Product Showcase
GB/T 714 Carbon Steel Plates
SHH STEEL offers GB/T 714-compliant Q345qD/Q460qD structural steel plates. GB/T 714 specifies high-strength low-alloy steels for welded structures in bridges and heavy engineering. Tough, weldable, certified quality, competitive prices, customizable. Trust SHH STEEL!
-
GB/T 714 Q370qNHD Weathering Bridge Steel Supplier
GB/T 714 Q370qNHD (Q370qDNH) is weathering bridge steel plate with 370 MPa minimum yield, 120 J Charpy at −20°C (12–100 mm), Cu-Cr-Ni chemistry and a weathering index I ≥6.0 for unpainted bridges. SHH STEEL supplies it mill-direct with Z15–Z35, UT and full heat and product analysis.View More -
GB/T 714 Q345qNHF Weathering Bridge Steel Supplier
Q345qNHF (standard notation Q345qFNH) is a GB/T 714-2015 weathering bridge steel with 345 MPa yield and −60°C Charpy. GB/T 714-2025 lists this level in C, D and E only, so SHH STEEL supplies it to the 2015 edition or as Q345qENH with an agreed −60°C test, mill-direct.View More -
GB/T 714 Q345qNHE Weathering Bridge Steel Supplier
GB/T 714 Q345qNHE (Q345qENH) is weathering bridge steel plate with 345 MPa minimum yield, 120 J Charpy at −40°C (12–100 mm), Cu-Cr-Ni chemistry and a weathering index I ≥6.0 for unpainted bridges. SHH STEEL supplies it mill-direct with Z15–Z35, UT and full heat and product analysis.View More -
GB/T 714 Q345qNHD Weathering Bridge Steel Supplier
GB/T 714 Q345qNHD (Q345qDNH) is weathering bridge steel plate with 345 MPa minimum yield, 120 J Charpy at −20°C (12–100 mm), Cu-Cr-Ni chemistry and a weathering index I ≥6.0 for unpainted bridges. SHH STEEL supplies it mill-direct with Z15–Z35, UT and full heat and product analysis.View More -
GB/T 714 Q690qF Bridge Steel Plate Supplier
GB/T 714 Q690qF is bridge structural steel plate with 690 MPa minimum yield, 770 MPa minimum tensile and Charpy V-notch impact of 77 J at −60°C for 12–100 mm plate. SHH STEEL supplies Q690qF mill-direct, TMCP / TMCP+T / QT, up to 100 mm, with Z15–Z35, UT and heat and product analysis.View More -
GB/T 714 Q690qE Bridge Steel Plate Supplier
GB/T 714 Q690qE is bridge structural steel plate with 690 MPa minimum yield, 770 MPa minimum tensile and Charpy V-notch impact of 120 J at −40°C for 12–100 mm plate. SHH STEEL supplies Q690qE mill-direct, TMCP / TMCP+T / QT, up to 100 mm, with Z15–Z35, UT and heat and product analysis.View More -
GB/T 714 Q690qD Bridge Steel Plate Supplier
GB/T 714 Q690qD is bridge structural steel plate with 690 MPa minimum yield, 770 MPa minimum tensile and Charpy V-notch impact of 120 J at −20°C for 12–100 mm plate. SHH STEEL supplies Q690qD mill-direct, TMCP / TMCP+T / QT, up to 100 mm, with Z15–Z35, UT and heat and product analysis.View More -
GB/T 714 Q620qF Bridge Steel Plate Supplier
GB/T 714 Q620qF is bridge structural steel plate with 620 MPa minimum yield, 720 MPa minimum tensile and Charpy V-notch impact of 69 J at −60°C for 12–100 mm plate. SHH STEEL supplies Q620qF mill-direct, TMCP / TMCP+T / QT, up to 100 mm, with Z15–Z35, UT and heat and product analysis.View More -
GB/T 714 Q620qE Bridge Steel Plate Supplier
GB/T 714 Q620qE is bridge structural steel plate with 620 MPa minimum yield, 720 MPa minimum tensile and Charpy V-notch impact of 120 J at −40°C for 12–100 mm plate. SHH STEEL supplies Q620qE mill-direct, TMCP / TMCP+T / QT, up to 100 mm, with Z15–Z35, UT and heat and product analysis.View More -
GB/T 714 Q620qD Bridge Steel Plate Supplier
GB/T 714 Q620qD is bridge structural steel plate with 620 MPa minimum yield, 720 MPa minimum tensile and Charpy V-notch impact of 120 J at −20°C for 12–100 mm plate. SHH STEEL supplies Q620qD mill-direct, TMCP / TMCP+T / QT, up to 100 mm, with Z15–Z35, UT and heat and product analysis.View More -
GB/T 714 Q550qF Bridge Steel Plate Supplier
GB/T 714 Q550qF is bridge structural steel plate with 550 MPa minimum yield, 660 MPa minimum tensile and Charpy V-notch impact of 60 J at −60°C for 12–100 mm plate. SHH STEEL supplies Q550qF mill-direct, TMCP / TMCP+T / QT, up to 100 mm, with Z15–Z35, UT and heat and product analysis.View More -
GB/T 714 Q550qE Bridge Steel Plate Supplier
GB/T 714 Q550qE is bridge structural steel plate with 550 MPa minimum yield, 660 MPa minimum tensile and Charpy V-notch impact of 120 J at −40°C for 12–100 mm plate. SHH STEEL supplies Q550qE mill-direct, TMCP / TMCP+T / QT, up to 100 mm, with Z15–Z35, UT and heat and product analysis.View More
GB/T 714 Carbon Steel Plates
High-Strength Low Alloy Plates
SHH STEEL, a leading High-Strength Low Alloy Plates exporter, produces and exports HSLA steel plates for construction, bridges, and automotive applications. Our plates, like ASTM A572 Grade 50, offer superior strength-to-weight ratios and excellent weldability, meeting global standards. With a 5,000-ton inventory, we ensure 3–5 day delivery for in-stock items, supported by SGS/TUV inspections and mill certificates. Trust SHH STEEL for durable high-strength low alloy plates and custom solutions for structural projects.
High-Strength Low Alloy Plates
X