 J | 0.030 / 0.025 |
| Q370qNHD | −20°C | 80 J | 120 J | 47 J | 0.025 / 0.015 |
| Q370qNHE | −40°C | 80 J | 120 J | 31 J | 0.020 / 0.010 |
| Q370qNHF | −60°C | 2015 edition only | 2015 edition only | — | 0.015 / 0.006 (2025 Table 1, F) |
For Q370qNHD the 2025 table stops at E. A −60°C requirement can still be met: by certifying to the 2015 edition where the contract allows, or by ordering Q370qENH with a supplementary −60°C test and an agreed energy. Where higher strength is acceptable, Q420qNHF is a listed −60°C weathering grade.
Q370qNHD: What Changed from GB/T 714-2015 to GB/T 714-2025
For Q370qNHD buyers the 2025 edition changes more than the year on the certificate. The points below come from the foreword of GB/T 714-2025 and its tables.
- The weathering requirement changed: Table 5 now requires a corrosion index I ≥ 6.0, and the 2015 Annex C guide for assessing weathering resistance was deleted.
- A Pcm table for weathering steel (Table 8) was added.
- Annex A now gives reference bridge-site environments for unpainted use (chloride, SO₂ and time-of-wetness limits).
- Mo maximum for Q370qNH was changed (now ≤0.20%; 2015-based sources quote ≤0.10%).
- Q370qNH is now listed in letters C, D and E. The 2015 edition listed it in D, E and F.
- Yield values above 100 mm were added for Q370qNH (320 MPa for >100–130 mm).
- Tensile strength is now banded by thickness (e.g. lower minimum Rm above 100 mm) instead of one value.
- Impact energy is set by thickness band (≤12 mm, 12–100 mm, >100 mm) in Table 10.
- Yield ratio is no longer a clause value; it is agreed in the contract, with recommendations in informative Annex C.
If a drawing cites 2015 and the plate is made to 2025, get the designer’s written acceptance; tensile strength above 100 mm and the yield-ratio basis differ.
Q370qNHD vs ASTM A709 and EN 10025: Which Grade Matches?
Can Q370qNHD replace a US or European bridge grade, or the other way round? Strength can match; toughness rules differ in kind, not only in number.
| Property | Q370qNHD | ASTM A709 Grade 50W | ASTM A709 HPS 50W | EN 10025-5 S355K2W |
|---|---|---|---|---|
| Min. yield (MPa) | 370 (≤50 mm) | 345 | 345 | 355 (≤16 mm) |
| Tensile (MPa) | 510 min | 485 min | 485 min | 470 – 630 |
| Charpy | 120 J at −20°C (12–100 mm) | CVN by temperature zone and member type (T / F) | CVN by temperature zone; fracture-critical (F) levels | 40 J at −20°C |
| Weathering chemistry | Yes, I ≥ 6.0 | Yes | Yes | Yes |
ASTM A709 sets Charpy requirements by temperature zone (1, 2, 3) and by member type: non-fracture-critical (T) or fracture-critical (F). GB/T 714 sets one value per letter, so compare the A709 zone with the GB/T 714 test temperature, not grade with grade.
EN 10025-5 weathering grades are general structural steels without a bridge-specific toughness level of 120 J; they suit many bridges but are not a one-to-one match.
The 120 J requirement for 12–100 mm plate is several times the 27–40 J typical of general weathering grades such as ASTM A588 or Corten A/B plate, which is why bridge owners specify Q370qNHD.
Q370qNHD Atmospheric Corrosion Index I and Unpainted Bridges
GB/T 714-2025 Table 5, footnote c, requires every Q370qNHD heat to reach an atmospheric corrosion index I of at least 6.0, calculated from the heat analysis:
I = 26.01(%Cu) + 3.88(%Ni) + 1.20(%Cr) + 1.49(%Si) + 17.28(%P) − 7.29(%Cu)(%Ni) − 9.10(%Ni)(%P) − 33.39(%Cu)²
This is the same predictive formula used with ASTM G101 for ASTM A709 Grade 50W and ASTM A709 HPS 70W, which makes Chinese and US ASTM A709 weathering steel plates easy to compare with Q370qNHD.
| Worked example (our calculation) | Cu | Ni | Cr | Si | P | I |
|---|---|---|---|---|---|---|
| All weathering elements at their Table 5 minimum | 0.25 | 0.30 | 0.40 | 0.15 | 0.010 | 5.88 |
| Illustrative mid-range heat | 0.32 | 0.36 | 0.55 | 0.30 | 0.012 | 6.74 |
Note the first row: a heat that only just meets every Table 5 minimum can still fall short of I = 6.0. That is why we ask the mill to print I on every Q370qNHD certificate, not just the chemistry.
Where can the steel be left unpainted? Annex A of GB/T 714-2025 gives reference bridge-site conditions:
- Rural or urban atmosphere with annual chloride deposition ≤ 3 mg/(m²·d)
- Annual SO₂ deposition ≤ 24 mg/(m²·d)
- Time of wetness ≤ 5,256 h per year (temperature above 0°C and relative humidity above 80%)
- Coastal sites only if they meet the same limits; for marine atmospheres Annex D points to T/CISA 073
Before omitting paint on Q370qNHD, measure or estimate chloride and SO₂ deposition at the site. One year of monitoring is a small cost against a bridge life of 100 years.
Welding Q370qNHD and Fatigue in Bridge Girders
GB/T 714-2025 clause 7.1.2 uses CEV for normalized, QT and TMCP steel with C >0.12%, and Pcm for weathering steel and TMCP steel with C ≤0.12%, both from the heat analysis:
CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15
Pcm = C + Si/30 + Mn/20 + Cu/20 + Ni/60 + Cr/20 + Mo/15 + V/10 + 5B
| Index | ≤50 mm | >50–100 mm | >100–130 mm |
|---|---|---|---|
| Pcm, Q370qNH (Table 8) | ≤ 0.22 | ≤ 0.24 | By agreement |
On thick Q370qNHD flanges, preheat, interpass control and low-hydrogen practice matter more than the grade itself. The certificate gives the data to set them. At −20°C, most procedures qualified on TMCP plate pass HAZ impact without special measures; keep multi-wire SAW heat input inside the qualified band.
Typical consumables for Q370qNHD: weathering-matched Ni-Cu consumables (AWS E8018-W2 type for 345–420 MPa), with higher-strength weathering wires for 460–500 MPa.
Fatigue. Welded details govern fatigue life in a bridge, and their fatigue strength is set by detail category, not by yield strength. Higher-strength plate can carry higher stress ranges only if detailing improves too.
Fatigue design follows JTG D64 (highway) and TB 10091 (railway) in China, EN 1993-1-9 in Europe and AASHTO LRFD in the US; fabrication commonly follows TB 10212, JTG/T 3650 or AWS D1.5.
Q370qDNHZ15, Z25 and Z35: Through-Thickness Plate for Bridges
Through-thickness properties matter wherever a full-penetration weld sits on the face of a plate, such as diaphragm-to-flange joints and cable anchor plates.
GB/T 714 adds the Z level to the end of the designation, for example Q370qDNHZ25. The test and acceptance follow GB/T 5313 and apply to plate 15 mm and thicker.
| Z grade | Heat sulfur, max (%) | Reduction of area, avg / single (%) |
|---|---|---|
| Z15 | 0.010 | 15 / 10 |
| Z25 | 0.007 | 25 / 15 |
| Z35 | 0.005 | 35 / 25 |
D chemistry allows S up to 0.015%. Z15 needs S ≤0.010% and Z25 needs ≤0.007%, so Z plate is still made from a dedicated low-sulfur heat.
A Z level on Q370qNHD does not change strength or impact rules. It adds a sulfur cap and a short-transverse tensile test. Z options apply across the GB/T 714 bridge steel range.
Equivalent Material Grades
Annex B of GB/T 714-2025 lists foreign grades against each strength level. It is informative: it tells you which families are close, not that the plates are interchangeable.
| Standard | Grade(s) | Fit for Q370qNHD |
|---|---|---|
| ASTM A709 | ASTM A709 Grade 50W, ASTM A709 HPS 50W | Closest; lower yield |
| EN 10025-5 | EN 10025-5 S355K2W | Closest; lower yield |
| ASTM A588 | ASTM A588 Grade C | Similar chemistry family |
| GB/T 714 (painted twin) | Q370qD | Same strength, no weathering elements |
For weathering grades also compare the corrosion index basis. Q370qNHD requires I ≥ 6.0 by the formula above; check that the substitute is assessed on the same basis.
Q370qNHD Testing, UT and Certificate
A batch of Q370qNHD is one grade, one heat, one thickness, one rolling schedule and one heat-treatment condition, up to 60 t. Table 12 of GB/T 714-2025 sets the tests:
| Test | Frequency | Method |
|---|---|---|
| Heat analysis | 1 per heat | GB/T 20066; GB/T 4336 / GB/T 223 |
| Weathering index I | Calculated per heat | Table 5 formula |
| Tensile | 1 per batch | GB/T 2975 / GB/T 228.1 |
| Bend 180° | 1 per batch (may be waived if guaranteed) | GB/T 232 |
| Charpy V at −20°C | 3 specimens per batch | GB/T 229 |
| Through-thickness (Z) | 3 specimens per batch, when ordered | GB/T 5313 |
| Ultrasonic | Every plate >20 mm, Class II or better | GB/T 2970 |
| Surface and dimensions | Every plate | Visual and gauges |
Impact retest: if a set fails, three more specimens are taken from the same batch. The average of all six must meet the requirement; two values may be below it, but only one below 70%. At −20°C the 120 J level is comfortable for well-made TMCP plate, but we still check each batch value, not just the average.
Dimensions
What we roll and cut in Q370qNHD:
- Thickness: 6 mm – 150 mm under GB/T 714 tensile tables; most orders 8 – 60 mm
- Width: 1500 – 4000 mm, depending on mill and thickness
- Length: 6000 – 18000 mm; longer by enquiry
- Edge: mill edge or cut edge
- Weight: theoretical, 7.85 g/cm³
Deck plate, webs, flanges, diaphragms and stiffeners are cut to drawing. For U-ribs and rolled sections on the same bridge, see steel beam profiles and steel structural profiles.
Tolerances
Q370qNHD plate is rolled to GB/T 709 tolerances. Class B (−0.30 mm) is standard; Class C (zero minus) can be agreed.
| Nominal thickness (mm) | Width ≤ 1500 mm | Width > 1500 – 2500 mm |
|---|---|---|
| > 8 – 15 | −0.30 / +0.80 | −0.30 / +1.00 |
| > 15 – 25 | −0.30 / +1.00 | −0.30 / +1.20 |
| > 25 – 40 | −0.30 / +1.10 | −0.30 / +1.30 |
| > 40 – 60 | −0.30 / +1.30 | −0.30 / +1.50 |
| > 60 – 100 | −0.30 / +1.50 | −0.30 / +1.80 |
| > 100 – 150 | −0.30 / +2.10 | −0.30 / +2.50 |
Bridge fabricators often ask for Class C (zero minus) on deck and flange plate so section properties are never under the design value. Wider plates follow the heavier GB/T 709 rows; we state them on the offer.
Q370qNHD Price Factors and How to Order
Two Q370qNHD quotes can differ a lot and both be fair. Base prices are similar; extras are where mills part.
| Cost driver | Effect on price |
|---|---|
| Strength level Q370q | Higher levels need more alloy and tighter rolling control |
| Quality letter | Small extra for −20°C testing and cleaner melt |
| Weathering alloys | Cu, Cr, Ni additions and I-index control add a weathering extra |
| Delivery route | TMCP / TMCP+T |
| Thickness | Over 60 mm and under 10 mm carry size extras |
| Z15 / Z25 / Z35 | Low-sulfur heat, Z test, UT; Z35 costs most |
| Width and length | Over 3000 mm wide or 15 m long needs mill confirmation |
| Quantity per size | Mill minimums per heat and size |
| Inspection and processing | 3.2 witness, profile cutting, blasting, priming quoted per item |
To get a firm quote in one round, send:
- Grade, edition and Z level, e.g. Q370qDNHZ25 to GB/T 714-2025
- Thickness × width × length and pieces or tonnes
- Delivery route and UT class if beyond Class II
- Certificate type and inspector
- Destination port and Incoterm
We quote plate price, extras and freight line by line. Need another letter? See Q370qNHE.
Applications
| Sector | Typical Q370qNHD components |
|---|---|
| Unpainted highway bridges | Plate girders and box girders in rural and urban atmospheres |
| Railway bridges | Truss members, plate girders, bracing |
| Remote and mountain sites | Bridges where repainting access is difficult or costly |
| Urban viaducts | Exposed girders with architectural rust finish |
| Pedestrian bridges | Unpainted box sections |
The letter D suits most highway and railway bridges in central and northern China, Europe and North America, where winter lows reach about −20°C.
Q370qNHD is the wrong plate for marine splash zones, tunnels, sites with heavy de-icing salt spray, or members that stay wet. There, use painted Q370qD or look at marine-atmosphere grades under T/CISA 073.
Supply Capability and Global Delivery
SHH STEEL sources Q370qNHD from first-line bridge-plate mills, including drafters of GB/T 714-2025 such as Ansteel, Valin Xiangtan, Jiangyin Xingcheng, Wuyang, Shougang and Xinyu.
- Certificates: EN 10204 3.1 standard; 3.2 with third-party witness (SGS, BV, TÜV or owner’s inspector)
- Tests: tensile, −20°C Charpy, bend, Z test, UT, product analysis, weathering index
- Processing: CNC plasma and flame cutting, bevelling, drilling, shot blasting and priming (or blasting only, for unpainted weathering steel)
- Terms: FOB Shanghai, CFR, CIF; TT, LC or TT + LC
- Marking: steel-stamped and paint-marked with grade, heat, size and mill, per GB/T 247
Q370qNHD goes from Shanghai to bridge sites and fabrication yards worldwide, usually as break-bulk for long plates.
Lead time: about 30–45 days from mill rolling; Z35, F letter or 3.2 inspection adds about 1–2 weeks. Sea time from Shanghai is about 7–12 days to Southeast Asia and 28–35 days to North Europe.
Why Choose SHH STEEL
As a steel manufacturer and exporter and global steel mill sourcing partner, SHH STEEL buys Q370qNHD straight from GB/T 714 mills, China origin. No mixed heats, no relabelled plate.
Before shipment we check four lines on every Q370qNHD certificate: yield and tensile for the actual thickness band, Charpy at −20°C, the Pcm and weathering index, and UT results. If one fails, the plate does not ship as Q370qNHD.
Use the same weathering consumables you qualified for Q345qNH, but re-check strength matching: Q370qNH has 510 MPa minimum tensile against 490 MPa.
We also tell buyers when another grade fits better. Neighbouring levels are Q345qNHD and Q390qNH. The painted counterpart is Q370qD. Browse more structural steel plates and high strength low alloy plates.
FAQ
-
What is Q370qNHD steel?
- Q370qNHD (Q370qDNH) is weathering bridge steel plate to GB/T 714-2025. It has 370 MPa minimum yield up to 50 mm, 510 MPa minimum tensile, Charpy impact of 120 J at −20°C for 12–100 mm plate, and Cu-Cr-Ni chemistry with a corrosion index I of at least 6.0 for unpainted bridges.
-
What is the difference between Q370qNHD and Q370qNHE?
- Strength and chemistry box are the same. Q370qNHD is Charpy tested at −20°C, Q370qNHE at −40°C, both needing 120 J for 12–100 mm plate. P/S caps are 0.025/0.015% for D and 0.020/0.010% for E. Choose by the lowest service or erection temperature.
-
What is the maximum thickness of Q370qNHD?
- 150 mm. GB/T 714-2025 covers single-rolled bridge plate up to 150 mm and gives Q370qNH tensile values for every band to 150 mm: 370 MPa yield to 50 mm, 360 MPa to 100 mm and 320 MPa above. Plate over 100 mm may be normalized by agreement (not for weathering grades).
-
What is the ASTM or EN equivalent of Q370qNHD?
- Close grades for Q370qNHD: No direct equivalent in Annex B / closest: ASTM A709 50W, HPS 50W / EN 10025-5 S355K2W. These are close families, not drop-in substitutes; compare yield at thickness, impact temperature and energy, and the weldability index before substituting.
-
Is GB/T 714-2015 still valid?
- No. GB/T 714-2025 was published on 31 October 2025 and took effect on 1 May 2026, fully replacing GB/T 714-2015. Contracts that still cite the 2015 edition can be certified to it, but new orders default to the 2025 edition.
-
Is Q370qNHD the same as Corten?
- No. Corten is a trade name for weathering steel used in many products. Q370qNHD is a bridge grade to GB/T 714 with 120 J impact for 12–100 mm plate in non-F letters, a Pcm cap, mandatory UT above 20 mm and I ≥6.0. Corten-type plate does not carry those bridge requirements.
Conclusion
Q370qNHD to GB/T 714 is weathering bridge steel with 370 MPa minimum yield, Cu-Cr-Ni chemistry, a weathering index of at least 6.0 and 120 J Charpy at −20°C for 12–100 mm plate.
It sits between Q345qNHD and Q390qNH in the weathering range, with Q370qNHE as sister letters. We check every Q370qNHD order against GB/T 714-2025 before quoting, so the offer, the test plan and the certificate all match the drawing.
SHH STEEL delivers Q370qNHD with the full GB/T 714 data set on an EN 10204 3.1 or 3.2 certificate. On request we add product analysis to GB/T 222, Z15–Z35, a tighter UT class, Class C tolerance, cutting and blasting.
We ship from Shanghai to bridge builders worldwide. Browse the full GB/T 714 range or other weathering steel plates.
Email the cutting list and the owner’s specification. We return a line-by-line offer with test plan and lead time. Contact SHH STEEL for Q370qNHD weathering bridge steel.