GB/T 714 Q420qF bridge steel plate stacked at SHH STEEL warehouse

GB/T 714 Q420qF Bridge Steel Plate Supplier

GB/T 714 Q420qF is bridge structural steel plate with 420 MPa minimum yield, 540 MPa minimum tensile and Charpy V-notch impact of 47 J at −60°C for 12–100 mm plate. SHH STEEL supplies Q420qF mill-direct, TMCP / TMCP+T, up to 130 mm, with Z15–Z35, UT and heat and product analysis.
Keywords
Q420qF, Q420qF steel plate, GB/T 714 Q420qF, Q420q-F, Q420q F, Q420qF bridge steel, Q420qFZ15, Q420qFZ25, Q420qFZ35, bridge steel plate, Q420qF supplier
Equivalent Grades:
EN 10025-4 S420M, S420ML (Annex B) / ASTM A572 Gr.60 (strength only) — Material Specification: GB/T 714-2025 (supersedes GB/T 714-2015) — Delivery: TMCP / TMCP+T
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Q420q Quality Grades
GB/T 714-2025 vs 2015
Q420qF vs ASTM A709 / EN 10025
TMCP vs Normalized vs QT
Welding and Fatigue
Z15 / Z25 / Z35
Equivalent Material Grades
Testing and Inspection
Dimensions
Tolerances
Price and Ordering
Applications
Supply Capability
Why Choose SHH STEEL
FAQ
Conclusion

What is GB/T 714 Q420qF Bridge Steel Plate?

Q420qF is bridge structural steel plate to GB/T 714. Q stands for yield, 420 is the minimum yield in MPa for plate up to 50 mm, q stands for qiao (bridge) and F is the quality grade: Charpy V-notch at −60°C on longitudinal specimens.

Q420q is the first of the lean-carbon high-strength bridge grades (C ≤0.11%), used for main trusses and box girders on long-span bridges. Q420q moves to a C ≤0.11% TMCP chemistry and is judged by Pcm (≤0.22%) instead of CEV. China’s first large Q420qE application was the Nanjing Dashengguan Yangtze River Bridge, a six-track high-speed railway arch bridge.

Q420qF is the lowest strength level that offers the F letter in GB/T 714: Charpy at −60°C with at least 47 J for plate over 12 mm. Buyers are Arctic and sub-Arctic projects, and owners who want −60°C proof on fracture-critical members.

The current text is GB/T 714-2025 (published 31 October 2025, effective 1 May 2026). It replaced GB/T 714-2015 completely and was drafted by Ansteel, Valin Xiangtan, Wuyang, Shougang and other plate mills together with the main bridge fabricators.

SHH STEEL (Shanghai Shenghonghe Import & Export Co., Ltd.) is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. We ship Q420qF cut to size with an EN 10204 3.1 or 3.2 certificate. Sister grades are listed under GB/T 714.

Material Specification

Specification element Requirement SHH STEEL compliance
Standard GB/T 714-2025 Q420qF Confirmed
Product Single-rolled plate ≤150 mm; hot-rolled strip and cut plate ≤25.4 mm Plate
Thickness with tensile values Up to 130 mm for Q420q Confirmed
Minimum yield ReL 420 MPa ≤50 mm; 410 MPa >50–100 mm Confirmed
Minimum tensile Rm 540 MPa ≤100 mm (no upper limit in the standard) Confirmed
Elongation A ≥ 19% Confirmed
Charpy V-notch −60°C, 47 J (12–100 mm), longitudinal Confirmed
Delivery condition TMCP or TMCP + tempering As ordered
Weldability index Pcm (Table 7) Printed on MTC
Ultrasonic testing Plate >20 mm: GB/T 2970, Class II or better Every plate
Through-thickness Z15, Z25 or Z35 to GB/T 5313, when ordered As ordered
Dimensions GB/T 709 Confirmed
Certificate GB/T 247; EN 10204 3.1 or 3.2 As ordered

Grades often compared with Q420qF are EN 10025-4 S420M, EN 10025-4 S420ML and ASTM A572 Gr.60; the comparison below shows where they differ.

Chemical Composition: Heat Analysis and Product Analysis

Bridge owners increasingly order a product analysis on finished plate. For Q420qF that check is judged against GB/T 714 heat limits plus the deviations in GB/T 222, not against the heat limits alone.

Table 1 below is the heat (ladle) analysis for Q420qF from GB/T 714-2025 Tables 1, 3.

Element Q420qF TMCP (%)
C, max 0.11
Si, max 0.55
Mn 0.80 – 1.70
P, max 0.015
S, max 0.006
Nb 0.010 – 0.090
V 0.010 – 0.080
Ti 0.006 – 0.030
Als 0.010 – 0.045
Cr, max 0.50
Ni, max 0.30
Cu, max 0.30
Mo, max 0.20
N, max 0.0080
B, max 0.0005 residual (≤0.0014 if C ≤0.10%)
H, max 0.0002

Nb, V, Ti and Al may be added singly or together. Added singly, each must meet the range above; added together, at least one must reach its minimum and Nb + V + Ti ≤ 0.22%.

Table 2 is the product analysis: the limits a check analysis on finished plate is judged against. GB/T 714-2025 clause 7.1.3 calls up GB/T 222 for the permitted deviations.

Element Heat limit (%) Deviation, GB/T 222-2025 Table 1 Q420qF product analysis (%)
C ≤ 0.11 +0.02 ≤ 0.13
Si ≤ 0.55 +0.05 ≤ 0.60
Mn 0.80 – 1.70 ±0.06 0.74 – 1.76
P ≤ 0.015 +0.005 ≤ 0.020
S ≤ 0.006 +0.005 ≤ 0.011
V 0.010 – 0.080 +0.02 / −0.01 ≤ 0.100
Ti 0.006 – 0.030 +0.02 / −0.01 ≤ 0.050
Nb 0.010 – 0.090 ±0.005 (listed for 0.015–0.060%) Above 0.060%: agree in contract
Cr ≤ 0.50 +0.05 ≤ 0.55
Ni ≤ 0.30 +0.05 ≤ 0.35
Cu ≤ 0.30 +0.05 ≤ 0.35
Als 0.010 – 0.045 ±0.003 Lower limit −0.003 (Table 1 row is for Al ≥0.015%; confirm)
Mo ≤ 0.20 Not listed in Table 1 Agree in contract
N ≤ 0.0080 Listed only for 0.010–0.020% Agree in contract

How to read Table 2. Q420q TMCP heats are low-alloy steel, so Table 1 of GB/T 222 applies. Si ≤0.55% is above 0.37%, so +0.05% applies; Mn falls in the 0.80–1.70% band, so ±0.06%. For one heat, an element may deviate in one direction only.

Mechanical Properties

Tensile values follow Table 9 of GB/T 714-2025 for Q420q. Tensile specimens are transverse; round specimens are used above 40 mm. Where yield is not distinct, Rp0.2 replaces ReL.

Nominal thickness ReL min (MPa) Rm min (MPa) A min
≤ 50 mm 420 540 19%
> 50 – 100 mm 410 540 19%
> 100 – 130 mm 365 460 19%

Impact values follow Table 10, on longitudinal specimens, average of three:

Letter / test temperature KV2 ≤12 mm KV2 >12 – 100 mm KV2 >100 – 150 mm
F / −60°C By agreement 47 J Not applicable

One single value may fall below the required average, but not below 70% of it. Plate over 8 mm and under 12 mm is tested with 7.5 mm specimens (75% of the value); 6–8 mm plate with 5 mm specimens (50%). Plate under 6 mm is not impact tested.

180° bend test, transverse: mandrel D = 2a up to 16 mm and 3a above 16 mm; may be omitted when the mill guarantees it. Yield ratio is not mandatory. If the contract asks for it, Annex C recommends ReL/Rm ≤ 0.88 up to 12 mm and ≤ 0.86 above 12 mm for TMCP plate.

Q420qD / Q420qE / Q420qF: Which Quality Grade?

Q420qF is tested at −60°C. It suits Arctic and sub-Arctic bridges, high-latitude rail lines and owners who want the largest toughness margin for fracture-critical members. F is the coldest letter in GB/T 714: Charpy at −60°C, P ≤0.015% and S ≤0.006%. It exists only for Q420q and above (and their NH versions), and its energy rises with strength.

Grade Test temp. KV2 ≤12 mm KV2 12–100 mm KV2 >100 mm P / S max (%)
Q420qD −20°C 80 J 120 J 47 J 0.025 / 0.015
Q420qE −40°C 80 J 120 J 31 J 0.020 / 0.010
Q420qF −60°C By agreement 47 J — 0.015 / 0.006

Note that F energy at Q420q is 47 J, not 120 J: the colder test uses a lower energy that GB/T 714-2025 raises with strength, from 47 J at Q420q/Q460q to 77 J at Q690q. Plate up to 12 mm needs an agreed value.

Q420qF: What Changed from GB/T 714-2015 to GB/T 714-2025

For Q420qF buyers the 2025 edition changes more than the year on the certificate. The points below come from the foreword of GB/T 714-2025 and its tables.

  • Yield values above 100 mm were added (365 MPa for >100–130 mm).
  • The Mn range for TMCP steel was revised: the minimum is now 0.80%, and the maximum may be raised to 2.00% by agreement.
  • CEV and Pcm limits were revised (Tables 6 and 7).
  • Tensile strength is now banded by thickness (e.g. lower minimum Rm above 100 mm) instead of one value.
  • Impact energy is set by thickness band (≤12 mm, 12–100 mm, >100 mm) in Table 10.
  • Yield ratio is no longer a clause value; it is agreed in the contract, with recommendations in informative Annex C.
  • Section products were removed; the standard now covers plate and strip only.
  • Delivery is TMCP, TMCP + tempering or QT; normalizing is kept only for Q345q/Q370q plate over 100 mm by agreement.

If a drawing cites 2015 and the plate is made to 2025, get the designer’s written acceptance; tensile strength above 100 mm and the yield-ratio basis differ.

Q420qF vs ASTM A709 and EN 10025: Which Grade Matches?

Can Q420qF replace a US or European bridge grade, or the other way round? Strength can match; toughness rules differ in kind, not only in number.

Property Q420qF EN 10025-4 S420M EN 10025-4 S420ML ASTM A572 Gr.60
Min. yield (MPa) 420 (≤50 mm) 420 (≤16 mm) 420 (≤16 mm) 415
Tensile (MPa) 540 min 520 – 680 520 – 680 520 min
Charpy 47 J at −60°C (12–100 mm) 40 J at −20°C 27 J at −50°C Supplementary only
Weathering chemistry No No No No

ASTM A709 sets Charpy requirements by temperature zone (1, 2, 3) and by member type: non-fracture-critical (T) or fracture-critical (F). GB/T 714 sets one value per letter, so compare the A709 zone with the GB/T 714 test temperature, not grade with grade.

EN 10025-3/-4/-6 grades show yield at the thinnest band; their values fall with thickness. GB/T 714 keeps 420 MPa to 50 mm. EN tensile ranges have upper limits; GB/T 714 gives minimums only.

At −60°C, the 47 J required for Q420qF is a demanding figure; general structural grades rarely prove any toughness that cold. For the C, D and E letters GB/T 714 asks 120 J, several times the 27–40 J typical of GB/T 1591 plate.

Q420qF Delivery Condition: TMCP vs Normalized vs Quenched and Tempered

GB/T 714-2025 clause 3.2 defines TMCP as rolling with the final deformation in a controlled temperature range, including accelerated cooling with or without tempering (self-tempering included) but excluding direct quenching and quench-and-temper. The delivery route must be stated on the certificate.

Route Available for Q420qF Weldability index Notes
TMCP Yes, standard Pcm (C ≤0.11%) Up to 130 mm
TMCP + tempering Yes Same as TMCP Common on thick or E/F plate
Normalized No — Dropped in 2025 for this level
Quenched and tempered Not listed — Use GB/T 16270 if QT is required

Q420q is a TMCP grade with C ≤0.11%, so weldability is judged by Pcm. TMCP + tempering is often used on E and F plate to improve toughness scatter. F-letter plate is often TMCP + tempering or, at the top strength levels, QT; ask which route the mill has qualified for −60°C.

Ask for the route on the purchase order. It changes the weldability index, the welding procedure and, for heavy plate, the price of Q420qF.

Welding Q420qF and Fatigue in Bridge Girders

GB/T 714-2025 clause 7.1.2 uses CEV for normalized, QT and TMCP steel with C >0.12%, and Pcm for weathering steel and TMCP steel with C ≤0.12%, both from the heat analysis:

CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15

Pcm = C + Si/30 + Mn/20 + Cu/20 + Ni/60 + Cr/20 + Mo/15 + V/10 + 5B

Index ≤50 mm >50–100 mm >100–130 mm
Pcm, TMCP (Table 7) ≤ 0.22 ≤ 0.22 ≤ 0.22

On thick Q420qF flanges, preheat, interpass control and low-hydrogen practice matter more than the grade itself. The certificate gives the data to set them. At −60°C, both weld metal and HAZ must prove toughness. Expect lower heat input, more passes and consumables qualified at −60°C.

Typical consumables for Q420qF: E55-class low-hydrogen consumables (AWS E8018 type).

Fatigue. Welded details govern fatigue life in a bridge, and their fatigue strength is set by detail category, not by yield strength. Higher-strength plate can carry higher stress ranges only if detailing improves too.

Fatigue design follows JTG D64 (highway) and TB 10091 (railway) in China, EN 1993-1-9 in Europe and AASHTO LRFD in the US; fabrication commonly follows TB 10212, JTG/T 3650 or AWS D1.5.

Q420qFZ15, Z25 and Z35: Through-Thickness Plate for Bridges

Z15, Z25 and Z35 tell the mill how much through-thickness ductility a plate must prove. The higher the number, the lower the sulfur and the higher the cost.

GB/T 714 adds the Z level to the end of the designation, for example Q420qFZ25. The test and acceptance follow GB/T 5313 and apply to plate 15 mm and thicker.

Z grade Heat sulfur, max (%) Reduction of area, avg / single (%)
Z15 0.010 15 / 10
Z25 0.007 25 / 15
Z35 0.005 35 / 25

F chemistry limits S to 0.006%, which already meets the Z25 sulfur cap (0.007%). Only Z35 (S ≤0.005%) needs a further step.

Put Z only where the joint needs it, usually node plates, anchor boxes and diaphragm-to-flange joints over about 25 mm. Keep the rest standard Q420qF. Z options apply across the GB/T 714 bridge steel range.

Equivalent Material Grades

Annex B of GB/T 714-2025 lists foreign grades against each strength level. It is informative: it tells you which families are close, not that the plates are interchangeable.

Standard Grade(s) Fit for Q420qF
EN 10025-4 EN 10025-4 S420M, EN 10025-4 S420ML Listed in Annex B
EN 10025-3 EN 10025-3 S420N, EN 10025-3 S420NL Normalized alternative
ASTM A572 ASTM A572 Gr.60 Strength only, not a bridge grade
GB/T 1591 GB/T 1591 Q420MF General structural
GB/T 714 (weathering twin) Q420qNHF Same strength, weathering chemistry

Before substituting, compare three things line by line: minimum yield at the actual thickness, the impact test temperature and energy, and the weldability index. For Q420qF, the 120 J impact level and the Pcm/CEV caps are usually the hardest to match.

Q420qF Testing, UT and Certificate

A batch of Q420qF is one grade, one heat, one thickness, one rolling schedule and one heat-treatment condition, up to 60 t. Table 12 of GB/T 714-2025 sets the tests:

Test Frequency Method
Heat analysis 1 per heat GB/T 20066; GB/T 4336 / GB/T 223
Tensile 1 per batch GB/T 2975 / GB/T 228.1
Bend 180° 1 per batch (may be waived if guaranteed) GB/T 232
Charpy V at −60°C 3 specimens per batch GB/T 229
Through-thickness (Z) 3 specimens per batch, when ordered GB/T 5313
Ultrasonic Every plate >20 mm, Class II or better GB/T 2970
Surface and dimensions Every plate Visual and gauges

Impact retest: if a set fails, three more specimens are taken from the same batch. The average of all six must meet the requirement; two values may be below it, but only one below 70%. At −60°C, mills may need trial heats before the production run; we agree the test plan before accepting the order.

Dimensions

Q420qF sizes we supply from mill and stock:

  • Thickness: 6 mm – 130 mm under GB/T 714 tensile tables; most orders 10 – 80 mm
  • Width: 1500 – 4000 mm, depending on mill and thickness
  • Length: 6000 – 18000 mm; longer by enquiry
  • Edge: mill edge or cut edge
  • Weight: theoretical, 7.85 g/cm³

Deck plate, webs, flanges, diaphragms and stiffeners are cut to drawing. For U-ribs and rolled sections on the same bridge, see steel beam profiles and steel structural profiles.

Tolerances

For Q420qF, thickness tolerance follows GB/T 709 Class B unless the order says otherwise: −0.30 mm at every thickness, with the plus side shown below.

Nominal thickness (mm) Width ≤ 1500 mm Width > 1500 – 2500 mm
> 8 – 15 −0.30 / +0.80 −0.30 / +1.00
> 15 – 25 −0.30 / +1.00 −0.30 / +1.20
> 25 – 40 −0.30 / +1.10 −0.30 / +1.30
> 40 – 60 −0.30 / +1.30 −0.30 / +1.50
> 60 – 100 −0.30 / +1.50 −0.30 / +1.80
> 100 – 150 −0.30 / +2.10 −0.30 / +2.50

Bridge fabricators often ask for Class C (zero minus) on deck and flange plate so section properties are never under the design value. Wider plates follow the heavier GB/T 709 rows; we state them on the offer.

Q420qF Price Factors and How to Order

Bridge plate prices move with the steel market, but for Q420qF the order details often matter more.

Cost driver Effect on price
Strength level Q420q Higher levels need more alloy and tighter rolling control
Quality letter Highest extra: −60°C testing, S ≤0.006%, limited mills
Delivery route TMCP / TMCP+T
Thickness Over 60 mm and under 10 mm carry size extras
Z15 / Z25 / Z35 Low-sulfur heat, Z test, UT; Z35 costs most
Width and length Over 3000 mm wide or 15 m long needs mill confirmation
Quantity per size Mill minimums per heat and size
Inspection and processing 3.2 witness, profile cutting, blasting, priming quoted per item

To get a firm quote in one round, send:

  • Grade, edition and Z level, e.g. Q420qFZ25 to GB/T 714-2025
  • Thickness × width × length and pieces or tonnes
  • Delivery route and UT class if beyond Class II
  • Certificate type and inspector
  • Destination port and Incoterm

We quote plate price, extras and freight line by line. Need another letter? See Q420qD, Q420qE.

Applications

Sector Typical Q420qF components
Long-span railway bridges Main truss chords and node plates
Cable-stayed bridges Steel box girders, anchor boxes
Suspension bridges Stiffening girders
Combined road-rail bridges Truss members carrying heavy rail load
Arch bridges Arch ribs and hangers’ anchorages

The letter F suits Arctic and sub-Arctic bridges, high-latitude rail lines and owners who want the largest toughness margin for fracture-critical members.

It is the wrong plate for pressure equipment (pressure vessel steel plates), unpainted exposure (weathering steel plates) or ship hulls (shipbuilding steel plates).

Supply Capability and Global Delivery

SHH STEEL sources Q420qF from first-line bridge-plate mills, including drafters of GB/T 714-2025 such as Ansteel, Valin Xiangtan, Jiangyin Xingcheng, Wuyang, Shougang and Xinyu.

  • Certificates: EN 10204 3.1 standard; 3.2 with third-party witness (SGS, BV, TÜV or owner’s inspector)
  • Tests: tensile, −60°C Charpy, bend, Z test, UT, product analysis
  • Processing: CNC plasma and flame cutting, bevelling, drilling, shot blasting and priming
  • Terms: FOB Shanghai, CFR, CIF; TT, LC or TT + LC
  • Marking: steel-stamped and paint-marked with grade, heat, size and mill, per GB/T 247

Q420qF goes from Shanghai to bridge sites and fabrication yards worldwide, usually as break-bulk for long plates.

Lead time: about 45–60 days from mill rolling; Z35, F letter or 3.2 inspection adds about 1–2 weeks. Sea time from Shanghai is about 7–12 days to Southeast Asia and 28–35 days to North Europe.

Why Choose SHH STEEL

Mill-direct, China origin: SHH STEEL is a steel manufacturer and exporter and global steel mill sourcing partner, and Q420qF is one of the bridge grades we handle regularly.

Before shipment we check four lines on every Q420qF certificate: yield and tensile for the actual thickness band, Charpy at −60°C, the CEV or Pcm for the delivery route, and UT results. If one fails, the plate does not ship as Q420qF.

For Q420qF under 12 mm the impact value is by agreement. Write the figure into the purchase order, or the certificate cannot show compliance.

We also tell buyers when another grade fits better. Neighbouring levels are Q390q and Q460qF. The weathering counterpart is Q420qNHF. Browse more structural steel plates and high strength low alloy plates.

FAQ

What is Q420qF steel?
Q420qF is bridge structural steel plate to GB/T 714-2025. It has 420 MPa minimum yield up to 50 mm, 540 MPa minimum tensile, 19% elongation and Charpy V-notch impact of 47 J at −60°C for 12–100 mm plate. It is delivered TMCP or TMCP + tempering.
What impact energy does Q420qF need at −60°C?
GB/T 714-2025 requires at least 47 J at −60°C on longitudinal specimens for Q420qF plate over 12 mm and up to 100 mm. For plate 12 mm and thinner the value is by agreement. F energy rises with strength: 47 J for Q420q and Q460q, 54 J for Q500q, 60 J for Q550q, 69 J for Q620q and 77 J for Q690q.
What is the maximum thickness of Q420qF?
GB/T 714-2025 covers bridge plate up to 150 mm, but tensile values for Q420q stop at 130 mm. Above that there is no table value, so Q420qF cannot be certified thicker than 130 mm without a special agreement.
What is the ASTM or EN equivalent of Q420qF?
Close grades for Q420qF: EN 10025-4 S420M, S420ML (Annex B) / ASTM A572 Gr.60 (strength only). These are close families, not drop-in substitutes; compare yield at thickness, impact temperature and energy, and the weldability index before substituting.
What does the q mean in GB/T 714 bridge steel grades?
The lowercase q stands for qiao, Chinese for bridge. In a grade such as Q420qD, Q means yield, 420 is the minimum yield in MPa, q marks bridge steel to GB/T 714 and D is the quality letter (−20°C Charpy). NH after the letter, as in Q420qDNH, marks weathering steel.
Does steel grade affect fatigue life of a Q420qF bridge girder?
Very little. Fatigue life of welded bridge details is governed by the detail category and stress range, not by yield strength. Higher-strength plate raises working stress, so detailing and weld quality must improve to keep the same fatigue life.

Conclusion

Q420qF to GB/T 714-2025 is bridge plate with 420 MPa minimum yield, 540 MPa minimum tensile and 47 J Charpy at −60°C for 12–100 mm plate.

It sits between Q390q and Q460qF in the bridge range, with Q420qD and Q420qE as sister letters. Choose the letter from the lowest service or erection temperature, here −60°C, and step up a letter for thick, restrained or fracture-critical members.

Every Q420qF plate from SHH STEEL ships with heat analysis, the weldability index, tensile and Charpy results on an EN 10204 3.1 or 3.2 certificate. Product analysis, Z15–Z35, extra UT and cut-to-size are options.

We ship from Shanghai to bridge builders worldwide. Browse the full GB/T 714 range or other high strength low alloy plates.

Ready to order? Send the drawing or cutting list, the certificate type and the destination port. Contact SHH STEEL for a mill-direct quotation on Q420qF bridge steel plate.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X