JIS G3463 SUS310STB Stainless Steel Tube
What is JIS G3463 SUS310STB Stainless Steel Tube
When the approved vendor list and tube-bundle notes say JIS G3463, the grade mark has to carry the TB suffix. SUS310STB is the full product symbol for this austenitic tube. If shutdown condensate and field welds share the same bundle, JIS G3463 SUS310STB is usually the safer 25-20 mark than high-C SUS310TB.
SHH STEEL can supply SUS310STB tube in seamless S or welded A/L/E routes, with plain or bevelled ends, random or cut lengths, and EN 10204 / JIS G 0415 style inspection documents when specified. Role on the line: lower-carbon 310S austenitic HX tube for oxidation duty with tighter carbon control than SUS310TB.
Equivalence talk to 310S / UNS S31008 belongs in engineering notes, not as a substitute for the JIS symbol. Lock JIS G3463 SUS310STB, OD × wall, manufacture/finish symbols, and any special quality annex items before melt. Watch-out: still oxidation-first — chloride process coolers usually need Mo austenitic, duplex, or 6Mo marks instead.
Related ASTM tube pages share chemistry families but not Japanese acceptance text — confirm before dual-cert claims. Sisters on this hub: SUS310TB, SUS309STB, SUS316TB, SUS321TB. Use thread: high-temperature process coolers, waste-heat boilers (tube side), incinerator HX, and welded hot-gas bundles that also wet out on shutdown. Document the medium, design temperature, and weld map beside the SUS310STB line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Application context for SUS310STB stays high-temperature process coolers, waste-heat boilers (tube side), incinerator HX, and welded hot-gas bundles that also wet out on shutdown.
Inside this JIS G3463 series, compare SUS310TB, SUS309STB, SUS316TB, SUS321TB. Hub: JIS G3463. ASTM/ASME related product pages (not interchangeable by default): A213 TP310S, ASTM A213.
Chemical Composition of JIS G3463 SUS310STB
Chemistry control on SUS310STB starts at the ladle. Expect C ≤0.08, Si ≤1.50, Mn ≤2.00, P ≤0.040, S ≤0.030, Ni 19.00–22.00, Cr 24.00–26.00 within Table 3, reported on the inspection document against the heat. Body alias 310S / UNS S31008 does not widen those windows. Every ladle analysis for SUS310STB is checked against those windows before the heat is released to piercing, welding, or finishing, and the same numbers reappear on the inspection document. This paragraph is locked to SUS310STB duty: lower-carbon 310S austenitic HX tube for oxidation duty with tighter carbon control than SUS310TB.
Read the table with the family in mind — austenitic — and with caution still oxidation-first — chloride process coolers usually need Mo austenitic, duplex, or 6Mo marks instead. Numbers without the matching heat-treatment row are incomplete purchase data. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for SUS310STB before the order is acknowledged. Corrosion framing beside SUS310STB: keeps 310-class scale resistance with a 0.08% carbon ceiling that helps as-welded aqueous stability.
| Grade | C | Si | Mn | P | S | Ni | Cr |
|---|---|---|---|---|---|---|---|
| SUS310STB | ≤0.08 | ≤1.50 | ≤2.00 | ≤0.040 | ≤0.030 | 19.00–22.00 | 24.00–26.00 |
Mechanical Properties of JIS G3463 SUS310STB
Proof stress and tensile minima for SUS310STB sit at Rm min 520 N/mm², proof stress min 206 N/mm², elongation min 35% (OD ≥20 mm, No.11/12). Flattening, flaring, and reverse-flattening (welded) testing backs ductility for the ordered process route. Watch-out: still oxidation-first — chloride process coolers usually need Mo austenitic, duplex, or 6Mo marks instead.
| Grade | Rm min (N/mm²) | Proof stress min (N/mm²) | A OD≥20 mm No.11/12 min (%) | A 10≤OD<20 mm No.11 min (%) | A OD<10 mm No.11 min (%) |
|---|---|---|---|---|---|
| SUS310STB | 520 | 206 | 35 | 30 | 27 |
Ambient values from JIS G3463 Table 4 for SUS310STB. Heat treatment (Table 2): 1030 °C min, rapid cool. Elongation reductions apply for walls under 8 mm on No.12 pieces. For heat-exchanger tube the purchaser may designate an upper tensile limit (Table 4 min + 200 N/mm²) when necessary.
Manufacture of JIS G3463 SUS310STB Tube (Seamless and Welded)
For SUS310STB, the mill path is not “seamless only.” Table 1 explicitly pairs austenitic, duplex, and ferritic marks with seamless or A/L/E welded process symbols and S-H/S-C/A/A-C/E-C finishes. Order the combination that matches hydrostatic or NDT preference, not a habit from ASTM A213 alone. Seamless and welded options remain available for SUS310STB; the acknowledgement repeats the Table 1 symbols so production cannot silently change route after the PO is firm. Corrosion framing beside SUS310STB: keeps 310-class scale resistance with a 0.08% carbon ceiling that helps as-welded aqueous stability.
Process control for SUS310STB ends with verified heat treatment (1030 °C min, rapid cool) and surface conditioning. Austenitic heats take solution annealing with rapid cooling; hot-finished seamless may omit separate solution treatment when hot-worked and rapidly cooled in-line under the Table 2 note, unless the purchaser forbids it. Pickling or bright-anneal decisions for SUS310STB stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive duties. Corrosion framing beside SUS310STB: keeps 310-class scale resistance with a 0.08% carbon ceiling that helps as-welded aqueous stability.
Bevel geometry for walls ≤22 mm defaults to the standard figure when bevels are ordered without a drawing. Size practice: cold-finished seamless for precision HX OD; hot-finished for heavier walls. Hydrostatic pressure or NDT class for SUS310STB is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Keep the SUS310STB caution visible here: still oxidation-first — chloride process coolers usually need Mo austenitic, duplex, or 6Mo marks instead.
Dimensions and Tolerances for JIS G3463 SUS310STB
Mass tables in JIS G3463 support Attached Table mass/OD×wall ordering for common austenitic marks; for SUS310STB, confirm whether your project uses schedule or measured wall. Context: cold-finished seamless for precision HX OD; hot-finished for heavier walls. Tolerance class follows the process route ordered for SUS310STB, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Application context for SUS310STB stays high-temperature process coolers, waste-heat boilers (tube side), incinerator HX, and welded hot-gas bundles that also wet out on shutdown.
For heat-exchange and building services, schedule tables often drive the BOM; for process plants, measured wall and corrosion allowance dominate. SUS310STB supports both conversations when the PO is clear. Fixed lengths and multiple cut lengths for SUS310STB are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Keep the SUS310STB caution visible here: still oxidation-first — chloride process coolers usually need Mo austenitic, duplex, or 6Mo marks instead.
Equivalent Grades for JIS G3463 SUS310STB
Do not treat 310S / UNS S31008 as interchangeable paperwork. Chemistry kinship is not acceptance kinship. Inside this series see SUS310TB, SUS309STB, SUS316TB, SUS321TB. Role: lower-carbon 310S austenitic HX tube for oxidation duty with tighter carbon control than SUS310TB. When a dual-cert path is required, list both JIS G3463 SUS310STB and the ASTM mark with separate test scopes instead of assuming one chemistry line clears both files. This paragraph is locked to SUS310STB duty: lower-carbon 310S austenitic HX tube for oxidation duty with tighter carbon control than SUS310TB.
Heat Treatment and Delivery Condition for JIS G3463 SUS310STB
Stabilisation or special anneals, where the standard allows purchaser options (notably Ti/Nb grades), must be written on the order — silence means Table 2 defaults only. For SUS310STB: 1030 °C min, rapid cool. Recorded furnace charts for SUS310STB should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Weld-shop note tied to SUS310STB: 310S/310L-class fillers; watch dilution and hot-crack risk on heavy returns.
After local hot work in the field, restore solution annealed practice when the corrosion file demands it. Caution: still oxidation-first — chloride process coolers usually need Mo austenitic, duplex, or 6Mo marks instead. Field heat treatment of SUS310STB after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. This paragraph is locked to SUS310STB duty: lower-carbon 310S austenitic HX tube for oxidation duty with tighter carbon control than SUS310TB.
Corrosion Resistance of JIS G3463 SUS310STB
Pick tests that match how SUS310STB is filed — austenitic. Corrosion thread: keeps 310-class scale resistance with a 0.08% carbon ceiling that helps as-welded aqueous stability. Caution: still oxidation-first — chloride process coolers usually need Mo austenitic, duplex, or 6Mo marks instead. Coupon orientation, weld condition, and surface finish for SUS310STB belong in the corrosion test order so annex results can be compared to the installed bundle honestly. Corrosion framing beside SUS310STB: keeps 310-class scale resistance with a 0.08% carbon ceiling that helps as-welded aqueous stability.
Fire-protection and potable-adjacent lines still need the right alloy — G3463 scope does not make every mark equal. Use thread: high-temperature process coolers, waste-heat boilers (tube side), incinerator HX, and welded hot-gas bundles that also wet out on shutdown. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for SUS310STB rather than relying on schedule thickness alone. Size practice for SUS310STB remains cold-finished seamless for precision HX OD; hot-finished for heavier walls.
Applications of JIS G3463 SUS310STB Tube
Project types that repeatedly call SUS310STB: high-temperature process coolers, waste-heat boilers (tube side), incinerator HX, and welded hot-gas bundles that also wet out on shutdown. Duty: lower-carbon 310S austenitic HX tube for oxidation duty with tighter carbon control than SUS310TB. Caution still applies: still oxidation-first — chloride process coolers usually need Mo austenitic, duplex, or 6Mo marks instead.
Superheater stubs, condenser bundles and corrosive process HX lines all appear in G3463’s scope — alloy choice still follows the medium. For this mark: lower-carbon 310S austenitic HX tube for oxidation duty with tighter carbon control than SUS310TB. Commissioning teams benefit when the as-built dossier repeats SUS310STB beside heat numbers, linking isometric revisions to the same mill certificates. This paragraph is locked to SUS310STB duty: lower-carbon 310S austenitic HX tube for oxidation duty with tighter carbon control than SUS310TB.
Weldability of JIS G3463 SUS310STB
Even seamless S tube of SUS310STB will see field welds. Use: 310S/310L-class fillers; watch dilution and hot-crack risk on heavy returns. Restore heat treatment when the WPS and corrosion file require it. Procedure qualification for SUS310STB should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. Corrosion framing beside SUS310STB: keeps 310-class scale resistance with a 0.08% carbon ceiling that helps as-welded aqueous stability.
Dissimilar welds to carbon steel need buttering and dilution control — especially on heat-facing and Mo grades. Role context: lower-carbon 310S austenitic HX tube for oxidation duty with tighter carbon control than SUS310TB. Consumable lot control and shielding-gas notes for SUS310STB stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. This paragraph is locked to SUS310STB duty: lower-carbon 310S austenitic HX tube for oxidation duty with tighter carbon control than SUS310TB.
Surface Finishes for JIS G3463 SUS310STB
Iron-free handling after pickle matters — carbon-steel strapping stains show up later as rust blooms on SUS310STB. Finish thread tied to austenitic. Roughness or polish callouts for SUS310STB must name OD, ID, or both; ambiguous “bright tube” language is clarified before finishing slots are booked. Application context for SUS310STB stays high-temperature process coolers, waste-heat boilers (tube side), incinerator HX, and welded hot-gas bundles that also wet out on shutdown.
OD stencil ink and marking paint should be chloride-lean and removable where coating systems follow. Role: lower-carbon 310S austenitic HX tube for oxidation duty with tighter carbon control than SUS310TB. Final visual standards for SUS310STB reject grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed. This paragraph is locked to SUS310STB duty: lower-carbon 310S austenitic HX tube for oxidation duty with tighter carbon control than SUS310TB.
Inspection and Testing for JIS G3463 SUS310STB
Clause 13/14 define sampling and retests. For SUS310STB, keep the heat/lot identity unbroken from melt to bundle tag. Duty: lower-carbon 310S austenitic HX tube for oxidation duty with tighter carbon control than SUS310TB. Sampling plans for SUS310STB keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. This paragraph is locked to SUS310STB duty: lower-carbon 310S austenitic HX tube for oxidation duty with tighter carbon control than SUS310TB.
Intergranular corrosion testing is annex/special — order it when polythionic or weld-decay risk is written into the duty file for SUS310STB. Non-conforming SUS310STB lengths are segregated and retested or rejected under retest clauses rather than reworked into unmarked stock. Size practice for SUS310STB remains cold-finished seamless for precision HX OD; hot-finished for heavier walls.
Packaging and Shipping for JIS G3463 SUS310STB
Small-OD SUS310STB often ships in crates; large-OD in strapped bundles with OD pads. Confirm destination handling limits on the RFQ. Use: high-temperature process coolers, waste-heat boilers (tube side), incinerator HX, and welded hot-gas bundles that also wet out on shutdown. Bundle tickets for SUS310STB repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Size practice for SUS310STB remains cold-finished seamless for precision HX OD; hot-finished for heavier walls.
Bevelled ends get protectors so landing edges survive trucking. Size hint: cold-finished seamless for precision HX OD; hot-finished for heavier walls. Desiccant and wrap choices for SUS310STB follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Size practice for SUS310STB remains cold-finished seamless for precision HX OD; hot-finished for heavier walls.
Storage advice on arrival: keep bundles dry and off carbon-steel floors. Use thread: high-temperature process coolers, waste-heat boilers (tube side), incinerator HX, and welded hot-gas bundles that also wet out on shutdown. Claims handling for SUS310STB starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Size practice for SUS310STB remains cold-finished seamless for precision HX OD; hot-finished for heavier walls.
Why Choose SHH STEEL
Project teams working to Japanese boiler/HX specs need a supplier that reads TB suffixes correctly. SHH STEEL can make SUS310STB to that discipline. Caution we keep visible: still oxidation-first — chloride process coolers usually need Mo austenitic, duplex, or 6Mo marks instead. SHH STEEL can produce and supply SUS310STB against the OD × wall, process symbol, and test scope on your RFQ without swapping in an unstated sister grade.
Dual-cert discussions (JIS + ASTM) are handled with two acceptance regimes in view, not one certificate stretched by hope. Sisters: SUS310TB, SUS309STB, SUS316TB, SUS321TB. Ask for a written acknowledgement that names SUS310STB, the manufacture process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS310STB to that written scope.
Supply Capability
Whether you need prototype bundles or project tonnage of SUS310STB, SHH STEEL can supply against a clear OD × wall and test matrix. Duty: high-temperature process coolers, waste-heat boilers (tube side), incinerator HX, and welded hot-gas bundles that also wet out on shutdown. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS310STB when the mill schedule allows.
| Item | Capability |
|---|---|
| Standard | JIS G3463 stainless steel tubes for boilers and heat exchangers |
| Grade symbol | SUS310STB |
| Product form | Seamless (S) and welded (A / L / E) tube; finishes S-H / S-C / A / A-C / E-C as marked |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered) |
| Typical OD practice | 15.9–139.8 mm per standard Note 1; other by agreement |
| Wall / gauge | OD × wall / BWG-class HX gauges within Attached Tables; other by agreement |
Stock / Available sizes
Stock / Available sizes: SHH STEEL quotes rolling/welding slots for SUS310STB rather than promising anonymous warehouse tons. Typical conversation starts around cold-finished seamless for precision HX OD; hot-finished for heavier walls. SHH STEEL can supply alternate schedules and measured walls for SUS310STB once the design pressure and corrosion allowance are clear. SHH STEEL can supply alternate schedules and measured walls for SUS310STB once design pressure and corrosion allowance are clear. Corrosion framing beside SUS310STB: keeps 310-class scale resistance with a 0.08% carbon ceiling that helps as-welded aqueous stability.
If the project needs dual JIS G3463 + ASTM documentation, say so before melt. Caution: still oxidation-first — chloride process coolers usually need Mo austenitic, duplex, or 6Mo marks instead. SHH STEEL can produce trial lengths of SUS310STB for procedure qualification before the bulk release when the project calendar needs it. SHH STEEL can produce trial lengths of SUS310STB for procedure qualification before bulk release when the project calendar needs it. This paragraph is locked to SUS310STB duty: lower-carbon 310S austenitic HX tube for oxidation duty with tighter carbon control than SUS310TB.
FAQ
-
What is JIS G3463 SUS310STB stainless steel tube used for?
- JIS G3463 SUS310STB is stainless tube for boiler and heat-exchanger service (superheater, HX, condenser, catalyser) — high-temperature process coolers, waste-heat boilers (tube side), incinerator HX, and welded hot-gas bundles that also wet out on shutdown. Role summary: lower-carbon 310S austenitic HX tube for oxidation duty with tighter carbon control than SUS310TB. It is a Japanese boiler/HX tube product standard mark, not an automatic ASTM A213 certificate.
-
Does JIS G3463 SUS310STB cover seamless and welded tube?
- Yes. Manufacture allows seamless and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish marks such as S-H, S-C, A-C, or E-C. SHH STEEL can produce and supply either route for SUS310STB when the mill can meet the ordered size and tests. The title omits Seamless/Welded because JIS G3463 covers both manufacture routes — the PO must still name the process mark.
-
What heat treatment applies to SUS310STB?
- SUS310STB is delivered solution annealed under JIS G3463. Table 2 reference: 1030 °C min, rapid cool. Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
-
How does SUS310STB compare with sister grades SUS310TB, SUS309STB, SUS316TB?
- SUS310STB is filed as austenitic. Typical sisters on the same RFQ are SUS310TB, SUS309STB, SUS316TB. Design caution: still oxidation-first — chloride process coolers usually need Mo austenitic, duplex, or 6Mo marks instead Pick the sister when the medium or strength floor outgrows this symbol rather than stretching wall alone.
-
What tests appear on the mill certificate for SUS310STB?
- Expect cast analysis (Table 3), room-temperature tensile results (Table 4), flattening/flaring as applicable, dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
-
Is 310S / UNS S31008 the same as ordering SUS310STB?
- No. 310S / UNS S31008 is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3463 and SUS310STB so cast limits, heat treatment, and process marks are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for JIS G3463 SUS310STB?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS310STB within the typical 15.9–139.8 mm OD practice, with measured walls by agreement. Size context: cold-finished seamless for precision HX OD; hot-finished for heavier walls. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
How should SUS310STB be welded?
- Shop guidance: 310S/310L-class fillers; watch dilution and hot-crack risk on heavy returns. Mill heat treatment of seamless or welded tube does not replace a qualified WPS on fabricator joints or tube-to-tubesheet welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: still oxidation-first — chloride process coolers usually need Mo austenitic, duplex, or 6Mo marks instead
-
When should I choose a duplex or higher-Mo grade instead of SUS310STB?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: still oxidation-first — chloride process coolers usually need Mo austenitic, duplex, or 6Mo marks instead Sister pointers: SUS310TB, SUS309STB, SUS316TB. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify JIS G3463 SUS310STB with ASTM A213 or ASME SA213?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3463 SUS310STB does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What surface finishes are available for SUS310STB?
- Pickled after heat treatment is the usual HX tube supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS310STB when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
JIS G3463 SUS310STB is stainless steel tube for boiler and heat-exchanger service — lower-carbon 310S austenitic HX tube for oxidation duty with tighter carbon control than SUS310TB. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS310TB, SUS309STB, SUS316TB. Related ASTM A213 pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process mark, and medium notes to start the quote.