JIS G3463 SUS409LTB Stainless Steel Tube

JIS G3463 SUS409LTB stainless steel tube (409L / low-C Ti-stabilised), ferritic, Table 3 cast analysis, Rm min 360 N/mm² / proof min 175 N/mm², annealed. SHH STEEL can produce and supply seamless or welded routes with mill certificates.
Grade
SUS409LTB (409L / low-C Ti-stabilised — body alias)
Standard
JIS G3463
Product form
Seamless and welded stainless steel boiler/HX tube, delivery annealed
Size
Typically OD 15.9–139.8 mm (Note 1); OD × wall (HX/boiler gauges) by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is JIS G3463 SUS409LTB Stainless Steel Tube

JIS G3463 is the Japanese Industrial Standard for stainless steel tubes used in boiler and heat-exchanger service (superheater, HX, condenser, catalyser). Grade symbol SUS409LTB sits in the ferritic set of Table 1. JIS G3463 SUS409LTB is the low-carbon ferritic sister for welded mild coolers — lock the L symbol when the weld map is dense.

SHH STEEL can produce and supply JIS G3463 SUS409LTB as seamless or welded tube across the enquiry OD×wall band, solution-annealed or annealed as Table 2 requires, pickled or bright-finished, and documented on mill test certificates tied to cast analysis and tensile results. Duty focus: low-carbon Ti-stabilised 11Cr ferritic for welded mild HX tube.

Shop language may still say “409L tube,” yet that commercial alias does not select Japanese cast limits, process symbols, or hydraulic/NDT rules. The purchase order has to name JIS G3463 and SUS409LTB so the mill applies the correct analysis, heat treatment, mechanical floors, and marking. Design caution: tensile floors may sit below SUS409TB — confirm Table 4 for the edition on the PO; not for aggressive chlorides.

Scope discipline: SUS409LTB is HX tube product under JIS G3463, not a piping product under JIS G3459 and not an ASTM A213 order by default. Sister marks often compared on the same RFQ include SUS409TB, SUS405TB, SUS430LXTB, SUS410TiTB. Role reminder: low-carbon Ti-stabilised 11Cr ferritic for welded mild HX tube. Document the medium, design temperature, and weld map beside the SUS409LTB line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Size practice for SUS409LTB remains commodity thin-wall OD; ERW or seamless by RFQ.

Inside this JIS G3463 series, compare SUS409TB, SUS405TB, SUS430LXTB, SUS410TiTB. Hub: JIS G3463. ASTM/ASME related product pages (not interchangeable by default): ASTM A213.

Chemical Composition of JIS G3463 SUS409LTB

Cast analysis for JIS G3463 SUS409LTB follows Table 3. Key windows on a typical certificate include C ≤0.030, Si ≤1.00, Mn ≤1.00, P ≤0.040, S ≤0.030, Cr 10.50–11.75, Ti 6×C%–0.75. SHH STEEL ties the heat number on the tube marking to the same cast line on the MTC. Commercial alias 409L / low-C Ti-stabilised is body text only. Corrosion thread: low C + Ti improves welded mild-service behaviour versus high-C 409.

Chemical limits for SUS409LTB under JIS G3463 appear in the table underneath. Source priority is the 2021 Table 3 extract cross-checked to public Nikko / supplier tables. If your client specification cites a different edition footnote, send it before the heat is melted. Duty thread: low-carbon Ti-stabilised 11Cr ferritic for welded mild HX tube.

Grade C Si Mn P S Cr Ti
SUS409LTB ≤0.030 ≤1.00 ≤1.00 ≤0.040 ≤0.030 10.50–11.75 6×C%–0.75

Mechanical Properties of JIS G3463 SUS409LTB

Ambient tensile floors for SUS409LTB come from JIS G3463 Table 4: Rm min 360 N/mm², proof stress min 175 N/mm², elongation min 20% (OD ≥20 mm, No.11/12). These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: ferritic. Caution: tensile floors may sit below SUS409TB — confirm Table 4 for the edition on the PO; not for aggressive chlorides.

Grade Rm min (N/mm²) Proof stress min (N/mm²) A OD≥20 mm No.11/12 min (%) A 10≤OD<20 mm No.11 min (%) A OD<10 mm No.11 min (%)
SUS409LTB 360 175 20 15 12

Ambient values from JIS G3463 Table 4 for SUS409LTB. Heat treatment (Table 2): 700 °C min, air or slow cool. Elongation reductions apply for walls under 8 mm on No.12 pieces. For heat-exchanger tube the purchaser may designate an upper tensile limit (Table 4 min + 200 N/mm²) when necessary.

Manufacture of JIS G3463 SUS409LTB Tube (Seamless and Welded)

Both seamless and welded SUS409LTB are legitimate under JIS G3463. Pick S when the design pressure, wall, or NDT plan favours a pierced/drawn route; pick A, L, or E when welded economics fit and the weld procedure is qualified. Finish symbols S-H/S-C/A/A-C/E-C ride with the process mark on the tube stencil. Seamless and welded options remain available for SUS409LTB; the acknowledgement repeats the Table 1 symbols so production cannot silently change route after the PO is firm. Corrosion framing beside SUS409LTB: low C + Ti improves welded mild-service behaviour versus high-C 409.

Ferritic heats are annealed (700 °C min, or 720 °C min for SUS430J1LTB) with rapid or slow cooling as Table 2 allows — not austenitic solution practice. Heat-treatment reference for SUS409LTB: 700 °C min, air or slow cool. Pickling follows unless bright heat treatment leaves a scale-free surface. Duty thread: low-carbon Ti-stabilised 11Cr ferritic for welded mild HX tube.

When dual documentation against ASTM A213 is requested for a related chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for SUS409LTB: commodity thin-wall OD; ERW or seamless by RFQ.

Dimensions and Tolerances for JIS G3463 SUS409LTB

SHH STEEL aligns nominal diameter (A/B), outside diameter, schedule or wall, and length tolerance for SUS409LTB before the mill slot is locked. Standard Note 1 frames typical OD from 15.9 mm to 139.8 mm (standard Note 1 general practice). Size hint: commodity thin-wall OD; ERW or seamless by RFQ. Tolerance class follows the process route ordered for SUS409LTB, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Size practice for SUS409LTB remains commodity thin-wall OD; ERW or seamless by RFQ.

Length supply may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against the packaging clause so pickled or polished finishes are not iron-stained in transit. Duty thread: low-carbon Ti-stabilised 11Cr ferritic for welded mild HX tube. Fixed lengths and multiple cut lengths for SUS409LTB are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Corrosion framing beside SUS409LTB: low C + Ti improves welded mild-service behaviour versus high-C 409.

Equivalent Grades for JIS G3463 SUS409LTB

Equivalence talk for SUS409LTB starts with 409L / low-C Ti-stabilised: that commercial / UNS framing is useful in body text and dual-cert discussions, but the H1 and order line stay on JIS G3463 SUS409LTB. ASTM A213 / A269 pages that share related chemistry are different product standards with different wall bases, mechanical tables, and tests. Sisters: SUS409TB, SUS405TB, SUS430LXTB, SUS410TiTB. Caution: tensile floors may sit below SUS409TB — confirm Table 4 for the edition on the PO; not for aggressive chlorides.

Heat Treatment and Delivery Condition for JIS G3463 SUS409LTB

SUS409LTB is delivered annealed under JIS G3463. Table 2 reference: 700 °C min, air or slow cool. Fabricator heat treatment after hot bending should chase the same family practice. Weld thread: 409L/ferritic fillers; keep interpass low. Recorded furnace charts for SUS409LTB should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Application context for SUS409LTB stays welded exhaust coolers, mild water exchangers, and ferritic HX where as-welded stability matters.

Cooling type matters — austenitic and duplex need rapid cool after solution treatment; ferritic anneal practice allows rapid or slow cool per Table 2. Duty thread: low-carbon Ti-stabilised 11Cr ferritic for welded mild HX tube. Field heat treatment of SUS409LTB after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Application context for SUS409LTB stays welded exhaust coolers, mild water exchangers, and ferritic HX where as-welded stability matters.

Corrosion Resistance of JIS G3463 SUS409LTB

Corrosion behaviour of JIS G3463 SUS409LTB tracks its ferritic balance: low C + Ti improves welded mild-service behaviour versus high-C 409. Optional annex corrosion tests (oxalic, Strauss, Huey, etc.) are special quality items — order them when the duty needs coupon evidence. Design caution: tensile floors may sit below SUS409TB — confirm Table 4 for the edition on the PO; not for aggressive chlorides.

For heat-facing austenitics, oxidation resistance may dominate over aqueous IGC talk; for duplex and Mo austenitics, chlorides dominate; for ferritics, mild aqueous and weld practice dominate. SUS409LTB is filed as ferritic. Caution: tensile floors may sit below SUS409TB — confirm Table 4 for the edition on the PO; not for aggressive chlorides.

Applications of JIS G3463 SUS409LTB Tube

Applications of JIS G3463 SUS409LTB tube centre on welded exhaust coolers, mild water exchangers, and ferritic HX where as-welded stability matters. Role summary: low-carbon Ti-stabilised 11Cr ferritic for welded mild HX tube. When a related chemistry is required under ASTM A213 or A269, open those sister pages — acceptance text is not automatic.

Downstream fabricators should inherit the same grade symbol on cut lists so informal alias substitutions do not creep in. Primary application sketch: welded exhaust coolers, mild water exchangers, and ferritic HX where as-welded stability matters. Duty thread: low-carbon Ti-stabilised 11Cr ferritic for welded mild HX tube. Commissioning teams benefit when the as-built dossier repeats SUS409LTB beside heat numbers, linking isometric revisions to the same mill certificates. Size practice for SUS409LTB remains commodity thin-wall OD; ERW or seamless by RFQ.

Weldability of JIS G3463 SUS409LTB

SUS409LTB is welded both as a mill product (A/L/E routes) and as fabricator joints on bundles. Shop guidance: 409L/ferritic fillers; keep interpass low. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Procedure qualification for SUS409LTB should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. Weld-shop note tied to SUS409LTB: 409L/ferritic fillers; keep interpass low.

Filler selection should match or over-alloy the base chemistry as the WPS demands. Heat input, interpass temperature, and shielding follow the family — austenitic, duplex, or ferritic — not a single shop habit. Caution: tensile floors may sit below SUS409TB — confirm Table 4 for the edition on the PO; not for aggressive chlorides.

Surface Finishes for JIS G3463 SUS409LTB

Surface supply for SUS409LTB is typically pickled after heat treatment, or bright-annealed when scale-free OD/ID is ordered. Polished or special roughness finishes are by agreement and must state which surface (OD, ID, or both) is in scope. Duty: low-carbon Ti-stabilised 11Cr ferritic for welded mild HX tube. Roughness or polish callouts for SUS409LTB must name OD, ID, or both; ambiguous “bright tube” language is clarified before finishing slots are booked. Corrosion framing beside SUS409LTB: low C + Ti improves welded mild-service behaviour versus high-C 409.

Passivation treatments, when ordered, follow agreed ASTM A967 / JIS practice analogues — they are not a substitute for correct heat treatment. Caution: tensile floors may sit below SUS409TB — confirm Table 4 for the edition on the PO; not for aggressive chlorides. Final visual standards for SUS409LTB reject grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed. Weld-shop note tied to SUS409LTB: 409L/ferritic fillers; keep interpass low.

Inspection and Testing for JIS G3463 SUS409LTB

Inspection for JIS G3463 SUS409LTB covers cast analysis, tensile tests, flattening or weld bend as applicable, hydrostatic test or NDT, dimensions, and appearance. Special quality annex items (IGC, grain size, etc.) apply only when ordered. Documents follow JIS G 0415 / purchaser-specified EN 10204 styles. Sampling plans for SUS409LTB keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Application context for SUS409LTB stays welded exhaust coolers, mild water exchangers, and ferritic HX where as-welded stability matters.

Marking includes SUS409LTB, manufacture/finish symbols, manufacturer, and other mandatory marking-clause data. Traceability from stencil to MTC is part of supply, not an upgrade. Use: welded exhaust coolers, mild water exchangers, and ferritic HX where as-welded stability matters. Non-conforming SUS409LTB lengths are segregated and retested or rejected under retest clauses rather than reworked into unmarked stock. Weld-shop note tied to SUS409LTB: 409L/ferritic fillers; keep interpass low.

Packaging and Shipping for JIS G3463 SUS409LTB

Packaging for SUS409LTB uses wooden boxes, plywood cases, or bundled frames with waterproof wrapping as the OD and finish demand. Soft separators protect pickled and polished surfaces. Ends receive caps or bevel protectors when ordered. Bundle tickets for SUS409LTB repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Weld-shop note tied to SUS409LTB: 409L/ferritic fillers; keep interpass low.

Carbon-steel strapping never contacts the stainless OD without a barrier. Mixed-grade bundles are forbidden when chemistry integrity matters. Caution: tensile floors may sit below SUS409TB — confirm Table 4 for the edition on the PO; not for aggressive chlorides. Desiccant and wrap choices for SUS409LTB follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Weld-shop note tied to SUS409LTB: 409L/ferritic fillers; keep interpass low.

Shipping documents list JIS G3463, SUS409LTB, sizes, quantities, heat numbers, and certificate type. SHH STEEL coordinates inland trucking and FOB/CIF packing scopes as the order states. Role: low-carbon Ti-stabilised 11Cr ferritic for welded mild HX tube. Claims handling for SUS409LTB starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. This paragraph is locked to SUS409LTB duty: low-carbon Ti-stabilised 11Cr ferritic for welded mild HX tube.

Why Choose SHH STEEL

SHH STEEL can produce and supply JIS G3463 SUS409LTB with the process route, heat treatment, and tests named on your enquiry — not a bait-and-switch alias. Mill partners run stainless tube capacity that covers seamless and welded Table 1 symbols for this mark. Duty focus: low-carbon Ti-stabilised 11Cr ferritic for welded mild HX tube.

Technical sales can map SUS409LTB against sisters SUS409TB, SUS405TB, SUS430LXTB, SUS410TiTB and live ASTM pages without pretending standards are identical. Inspection coordination and export packing are in-house habits, not afterthoughts. Ask for a written acknowledgement that names SUS409LTB, the manufacture process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS409LTB to that written scope.

Supply Capability

SHH STEEL can produce and supply JIS G3463 SUS409LTB across enquiry-oriented OD × wall bands, in seamless or welded routes, with certificates and optional annex tests as ordered. Summary capability follows in the table; stock language below is an RFQ map, not a frozen tonnage catalogue. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS409LTB when the mill schedule allows.

Item Capability
Standard JIS G3463 stainless steel tubes for boilers and heat exchangers
Grade symbol SUS409LTB
Product form Seamless (S) and welded (A / L / E) tube; finishes S-H / S-C / A / A-C / E-C as marked
Delivery condition annealed
Documents Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered)
Typical OD practice 15.9–139.8 mm per standard Note 1; other by agreement
Wall / gauge OD × wall / BWG-class HX gauges within Attached Tables; other by agreement

Stock / Available sizes

SHH STEEL can produce and supply JIS G3463 SUS409LTB. Stock / Available sizes: enquiry band typically aligns with 15.9–139.8 mm OD practice under G3463 Note 1, with OD×wall HX gauges; schedule 5S–80 (and heavier by agreement) depending on grade family. For SUS409LTB, practical fast-track sizes often sit in mid-bore process and utility ranges — send the OD × wall list for a firm acknowledgement. Context: commodity thin-wall OD; ERW or seamless by RFQ.

Cut lengths, bevels, special NDT, and IGC annex tests add lead time — call them early. Sisters often quoted alongside: SUS409TB, SUS405TB, SUS430LXTB, SUS410TiTB. Email the size list to start. SHH STEEL can produce trial lengths of SUS409LTB for procedure qualification before the bulk release when the project calendar needs it. SHH STEEL can produce trial lengths of SUS409LTB for procedure qualification before bulk release when the project calendar needs it. Keep the SUS409LTB caution visible here: tensile floors may sit below SUS409TB — confirm Table 4 for the edition on the PO; not for aggressive chlorides.

FAQ

What is JIS G3463 SUS409LTB stainless steel tube used for?
JIS G3463 SUS409LTB is stainless tube for boiler and heat-exchanger service (superheater, HX, condenser, catalyser) — welded exhaust coolers, mild water exchangers, and ferritic HX where as-welded stability matters. Role summary: low-carbon Ti-stabilised 11Cr ferritic for welded mild HX tube. It is a Japanese boiler/HX tube product standard mark, not an automatic ASTM A213 certificate.
Does JIS G3463 SUS409LTB cover seamless and welded tube?
Yes. Manufacture allows seamless and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish marks such as S-H, S-C, A-C, or E-C. SHH STEEL can produce and supply either route for SUS409LTB when the mill can meet the ordered size and tests. The title omits Seamless/Welded because JIS G3463 covers both manufacture routes — the PO must still name the process mark.
What heat treatment applies to SUS409LTB?
SUS409LTB is delivered annealed under JIS G3463. Table 2 reference: 700 °C min, air or slow cool. Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
How does SUS409LTB compare with sister grades SUS409TB, SUS405TB, SUS430LXTB?
SUS409LTB is filed as ferritic. Typical sisters on the same RFQ are SUS409TB, SUS405TB, SUS430LXTB. Design caution: tensile floors may sit below SUS409TB — confirm Table 4 for the edition on the PO; not for aggressive chlorides Pick the sister when the medium or strength floor outgrows this symbol rather than stretching wall alone.
What tests appear on the mill certificate for SUS409LTB?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), flattening/flaring as applicable, dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
Is 409L / low-C Ti-stabilised the same as ordering SUS409LTB?
No. 409L / low-C Ti-stabilised is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3463 and SUS409LTB so cast limits, heat treatment, and process marks are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for JIS G3463 SUS409LTB?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS409LTB within the typical 15.9–139.8 mm OD practice, with measured walls by agreement. Size context: commodity thin-wall OD; ERW or seamless by RFQ. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should SUS409LTB be welded?
Shop guidance: 409L/ferritic fillers; keep interpass low. Mill heat treatment of seamless or welded tube does not replace a qualified WPS on fabricator joints or tube-to-tubesheet welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: tensile floors may sit below SUS409TB — confirm Table 4 for the edition on the PO; not for aggressive chlorides
When should I choose a duplex or higher-Mo grade instead of SUS409LTB?
Move when chloride pitting, crevice attack, or SCC risk exceeds what ferritic practice can defend for the temperature and stress state. Caution for this mark: tensile floors may sit below SUS409TB — confirm Table 4 for the edition on the PO; not for aggressive chlorides Sister pointers: SUS409TB, SUS405TB, SUS430LXTB. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify JIS G3463 SUS409LTB with ASTM A213 or ASME SA213?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3463 SUS409LTB does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for SUS409LTB?
Pickled after heat treatment is the usual HX tube supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS409LTB when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

JIS G3463 SUS409LTB is stainless steel tube for boiler and heat-exchanger service — low-carbon Ti-stabilised 11Cr ferritic for welded mild HX tube. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS409TB, SUS405TB, SUS430LXTB. Related ASTM A213 pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process mark, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X