GB/T 714 Q345qD Bridge Steel Plate Supplier
General Description
Q345qD is bridge structural steel plate to GB/T 714. Q stands for yield, 345 is the minimum yield in MPa for plate up to 50 mm, q stands for qiao (bridge) and D is the quality grade: Charpy V-notch at −20°C on longitudinal specimens.
Q345q is the workhorse of Chinese steel bridges: plate girders, box girders, orthotropic deck plate, cross beams and stiffeners on railway and highway spans. Most bridge drawings issued in China still start at Q345q. It has the widest thickness range in GB/T 714 (up to 150 mm) and the lowest carbon-equivalent cap of any TMCP grade.
Q345qD is the default bridge plate in China. When a highway or railway drawing simply says ‘bridge steel’, it usually means Q345qD: 345 MPa yield, −20°C Charpy, TMCP. Most of our bridge tonnage is this grade, and most mills keep Q345qD in their regular rolling cycle.
GB/T 714-2025 is the current edition. It was issued on 31 October 2025, took effect on 1 May 2026 and fully supersedes GB/T 714-2015, the fourth revision since the standard was first issued in 1965. We certify to the edition written on the purchase order.
SHH STEEL (Shanghai Shenghonghe Import & Export Co., Ltd.) is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. We ship Q345qD cut to size with an EN 10204 3.1 or 3.2 certificate. Sister grades are listed under GB/T 714.
Material Specification
| Specification element | Requirement | SHH STEEL compliance |
|---|---|---|
| Standard | GB/T 714-2025 Q345qD | Confirmed |
| Product | Single-rolled plate ≤150 mm; hot-rolled strip and cut plate ≤25.4 mm | Plate |
| Thickness with tensile values | Up to 150 mm for Q345q | Confirmed |
| Minimum yield ReL | 345 MPa ≤50 mm; 335 MPa >50–100 mm | Confirmed |
| Minimum tensile Rm | 490 MPa ≤100 mm (no upper limit in the standard) | Confirmed |
| Elongation A | ≥ 20% | Confirmed |
| Charpy V-notch | −20°C, 120 J (12–100 mm), longitudinal | Confirmed |
| Delivery condition | TMCP or TMCP + tempering; normalized by agreement for >100–150 mm | As ordered |
| Weldability index | CEV (Table 6) and Pcm (Table 7) | Printed on MTC |
| Ultrasonic testing | Plate >20 mm: GB/T 2970, Class II or better | Every plate |
| Through-thickness | Z15, Z25 or Z35 to GB/T 5313, when ordered | As ordered |
| Dimensions | GB/T 709 | Confirmed |
| Certificate | GB/T 247; EN 10204 3.1 or 3.2 | As ordered |
Grades often compared with Q345qD are ASTM A709 Grade 50, ASTM A709 HPS 50W and EN 10025-4 S355M; the comparison below shows where they differ.
Chemical Composition
Two analyses matter for Q345qD. The heat (ladle) analysis is taken during casting and printed on the certificate. The product analysis is taken from finished plate and judged with the wider GB/T 222 tolerances. Mixing the two is the most common reason for disputed rejections.
Table 1 below is the heat (ladle) analysis for Q345qD from GB/T 714-2025 Tables 1, 2 and 3.
| Element | Q345qD TMCP (%) | Q345q normalized, >100–150 mm (%) |
|---|---|---|
| C, max | 0.14 | 0.18 |
| Si, max | 0.55 | 0.55 |
| Mn | 0.80 – 1.60 | 0.90 – 1.60 |
| P, max | 0.025 | 0.025 |
| S, max | 0.015 | 0.015 |
| Nb | 0.010 – 0.090 | 0.005 – 0.060 |
| V | 0.010 – 0.080 | 0.010 – 0.080 |
| Ti | 0.006 – 0.030 | 0.006 – 0.030 |
| Als | 0.010 – 0.045 | 0.010 – 0.045 |
| Cr, max | 0.30 | 0.30 |
| Ni, max | 0.30 | 0.30 |
| Cu, max | 0.30 | 0.30 |
| Mo, max | — | — |
| N, max | 0.0080 | 0.0080 |
| B, max | 0.0005 residual (≤0.0014 if C ≤0.10%) | 0.0005 residual |
| H, max | 0.0002 | 0.0002 |
Nb, V, Ti and Al may be added singly or together. Added singly, each must meet the range above; added together, at least one must reach its minimum and Nb + V + Ti ≤ 0.22%.
Table 2 is the product analysis: the limits a check analysis on finished plate is judged against. GB/T 714-2025 clause 7.1.3 calls up GB/T 222 for the permitted deviations.
| Element | Heat limit (%) | Deviation, GB/T 222-2025 Table 1 | Q345qD product analysis (%) |
|---|---|---|---|
| C | ≤ 0.14 | +0.02 | ≤ 0.16 |
| Si | ≤ 0.55 | +0.05 | ≤ 0.60 |
| Mn | 0.80 – 1.60 | ±0.06 | 0.74 – 1.66 |
| P | ≤ 0.025 | +0.005 | ≤ 0.030 |
| S | ≤ 0.015 | +0.005 | ≤ 0.020 |
| V | 0.010 – 0.080 | +0.02 / −0.01 | ≤ 0.100 |
| Ti | 0.006 – 0.030 | +0.02 / −0.01 | ≤ 0.050 |
| Nb | 0.010 – 0.090 | ±0.005 (listed for 0.015–0.060%) | Above 0.060%: agree in contract |
| Cr | ≤ 0.30 | +0.05 | ≤ 0.35 |
| Ni | ≤ 0.30 | +0.05 | ≤ 0.35 |
| Cu | ≤ 0.30 | +0.05 | ≤ 0.35 |
| Als | 0.010 – 0.045 | ±0.003 | Lower limit −0.003 (Table 1 row is for Al ≥0.015%; confirm) |
| Mo | — | Not listed in Table 1 | — |
| N | ≤ 0.0080 | Listed only for 0.010–0.020% | Agree in contract |
How to read Table 2. Q345q TMCP heats are low-alloy steel, so Table 1 of GB/T 222 applies. Si ≤0.55% is above 0.37%, so +0.05% applies; Mn falls in the 0.80–1.70% band, so ±0.06%. For one heat, an element may deviate in one direction only.
Mechanical Properties
Tensile values follow Table 9 of GB/T 714-2025 for Q345q. Tensile specimens are transverse; round specimens are used above 40 mm. Where yield is not distinct, Rp0.2 replaces ReL.
| Nominal thickness | ReL min (MPa) | Rm min (MPa) | A min |
|---|---|---|---|
| ≤ 50 mm | 345 | 490 | 20% |
| > 50 – 100 mm | 335 | 490 | 20% |
| > 100 – 130 mm | 305 | 430 | 20% |
| > 130 – 150 mm | 305 | 430 | 20% |
Impact values follow Table 10, on longitudinal specimens, average of three:
| Letter / test temperature | KV2 ≤12 mm | KV2 >12 – 100 mm | KV2 >100 – 150 mm |
|---|---|---|---|
| D / −20°C | 80 J | 120 J | 47 J |
One single value may fall below the required average, but not below 70% of it. Plate over 8 mm and under 12 mm is tested with 7.5 mm specimens (75% of the value); 6–8 mm plate with 5 mm specimens (50%). Plate under 6 mm is not impact tested.
180° bend test, transverse: mandrel D = 2a up to 16 mm and 3a above 16 mm; may be omitted when the mill guarantees it. Yield ratio is not mandatory. If the contract asks for it, Annex C recommends ReL/Rm ≤ 0.88 up to 12 mm and ≤ 0.85 above 12 mm for TMCP plate.
Q345q Quality Grades
Q345qD is tested at −20°C. It suits most highway and railway bridges in central and northern China, Europe and North America, where winter lows reach about −20°C. D is the most specified letter on Chinese bridge drawings. It is tested at −20°C and the melt is tighter than C: P ≤0.025%, S ≤0.015%.
| Grade | Test temp. | KV2 ≤12 mm | KV2 12–100 mm | KV2 >100 mm | P / S max (%) |
|---|---|---|---|---|---|
| Q345qC | 0°C | 80 J | 120 J | 55 J | 0.030 / 0.025 |
| Q345qD | −20°C | 80 J | 120 J | 47 J | 0.025 / 0.015 |
| Q345qE | −40°C | 80 J | 120 J | 31 J | 0.020 / 0.010 |
Over-specifying the letter costs money; under-specifying it costs safety. Choose from the lowest service or erection temperature, then step up one letter for thick, restrained or fracture-critical members.
GB/T 714-2025 vs 2015
For Q345qD buyers the 2025 edition changes more than the year on the certificate. The points below come from the foreword of GB/T 714-2025 and its tables.
- The Mn range for TMCP steel was revised: the minimum is now 0.80%, and the maximum may be raised to 2.00% by agreement.
- CEV and Pcm limits were revised (Tables 6 and 7).
- Normalized grades were dropped except for plate over 100 mm by agreement.
- Tensile strength is now banded by thickness (e.g. lower minimum Rm above 100 mm) instead of one value.
- Impact energy is set by thickness band (≤12 mm, 12–100 mm, >100 mm) in Table 10.
- Yield ratio is no longer a clause value; it is agreed in the contract, with recommendations in informative Annex C.
- Section products were removed; the standard now covers plate and strip only.
- Delivery is TMCP, TMCP + tempering or QT; normalizing is kept only for Q345q/Q370q plate over 100 mm by agreement.
If a drawing cites 2015 and the plate is made to 2025, get the designer’s written acceptance; tensile strength above 100 mm and the yield-ratio basis differ.
Q345qD vs ASTM A709 / EN 10025
Can Q345qD replace a US or European bridge grade, or the other way round? Strength can match; toughness rules differ in kind, not only in number.
| Property | Q345qD | ASTM A709 Grade 50 | ASTM A709 HPS 50W | EN 10025-4 S355M |
|---|---|---|---|---|
| Min. yield (MPa) | 345 (≤50 mm) | 345 | 345 | 355 (≤16 mm) |
| Tensile (MPa) | 490 min | 450 min | 485 min | 470 – 630 |
| Charpy | 120 J at −20°C (12–100 mm) | CVN by temperature zone and member type (T / F) | CVN by temperature zone; fracture-critical (F) levels | 40 J at −20°C |
| Weathering chemistry | No | No | Yes | No |
ASTM A709 sets Charpy requirements by temperature zone (1, 2, 3) and by member type: non-fracture-critical (T) or fracture-critical (F). GB/T 714 sets one value per letter, so compare the A709 zone with the GB/T 714 test temperature, not grade with grade.
EN 10025-3/-4/-6 grades show yield at the thinnest band; their values fall with thickness. GB/T 714 keeps 345 MPa to 50 mm. EN tensile ranges have upper limits; GB/T 714 gives minimums only.
The 120 J requirement in GB/T 714 for 12–100 mm plate is several times the 27–40 J typical of general structural grades. That margin is the main reason bridge owners specify Q345qD rather than GB/T 1591 plate.
TMCP vs Normalized vs QT
GB/T 714-2025 clause 3.2 defines TMCP as rolling with the final deformation in a controlled temperature range, including accelerated cooling with or without tempering (self-tempering included) but excluding direct quenching and quench-and-temper. The delivery route must be stated on the certificate.
| Route | Available for Q345qD | Weldability index | Notes |
|---|---|---|---|
| TMCP | Yes, standard | CEV (C >0.12%) or Pcm (C ≤0.12%) | C ≤0.14%; most plate up to 100 mm |
| TMCP + tempering | Yes | Same as TMCP | Used to relieve stresses or tune yield ratio |
| Normalized | Only >100–150 mm, by agreement | CEV by agreement | C ≤0.18%; heavy plate only |
| Quenched and tempered | Not listed | — | Not a GB/T 714 route at this level |
For Q345q we supply TMCP as standard. Normalized plate makes sense only for heavy sections over 100 mm, where accelerated cooling gives less benefit; CEV is then agreed in the contract. D-letter plate is usually plain TMCP; tempering is added mainly for heavy plate or tight yield-ratio limits.
Ask for the route on the purchase order. It changes the weldability index, the welding procedure and, for heavy plate, the price of Q345qD.
Welding and Fatigue
GB/T 714-2025 clause 7.1.2 uses CEV for normalized, QT and TMCP steel with C >0.12%, and Pcm for weathering steel and TMCP steel with C ≤0.12%, both from the heat analysis:
CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15
Pcm = C + Si/30 + Mn/20 + Cu/20 + Ni/60 + Cr/20 + Mo/15 + V/10 + 5B
| Index | ≤50 mm | >50–100 mm | >100–130 mm |
|---|---|---|---|
| CEV, TMCP, C >0.12% (Table 6) | ≤ 0.38 | ≤ 0.40 | by agreement |
| Pcm, TMCP (Table 7) | ≤ 0.20 | ≤ 0.20 | ≤ 0.20 |
| CEV, normalized | — | — | By agreement |
We send the actual heat analysis of Q345qD before shipment, so the fabricator can check preheat and interpass limits against the procedure qualification record. At −20°C, most procedures qualified on TMCP plate pass HAZ impact without special measures; keep multi-wire SAW heat input inside the qualified band.
Typical consumables for Q345qD: E50-class low-hydrogen electrodes (AWS E7018 type) and matching SAW wire/flux.
Fatigue. Welded details govern fatigue life in a bridge, and their fatigue strength is set by detail category, not by yield strength. Higher-strength plate can carry higher stress ranges only if detailing improves too.
Fatigue design follows JTG D64 (highway) and TB 10091 (railway) in China, EN 1993-1-9 in Europe and AASHTO LRFD in the US; fabrication commonly follows TB 10212, JTG/T 3650 or AWS D1.5.
Z15 / Z25 / Z35
Lamellar tearing appears in thick plate loaded across its thickness, typically at cruciform joints and anchor plates. A Z grade adds a short-transverse tensile test and a lower sulfur cap.
GB/T 714 adds the Z level to the end of the designation, for example Q345qDZ25. The test and acceptance follow GB/T 5313 and apply to plate 15 mm and thicker.
| Z grade | Heat sulfur, max (%) | Reduction of area, avg / single (%) |
|---|---|---|
| Z15 | 0.010 | 15 / 10 |
| Z25 | 0.007 | 25 / 15 |
| Z35 | 0.005 | 35 / 25 |
D chemistry allows S up to 0.015%. Z15 needs S ≤0.010% and Z25 needs ≤0.007%, so Z plate is still made from a dedicated low-sulfur heat.
Most bridges need Z on a small share of the tonnage. Mark it item by item on the cutting list rather than on the whole Q345qD order. Z options apply across the GB/T 714 bridge steel range.
Equivalent Material Grades
Annex B of GB/T 714-2025 lists foreign grades against each strength level. It is informative: it tells you which families are close, not that the plates are interchangeable.
| Standard | Grade(s) | Fit for Q345qD |
|---|---|---|
| ASTM A709 | ASTM A709 Grade 50, ASTM A709 Grade 50W, ASTM A709 HPS 50W | Listed in Annex B |
| EN 10025-3 | EN 10025-3 S355N, EN 10025-3 S355NL | Listed in Annex B |
| EN 10025-4 | EN 10025-4 S355M, EN 10025-4 S355ML | Listed in Annex B |
| GB/T 1591 | GB/T 1591 Q355MD | General structural, lower impact |
| JIS G3106 | JIS G3106 SM490C | Closest by strength |
| GB/T 714 (weathering twin) | Q345qNHD | Same strength, weathering chemistry |
Before substituting, compare three things line by line: minimum yield at the actual thickness, the impact test temperature and energy, and the weldability index. For Q345qD, the 120 J impact level and the Pcm/CEV caps are usually the hardest to match.
Testing and Inspection
A batch of Q345qD is one grade, one heat, one thickness, one rolling schedule and one heat-treatment condition, up to 60 t. Table 12 of GB/T 714-2025 sets the tests:
| Test | Frequency | Method |
|---|---|---|
| Heat analysis | 1 per heat | GB/T 20066; GB/T 4336 / GB/T 223 |
| Tensile | 1 per batch | GB/T 2975 / GB/T 228.1 |
| Bend 180° | 1 per batch (may be waived if guaranteed) | GB/T 232 |
| Charpy V at −20°C | 3 specimens per batch | GB/T 229 |
| Through-thickness (Z) | 3 specimens per batch, when ordered | GB/T 5313 |
| Ultrasonic | Every plate >20 mm, Class II or better | GB/T 2970 |
| Surface and dimensions | Every plate | Visual and gauges |
Impact retest: if a set fails, three more specimens are taken from the same batch. The average of all six must meet the requirement; two values may be below it, but only one below 70%. At −20°C the 120 J level is comfortable for well-made TMCP plate, but we still check each batch value, not just the average.
Dimensions
Q345qD sizes we supply from mill and stock:
- Thickness: 6 mm – 150 mm under GB/T 714 tensile tables; most orders 8 – 60 mm
- Width: 1500 – 4000 mm, depending on mill and thickness
- Length: 6000 – 18000 mm; longer by enquiry
- Edge: mill edge or cut edge
- Weight: theoretical, 7.85 g/cm³
Deck plate, webs, flanges, diaphragms and stiffeners are cut to drawing. For U-ribs and rolled sections on the same bridge, see steel beam profiles and steel structural profiles.
Tolerances
Dimensional tolerances for Q345qD follow GB/T 709, as GB/T 714 directs. The default is Class B, which fixes the minus side at 0.30 mm.
| Nominal thickness (mm) | Width ≤ 1500 mm | Width > 1500 – 2500 mm |
|---|---|---|
| > 8 – 15 | −0.30 / +0.80 | −0.30 / +1.00 |
| > 15 – 25 | −0.30 / +1.00 | −0.30 / +1.20 |
| > 25 – 40 | −0.30 / +1.10 | −0.30 / +1.30 |
| > 40 – 60 | −0.30 / +1.30 | −0.30 / +1.50 |
| > 60 – 100 | −0.30 / +1.50 | −0.30 / +1.80 |
| > 100 – 150 | −0.30 / +2.10 | −0.30 / +2.50 |
Bridge fabricators often ask for Class C (zero minus) on deck and flange plate so section properties are never under the design value. Wider plates follow the heavier GB/T 709 rows; we state them on the offer.
Price and Ordering
Two Q345qD quotes can differ a lot and both be fair. Base prices are similar; extras are where mills part.
| Cost driver | Effect on price |
|---|---|
| Strength level Q345q | Higher levels need more alloy and tighter rolling control |
| Quality letter | Small extra for −20°C testing and cleaner melt |
| Delivery route | TMCP / TMCP+T (N >100 mm by agreement) |
| Thickness | Over 60 mm and under 10 mm carry size extras |
| Z15 / Z25 / Z35 | Low-sulfur heat, Z test, UT; Z35 costs most |
| Width and length | Over 3000 mm wide or 15 m long needs mill confirmation |
| Quantity per size | Mill minimums per heat and size |
| Inspection and processing | 3.2 witness, profile cutting, blasting, priming quoted per item |
To get a firm quote in one round, send:
- Grade, edition and Z level, e.g. Q345qDZ25 to GB/T 714-2025
- Thickness × width × length and pieces or tonnes
- Delivery route and UT class if beyond Class II
- Certificate type and inspector
- Destination port and Incoterm
We quote plate price, extras and freight line by line. Need another letter? See Q345qC, Q345qE.
Applications
| Sector | Typical Q345qD components |
|---|---|
| Highway bridges | Steel box girders, I-girders, orthotropic deck plate, U-ribs, diaphragms |
| Railway bridges | Plate girders, truss chords and diagonals, gusset plates, bearing stiffeners |
| Urban viaducts | Curved box girders, pier caps, steel-concrete composite girders |
| Pedestrian bridges | Box sections, cable anchor plates |
| Long-span bridges | Secondary members, cross frames, deck plate on cable-stayed spans |
The letter D suits most highway and railway bridges in central and northern China, Europe and North America, where winter lows reach about −20°C.
It is the wrong plate for pressure equipment (pressure vessel steel plates), unpainted exposure (weathering steel plates) or ship hulls (shipbuilding steel plates).
Supply Capability
SHH STEEL sources Q345qD from first-line bridge-plate mills, including drafters of GB/T 714-2025 such as Ansteel, Valin Xiangtan, Jiangyin Xingcheng, Wuyang, Shougang and Xinyu.
- Certificates: EN 10204 3.1 standard; 3.2 with third-party witness (SGS, BV, TÜV or owner’s inspector)
- Tests: tensile, −20°C Charpy, bend, Z test, UT, product analysis
- Processing: CNC plasma and flame cutting, bevelling, drilling, shot blasting and priming
- Terms: FOB Shanghai, CFR, CIF; TT, LC or TT + LC
- Marking: steel-stamped and paint-marked with grade, heat, size and mill, per GB/T 247
Q345qD leaves Shanghai for bridge projects designed to Chinese codes abroad, mainly through EPC contractors in Southeast Asia, Central Asia, the Middle East and Africa.
Lead time: about 30–45 days from mill rolling; Z35, F letter or 3.2 inspection adds about 1–2 weeks. Sea time from Shanghai is about 7–12 days to Southeast Asia and 28–35 days to North Europe.
Why Choose SHH STEEL
SHH STEEL works mill-direct as a steel manufacturer and exporter and global steel mill sourcing partner, China origin. Every Q345qD plate is traced to its heat.
Before shipment we check four lines on every Q345qD certificate: yield and tensile for the actual thickness band, Charpy at −20°C, the CEV or Pcm for the delivery route, and UT results. If one fails, the plate does not ship as Q345qD.
Because Q345qD is rolled so often, lead times are shorter than for E or F letters, and odd sizes can often be combined into a mill campaign. Send the full size list early.
We also tell buyers when another grade fits better. Neighbouring levels are Q370qD. The weathering counterpart is Q345qNHD. Browse more structural steel plates and high strength low alloy plates.
FAQ
-
What is Q345qD steel?
- Q345qD is bridge structural steel plate to GB/T 714-2025. It has 345 MPa minimum yield up to 50 mm, 490 MPa minimum tensile, 20% elongation and Charpy V-notch impact of 120 J at −20°C for 12–100 mm plate. It is delivered TMCP or TMCP + tempering, with normalizing allowed above 100 mm by agreement.
-
What is the difference between Q345qD and Q345qE?
- Strength and chemistry box are the same. Q345qD is Charpy tested at −20°C, Q345qE at −40°C, both needing 120 J for 12–100 mm plate. P/S caps are 0.025/0.015% for D and 0.020/0.010% for E. Choose by the lowest service or erection temperature.
-
What is the maximum thickness of Q345qD?
- 150 mm. GB/T 714-2025 covers single-rolled bridge plate up to 150 mm and gives Q345q tensile values for every band to 150 mm: 345 MPa yield to 50 mm, 335 MPa to 100 mm and 305 MPa above. Plate over 100 mm may be normalized by agreement.
-
What is the ASTM or EN equivalent of Q345qD?
- Close grades for Q345qD: ASTM A709 Grade 50, 50W, HPS 50W / EN 10025-3 S355N, S355NL / EN 10025-4 S355M, S355ML. These are close families, not drop-in substitutes; compare yield at thickness, impact temperature and energy, and the weldability index before substituting.
-
Does Q345qD have a yield ratio requirement?
- Not a mandatory one. GB/T 714-2025 clause 7.7 lets the buyer set a yield ratio in the contract. Annex C recommends ReL/Rm ≤0.88 up to 12 mm and ≤0.85 above 12 mm for TMCP plate at the Q345q level.
-
Is Q345qD weldable?
- Yes. GB/T 714-2025 caps the weldability index for Q345qD up to 50 mm at CEV ≤0.38% (C >0.12%) or Pcm ≤0.20%. Preheat depends on actual chemistry, thickness and restraint, and is fixed by the qualified welding procedure.
Conclusion
Q345qD to GB/T 714-2025 is bridge plate with 345 MPa minimum yield, 490 MPa minimum tensile and 120 J Charpy at −20°C for 12–100 mm plate.
The next strength level is Q370qD, with Q345qC and Q345qE as sister letters. For Q345qD, the deciding numbers on the certificate are yield at the actual thickness, Charpy at −20°C and the weldability index for the delivery route.
Every Q345qD plate from SHH STEEL ships with heat analysis, the weldability index, tensile and Charpy results on an EN 10204 3.1 or 3.2 certificate. Product analysis, Z15–Z35, extra UT and cut-to-size are options.
We ship from Shanghai to bridge builders worldwide. Browse the full GB/T 714 range or other high strength low alloy plates.
Share your size list, Z level and edition, and we reply with mill, route, lead time, test plan and price in one message. Contact SHH STEEL for a mill-direct Q345qD bridge steel plate quotation.