GB/T 714 Q460qF Bridge Steel Plate | GB/T 714 Bridge Steel - SHH STEEL

GB/T 714 Q460qF Bridge Steel Plate Supplier

GB/T 714 Q460qF is bridge structural steel plate with 460 MPa minimum yield, 570 MPa minimum tensile and Charpy V-notch impact of 47 J at −60°C for 12–100 mm plate. SHH STEEL supplies Q460qF mill-direct, TMCP / TMCP+T, up to 130 mm, with Z15–Z35, UT and heat and product analysis.
Keywords
Q460qF, Q460qF steel plate, GB/T 714 Q460qF, Q460q-F, Q460q F, Q460qF bridge steel, Q460qFZ15, Q460qFZ25, Q460qFZ35, bridge steel plate, Q460qF supplier
Equivalent Grades:
ASTM A709 HPS 70W / EN 10025-4 S460M, S460ML / EN 10025-6 S460Q, S460QL, S460QL1 (Annex B) — Material Specification: GB/T 714-2025 (supersedes GB/T 714-2015) — Delivery: TMCP / TMCP+T
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Q460q Quality Grades
GB/T 714-2025 vs 2015
Q460qF vs ASTM A709 / EN 10025
TMCP vs Normalized vs QT
Welding and Fatigue
Z15 / Z25 / Z35
Equivalent Material Grades
Testing and Inspection
Dimensions
Tolerances
Price and Ordering
Applications
Supply Capability
Why Choose SHH STEEL
FAQ
Conclusion

What is GB/T 714 Q460qF Bridge Steel Plate?

Q460qF is bridge structural steel plate to GB/T 714. Q stands for yield, 460 is the minimum yield in MPa for plate up to 50 mm, q stands for qiao (bridge) and F is the quality grade: Charpy V-notch at −60°C on longitudinal specimens.

Q460q is high-strength TMCP plate for main load paths on long-span bridges, where 460 MPa yield cuts flange thickness and weld volume. Annex B of GB/T 714-2025 lists ASTM A709 HPS 70W against Q460q. In practice, Q460q is chosen where Q420q flanges would exceed about 50–60 mm and welding cost starts to dominate.

Q460qF combines 460 MPa yield with −60°C Charpy (47 J over 12 mm). It suits fracture-critical members on bridges in permafrost regions and very cold mountain passes.

GB/T 714-2025 has been in force since 1 May 2026, replacing GB/T 714-2015 in full. If your specification was written earlier, check the edition before ordering: some table values changed, and a few grades were added or dropped.

SHH STEEL (Shanghai Shenghonghe Import & Export Co., Ltd.) is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. We ship Q460qF cut to size with an EN 10204 3.1 or 3.2 certificate. Sister grades are listed under GB/T 714.

Material Specification

Specification element Requirement SHH STEEL compliance
Standard GB/T 714-2025 Q460qF Confirmed
Product Single-rolled plate ≤150 mm; hot-rolled strip and cut plate ≤25.4 mm Plate
Thickness with tensile values Up to 130 mm for Q460q Confirmed
Minimum yield ReL 460 MPa ≤50 mm; 450 MPa >50–100 mm Confirmed
Minimum tensile Rm 570 MPa ≤100 mm (no upper limit in the standard) Confirmed
Elongation A ≥ 18% Confirmed
Charpy V-notch −60°C, 47 J (12–100 mm), longitudinal Confirmed
Delivery condition TMCP or TMCP + tempering As ordered
Weldability index Pcm (Table 7) Printed on MTC
Ultrasonic testing Plate >20 mm: GB/T 2970, Class II or better Every plate
Through-thickness Z15, Z25 or Z35 to GB/T 5313, when ordered As ordered
Dimensions GB/T 709 Confirmed
Certificate GB/T 247; EN 10204 3.1 or 3.2 As ordered

Grades often compared with Q460qF are ASTM A709 HPS 70W, EN 10025-4 S460M and EN 10025-4 S460ML; the comparison below shows where they differ.

Chemical Composition: Heat Analysis and Product Analysis

A check analysis on finished plate often reads a few hundredths higher than the mill certificate. That is not automatically a failure. The certificate shows the heat (ladle) analysis; plate drilled after rolling is judged as product analysis, with the tolerances of GB/T 222.

Table 1 below is the heat (ladle) analysis for Q460qF from GB/T 714-2025 Tables 1, 3.

Element Q460qF TMCP (%)
C, max 0.11
Si, max 0.55
Mn 0.80 – 1.70
P, max 0.015
S, max 0.006
Nb 0.010 – 0.090
V 0.010 – 0.080
Ti 0.006 – 0.030
Als 0.010 – 0.045
Cr, max 0.50
Ni, max 0.30
Cu, max 0.30
Mo, max 0.25
N, max 0.0080
B, max 0.0005 residual (≤0.0014 if C ≤0.10%)
H, max 0.0002

Nb, V, Ti and Al may be added singly or together. Added singly, each must meet the range above; added together, at least one must reach its minimum and Nb + V + Ti ≤ 0.22%.

Table 2 is the product analysis: the limits a check analysis on finished plate is judged against. GB/T 714-2025 clause 7.1.3 calls up GB/T 222 for the permitted deviations.

Element Heat limit (%) Deviation, GB/T 222-2025 Table 1 Q460qF product analysis (%)
C ≤ 0.11 +0.02 ≤ 0.13
Si ≤ 0.55 +0.05 ≤ 0.60
Mn 0.80 – 1.70 ±0.06 0.74 – 1.76
P ≤ 0.015 +0.005 ≤ 0.020
S ≤ 0.006 +0.005 ≤ 0.011
V 0.010 – 0.080 +0.02 / −0.01 ≤ 0.100
Ti 0.006 – 0.030 +0.02 / −0.01 ≤ 0.050
Nb 0.010 – 0.090 ±0.005 (listed for 0.015–0.060%) Above 0.060%: agree in contract
Cr ≤ 0.50 +0.05 ≤ 0.55
Ni ≤ 0.30 +0.05 ≤ 0.35
Cu ≤ 0.30 +0.05 ≤ 0.35
Als 0.010 – 0.045 ±0.003 Lower limit −0.003 (Table 1 row is for Al ≥0.015%; confirm)
Mo ≤ 0.25 Not listed in Table 1 Agree in contract
N ≤ 0.0080 Listed only for 0.010–0.020% Agree in contract

How to read Table 2. Q460q TMCP heats are low-alloy steel, so Table 1 of GB/T 222 applies. Si ≤0.55% is above 0.37%, so +0.05% applies; Mn falls in the 0.80–1.70% band, so ±0.06%. For one heat, an element may deviate in one direction only.

Mechanical Properties

Tensile values follow Table 9 of GB/T 714-2025 for Q460q. Tensile specimens are transverse; round specimens are used above 40 mm. Where yield is not distinct, Rp0.2 replaces ReL.

Nominal thickness ReL min (MPa) Rm min (MPa) A min
≤ 50 mm 460 570 18%
> 50 – 100 mm 450 570 18%
> 100 – 130 mm 385 490 18%

Impact values follow Table 10, on longitudinal specimens, average of three:

Letter / test temperature KV2 ≤12 mm KV2 >12 – 100 mm KV2 >100 – 150 mm
F / −60°C By agreement 47 J Not applicable

One single value may fall below the required average, but not below 70% of it. Plate over 8 mm and under 12 mm is tested with 7.5 mm specimens (75% of the value); 6–8 mm plate with 5 mm specimens (50%). Plate under 6 mm is not impact tested.

180° bend test, transverse: mandrel D = 2a up to 16 mm and 3a above 16 mm; may be omitted when the mill guarantees it. Yield ratio is not mandatory. If the contract asks for it, Annex C recommends ReL/Rm ≤ 0.88 up to 12 mm and ≤ 0.86 above 12 mm for TMCP plate.

Q460qD / Q460qE / Q460qF: Which Quality Grade?

Q460qF is tested at −60°C. It suits Arctic and sub-Arctic bridges, high-latitude rail lines and owners who want the largest toughness margin for fracture-critical members. F is the coldest letter in GB/T 714: Charpy at −60°C, P ≤0.015% and S ≤0.006%. It exists only for Q420q and above (and their NH versions), and its energy rises with strength.

Grade Test temp. KV2 ≤12 mm KV2 12–100 mm KV2 >100 mm P / S max (%)
Q460qD −20°C 80 J 120 J 47 J 0.025 / 0.015
Q460qE −40°C 80 J 120 J 31 J 0.020 / 0.010
Q460qF −60°C By agreement 47 J — 0.015 / 0.006

Note that F energy at Q460q is 47 J, not 120 J: the colder test uses a lower energy that GB/T 714-2025 raises with strength, from 47 J at Q420q/Q460q to 77 J at Q690q. Plate up to 12 mm needs an agreed value.

Q460qF: What Changed from GB/T 714-2015 to GB/T 714-2025

For Q460qF buyers the 2025 edition changes more than the year on the certificate. The points below come from the foreword of GB/T 714-2025 and its tables.

  • Yield values above 100 mm were added (385 MPa for >100–130 mm).
  • The Mn range for TMCP steel was revised: the minimum is now 0.80%, and the maximum may be raised to 2.00% by agreement.
  • CEV and Pcm limits were revised (Tables 6 and 7).
  • Tensile strength is now banded by thickness (e.g. lower minimum Rm above 100 mm) instead of one value.
  • Impact energy is set by thickness band (≤12 mm, 12–100 mm, >100 mm) in Table 10.
  • Yield ratio is no longer a clause value; it is agreed in the contract, with recommendations in informative Annex C.
  • Section products were removed; the standard now covers plate and strip only.
  • Delivery is TMCP, TMCP + tempering or QT; normalizing is kept only for Q345q/Q370q plate over 100 mm by agreement.

If a drawing cites 2015 and the plate is made to 2025, get the designer’s written acceptance; tensile strength above 100 mm and the yield-ratio basis differ.

Q460qF vs ASTM A709 and EN 10025: Which Grade Matches?

Can Q460qF replace a US or European bridge grade, or the other way round? Strength can match; toughness rules differ in kind, not only in number.

Property Q460qF ASTM A709 HPS 70W EN 10025-4 S460M EN 10025-4 S460ML
Min. yield (MPa) 460 (≤50 mm) 485 460 (≤16 mm) 460 (≤16 mm)
Tensile (MPa) 570 min 585 – 760 540 – 720 540 – 720
Charpy 47 J at −60°C (12–100 mm) CVN by temperature zone; fracture-critical (F) levels 40 J at −20°C 27 J at −50°C
Weathering chemistry No Yes No No

ASTM A709 sets Charpy requirements by temperature zone (1, 2, 3) and by member type: non-fracture-critical (T) or fracture-critical (F). GB/T 714 sets one value per letter, so compare the A709 zone with the GB/T 714 test temperature, not grade with grade.

EN 10025-3/-4/-6 grades show yield at the thinnest band; their values fall with thickness. GB/T 714 keeps 460 MPa to 50 mm. EN tensile ranges have upper limits; GB/T 714 gives minimums only.

At −60°C, the 47 J required for Q460qF is a demanding figure; general structural grades rarely prove any toughness that cold. For the C, D and E letters GB/T 714 asks 120 J, several times the 27–40 J typical of GB/T 1591 plate.

Q460qF Delivery Condition: TMCP vs Normalized vs Quenched and Tempered

GB/T 714-2025 clause 3.2 defines TMCP as rolling with the final deformation in a controlled temperature range, including accelerated cooling with or without tempering (self-tempering included) but excluding direct quenching and quench-and-temper. The delivery route must be stated on the certificate.

Route Available for Q460qF Weldability index Notes
TMCP Yes, standard Pcm (C ≤0.11%) Up to 130 mm
TMCP + tempering Yes Same as TMCP Common on thick or E/F plate
Normalized No — Dropped in 2025 for this level
Quenched and tempered Not listed — Use GB/T 16270 if QT is required

Q460q is TMCP or TMCP + tempering. If a project insists on QT, GB/T 16270 Q460 grades are the alternative, with different toughness rules. F-letter plate is often TMCP + tempering or, at the top strength levels, QT; ask which route the mill has qualified for −60°C.

Ask for the route on the purchase order. It changes the weldability index, the welding procedure and, for heavy plate, the price of Q460qF.

Welding Q460qF and Fatigue in Bridge Girders

GB/T 714-2025 clause 7.1.2 uses CEV for normalized, QT and TMCP steel with C >0.12%, and Pcm for weathering steel and TMCP steel with C ≤0.12%, both from the heat analysis:

CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15

Pcm = C + Si/30 + Mn/20 + Cu/20 + Ni/60 + Cr/20 + Mo/15 + V/10 + 5B

Index ≤50 mm >50–100 mm >100–130 mm
Pcm, TMCP (Table 7) ≤ 0.22 ≤ 0.23 ≤ 0.23

We send the actual heat analysis of Q460qF before shipment, so the fabricator can check preheat and interpass limits against the procedure qualification record. At −60°C, both weld metal and HAZ must prove toughness. Expect lower heat input, more passes and consumables qualified at −60°C.

Typical consumables for Q460qF: E55/E62-class consumables (AWS E8018 / E9018 type).

Fatigue. Welded details govern fatigue life in a bridge, and their fatigue strength is set by detail category, not by yield strength. Higher-strength plate can carry higher stress ranges only if detailing improves too.

Fatigue design follows JTG D64 (highway) and TB 10091 (railway) in China, EN 1993-1-9 in Europe and AASHTO LRFD in the US; fabrication commonly follows TB 10212, JTG/T 3650 or AWS D1.5.

Q460qFZ15, Z25 and Z35: Through-Thickness Plate for Bridges

Through-thickness properties matter wherever a full-penetration weld sits on the face of a plate, such as diaphragm-to-flange joints and cable anchor plates.

GB/T 714 adds the Z level to the end of the designation, for example Q460qFZ25. The test and acceptance follow GB/T 5313 and apply to plate 15 mm and thicker.

Z grade Heat sulfur, max (%) Reduction of area, avg / single (%)
Z15 0.010 15 / 10
Z25 0.007 25 / 15
Z35 0.005 35 / 25

F chemistry limits S to 0.006%, which already meets the Z25 sulfur cap (0.007%). Only Z35 (S ≤0.005%) needs a further step.

Z plate for Q460qF should also get ultrasonic testing beyond the Class II minimum if the joint is critical. Write the UT class next to the Z level. Z options apply across the GB/T 714 bridge steel range.

Equivalent Material Grades

Annex B of GB/T 714-2025 lists foreign grades against each strength level. It is informative: it tells you which families are close, not that the plates are interchangeable.

Standard Grade(s) Fit for Q460qF
ASTM A709 ASTM A709 HPS 70W Listed in Annex B
EN 10025-4 EN 10025-4 S460M, EN 10025-4 S460ML Listed in Annex B
EN 10025-6 EN 10025-6 S460Q, EN 10025-6 S460QL, EN 10025-6 S460QL1 Listed in Annex B
GB/T 16270 GB/T 16270 Q460F QT alternative
GB/T 1591 GB/T 1591 Q460MF General structural
GB/T 714 (weathering twin) Q460qNHF Same strength, weathering chemistry

Before substituting, compare three things line by line: minimum yield at the actual thickness, the impact test temperature and energy, and the weldability index. For Q460qF, the 120 J impact level and the Pcm/CEV caps are usually the hardest to match.

Q460qF Testing, UT and Certificate

A batch of Q460qF is one grade, one heat, one thickness, one rolling schedule and one heat-treatment condition, up to 60 t. Table 12 of GB/T 714-2025 sets the tests:

Test Frequency Method
Heat analysis 1 per heat GB/T 20066; GB/T 4336 / GB/T 223
Tensile 1 per batch GB/T 2975 / GB/T 228.1
Bend 180° 1 per batch (may be waived if guaranteed) GB/T 232
Charpy V at −60°C 3 specimens per batch GB/T 229
Through-thickness (Z) 3 specimens per batch, when ordered GB/T 5313
Ultrasonic Every plate >20 mm, Class II or better GB/T 2970
Surface and dimensions Every plate Visual and gauges

Impact retest: if a set fails, three more specimens are taken from the same batch. The average of all six must meet the requirement; two values may be below it, but only one below 70%. At −60°C, mills may need trial heats before the production run; we agree the test plan before accepting the order.

Dimensions

Size range for Q460qF plate:

  • Thickness: 6 mm – 130 mm under GB/T 714 tensile tables; most orders 10 – 80 mm
  • Width: 1500 – 4000 mm, depending on mill and thickness
  • Length: 6000 – 18000 mm; longer by enquiry
  • Edge: mill edge or cut edge
  • Weight: theoretical, 7.85 g/cm³

Deck plate, webs, flanges, diaphragms and stiffeners are cut to drawing. For U-ribs and rolled sections on the same bridge, see steel beam profiles and steel structural profiles.

Tolerances

GB/T 714 does not set its own size tolerances; Q460qF follows GB/T 709. Other tolerance standards can be agreed in the contract (clause 7.6.2).

Nominal thickness (mm) Width ≤ 1500 mm Width > 1500 – 2500 mm
> 8 – 15 −0.30 / +0.80 −0.30 / +1.00
> 15 – 25 −0.30 / +1.00 −0.30 / +1.20
> 25 – 40 −0.30 / +1.10 −0.30 / +1.30
> 40 – 60 −0.30 / +1.30 −0.30 / +1.50
> 60 – 100 −0.30 / +1.50 −0.30 / +1.80
> 100 – 150 −0.30 / +2.10 −0.30 / +2.50

Bridge fabricators often ask for Class C (zero minus) on deck and flange plate so section properties are never under the design value. Wider plates follow the heavier GB/T 709 rows; we state them on the offer.

Q460qF Price Factors and How to Order

A Q460qF price per ton is a base price plus extras. The extras explain most gaps between quotes.

Cost driver Effect on price
Strength level Q460q Higher levels need more alloy and tighter rolling control
Quality letter Highest extra: −60°C testing, S ≤0.006%, limited mills
Delivery route TMCP / TMCP+T
Thickness Over 60 mm and under 10 mm carry size extras
Z15 / Z25 / Z35 Low-sulfur heat, Z test, UT; Z35 costs most
Width and length Over 3000 mm wide or 15 m long needs mill confirmation
Quantity per size Mill minimums per heat and size
Inspection and processing 3.2 witness, profile cutting, blasting, priming quoted per item

To get a firm quote in one round, send:

  • Grade, edition and Z level, e.g. Q460qFZ25 to GB/T 714-2025
  • Thickness × width × length and pieces or tonnes
  • Delivery route and UT class if beyond Class II
  • Certificate type and inspector
  • Destination port and Incoterm

We quote plate price, extras and freight line by line. Need another letter? See Q460qD, Q460qE.

Applications

Sector Typical Q460qF components
Long-span truss bridges Highly stressed chords and node plates
Cable-stayed bridges Pylon steel anchor boxes, main girder flanges
Suspension bridges Stiffening truss chords
Railway bridges Heavy-haul truss members
Arch bridges Arch rib plate

The letter F suits Arctic and sub-Arctic bridges, high-latitude rail lines and owners who want the largest toughness margin for fracture-critical members.

It is the wrong plate for pressure equipment (pressure vessel steel plates), unpainted exposure (weathering steel plates) or ship hulls (shipbuilding steel plates).

Supply Capability and Global Delivery

SHH STEEL sources Q460qF from first-line bridge-plate mills, including drafters of GB/T 714-2025 such as Ansteel, Valin Xiangtan, Jiangyin Xingcheng, Wuyang, Shougang and Xinyu.

  • Certificates: EN 10204 3.1 standard; 3.2 with third-party witness (SGS, BV, TÜV or owner’s inspector)
  • Tests: tensile, −60°C Charpy, bend, Z test, UT, product analysis
  • Processing: CNC plasma and flame cutting, bevelling, drilling, shot blasting and priming
  • Terms: FOB Shanghai, CFR, CIF; TT, LC or TT + LC
  • Marking: steel-stamped and paint-marked with grade, heat, size and mill, per GB/T 247

Q460qF leaves Shanghai for bridge projects designed to Chinese codes abroad, mainly through EPC contractors in Southeast Asia, Central Asia, the Middle East and Africa.

Lead time: about 45–60 days from mill rolling; Z35, F letter or 3.2 inspection adds about 1–2 weeks. Sea time from Shanghai is about 7–12 days to Southeast Asia and 28–35 days to North Europe.

Why Choose SHH STEEL

As a steel manufacturer and exporter and global steel mill sourcing partner, SHH STEEL buys Q460qF straight from GB/T 714 mills, China origin. No mixed heats, no relabelled plate.

Before shipment we check four lines on every Q460qF certificate: yield and tensile for the actual thickness band, Charpy at −60°C, the CEV or Pcm for the delivery route, and UT results. If one fails, the plate does not ship as Q460qF.

Q460qF is a mill campaign item. Plan at least one full rolling cycle and combine sizes to meet the mill minimum per heat.

We also tell buyers when another grade fits better. Neighbouring levels are Q420qF and Q500qF. The weathering counterpart is Q460qNHF. Browse more structural steel plates and high strength low alloy plates.

FAQ

What is Q460qF steel?
Q460qF is bridge structural steel plate to GB/T 714-2025. It has 460 MPa minimum yield up to 50 mm, 570 MPa minimum tensile, 18% elongation and Charpy V-notch impact of 47 J at −60°C for 12–100 mm plate. It is delivered TMCP or TMCP + tempering.
What impact energy does Q460qF need at −60°C?
GB/T 714-2025 requires at least 47 J at −60°C on longitudinal specimens for Q460qF plate over 12 mm and up to 100 mm. For plate 12 mm and thinner the value is by agreement. F energy rises with strength: 47 J for Q420q and Q460q, 54 J for Q500q, 60 J for Q550q, 69 J for Q620q and 77 J for Q690q.
What is the yield strength of Q460qF?
Q460qF has a minimum lower yield strength of 460 MPa up to 50 mm and 450 MPa from 50 to 100 mm, and 385 MPa from 100 to 130 mm (GB/T 714-2025 Table 9). Minimum tensile is 570 MPa up to 100 mm. There is no upper tensile limit in the standard.
What is the ASTM or EN equivalent of Q460qF?
Close grades for Q460qF: ASTM A709 HPS 70W / EN 10025-4 S460M, S460ML / EN 10025-6 S460Q, S460QL, S460QL1 (Annex B). These are close families, not drop-in substitutes; compare yield at thickness, impact temperature and energy, and the weldability index before substituting.
Does GB/T 714 require ultrasonic testing?
Yes. GB/T 714-2025 clause 7.5 requires every single-rolled plate over 20 mm to be ultrasonically tested to GB/T 2970, with acceptance Class II or better. Thinner plate is tested only by agreement.
Does steel grade affect fatigue life of a Q460qF bridge girder?
Very little. Fatigue life of welded bridge details is governed by the detail category and stress range, not by yield strength. Higher-strength plate raises working stress, so detailing and weld quality must improve to keep the same fatigue life.

Conclusion

Q460qF to GB/T 714-2025 is bridge plate with 460 MPa minimum yield, 570 MPa minimum tensile and 47 J Charpy at −60°C for 12–100 mm plate.

It sits between Q420qF and Q500qF in the bridge range, with Q460qD and Q460qE as sister letters. If the drawing still cites GB/T 714-2015, we can certify Q460qF to it, but we recommend confirming with the designer that the 2025 values are accepted.

From SHH STEEL, Q460qF arrives with traceable heat numbers, a complete EN 10204 3.1 or 3.2 certificate and, if ordered, third-party witness, product analysis and Z testing.

We ship from Shanghai to bridge builders worldwide. Browse the full GB/T 714 range or other high strength low alloy plates.

Contact SHH STEEL with your Q460qF requirements. We confirm the mill, delivery route, testing and price before you commit.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X