GB/T 714 Q690qD bridge steel plate stacked at SHH STEEL warehouse

GB/T 714 Q690qD Bridge Steel Plate Supplier

GB/T 714 Q690qD is bridge structural steel plate with 690 MPa minimum yield, 770 MPa minimum tensile and Charpy V-notch impact of 120 J at −20°C for 12–100 mm plate. SHH STEEL supplies Q690qD mill-direct, TMCP / TMCP+T / QT, up to 100 mm, with Z15–Z35, UT and heat and product analysis.
Keywords
Q690qD, Q690qD steel plate, GB/T 714 Q690qD, Q690q-D, Q690q D, Q690qD bridge steel, Q690qDZ15, Q690qDZ25, Q690qDZ35, bridge steel plate, Q690qD supplier
Equivalent Grades:
ASTM A709 HPS 100W / EN 10025-6 S690Q, S690QL, S690QL1 (Annex B) — Material Specification: GB/T 714-2025 (supersedes GB/T 714-2015) — Delivery: TMCP / TMCP+T / QT
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Q690q Quality Grades
GB/T 714-2025 vs 2015
Q690qD vs ASTM A709 / EN 10025
TMCP vs Normalized vs QT
Welding and Fatigue
Z15 / Z25 / Z35
Equivalent Material Grades
Testing and Inspection
Dimensions
Tolerances
Price and Ordering
Applications
Supply Capability
Why Choose SHH STEEL
FAQ
Conclusion

What is GB/T 714 Q690qD Bridge Steel Plate?

Q690qD is bridge structural steel plate to GB/T 714. Q stands for yield, 690 is the minimum yield in MPa for plate up to 50 mm, q stands for qiao (bridge) and D is the quality grade: Charpy V-notch at −20°C on longitudinal specimens.

Q690q is the top strength level of GB/T 714, with 690 MPa yield up to 50 mm and 650 MPa to 100 mm. Annex B lists ASTM A709 HPS 100W against Q690q. It is a specialist plate: thin, highly stressed members on record spans, where every tonne of girder weight saved reduces cable, pylon and foundation size.

Q690qD is the top strength level of GB/T 714 with a −20°C Charpy: 690 MPa yield to 50 mm, 650 MPa to 100 mm and 770 MPa minimum tensile. It is mapped to ASTM A709 HPS 100W in Annex B.

GB/T 714-2015 is no longer current. Its replacement, GB/T 714-2025, was published on 31 October 2025 and became effective on 1 May 2026. Where a contract still names the 2015 edition, we certify to it and flag any difference from 2025.

SHH STEEL (Shanghai Shenghonghe Import & Export Co., Ltd.) is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. We ship Q690qD cut to size with an EN 10204 3.1 or 3.2 certificate. Sister grades are listed under GB/T 714.

Material Specification

Specification element Requirement SHH STEEL compliance
Standard GB/T 714-2025 Q690qD Confirmed
Product Single-rolled plate ≤150 mm; hot-rolled strip and cut plate ≤25.4 mm Plate
Thickness with tensile values Up to 100 mm for Q690q Confirmed
Minimum yield ReL 690 MPa ≤50 mm; 650 MPa >50–100 mm Confirmed
Minimum tensile Rm 770 MPa ≤100 mm (no upper limit in the standard) Confirmed
Elongation A ≥ 14% Confirmed
Charpy V-notch −20°C, 120 J (12–100 mm), longitudinal Confirmed
Delivery condition TMCP, TMCP + tempering, or quenched and tempered (QT) As ordered
Weldability index Pcm (Table 7) for TMCP; CEV (Table 6) for QT Printed on MTC
Ultrasonic testing Plate >20 mm: GB/T 2970, Class II or better Every plate
Through-thickness Z15, Z25 or Z35 to GB/T 5313, when ordered As ordered
Dimensions GB/T 709 Confirmed
Certificate GB/T 247; EN 10204 3.1 or 3.2 As ordered

Grades often compared with Q690qD are ASTM A709 HPS 100W and ASTM A514 Grade Q; the comparison below shows where they differ.

Chemical Composition: Heat Analysis and Product Analysis

A check analysis on finished plate often reads a few hundredths higher than the mill certificate. That is not automatically a failure. The certificate shows the heat (ladle) analysis; plate drilled after rolling is judged as product analysis, with the tolerances of GB/T 222.

Table 1 below is the heat (ladle) analysis for Q690qD from GB/T 714-2025 Tables 1, 2, 3 and 4.

Element Q690qD TMCP (%) Q690q quenched and tempered (%)
C, max 0.11 0.15
Si, max 0.50 0.55
Mn 0.80 – 1.70 0.80 – 1.70
P, max 0.025 0.025
S, max 0.015 0.015
Nb 0.005 – 0.090 0.005 – 0.090
V 0.010 – 0.080 0.010 – 0.080
Ti 0.006 – 0.030 0.006 – 0.030
Als 0.010 – 0.045 0.010 – 0.045
Cr, max 1.00 0.40 – 1.00
Ni, max 1.20 0.25 – 1.20
Cu, max 0.55 0.15 – 0.55
Mo, max 0.60 0.20 – 0.60
N, max 0.0080 0.0080
B, max 0.0005 residual (≤0.0014 if C ≤0.10%) 0.0005–0.0030 may be added
H, max 0.0002 0.0002

Nb, V, Ti and Al may be added singly or together. Added singly, each must meet the range above; added together, at least one must reach its minimum and Nb + V + Ti ≤ 0.22%.

Table 2 is the product analysis: the limits a check analysis on finished plate is judged against. GB/T 714-2025 clause 7.1.3 calls up GB/T 222 for the permitted deviations.

Element Heat limit (%) Deviation, GB/T 222-2025 Table 2 (alloy) Q690qD product analysis (%)
C ≤ 0.11 +0.01 ≤ 0.12
Si ≤ 0.50 +0.04 ≤ 0.54
Mn 0.80 – 1.70 ±0.04 0.76 – 1.74
P ≤ 0.025 +0.005 (see note) ≤ 0.030
S ≤ 0.015 +0.005 (see note) ≤ 0.020
Cr ≤ 1.00 +0.05 (0.90–2.10% band) ≤ 1.05
Ni ≤ 1.20 +0.05 (1.00–2.00% band) ≤ 1.25
Cu ≤ 0.55 +0.03 ≤ 0.58
Mo ≤ 0.60 +0.02 (0.30–0.60% band) ≤ 0.62
V 0.010 – 0.080 +0.01 (≤0.10% band) ≤ 0.090
Ti 0.006 – 0.030 +0.02 ≤ 0.050
Nb, B, N See heat table Not read in our copy of Table 2 Agree in contract

How to read Table 2. With Ni up to 1.20% and Mo up to 0.60%, Q690q heats are normally classed as alloy steel under GB/T 13304, so the alloy-steel table of GB/T 222 applies. One steel uses one table only; the certificate should say which.

Mechanical Properties

Tensile values follow Table 9 of GB/T 714-2025 for Q690q. Tensile specimens are transverse; round specimens are used above 40 mm. Where yield is not distinct, Rp0.2 replaces ReL.

Nominal thickness ReL min (MPa) Rm min (MPa) A min
≤ 50 mm 690 770 14%
> 50 – 100 mm 650 770 14%

Impact values follow Table 10, on longitudinal specimens, average of three:

Letter / test temperature KV2 ≤12 mm KV2 >12 – 100 mm KV2 >100 – 150 mm
D / −20°C 80 J 120 J Not applicable

One single value may fall below the required average, but not below 70% of it. Plate over 8 mm and under 12 mm is tested with 7.5 mm specimens (75% of the value); 6–8 mm plate with 5 mm specimens (50%). Plate under 6 mm is not impact tested.

180° bend test, transverse: mandrel D = 2a up to 16 mm and 3a above 16 mm; may be omitted when the mill guarantees it. Yield ratio is not mandatory and Annex C gives no recommended value at this level; agree a limit in the contract if the design needs one.

Q690qD / Q690qE / Q690qF: Which Quality Grade?

Q690qD is tested at −20°C. It suits most highway and railway bridges in central and northern China, Europe and North America, where winter lows reach about −20°C. D is the most specified letter on Chinese bridge drawings. It is tested at −20°C and the melt is tighter than C: P ≤0.025%, S ≤0.015%.

Grade Test temp. KV2 ≤12 mm KV2 12–100 mm KV2 >100 mm P / S max (%)
Q690qD −20°C 80 J 120 J — 0.025 / 0.015
Q690qE −40°C 80 J 120 J — 0.020 / 0.010
Q690qF −60°C By agreement 77 J — 0.015 / 0.006

Over-specifying the letter costs money; under-specifying it costs safety. Choose from the lowest service or erection temperature, then step up one letter for thick, restrained or fracture-critical members.

Q690qD: What Changed from GB/T 714-2015 to GB/T 714-2025

For Q690qD buyers the 2025 edition changes more than the year on the certificate. The points below come from the foreword of GB/T 714-2025 and its tables.

  • A TMCP route was added for Q690q (C ≤0.11%, Pcm ≤0.24% to 50 mm). In 2015 it was QT only.
  • CEV and Pcm limits were revised (Tables 6 and 7).
  • Tensile strength is now banded by thickness (e.g. lower minimum Rm above 100 mm) instead of one value.
  • Impact energy is set by thickness band (≤12 mm, 12–100 mm, >100 mm) in Table 10.
  • Yield ratio is no longer a clause value; it is agreed in the contract, with recommendations in informative Annex C.
  • Section products were removed; the standard now covers plate and strip only.
  • Delivery is TMCP, TMCP + tempering or QT; normalizing is kept only for Q345q/Q370q plate over 100 mm by agreement.

If a drawing cites 2015 and the plate is made to 2025, get the designer’s written acceptance; tensile strength above 100 mm and the yield-ratio basis differ.

Q690qD vs ASTM A709 and EN 10025: Which Grade Matches?

Can Q690qD replace a US or European bridge grade, or the other way round? Strength can match; toughness rules differ in kind, not only in number.

Property Q690qD ASTM A709 HPS 100W ASTM A514 Grade Q EN 10025-6 S690Q
Min. yield (MPa) 690 (≤50 mm) 690 (≤65 mm) 690 (≤65 mm) 690 (≤50 mm)
Tensile (MPa) 770 min 760 – 895 760 – 895 770 – 940
Charpy 120 J at −20°C (12–100 mm) CVN by temperature zone; fracture-critical (F) levels Supplementary only Q / QL / QL1: −20 / −40 / −60°C
Weathering chemistry No Yes No No

ASTM A709 sets Charpy requirements by temperature zone (1, 2, 3) and by member type: non-fracture-critical (T) or fracture-critical (F). GB/T 714 sets one value per letter, so compare the A709 zone with the GB/T 714 test temperature, not grade with grade.

EN 10025-3/-4/-6 grades show yield at the thinnest band; their values fall with thickness. GB/T 714 keeps 690 MPa to 50 mm. EN tensile ranges have upper limits; GB/T 714 gives minimums only.

The 120 J requirement in GB/T 714 for 12–100 mm plate is several times the 27–40 J typical of general structural grades. That margin is the main reason bridge owners specify Q690qD rather than GB/T 1591 plate.

Q690qD Delivery Condition: TMCP vs Normalized vs Quenched and Tempered

GB/T 714-2025 clause 3.2 defines TMCP as rolling with the final deformation in a controlled temperature range, including accelerated cooling with or without tempering (self-tempering included) but excluding direct quenching and quench-and-temper. The delivery route must be stated on the certificate.

Route Available for Q690qD Weldability index Notes
TMCP Yes Pcm ≤0.24% (≤50 mm) C ≤0.11%; up to 100 mm
TMCP + tempering Yes Pcm Improves toughness uniformity
Quenched and tempered Yes CEV ≤0.60% (≤50 mm) C ≤0.15%; B 0.0005–0.0030% may be added
Normalized No — Not listed

Q690q can be TMCP or QT. A published study on 40 mm Q690qNH plate found QT plate more uniform in strength and toughness through the thickness than TMCP + tempered plate; we discuss route choice with the owner on every Q690q enquiry. D-letter plate is usually plain TMCP; tempering is added mainly for heavy plate or tight yield-ratio limits.

Ask for the route on the purchase order. It changes the weldability index, the welding procedure and, for heavy plate, the price of Q690qD.

Welding Q690qD and Fatigue in Bridge Girders

GB/T 714-2025 clause 7.1.2 uses CEV for normalized, QT and TMCP steel with C >0.12%, and Pcm for weathering steel and TMCP steel with C ≤0.12%, both from the heat analysis:

CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15

Pcm = C + Si/30 + Mn/20 + Cu/20 + Ni/60 + Cr/20 + Mo/15 + V/10 + 5B

Index ≤50 mm >50–100 mm >100–130 mm
Pcm, TMCP (Table 7) ≤ 0.24 ≤ 0.25 —
CEV, QT (Table 6) ≤ 0.60 ≤ 0.65 —

The index caps in GB/T 714 are maximums. Real Q690qD heats often sit well below them, and preheat should be set from the actual value, not the cap. At −20°C, most procedures qualified on TMCP plate pass HAZ impact without special measures; keep multi-wire SAW heat input inside the qualified band.

Typical consumables for Q690qD: E76-class consumables (AWS E11018M type).

Fatigue. Welded details govern fatigue life in a bridge, and their fatigue strength is set by detail category, not by yield strength. Higher-strength plate can carry higher stress ranges only if detailing improves too.

Fatigue design follows JTG D64 (highway) and TB 10091 (railway) in China, EN 1993-1-9 in Europe and AASHTO LRFD in the US; fabrication commonly follows TB 10212, JTG/T 3650 or AWS D1.5.

Q690qDZ15, Z25 and Z35: Through-Thickness Plate for Bridges

Z15, Z25 and Z35 tell the mill how much through-thickness ductility a plate must prove. The higher the number, the lower the sulfur and the higher the cost.

GB/T 714 adds the Z level to the end of the designation, for example Q690qDZ25. The test and acceptance follow GB/T 5313 and apply to plate 15 mm and thicker.

Z grade Heat sulfur, max (%) Reduction of area, avg / single (%)
Z15 0.010 15 / 10
Z25 0.007 25 / 15
Z35 0.005 35 / 25

D chemistry allows S up to 0.015%. Z15 needs S ≤0.010% and Z25 needs ≤0.007%, so Z plate is still made from a dedicated low-sulfur heat.

For Q690qD, we test Z per GB/T 5313 batch rules and print the three reduction-of-area values on the certificate. Z options apply across the GB/T 714 bridge steel range.

Equivalent Material Grades

Annex B of GB/T 714-2025 lists foreign grades against each strength level. It is informative: it tells you which families are close, not that the plates are interchangeable.

Standard Grade(s) Fit for Q690qD
ASTM A709 ASTM A709 HPS 100W Listed in Annex B
EN 10025-6 EN 10025-6 S690Q, EN 10025-6 S690QL, EN 10025-6 S690QL1 Listed in Annex B
ASTM A514 ASTM A514 Grade Q QT, strength only
GB/T 16270 GB/T 16270 Q690D QT alternative, different toughness rules
GB/T 1591 GB/T 1591 Q690MD TMCP general structural

Before substituting, compare three things line by line: minimum yield at the actual thickness, the impact test temperature and energy, and the weldability index. For Q690qD, the 120 J impact level and the Pcm/CEV caps are usually the hardest to match.

Q690qD Testing, UT and Certificate

A batch of Q690qD is one grade, one heat, one thickness, one rolling schedule and one heat-treatment condition, up to 60 t. Table 12 of GB/T 714-2025 sets the tests:

Test Frequency Method
Heat analysis 1 per heat GB/T 20066; GB/T 4336 / GB/T 223
Tensile 1 per batch GB/T 2975 / GB/T 228.1
Bend 180° 1 per batch (may be waived if guaranteed) GB/T 232
Charpy V at −20°C 3 specimens per batch GB/T 229
Through-thickness (Z) 3 specimens per batch, when ordered GB/T 5313
Ultrasonic Every plate >20 mm, Class II or better GB/T 2970
Surface and dimensions Every plate Visual and gauges

Impact retest: if a set fails, three more specimens are taken from the same batch. The average of all six must meet the requirement; two values may be below it, but only one below 70%. At −20°C the 120 J level is comfortable for well-made TMCP plate, but we still check each batch value, not just the average.

Dimensions

Q690qD plate sizes we regularly ship:

  • Thickness: 6 mm – 100 mm under GB/T 714 tensile tables; most orders 10 – 60 mm
  • Width: 1500 – 4000 mm, depending on mill and thickness
  • Length: 6000 – 18000 mm; longer by enquiry
  • Edge: mill edge or cut edge
  • Weight: theoretical, 7.85 g/cm³

Deck plate, webs, flanges, diaphragms and stiffeners are cut to drawing. For U-ribs and rolled sections on the same bridge, see steel beam profiles and steel structural profiles.

Tolerances

Q690qD plate is rolled to GB/T 709 tolerances. Class B (−0.30 mm) is standard; Class C (zero minus) can be agreed.

Nominal thickness (mm) Width ≤ 1500 mm Width > 1500 – 2500 mm
> 8 – 15 −0.30 / +0.80 −0.30 / +1.00
> 15 – 25 −0.30 / +1.00 −0.30 / +1.20
> 25 – 40 −0.30 / +1.10 −0.30 / +1.30
> 40 – 60 −0.30 / +1.30 −0.30 / +1.50
> 60 – 100 −0.30 / +1.50 −0.30 / +1.80
> 100 – 150 −0.30 / +2.10 −0.30 / +2.50

Bridge fabricators often ask for Class C (zero minus) on deck and flange plate so section properties are never under the design value. Wider plates follow the heavier GB/T 709 rows; we state them on the offer.

Q690qD Price Factors and How to Order

A Q690qD price per ton is a base price plus extras. The extras explain most gaps between quotes.

Cost driver Effect on price
Strength level Q690q Higher levels need more alloy and tighter rolling control
Quality letter Small extra for −20°C testing and cleaner melt
Delivery route TMCP / TMCP+T / QT; QT costs more than TMCP
Thickness Over 60 mm and under 10 mm carry size extras
Z15 / Z25 / Z35 Low-sulfur heat, Z test, UT; Z35 costs most
Width and length Over 3000 mm wide or 15 m long needs mill confirmation
Quantity per size Mill minimums per heat and size
Inspection and processing 3.2 witness, profile cutting, blasting, priming quoted per item

To get a firm quote in one round, send:

  • Grade, edition and Z level, e.g. Q690qDZ25 to GB/T 714-2025
  • Thickness × width × length and pieces or tonnes
  • Delivery route and UT class if beyond Class II
  • Certificate type and inspector
  • Destination port and Incoterm

We quote plate price, extras and freight line by line. Need another letter? See Q690qE, Q690qF.

Applications

Sector Typical Q690qD components
Record-span bridges Main truss chords and node plates
Cable anchorages Anchor boxes and anchor plates
Steel pylons Highly stressed pylon walls
Movable and military bridges Lightweight girders
Retrofit High-strength replacement members

The letter D suits most highway and railway bridges in central and northern China, Europe and North America, where winter lows reach about −20°C.

It is the wrong plate for pressure equipment (pressure vessel steel plates), unpainted exposure (weathering steel plates) or ship hulls (shipbuilding steel plates).

Supply Capability and Global Delivery

SHH STEEL sources Q690qD from first-line bridge-plate mills, including drafters of GB/T 714-2025 such as Ansteel, Valin Xiangtan, Jiangyin Xingcheng, Wuyang, Shougang and Xinyu.

  • Certificates: EN 10204 3.1 standard; 3.2 with third-party witness (SGS, BV, TÜV or owner’s inspector)
  • Tests: tensile, −20°C Charpy, bend, Z test, UT, product analysis
  • Processing: CNC plasma and flame cutting, bevelling, drilling, shot blasting and priming
  • Terms: FOB Shanghai, CFR, CIF; TT, LC or TT + LC
  • Marking: steel-stamped and paint-marked with grade, heat, size and mill, per GB/T 247

Our Q690qD exports follow Chinese bridge design abroad: railway and highway bridges built by EPC contractors in Asia, Africa and Latin America.

Lead time: about 45–60 days from mill rolling; Z35, F letter or 3.2 inspection adds about 1–2 weeks. Sea time from Shanghai is about 7–12 days to Southeast Asia and 28–35 days to North Europe.

Why Choose SHH STEEL

Mill-direct, China origin: SHH STEEL is a steel manufacturer and exporter and global steel mill sourcing partner, and Q690qD is one of the bridge grades we handle regularly.

Before shipment we check four lines on every Q690qD certificate: yield and tensile for the actual thickness band, Charpy at −20°C, the CEV or Pcm for the delivery route, and UT results. If one fails, the plate does not ship as Q690qD.

Q690q welding is specialist work. We supply the heat chemistry early so the fabricator can qualify procedures before the main delivery.

We also tell buyers when another grade fits better. Neighbouring levels are Q620qD. Browse more structural steel plates and high strength low alloy plates.

FAQ

What is Q690qD steel?
Q690qD is bridge structural steel plate to GB/T 714-2025. It has 690 MPa minimum yield up to 50 mm, 770 MPa minimum tensile, 14% elongation and Charpy V-notch impact of 120 J at −20°C for 12–100 mm plate. It is delivered TMCP, TMCP + tempering, or quenched and tempered.
What is the difference between Q690qD and Q690qE?
Strength and chemistry box are the same. Q690qD is Charpy tested at −20°C, Q690qE at −40°C, both needing 120 J for 12–100 mm plate. P/S caps are 0.025/0.015% for D and 0.020/0.010% for E. Choose by the lowest service or erection temperature.
Is Q690qD the same as Q690D?
No. Q690D is general structural steel (GB/T 1591), while Q690qD is bridge steel to GB/T 714 with lower P and S, controlled weldability index, mandatory UT above 20 mm and 120 J impact for 12–100 mm plate. Bridge plate can replace general plate, not the reverse.
What is the ASTM or EN equivalent of Q690qD?
Close grades for Q690qD: ASTM A709 HPS 100W / EN 10025-6 S690Q, S690QL, S690QL1 (Annex B). These are close families, not drop-in substitutes; compare yield at thickness, impact temperature and energy, and the weldability index before substituting.
Does Q690qD have a yield ratio requirement?
Not a mandatory one. GB/T 714-2025 clause 7.7 lets the buyer set a yield ratio in the contract, and Annex C gives no recommended value for Q690q, so the limit must be agreed.
Is Q690qD weldable?
Yes. GB/T 714-2025 caps the weldability index for Q690qD up to 50 mm at Pcm ≤0.24% (TMCP) or CEV ≤0.60% (QT). Preheat depends on actual chemistry, thickness and restraint, and is fixed by the qualified welding procedure.

Conclusion

Q690qD to GB/T 714-2025 is bridge plate with 690 MPa minimum yield, 770 MPa minimum tensile and 120 J Charpy at −20°C for 12–100 mm plate.

The next strength level is Q620qD, with Q690qE and Q690qF as sister letters. Before ordering Q690qD, confirm the edition on the drawing, the delivery route and any Z level; those three choices drive cost, lead time and welding.

SHH STEEL ships Q690qD with heat analysis, weldability index and mechanical results on every certificate. Third-party inspection, product analysis and Z testing are added on request.

We ship from Shanghai to bridge builders worldwide. Browse the full GB/T 714 range or other high strength low alloy plates.

Email the cutting list and the owner’s specification. We return a line-by-line offer with test plan and lead time. Contact SHH STEEL for Q690qD bridge steel plate.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X