JIS G3463 SUS410TB Stainless Steel Tube | JIS G3463 Stainless Steel Tube - SHH STEEL

JIS G3463 SUS410TB Stainless Steel Tube

JIS G3463 SUS410TB stainless steel tube (410 / UNS S41000 class (tube as annealed ferritic practice)), ferritic, Table 3 cast analysis, Rm min 412 N/mm² / proof min 206 N/mm², annealed. SHH STEEL can produce and supply seamless or welded routes with mill certificates.
Grade
SUS410TB (410 / UNS S41000 class (tube as annealed ferritic practice) — body alias)
Standard
JIS G3463
Product form
Seamless and welded stainless steel boiler/HX tube, delivery annealed
Size
Typically OD 15.9–139.8 mm (Note 1); OD × wall (HX/boiler gauges) by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is JIS G3463 SUS410TB Stainless Steel Tube

JIS G3463 is the Japanese Industrial Standard for stainless steel tubes used in boiler and heat-exchanger service (superheater, HX, condenser, catalyser). Grade symbol SUS410TB sits in the ferritic set of Table 1. Order JIS G3463 SUS410TB only when annealed 12Cr HX properties are what the design file actually wants — not when someone meant 410 stainless bar hardness.

SHH STEEL can produce and supply JIS G3463 SUS410TB as seamless or welded tube across the enquiry OD×wall band, solution-annealed or annealed as Table 2 requires, pickled or bright-finished, and documented on mill test certificates tied to cast analysis and tensile results. Duty focus: 12Cr tube supplied annealed for mild HX duty in the 410 family.

Shop language may still say “410 tube,” yet that commercial alias does not select Japanese cast limits, process symbols, or hydraulic/NDT rules. The purchase order has to name JIS G3463 and SUS410TB so the mill applies the correct analysis, heat treatment, mechanical floors, and marking. Design caution: delivered annealed under G3463 heat-treatment practice — do not assume quenched-and-tempered martensitic properties.

Scope discipline: SUS410TB is HX tube product under JIS G3463, not a piping product under JIS G3459 and not an ASTM A213 order by default. Sister marks often compared on the same RFQ include SUS410TiTB, SUS405TB, SUS430TB, SUS409TB. Role reminder: 12Cr tube supplied annealed for mild HX duty in the 410 family.

Inside this JIS G3463 series, compare SUS410TiTB, SUS405TB, SUS430TB, SUS409TB. Hub: JIS G3463. ASTM/ASME related product pages (not interchangeable by default): ASTM A213.

Chemical Composition of JIS G3463 SUS410TB

Cast analysis for JIS G3463 SUS410TB follows Table 3. Key windows on a typical certificate include C ≤0.15, Si ≤1.00, Mn ≤1.00, P ≤0.040, S ≤0.030, Cr 11.50–13.50. SHH STEEL ties the heat number on the tube marking to the same cast line on the MTC. Commercial alias 410 / UNS S41000 class (tube as annealed ferritic practice) is body text only. Corrosion thread: 12Cr aqueous resistance is mild-service only; chlorides and weld HAZ need care.

Chemical limits for SUS410TB under JIS G3463 appear in the table underneath. Source priority is the 2021 Table 3 extract cross-checked to public Nikko / supplier tables. If your client specification cites a different edition footnote, send it before the heat is melted. Duty thread: 12Cr tube supplied annealed for mild HX duty in the 410 family.

Grade C Si Mn P S Cr
SUS410TB ≤0.15 ≤1.00 ≤1.00 ≤0.040 ≤0.030 11.50–13.50

Mechanical Properties of JIS G3463 SUS410TB

Ambient tensile floors for SUS410TB come from JIS G3463 Table 4: Rm min 412 N/mm², proof stress min 206 N/mm², elongation min 20% (OD ≥20 mm, No.11/12). These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: ferritic. Caution: delivered annealed under G3463 heat-treatment practice — do not assume quenched-and-tempered martensitic properties.

Grade Rm min (N/mm²) Proof stress min (N/mm²) A OD≥20 mm No.11/12 min (%) A 10≤OD<20 mm No.11 min (%) A OD<10 mm No.11 min (%)
SUS410TB 412 206 20 15 12

Ambient values from JIS G3463 Table 4 for SUS410TB. Heat treatment (Table 2): 700 °C min, air or slow cool. Elongation reductions apply for walls under 8 mm on No.12 pieces. For heat-exchanger tube the purchaser may designate an upper tensile limit (Table 4 min + 200 N/mm²) when necessary.

Manufacture of JIS G3463 SUS410TB Tube (Seamless and Welded)

For SUS410TB, the mill path is not “seamless only.” Table 1 explicitly pairs austenitic, duplex, and ferritic marks with seamless or A/L/E welded process symbols and S-H/S-C/A/A-C/E-C finishes. Order the combination that matches hydrostatic or NDT preference, not a habit from ASTM A213 alone. Seamless and welded options remain available for SUS410TB; the acknowledgement repeats the Table 1 symbols so production cannot silently change route after the PO is firm. Application context for SUS410TB stays mild water coolers, utility exchangers, and heat-adjacent ferritic bundles specified as 410 tube.

Ferritic heats are annealed (700 °C min, or 720 °C min for SUS430J1LTB) with rapid or slow cooling as Table 2 allows — not austenitic solution practice. Heat-treatment reference for SUS410TB: 700 °C min, air or slow cool. Pickling follows unless bright heat treatment leaves a scale-free surface. Duty thread: 12Cr tube supplied annealed for mild HX duty in the 410 family.

When dual documentation against ASTM A213 is requested for a related chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for SUS410TB: annealed HX gauges; confirm hardness annex if ordered.

Dimensions and Tolerances for JIS G3463 SUS410TB

SHH STEEL aligns nominal diameter (A/B), outside diameter, schedule or wall, and length tolerance for SUS410TB before the mill slot is locked. Standard Note 1 frames typical OD from 15.9 mm to 139.8 mm (standard Note 1 general practice). Size hint: annealed HX gauges; confirm hardness annex if ordered. Tolerance class follows the process route ordered for SUS410TB, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Application context for SUS410TB stays mild water coolers, utility exchangers, and heat-adjacent ferritic bundles specified as 410 tube.

Length supply may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against the packaging clause so pickled or polished finishes are not iron-stained in transit. Duty thread: 12Cr tube supplied annealed for mild HX duty in the 410 family. Fixed lengths and multiple cut lengths for SUS410TB are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Application context for SUS410TB stays mild water coolers, utility exchangers, and heat-adjacent ferritic bundles specified as 410 tube.

Equivalent Grades for JIS G3463 SUS410TB

Equivalence talk for SUS410TB starts with 410 / UNS S41000 class (tube as annealed ferritic practice): that commercial / UNS framing is useful in body text and dual-cert discussions, but the H1 and order line stay on JIS G3463 SUS410TB. ASTM A213 / A269 pages that share related chemistry are different product standards with different wall bases, mechanical tables, and tests. Sisters: SUS410TiTB, SUS405TB, SUS430TB, SUS409TB. Caution: delivered annealed under G3463 heat-treatment practice — do not assume quenched-and-tempered martensitic properties.

Heat Treatment and Delivery Condition for JIS G3463 SUS410TB

SUS410TB is delivered annealed under JIS G3463. Table 2 reference: 700 °C min, air or slow cool. Fabricator heat treatment after hot bending should chase the same family practice. Weld thread: 410/ferritic or matching practices per WPS; post-weld heat treatment when required by design. Recorded furnace charts for SUS410TB should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Keep the SUS410TB caution visible here: delivered annealed under G3463 heat-treatment practice — do not assume quenched-and-tempered martensitic properties.

Cooling type matters — austenitic and duplex need rapid cool after solution treatment; ferritic anneal practice allows rapid or slow cool per Table 2. Duty thread: 12Cr tube supplied annealed for mild HX duty in the 410 family. Field heat treatment of SUS410TB after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Weld-shop note tied to SUS410TB: 410/ferritic or matching practices per WPS; post-weld heat treatment when required by design.

Corrosion Resistance of JIS G3463 SUS410TB

Corrosion behaviour of JIS G3463 SUS410TB tracks its ferritic balance: 12Cr aqueous resistance is mild-service only; chlorides and weld HAZ need care. Optional annex corrosion tests (oxalic, Strauss, Huey, etc.) are special quality items — order them when the duty needs coupon evidence. Design caution: delivered annealed under G3463 heat-treatment practice — do not assume quenched-and-tempered martensitic properties.

For heat-facing austenitics, oxidation resistance may dominate over aqueous IGC talk; for duplex and Mo austenitics, chlorides dominate; for ferritics, mild aqueous and weld practice dominate. SUS410TB is filed as ferritic. Caution: delivered annealed under G3463 heat-treatment practice — do not assume quenched-and-tempered martensitic properties. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for SUS410TB rather than relying on schedule thickness alone. This paragraph is locked to SUS410TB duty: 12Cr tube supplied annealed for mild HX duty in the 410 family.

Applications of JIS G3463 SUS410TB Tube

Applications of JIS G3463 SUS410TB tube centre on mild water coolers, utility exchangers, and heat-adjacent ferritic bundles specified as 410 tube. Role summary: 12Cr tube supplied annealed for mild HX duty in the 410 family. When a related chemistry is required under ASTM A213 or A269, open those sister pages — acceptance text is not automatic.

Downstream fabricators should inherit the same grade symbol on cut lists so informal alias substitutions do not creep in. Primary application sketch: mild water coolers, utility exchangers, and heat-adjacent ferritic bundles specified as 410 tube. Duty thread: 12Cr tube supplied annealed for mild HX duty in the 410 family. Commissioning teams benefit when the as-built dossier repeats SUS410TB beside heat numbers, linking isometric revisions to the same mill certificates. Size practice for SUS410TB remains annealed HX gauges; confirm hardness annex if ordered.

Weldability of JIS G3463 SUS410TB

SUS410TB is welded both as a mill product (A/L/E routes) and as fabricator joints on bundles. Shop guidance: 410/ferritic or matching practices per WPS; post-weld heat treatment when required by design. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Procedure qualification for SUS410TB should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. Weld-shop note tied to SUS410TB: 410/ferritic or matching practices per WPS; post-weld heat treatment when required by design.

Filler selection should match or over-alloy the base chemistry as the WPS demands. Heat input, interpass temperature, and shielding follow the family — austenitic, duplex, or ferritic — not a single shop habit. Caution: delivered annealed under G3463 heat-treatment practice — do not assume quenched-and-tempered martensitic properties. Consumable lot control and shielding-gas notes for SUS410TB stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Corrosion framing beside SUS410TB: 12Cr aqueous resistance is mild-service only; chlorides and weld HAZ need care.

Surface Finishes for JIS G3463 SUS410TB

Surface supply for SUS410TB is typically pickled after heat treatment, or bright-annealed when scale-free OD/ID is ordered. Polished or special roughness finishes are by agreement and must state which surface (OD, ID, or both) is in scope. Duty: 12Cr tube supplied annealed for mild HX duty in the 410 family. Roughness or polish callouts for SUS410TB must name OD, ID, or both; ambiguous “bright tube” language is clarified before finishing slots are booked. Application context for SUS410TB stays mild water coolers, utility exchangers, and heat-adjacent ferritic bundles specified as 410 tube.

Passivation treatments, when ordered, follow agreed ASTM A967 / JIS practice analogues — they are not a substitute for correct heat treatment. Caution: delivered annealed under G3463 heat-treatment practice — do not assume quenched-and-tempered martensitic properties. Final visual standards for SUS410TB reject grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed. Keep the SUS410TB caution visible here: delivered annealed under G3463 heat-treatment practice — do not assume quenched-and-tempered martensitic properties.

Inspection and Testing for JIS G3463 SUS410TB

Inspection for JIS G3463 SUS410TB covers cast analysis, tensile tests, flattening or weld bend as applicable, hydrostatic test or NDT, dimensions, and appearance. Special quality annex items (IGC, grain size, etc.) apply only when ordered. Documents follow JIS G 0415 / purchaser-specified EN 10204 styles. Sampling plans for SUS410TB keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Application context for SUS410TB stays mild water coolers, utility exchangers, and heat-adjacent ferritic bundles specified as 410 tube.

Marking includes SUS410TB, manufacture/finish symbols, manufacturer, and other mandatory marking-clause data. Traceability from stencil to MTC is part of supply, not an upgrade. Use: mild water coolers, utility exchangers, and heat-adjacent ferritic bundles specified as 410 tube. Non-conforming SUS410TB lengths are segregated and retested or rejected under retest clauses rather than reworked into unmarked stock. Weld-shop note tied to SUS410TB: 410/ferritic or matching practices per WPS; post-weld heat treatment when required by design.

Packaging and Shipping for JIS G3463 SUS410TB

Packaging for SUS410TB uses wooden boxes, plywood cases, or bundled frames with waterproof wrapping as the OD and finish demand. Soft separators protect pickled and polished surfaces. Ends receive caps or bevel protectors when ordered. Bundle tickets for SUS410TB repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Application context for SUS410TB stays mild water coolers, utility exchangers, and heat-adjacent ferritic bundles specified as 410 tube.

Carbon-steel strapping never contacts the stainless OD without a barrier. Mixed-grade bundles are forbidden when chemistry integrity matters. Caution: delivered annealed under G3463 heat-treatment practice — do not assume quenched-and-tempered martensitic properties. Desiccant and wrap choices for SUS410TB follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Application context for SUS410TB stays mild water coolers, utility exchangers, and heat-adjacent ferritic bundles specified as 410 tube.

Shipping documents list JIS G3463, SUS410TB, sizes, quantities, heat numbers, and certificate type. SHH STEEL coordinates inland trucking and FOB/CIF packing scopes as the order states. Role: 12Cr tube supplied annealed for mild HX duty in the 410 family. Claims handling for SUS410TB starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Weld-shop note tied to SUS410TB: 410/ferritic or matching practices per WPS; post-weld heat treatment when required by design.

Why Choose SHH STEEL

SHH STEEL can produce and supply JIS G3463 SUS410TB with the process route, heat treatment, and tests named on your enquiry — not a bait-and-switch alias. Mill partners run stainless tube capacity that covers seamless and welded Table 1 symbols for this mark. Duty focus: 12Cr tube supplied annealed for mild HX duty in the 410 family.

Technical sales can map SUS410TB against sisters SUS410TiTB, SUS405TB, SUS430TB, SUS409TB and live ASTM pages without pretending standards are identical. Inspection coordination and export packing are in-house habits, not afterthoughts. Ask for a written acknowledgement that names SUS410TB, the manufacture process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS410TB to that written scope.

Supply Capability

SHH STEEL can produce and supply JIS G3463 SUS410TB across enquiry-oriented OD × wall bands, in seamless or welded routes, with certificates and optional annex tests as ordered. Summary capability follows in the table; stock language below is an RFQ map, not a frozen tonnage catalogue. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS410TB when the mill schedule allows.

Item Capability
Standard JIS G3463 stainless steel tubes for boilers and heat exchangers
Grade symbol SUS410TB
Product form Seamless (S) and welded (A / L / E) tube; finishes S-H / S-C / A / A-C / E-C as marked
Delivery condition annealed
Documents Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered)
Typical OD practice 15.9–139.8 mm per standard Note 1; other by agreement
Wall / gauge OD × wall / BWG-class HX gauges within Attached Tables; other by agreement

Stock / Available sizes

SHH STEEL can produce and supply JIS G3463 SUS410TB. Stock / Available sizes: enquiry band typically aligns with 15.9–139.8 mm OD practice under G3463 Note 1, with OD×wall HX gauges; schedule 5S–80 (and heavier by agreement) depending on grade family. For SUS410TB, practical fast-track sizes often sit in mid-bore process and utility ranges — send the OD × wall list for a firm acknowledgement. Context: annealed HX gauges; confirm hardness annex if ordered.

Cut lengths, bevels, special NDT, and IGC annex tests add lead time — call them early. Sisters often quoted alongside: SUS410TiTB, SUS405TB, SUS430TB, SUS409TB. Email the size list to start. SHH STEEL can produce trial lengths of SUS410TB for procedure qualification before the bulk release when the project calendar needs it. SHH STEEL can produce trial lengths of SUS410TB for procedure qualification before bulk release when the project calendar needs it. Corrosion framing beside SUS410TB: 12Cr aqueous resistance is mild-service only; chlorides and weld HAZ need care.

FAQ

What is JIS G3463 SUS410TB stainless steel tube used for?
JIS G3463 SUS410TB is stainless tube for boiler and heat-exchanger service (superheater, HX, condenser, catalyser) — mild water coolers, utility exchangers, and heat-adjacent ferritic bundles specified as 410 tube. Role summary: 12Cr tube supplied annealed for mild HX duty in the 410 family. It is a Japanese boiler/HX tube product standard mark, not an automatic ASTM A213 certificate.
Does JIS G3463 SUS410TB cover seamless and welded tube?
Yes. Manufacture allows seamless and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish marks such as S-H, S-C, A-C, or E-C. SHH STEEL can produce and supply either route for SUS410TB when the mill can meet the ordered size and tests. The title omits Seamless/Welded because JIS G3463 covers both manufacture routes — the PO must still name the process mark.
What heat treatment applies to SUS410TB?
SUS410TB is delivered annealed under JIS G3463. Table 2 reference: 700 °C min, air or slow cool. Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
How does SUS410TB compare with sister grades SUS410TiTB, SUS405TB, SUS430TB?
SUS410TB is filed as ferritic. Typical sisters on the same RFQ are SUS410TiTB, SUS405TB, SUS430TB. Design caution: delivered annealed under G3463 heat-treatment practice — do not assume quenched-and-tempered martensitic properties Pick the sister when the medium or strength floor outgrows this symbol rather than stretching wall alone.
What tests appear on the mill certificate for SUS410TB?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), flattening/flaring as applicable, dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
Is 410 / UNS S41000 class (tube as annealed ferritic practice) the same as ordering SUS410TB?
No. 410 / UNS S41000 class (tube as annealed ferritic practice) is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3463 and SUS410TB so cast limits, heat treatment, and process marks are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for JIS G3463 SUS410TB?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS410TB within the typical 15.9–139.8 mm OD practice, with measured walls by agreement. Size context: annealed HX gauges; confirm hardness annex if ordered. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should SUS410TB be welded?
Shop guidance: 410/ferritic or matching practices per WPS; post-weld heat treatment when required by design. Mill heat treatment of seamless or welded tube does not replace a qualified WPS on fabricator joints or tube-to-tubesheet welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: delivered annealed under G3463 heat-treatment practice — do not assume quenched-and-tempered martensitic properties
When should I choose a duplex or higher-Mo grade instead of SUS410TB?
Move when chloride pitting, crevice attack, or SCC risk exceeds what ferritic practice can defend for the temperature and stress state. Caution for this mark: delivered annealed under G3463 heat-treatment practice — do not assume quenched-and-tempered martensitic properties Sister pointers: SUS410TiTB, SUS405TB, SUS430TB. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify JIS G3463 SUS410TB with ASTM A213 or ASME SA213?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3463 SUS410TB does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for SUS410TB?
Pickled after heat treatment is the usual HX tube supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS410TB when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

JIS G3463 SUS410TB is stainless steel tube for boiler and heat-exchanger service — 12Cr tube supplied annealed for mild HX duty in the 410 family. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS410TiTB, SUS405TB, SUS430TB. Related ASTM A213 pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process mark, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X