GB/T 714 Q460qNHD Weathering Bridge Steel Supplier
What is GB/T 714 Q460qNHD Weathering Bridge Steel?
Q460qNHD is weathering bridge structural steel to GB/T 714. In the standard’s own notation it is written Q460qDNH: Q for yield, 460 for the minimum yield in MPa, q for qiao (bridge), the quality letter, and NH for nai hou, weathering. The letter D means Charpy V-notch testing at −20°C.
Q460qNH is high-strength weathering plate for unpainted main girders and truss chords. Q460qNH is the weathering grade closest to ASTM A709 HPS 70W, which Annex B of GB/T 714-2025 also maps to Q460q. Pcm is capped at 0.23% to 50 mm and 0.25% to 100 mm.
Q460qNHD (Q460qDNH) gives 460 MPa yield, −20°C Charpy and weathering chemistry. It is the closest Chinese grade to ASTM A709 HPS 70W for unpainted girders.
GB/T 714-2025, in force since 1 May 2026, fully replaces GB/T 714-2015; the changes for weathering grades are listed below.
SHH STEEL (Shanghai Shenghonghe Import & Export Co., Ltd.) is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. We ship Q460qNHD cut to size with an EN 10204 3.1 or 3.2 certificate. Sister grades are listed under GB/T 714; other unpainted options are under weathering steel plates and EN 10025-5.
Material Specification
| Specification element | Requirement | SHH STEEL compliance |
|---|---|---|
| Standard | GB/T 714-2025 Q460qDNH | Confirmed |
| Product | Single-rolled plate ≤150 mm; hot-rolled strip and cut plate ≤25.4 mm | Plate |
| Thickness with tensile values | Up to 130 mm for Q460qNH | Confirmed |
| Minimum yield ReL | 460 MPa ≤50 mm; 450 MPa >50–100 mm | Confirmed |
| Minimum tensile Rm | 570 MPa ≤100 mm (no upper limit in the standard) | Confirmed |
| Elongation A | ≥ 18% | Confirmed |
| Charpy V-notch | −20°C, 120 J (12–100 mm), longitudinal | Confirmed |
| Weathering index | I ≥ 6.0 (Table 5, footnote c) | Calculated on MTC |
| Delivery condition | TMCP or TMCP + tempering | As ordered |
| Weldability index | Pcm (Table 8) | Printed on MTC |
| Ultrasonic testing | Plate >20 mm: GB/T 2970, Class II or better | Every plate |
| Through-thickness | Z15, Z25 or Z35 to GB/T 5313, when ordered | As ordered |
| Dimensions | GB/T 709 | Confirmed |
| Certificate | GB/T 247; EN 10204 3.1 or 3.2 | As ordered |
Grades often compared with Q460qNHD are ASTM A709 HPS 70W and EN 10025-4 S460ML; the comparison below shows where they differ.
Chemical Composition: Heat Analysis and Product Analysis
For Q460qNHD we report heat analysis on every certificate and add a product analysis when the buyer asks for it. The two use different limits: heat values follow GB/T 714, product values add the GB/T 222 deviations.
Table 1 below is the heat (ladle) analysis for Q460qNHD from GB/T 714-2025 Tables 1, 5.
| Element | Q460qNHD heat analysis (%) | Note |
|---|---|---|
| C, max | 0.11 | |
| Si | 0.15 – 0.50 | Counts in I |
| Mn | 1.10 – 1.50 | Min 0.50% for coil only |
| P, max | 0.025 | Letter D |
| S, max | 0.015 | Letter D |
| Cu | 0.25 – 0.50 | Main weathering element |
| Cr | 0.40 – 0.70 | Weathering element |
| Ni | 0.30 – 0.40 | Weathering element |
| Mo, max | 0.20 | |
| Nb | 0.010 – 0.100 | Microalloy (see note) |
| V | 0.010 – 0.100 | Microalloy (see note) |
| Ti | 0.006 – 0.030 | Microalloy (see note) |
| Als | 0.015 – 0.050 | Alt 0.020–0.055% if total Al is used |
| N, max | 0.0080 | |
| B, max (residual) | 0.0005 | ≤0.0014% if C ≤0.06% |
| H, max (residual) | 0.0002 | |
| Weathering index I | ≥ 6.0 | Calculated from heat analysis |
Nb, V, Ti and Al may be added singly or together. Added singly, each must meet the range above; added together, at least one must reach its minimum and Nb + V + Ti ≤ 0.22%. Calcium treatment is required to control sulfide shape.
Table 2 is the product analysis: the limits a check analysis on finished plate is judged against. GB/T 714-2025 clause 7.1.3 calls up GB/T 222 for the permitted deviations.
| Element | Heat limit (%) | Deviation, GB/T 222-2025 Table 1 | Q460qNHD product analysis (%) |
|---|---|---|---|
| C | ≤ 0.11 | +0.02 | ≤ 0.13 |
| Si | 0.15 – 0.50 | ±0.05 | 0.10 – 0.55 |
| Mn | 1.10 – 1.50 | ±0.06 | 1.04 – 1.56 |
| P | ≤ 0.025 | +0.005 | ≤ 0.030 |
| S | ≤ 0.015 | +0.005 | ≤ 0.020 |
| V | 0.010 – 0.100 | +0.02 / −0.01 | ≤ 0.120 |
| Ti | 0.006 – 0.030 | +0.02 / −0.01 | ≤ 0.050 |
| Nb | 0.010 – 0.100 | ±0.005 (listed for 0.015–0.060%) | Above 0.060%: agree in contract |
| Cu | 0.25 – 0.50 | ±0.05 | 0.20 – 0.55 |
| Cr | 0.40 – 0.70 | ±0.05 | 0.35 – 0.75 |
| Ni | 0.30 – 0.40 | ±0.05 | 0.25 – 0.45 |
| Als | 0.015 – 0.050 | ±0.003 | Lower limit −0.003 (Table 1 row is for Al ≥0.015%; confirm) |
| Mo | ≤ 0.20 | Not listed in Table 1 | Agree in contract |
| N | ≤ 0.0080 | Listed only for 0.010–0.020% | Agree in contract |
How to read Table 2. Weathering bridge steel is normally classed as low-alloy steel, so Table 1 of GB/T 222 applies. Where the heat limit is a range, the deviation applies to both ends; for one heat, an element may deviate in one direction only.
Mechanical Properties
Tensile values follow Table 9 of GB/T 714-2025 for Q460qNH. Tensile specimens are transverse; round specimens are used above 40 mm. Where yield is not distinct, Rp0.2 replaces ReL.
| Nominal thickness | ReL min (MPa) | Rm min (MPa) | A min |
|---|---|---|---|
| ≤ 50 mm | 460 | 570 | 18% |
| > 50 – 100 mm | 450 | 570 | 18% |
| > 100 – 130 mm | 385 | 490 | 18% |
Impact values follow Table 10, on longitudinal specimens, average of three:
| Letter / test temperature | KV2 ≤12 mm | KV2 >12 – 100 mm | KV2 >100 – 150 mm |
|---|---|---|---|
| D / −20°C | 80 J | 120 J | 47 J |
One single value may fall below the required average, but not below 70% of it. Plate over 8 mm and under 12 mm is tested with 7.5 mm specimens (75% of the value); 6–8 mm plate with 5 mm specimens (50%). Plate under 6 mm is not impact tested.
180° bend test, transverse: mandrel D = 2a up to 16 mm and 3a above 16 mm; may be omitted when the mill guarantees it. Yield ratio is not mandatory. If the contract asks for it, Annex C recommends ReL/Rm ≤ 0.88 up to 12 mm and ≤ 0.86 above 12 mm for TMCP plate.
Q460qNHD / Q460qNHE / Q460qNHF: Which Quality Grade?
Q460qNHD is tested at −20°C. It suits most highway and railway bridges in central and northern China, Europe and North America, where winter lows reach about −20°C. D is the most specified letter on Chinese bridge drawings. It is tested at −20°C and the melt is tighter than C: P ≤0.025%, S ≤0.015%.
| Grade | Test temp. | KV2 ≤12 mm | KV2 12–100 mm | KV2 >100 mm | P / S max (%) |
|---|---|---|---|---|---|
| Q460qNHD | −20°C | 80 J | 120 J | 47 J | 0.025 / 0.015 |
| Q460qNHE | −40°C | 80 J | 120 J | 31 J | 0.020 / 0.010 |
| Q460qNHF | −60°C | By agreement | 47 J | — | 0.015 / 0.006 |
Over-specifying the letter costs money; under-specifying it costs safety. Choose from the lowest service or erection temperature, then step up one letter for thick, restrained or fracture-critical members.
Q460qNHD: What Changed from GB/T 714-2015 to GB/T 714-2025
For Q460qNHD buyers the 2025 edition changes more than the year on the certificate. The points below come from the foreword of GB/T 714-2025 and its tables.
- The weathering requirement changed: Table 5 now requires a corrosion index I ≥ 6.0, and the 2015 Annex C guide for assessing weathering resistance was deleted.
- A Pcm table for weathering steel (Table 8) was added.
- Annex A now gives reference bridge-site environments for unpainted use (chloride, SO₂ and time-of-wetness limits).
- Yield values above 100 mm were added for Q460qNH (385 MPa for >100–130 mm).
- Tensile strength is now banded by thickness (e.g. lower minimum Rm above 100 mm) instead of one value.
- Impact energy is set by thickness band (≤12 mm, 12–100 mm, >100 mm) in Table 10.
- Yield ratio is no longer a clause value; it is agreed in the contract, with recommendations in informative Annex C.
If a drawing cites 2015 and the plate is made to 2025, get the designer’s written acceptance; tensile strength above 100 mm and the yield-ratio basis differ.
Q460qNHD vs ASTM A709 and EN 10025: Which Grade Matches?
Can Q460qNHD replace a US or European bridge grade, or the other way round? Strength can match; toughness rules differ in kind, not only in number.
| Property | Q460qNHD | ASTM A709 HPS 70W | EN 10025-4 S460ML |
|---|---|---|---|
| Min. yield (MPa) | 460 (≤50 mm) | 485 | 460 (≤16 mm) |
| Tensile (MPa) | 570 min | 585 – 760 | 540 – 720 |
| Charpy | 120 J at −20°C (12–100 mm) | CVN by temperature zone; fracture-critical (F) levels | 27 J at −50°C |
| Weathering chemistry | Yes, I ≥ 6.0 | Yes | No |
ASTM A709 sets Charpy requirements by temperature zone (1, 2, 3) and by member type: non-fracture-critical (T) or fracture-critical (F). GB/T 714 sets one value per letter, so compare the A709 zone with the GB/T 714 test temperature, not grade with grade.
EN 10025-5 weathering grades are general structural steels without a bridge-specific toughness level of 120 J; they suit many bridges but are not a one-to-one match.
The 120 J requirement for 12–100 mm plate is several times the 27–40 J typical of general weathering grades such as ASTM A588 or Corten A/B plate, which is why bridge owners specify Q460qNHD.
Q460qNHD Atmospheric Corrosion Index I and Unpainted Bridges
GB/T 714-2025 Table 5, footnote c, requires every Q460qNHD heat to reach an atmospheric corrosion index I of at least 6.0, calculated from the heat analysis:
I = 26.01(%Cu) + 3.88(%Ni) + 1.20(%Cr) + 1.49(%Si) + 17.28(%P) − 7.29(%Cu)(%Ni) − 9.10(%Ni)(%P) − 33.39(%Cu)²
This is the same predictive formula used with ASTM G101 for ASTM A709 Grade 50W and ASTM A709 HPS 70W, which makes Chinese and US ASTM A709 weathering steel plates easy to compare with Q460qNHD.
| Worked example (our calculation) | Cu | Ni | Cr | Si | P | I |
|---|---|---|---|---|---|---|
| All weathering elements at their Table 5 minimum | 0.25 | 0.30 | 0.40 | 0.15 | 0.010 | 5.88 |
| Illustrative mid-range heat | 0.32 | 0.36 | 0.55 | 0.30 | 0.012 | 6.74 |
Note the first row: a heat that only just meets every Table 5 minimum can still fall short of I = 6.0. That is why we ask the mill to print I on every Q460qNHD certificate, not just the chemistry.
Where can the steel be left unpainted? Annex A of GB/T 714-2025 gives reference bridge-site conditions:
- Rural or urban atmosphere with annual chloride deposition ≤ 3 mg/(m²·d)
- Annual SO₂ deposition ≤ 24 mg/(m²·d)
- Time of wetness ≤ 5,256 h per year (temperature above 0°C and relative humidity above 80%)
- Coastal sites only if they meet the same limits; for marine atmospheres Annex D points to T/CISA 073
Weathering steel is not stainless. Q460qNHD corrodes slowly once a stable patina forms, which takes a few years of wet-dry cycles. Designers usually add a corrosion allowance and design drainage so no surface stays wet.
Welding Q460qNHD and Fatigue in Bridge Girders
GB/T 714-2025 clause 7.1.2 uses CEV for normalized, QT and TMCP steel with C >0.12%, and Pcm for weathering steel and TMCP steel with C ≤0.12%, both from the heat analysis:
CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15
Pcm = C + Si/30 + Mn/20 + Cu/20 + Ni/60 + Cr/20 + Mo/15 + V/10 + 5B
| Index | ≤50 mm | >50–100 mm | >100–130 mm |
|---|---|---|---|
| Pcm, Q460qNH (Table 8) | ≤ 0.23 | ≤ 0.25 | By agreement |
We send the actual heat analysis of Q460qNHD before shipment, so the fabricator can check preheat and interpass limits against the procedure qualification record. At −20°C, most procedures qualified on TMCP plate pass HAZ impact without special measures; keep multi-wire SAW heat input inside the qualified band.
Typical consumables for Q460qNHD: weathering-matched Ni-Cu consumables (AWS E8018-W2 type for 345–420 MPa), with higher-strength weathering wires for 460–500 MPa.
Fatigue. Welded details govern fatigue life in a bridge, and their fatigue strength is set by detail category, not by yield strength. Higher-strength plate can carry higher stress ranges only if detailing improves too.
Fatigue design follows JTG D64 (highway) and TB 10091 (railway) in China, EN 1993-1-9 in Europe and AASHTO LRFD in the US; fabrication commonly follows TB 10212, JTG/T 3650 or AWS D1.5.
Q460qDNHZ15, Z25 and Z35: Through-Thickness Plate for Bridges
Z15, Z25 and Z35 tell the mill how much through-thickness ductility a plate must prove. The higher the number, the lower the sulfur and the higher the cost.
GB/T 714 adds the Z level to the end of the designation, for example Q460qDNHZ25. The test and acceptance follow GB/T 5313 and apply to plate 15 mm and thicker.
| Z grade | Heat sulfur, max (%) | Reduction of area, avg / single (%) |
|---|---|---|
| Z15 | 0.010 | 15 / 10 |
| Z25 | 0.007 | 25 / 15 |
| Z35 | 0.005 | 35 / 25 |
D chemistry allows S up to 0.015%. Z15 needs S ≤0.010% and Z25 needs ≤0.007%, so Z plate is still made from a dedicated low-sulfur heat.
Ask your designer which Q460qNHD plates are loaded through the thickness. Ordering Z35 on everything costs money and time without adding safety. Z options apply across the GB/T 714 bridge steel range.
Equivalent Material Grades
Annex B of GB/T 714-2025 lists foreign grades against each strength level. It is informative: it tells you which families are close, not that the plates are interchangeable.
| Standard | Grade(s) | Fit for Q460qNHD |
|---|---|---|
| ASTM A709 | ASTM A709 HPS 70W | Listed against Q460q in Annex B |
| EN 10025-4 | EN 10025-4 S460ML | Strength match, not weathering |
| EN 10025-6 | EN 10025-6 S460QL | QT, not weathering |
| GB/T 714 (painted twin) | Q460qD | Same strength, no weathering elements |
For weathering grades also compare the corrosion index basis. Q460qNHD requires I ≥ 6.0 by the formula above; check that the substitute is assessed on the same basis.
Q460qNHD Testing, UT and Certificate
A batch of Q460qNHD is one grade, one heat, one thickness, one rolling schedule and one heat-treatment condition, up to 60 t. Table 12 of GB/T 714-2025 sets the tests:
| Test | Frequency | Method |
|---|---|---|
| Heat analysis | 1 per heat | GB/T 20066; GB/T 4336 / GB/T 223 |
| Weathering index I | Calculated per heat | Table 5 formula |
| Tensile | 1 per batch | GB/T 2975 / GB/T 228.1 |
| Bend 180° | 1 per batch (may be waived if guaranteed) | GB/T 232 |
| Charpy V at −20°C | 3 specimens per batch | GB/T 229 |
| Through-thickness (Z) | 3 specimens per batch, when ordered | GB/T 5313 |
| Ultrasonic | Every plate >20 mm, Class II or better | GB/T 2970 |
| Surface and dimensions | Every plate | Visual and gauges |
Impact retest: if a set fails, three more specimens are taken from the same batch. The average of all six must meet the requirement; two values may be below it, but only one below 70%. At −20°C the 120 J level is comfortable for well-made TMCP plate, but we still check each batch value, not just the average.
Dimensions
Typical Q460qNHD dimensions on our offers:
- Thickness: 6 mm – 130 mm under GB/T 714 tensile tables; most orders 10 – 80 mm
- Width: 1500 – 4000 mm, depending on mill and thickness
- Length: 6000 – 18000 mm; longer by enquiry
- Edge: mill edge or cut edge
- Weight: theoretical, 7.85 g/cm³
Deck plate, webs, flanges, diaphragms and stiffeners are cut to drawing. For U-ribs and rolled sections on the same bridge, see steel beam profiles and steel structural profiles.
Tolerances
Thickness, width, length, flatness and camber of Q460qNHD follow GB/T 709. The table shows Class B thickness limits for common sizes.
| Nominal thickness (mm) | Width ≤ 1500 mm | Width > 1500 – 2500 mm |
|---|---|---|
| > 8 – 15 | −0.30 / +0.80 | −0.30 / +1.00 |
| > 15 – 25 | −0.30 / +1.00 | −0.30 / +1.20 |
| > 25 – 40 | −0.30 / +1.10 | −0.30 / +1.30 |
| > 40 – 60 | −0.30 / +1.30 | −0.30 / +1.50 |
| > 60 – 100 | −0.30 / +1.50 | −0.30 / +1.80 |
| > 100 – 150 | −0.30 / +2.10 | −0.30 / +2.50 |
Bridge fabricators often ask for Class C (zero minus) on deck and flange plate so section properties are never under the design value. Wider plates follow the heavier GB/T 709 rows; we state them on the offer.
Q460qNHD Price Factors and How to Order
When you compare Q460qNHD offers, compare extras line by line. These are the items that move the price.
| Cost driver | Effect on price |
|---|---|
| Strength level Q460q | Higher levels need more alloy and tighter rolling control |
| Quality letter | Small extra for −20°C testing and cleaner melt |
| Weathering alloys | Cu, Cr, Ni additions and I-index control add a weathering extra |
| Delivery route | TMCP / TMCP+T |
| Thickness | Over 60 mm and under 10 mm carry size extras |
| Z15 / Z25 / Z35 | Low-sulfur heat, Z test, UT; Z35 costs most |
| Width and length | Over 3000 mm wide or 15 m long needs mill confirmation |
| Quantity per size | Mill minimums per heat and size |
| Inspection and processing | 3.2 witness, profile cutting, blasting, priming quoted per item |
To get a firm quote in one round, send:
- Grade, edition and Z level, e.g. Q460qDNHZ25 to GB/T 714-2025
- Thickness × width × length and pieces or tonnes
- Delivery route and UT class if beyond Class II
- Certificate type and inspector
- Destination port and Incoterm
We quote plate price, extras and freight line by line. Need another letter? See Q460qNHE, Q460qNHF.
Applications
| Sector | Typical Q460qNHD components |
|---|---|
| Unpainted highway bridges | Plate girders and box girders in rural and urban atmospheres |
| Railway bridges | Truss members, plate girders, bracing |
| Remote and mountain sites | Bridges where repainting access is difficult or costly |
| Urban viaducts | Exposed girders with architectural rust finish |
| Pedestrian bridges | Unpainted box sections |
The letter D suits most highway and railway bridges in central and northern China, Europe and North America, where winter lows reach about −20°C.
Q460qNHD is the wrong plate for marine splash zones, tunnels, sites with heavy de-icing salt spray, or members that stay wet. There, use painted Q460qD or look at marine-atmosphere grades under T/CISA 073.
Supply Capability and Global Delivery
SHH STEEL sources Q460qNHD from first-line bridge-plate mills, including drafters of GB/T 714-2025 such as Ansteel, Valin Xiangtan, Jiangyin Xingcheng, Wuyang, Shougang and Xinyu.
- Certificates: EN 10204 3.1 standard; 3.2 with third-party witness (SGS, BV, TÜV or owner’s inspector)
- Tests: tensile, −20°C Charpy, bend, Z test, UT, product analysis, weathering index
- Processing: CNC plasma and flame cutting, bevelling, drilling, shot blasting and priming (or blasting only, for unpainted weathering steel)
- Terms: FOB Shanghai, CFR, CIF; TT, LC or TT + LC
- Marking: steel-stamped and paint-marked with grade, heat, size and mill, per GB/T 247
Q460qNHD leaves Shanghai for bridge projects designed to Chinese codes abroad, mainly through EPC contractors in Southeast Asia, Central Asia, the Middle East and Africa.
Lead time: about 45–60 days from mill rolling; Z35, F letter or 3.2 inspection adds about 1–2 weeks. Sea time from Shanghai is about 7–12 days to Southeast Asia and 28–35 days to North Europe.
Why Choose SHH STEEL
Mill-direct, China origin: SHH STEEL is a steel manufacturer and exporter and global steel mill sourcing partner, and Q460qNHD is one of the bridge grades we handle regularly.
Before shipment we check four lines on every Q460qNHD certificate: yield and tensile for the actual thickness band, Charpy at −20°C, the Pcm and weathering index, and UT results. If one fails, the plate does not ship as Q460qNHD.
If your project was designed in HPS 70W, compare Q460qNHD line by line with us: strength, toughness zone and weathering index all need checking.
We also tell buyers when another grade fits better. Neighbouring levels are Q420qNHD and Q500qNHD. The painted counterpart is Q460qD. Browse more structural steel plates and high strength low alloy plates.
FAQ
-
What is Q460qNHD steel?
- Q460qNHD (Q460qDNH) is weathering bridge steel plate to GB/T 714-2025. It has 460 MPa minimum yield up to 50 mm, 570 MPa minimum tensile, Charpy impact of 120 J at −20°C for 12–100 mm plate, and Cu-Cr-Ni chemistry with a corrosion index I of at least 6.0 for unpainted bridges.
-
What is the difference between Q460qNHD and Q460qNHE?
- Strength and chemistry box are the same. Q460qNHD is Charpy tested at −20°C, Q460qNHE at −40°C, both needing 120 J for 12–100 mm plate. P/S caps are 0.025/0.015% for D and 0.020/0.010% for E. Choose by the lowest service or erection temperature.
-
Is Q460qNHD the same as Q460D?
- No. Q460D is general structural steel (GB/T 1591), while Q460qNHD is bridge steel to GB/T 714 with lower P and S, controlled weldability index, mandatory UT above 20 mm and 120 J impact for 12–100 mm plate. Bridge plate can replace general plate, not the reverse.
-
What is the ASTM or EN equivalent of Q460qNHD?
- Close grades for Q460qNHD: ASTM A709 HPS 70W (Annex B lists it against Q460q) / EN 10025-4 S460ML (not weathering). These are close families, not drop-in substitutes; compare yield at thickness, impact temperature and energy, and the weldability index before substituting.
-
Is GB/T 714-2015 still valid?
- No. GB/T 714-2025 was published on 31 October 2025 and took effect on 1 May 2026, fully replacing GB/T 714-2015. Contracts that still cite the 2015 edition can be certified to it, but new orders default to the 2025 edition.
-
What is the weathering index I in GB/T 714?
- It is a corrosion index calculated from the heat analysis: I = 26.01Cu + 3.88Ni + 1.20Cr + 1.49Si + 17.28P − 7.29Cu·Ni − 9.10Ni·P − 33.39Cu². GB/T 714-2025 requires I ≥6.0 for every weathering grade, the same basis ASTM G101 uses for A709 weathering steels.
Conclusion
Q460qNHD to GB/T 714 is weathering bridge steel with 460 MPa minimum yield, Cu-Cr-Ni chemistry, a weathering index of at least 6.0 and 120 J Charpy at −20°C for 12–100 mm plate.
It sits between Q420qNHD and Q500qNHD in the weathering range, with Q460qNHE and Q460qNHF as sister letters. The most common ordering mistake with Q460qNHD is leaving the Z level, UT class or impact position off the order; add them at enquiry stage, not after rolling.
With SHH STEEL the Q460qNHD certificate is complete: heat chemistry, weldability index, yield, tensile, elongation and Charpy, to EN 10204 3.1 or 3.2. Add product analysis, a Z level or a stricter UT class as needed.
We ship from Shanghai to bridge builders worldwide. Browse the full GB/T 714 range or other weathering steel plates.
Send your enquiry with grade, edition, sizes and inspection needs, and we will answer within one working day. Contact SHH STEEL for Q460qNHD weathering bridge steel.