Product Showcase
EN 10149-2 Carbon Steel Plates
SHH STEEL offers EN 10149-2-compliant S355MC high-yield thermomechanical rolled steel plates. EN 10149-2 specifies hot-rolled flat products for cold forming in automotive and machinery structures. High ductility, certified quality, competitive prices, customizable. Trust SHH STEEL!
-
EN 10149-2 S960MC Steel Sheet and Plate
EN 10149-2 S960MC is a thermomechanically rolled high yield strength steel flat product for cold forming. It is the highest-strength grade in EN 10149-2:2013. Table 2 gives a minimum yield strength of 960 MPa and a tensile range of 980–1250 MPa. The grade applies from 2 mm to 10 mm. Delivery is thermomechanically rolled, not normalized. Heating above 400 °C is not recommended unless properties after heating are agreed. SHH STEEL produces and exports this sheet and plate to the ordered thickness, tests and documentation.View More -
EN 10149-2 S900MC Steel Sheet and Plate
EN 10149-2 S900MC is a thermomechanically rolled high yield strength steel flat product for cold forming. It is one of eleven grades in EN 10149-2:2013. Table 2 gives a minimum yield strength of 900 MPa and a tensile range of 930–1200 MPa. The grade applies from 2 mm to 10 mm. Delivery is thermomechanically rolled, not normalized. Heating above 400 °C is not recommended unless properties after heating are agreed. SHH STEEL produces and exports this sheet and plate to the ordered thickness and documentation.View More -
EN 10149-2 S700MC Steel Sheet and Plate
EN 10149-2 S700MC is a thermomechanically rolled high yield strength steel flat product for cold forming. It is one of eleven grades in EN 10149-2:2013. Table 2 gives a minimum yield strength of 700 MPa and a tensile range of 750–950 MPa. Over 8 mm that yield can be 20 MPa lower. The grade applies from 1.5 mm to 16 mm. Delivery is thermomechanically rolled, not normalized. SHH STEEL produces and exports EN 10149-2 S700MC sheet and plate to the ordered thickness, tests and documentation.View More -
EN 10149-2 S650MC Steel Sheet and Plate
EN 10149-2 S650MC is a thermomechanically rolled high yield strength steel flat product for cold forming. It is one of eleven grades in EN 10149-2:2013. Table 2 gives a minimum yield strength of 650 MPa and a tensile range of 700–880 MPa. Over 8 mm that yield can be 20 MPa lower. The grade applies from 1.5 mm to 16 mm. Delivery is thermomechanically rolled, not normalized. SHH STEEL produces and exports this sheet and plate to the ordered thickness, tests and documentation.View More -
EN 10149-2 S600MC Steel Sheet and Plate
EN 10149-2 S600MC is a thermomechanically rolled high yield strength steel flat product for cold forming. It is one of eleven grades in EN 10149-2:2013 and an alloy special steel under EN 10020. Table 2 gives a minimum yield strength of 600 MPa and a tensile range of 650–820 MPa. The grade applies from 1.5 mm to 16 mm. Delivery is thermomechanically rolled, not normalized. SHH STEEL produces and exports EN 10149-2 S600MC sheet and plate to the ordered thickness, tests and documentation.View More -
EN 10149-2 S550MC Steel Sheet and Plate
EN 10149-2 S550MC is a thermomechanically rolled high yield strength steel flat product for cold forming. It is one of eleven grades in EN 10149-2:2013. Table 2 gives a minimum yield strength of 550 MPa and a tensile range of 600–760 MPa. The grade applies from 1.5 mm to 16 mm. Delivery is thermomechanically rolled, not normalized. These products are not suitable for hot forming. SHH STEEL produces and exports this sheet and plate to the ordered thickness, tests and documentation.View More -
EN 10149-2 S500MC Steel Sheet and Plate
EN 10149-2 S500MC is a thermomechanically rolled high yield strength steel flat product for cold forming. It is one of eleven grades in EN 10149-2:2013. Table 2 gives a minimum yield strength of 500 MPa and a tensile range of 550–700 MPa. The grade applies from 1.5 mm to 16 mm. Delivery is thermomechanically rolled, not normalized. These products are not suitable for hot forming. SHH STEEL produces and exports EN 10149-2 S500MC sheet and plate to the ordered thickness, tests and documentation.View More -
EN 10149-2 S460MC Steel Sheet and Plate
EN 10149-2 S460MC is a thermomechanically rolled high yield strength steel flat product for cold forming. It is one of eleven grades in EN 10149-2:2013. Table 2 gives a minimum yield strength of 460 MPa and a tensile range of 520–670 MPa. The grade applies from 1.5 mm to 20 mm. Delivery is thermomechanically rolled, not normalized. These products are not suitable for hot forming. SHH STEEL produces and exports this sheet and plate to the ordered thickness, tests and documentation.View More -
EN 10149-2 S420MC Steel Sheet and Plate
EN 10149-2 S420MC is a thermomechanically rolled high yield strength steel flat product for cold forming. It is one of eleven grades in EN 10149-2:2013. Table 2 gives a minimum yield strength of 420 MPa and a tensile range of 480–620 MPa. The grade applies from 1.5 mm to 20 mm. Delivery is thermomechanically rolled, not normalized. These products are not suitable for hot forming. SHH STEEL produces and exports EN 10149-2 S420MC sheet and plate to the ordered thickness, tests and documentation.View More -
EN 10149-2 S355MC Steel Sheet and Plate
EN 10149-2 S355MC is a thermomechanically rolled high yield strength steel flat product for cold forming. It is one of eleven grades in EN 10149-2:2013. Table 2 gives a minimum yield strength of 355 MPa and a tensile range of 430–550 MPa. The grade applies from 1.5 mm to 20 mm. Delivery is thermomechanically rolled, not normalized. These products are not suitable for hot forming. SHH STEEL produces and exports this sheet and plate to the ordered thickness, tests and documentation.View More -
EN 10149-2 S315MC Steel Sheet and Plate
EN 10149-2 S315MC is a thermomechanically rolled high yield strength steel flat product for cold forming. It is one of eleven grades in EN 10149-2:2013. Table 2 gives a minimum yield strength of 315 MPa and a tensile range of 390–510 MPa. The grade applies from 1.5 mm to 20 mm. Delivery is thermomechanically rolled, not normalized. These products are not suitable for hot forming. SHH STEEL produces and exports EN 10149-2 S315MC sheet and plate to the ordered thickness, tests and documentation.View More
EN 10149-2 Carbon Steel Plates
High-Strength Low Alloy Plates
SHH STEEL, a leading High-Strength Low Alloy Plates exporter, produces and exports HSLA steel plates for construction, bridges, and automotive applications. Our plates, like ASTM A572 Grade 50, offer superior strength-to-weight ratios and excellent weldability, meeting global standards. With a 5,000-ton inventory, we ensure 3–5 day delivery for in-stock items, supported by SGS/TUV inspections and mill certificates. Trust SHH STEEL for durable high-strength low alloy plates and custom solutions for structural projects.