JIS G3463 SUS890LTB Stainless Steel Tube
What is JIS G3463 SUS890LTB Stainless Steel Tube
Boiler and heat-exchanger packages that cite Japanese product standards look to JIS G3463 — Stainless steel boiler and heat exchanger tubes — rather than inventing a mill grade from AISI shorthand alone. SUS890LTB is the Table 1 symbol for this austenitic chemistry. JIS G3463 SUS890LTB is the Japanese 904L-class HX tube symbol — order it by that name, not by hoping “904L tube” lands the same Table 3 windows.
Mill path for SUS890LTB: Table 1 manufacture/finish symbols, Table 2 heat treatment, Table 3 cast chemistry, Table 4 tensile floors. SHH STEEL can make and supply the grade to that stack with hydrostatic or NDT acceptance as ordered. Typical use: sulphuric coolers, chemical condensers, and process HX written around 904L-family chemistry. Size and test clarity on the RFQ lets SHH STEEL lock the correct Table 1 symbols for SUS890LTB before production starts. Size practice for SUS890LTB remains seamless HX gauges; welded only with qualified high-alloy procedures.
Body text may mention ~904L-class Cu-Mo austenitic (JIS SUS890L) for cross-reference, but the H1 and order line stay on SUS890LTB. Silent alias swaps are how wrong carbon ceilings and wrong tensile tables enter the MTC. Keep this caution in view: lower Rm/proof floors than many 6Mo marks; confirm Cu 1–2% on the cast line.
Order the standard the drawing and regulatory file actually require. Inside this G3463 series, compare SUS836LTB, SUS317LTB, SUS312LTB, SUS316LTB before stretching surface finish or schedule alone. Duty thread: Cu-Mo high-Ni austenitic (~904L class) for sulphuric and chloride chemical HX tube. Document the medium, design temperature, and weld map beside the SUS890LTB line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Weld-shop note tied to SUS890LTB: 904L-class / high-Ni Cu-Mo fillers; control segregation and heat input.
Inside this JIS G3463 series, compare SUS836LTB, SUS317LTB, SUS312LTB, SUS316LTB. Hub: JIS G3463. ASTM/ASME related product pages (not interchangeable by default): ASTM A213.
Chemical Composition of JIS G3463 SUS890LTB
Table 3 sets the melt limits for SUS890LTB. Highlight band: C ≤0.020, Si ≤1.00, Mn ≤2.00, P ≤0.040, S ≤0.030, Ni 23.00–28.00, Cr 19.00–23.00. Product analysis, when ordered, applies JIS G 0321 stainless product tolerances on top of Table 3. Alias note: ~904L-class Cu-Mo austenitic (JIS SUS890L). Every ladle analysis for SUS890LTB is checked against those windows before the heat is released to piercing, welding, or finishing, and the same numbers reappear on the inspection document. Weld-shop note tied to SUS890LTB: 904L-class / high-Ni Cu-Mo fillers; control segregation and heat input.
The composition table below is the cast window SHH STEEL quotes against for SUS890LTB. Edition framing is JIS G3463. Use thread: sulphuric coolers, chemical condensers, and process HX written around 904L-family chemistry. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for SUS890LTB before the order is acknowledged. Weld-shop note tied to SUS890LTB: 904L-class / high-Ni Cu-Mo fillers; control segregation and heat input.
| Grade | C | Si | Mn | P | S | Ni | Cr | Mo | Cu |
|---|---|---|---|---|---|---|---|---|---|
| SUS890LTB | ≤0.020 | ≤1.00 | ≤2.00 | ≤0.040 | ≤0.030 | 23.00–28.00 | 19.00–23.00 | 4.00–5.00 | 1.00–2.00 |
Mechanical Properties of JIS G3463 SUS890LTB
Table 4 mechanical acceptance for SUS890LTB: Rm min 481 N/mm², proof stress min 177 N/mm², elongation min 35% (OD ≥20 mm, No.11/12). Elongation rules change for walls under 8 mm and are not mandatory below 40 mm OD (record only unless agreed). Delivery framing: solution annealed. Tensile sampling follows tensile sampling clauses for the ordered test unit of SUS890LTB, and retests follow retest clauses when a result sits under the Table 4 floor. This paragraph is locked to SUS890LTB duty: Cu-Mo high-Ni austenitic (~904L class) for sulphuric and chloride chemical HX tube.
| Grade | Rm min (N/mm²) | Proof stress min (N/mm²) | A OD≥20 mm No.11/12 min (%) | A 10≤OD<20 mm No.11 min (%) | A OD<10 mm No.11 min (%) |
|---|---|---|---|---|---|
| SUS890LTB | 481 | 177 | 35 | 30 | 27 |
Ambient values from JIS G3463 Table 4 for SUS890LTB. Heat treatment (Table 2): 1030 °C min, rapid cool. Elongation reductions apply for walls under 8 mm on No.12 pieces. For heat-exchanger tube the purchaser may designate an upper tensile limit (Table 4 min + 200 N/mm²) when necessary.
Manufacture of JIS G3463 SUS890LTB Tube (Seamless and Welded)
For SUS890LTB, the mill path is not “seamless only.” Table 1 explicitly pairs austenitic, duplex, and ferritic marks with seamless or A/L/E welded process symbols and S-H/S-C/A/A-C/E-C finishes. Order the combination that matches hydrostatic or NDT preference, not a habit from ASTM A213 alone. Seamless and welded options remain available for SUS890LTB; the acknowledgement repeats the Table 1 symbols so production cannot silently change route after the PO is firm. Weld-shop note tied to SUS890LTB: 904L-class / high-Ni Cu-Mo fillers; control segregation and heat input.
After forming, SUS890LTB receives Table 2 treatment — 1030 °C min, rapid cool. Austenitic heats take solution annealing with rapid cooling; hot-finished seamless may omit separate solution treatment when hot-worked and rapidly cooled in-line under the Table 2 note, unless the purchaser forbids it. Use thread: sulphuric coolers, chemical condensers, and process HX written around 904L-family chemistry.
Marking carries the grade symbol SUS890LTB, process/finish marks, manufacturer ID, and other marking-clause items. Size hint: seamless HX gauges; welded only with qualified high-alloy procedures. Weld thread: 904L-class / high-Ni Cu-Mo fillers; control segregation and heat input. Hydrostatic pressure or NDT class for SUS890LTB is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Application context for SUS890LTB stays sulphuric coolers, chemical condensers, and process HX written around 904L-family chemistry.
Dimensions and Tolerances for JIS G3463 SUS890LTB
Dimensional order lines for SUS890LTB should state OD × wall (or OD×wall HX gauges; schedule 5S/10S/20S/40/80/…), length type, and end finish. Tolerances follow dimensional tolerance clauses by process route. Use: sulphuric coolers, chemical condensers, and process HX written around 904L-family chemistry. Tolerance class follows the process route ordered for SUS890LTB, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. This paragraph is locked to SUS890LTB duty: Cu-Mo high-Ni austenitic (~904L class) for sulphuric and chloride chemical HX tube.
OD and wall tolerances differ for hot-finished seamless versus cold-finished / welded routes — quote the process symbol with the size. Caution: lower Rm/proof floors than many 6Mo marks; confirm Cu 1–2% on the cast line. Fixed lengths and multiple cut lengths for SUS890LTB are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Keep the SUS890LTB caution visible here: lower Rm/proof floors than many 6Mo marks; confirm Cu 1–2% on the cast line.
Equivalent Grades for JIS G3463 SUS890LTB
Lock SUS890LTB on the purchase order: it is the JIS G3463 Cu-Mo high-nickel austenitic heat-exchanger tube mark in the ~904L chemistry conversation. Alias “~904L-class Cu-Mo austenitic (JIS SUS890L)” appears only as a cross-walk in body text — useful for dual-cert talk, not as the MTC grade by itself. ASTM or EN 904L-family pages share related chemistry but different product rules; lower Rm/proof floors than many 6Mo marks mean you must not assume a 6Mo mechanical table.
| System | Designation | Notes |
|---|---|---|
| JIS G3463 | SUS890LTB | Governing HX/boiler tube grade for this page |
| Commercial / UNS (body only) | ~904L-class / UNS N08904 talk (JIS SUS890L) | Useful in dual-cert talk; confirm Cu 1–2% on the cast line |
| ASTM A213 / A269 related | 904L-family austenitic tube practice (related, not identical paperwork) | Related chemistry family — different product standard; not interchangeable by default |
| EN / other | 1.4539 (X1NiCrMoCu25-20-5) approximate wrought name | Starting point for comparison only; no automatic dual-cert |
Sisters when sulphuric or chloride duty changes: SUS836LTB, SUS317LTB, SUS312LTB, SUS316LTB. Confirm Cu on every heat — that window is intentional for SUS890LTB sulphuric cooler work. Series hub: JIS G3463.
Heat Treatment and Delivery Condition for JIS G3463 SUS890LTB
Mill heat treatment for SUS890LTB: 1030 °C min, rapid cool. Bright annealing may omit pickling when the surface is scale-free. Delivery label: solution annealed. Recorded furnace charts for SUS890LTB should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Keep the SUS890LTB caution visible here: lower Rm/proof floors than many 6Mo marks; confirm Cu 1–2% on the cast line.
Certificate wording for SUS890LTB should show the heat-treatment condition actually performed, not a generic “annealed” stamp that hides temperature. Use: sulphuric coolers, chemical condensers, and process HX written around 904L-family chemistry. Field heat treatment of SUS890LTB after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Keep the SUS890LTB caution visible here: lower Rm/proof floors than many 6Mo marks; confirm Cu 1–2% on the cast line.
Corrosion Resistance of JIS G3463 SUS890LTB
Cu + Mo + high Ni helps in reducing acids and many chloride duties; verify temperature limits Special quality annex tests are available by agreement; they are not a blanket warranty for every process medium. Family filing: austenitic. Coupon orientation, weld condition, and surface finish for SUS890LTB belong in the corrosion test order so annex results can be compared to the installed bundle honestly. Corrosion framing beside SUS890LTB: Cu + Mo + high Ni helps in reducing acids and many chloride duties; verify temperature limits.
Do not market invented PREN digits. Bring medium chemistry and SHH STEEL will map SUS890LTB honestly against SUS836LTB, SUS317LTB, SUS312LTB, SUS316LTB. Role: Cu-Mo high-Ni austenitic (~904L class) for sulphuric and chloride chemical HX tube. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for SUS890LTB rather than relying on schedule thickness alone. Application context for SUS890LTB stays sulphuric coolers, chemical condensers, and process HX written around 904L-family chemistry.
Applications of JIS G3463 SUS890LTB Tube
Typical BOM language pairs JIS G3463 SUS890LTB with OD × wall (or schedule), manufacture/finish symbols, and heat-treatment condition. Primary sketch: sulphuric coolers, chemical condensers, and process HX written around 904L-family chemistry. Spool fabricators should copy SUS890LTB onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Application context for SUS890LTB stays sulphuric coolers, chemical condensers, and process HX written around 904L-family chemistry.
Spell SUS890LTB on tube-sheet drawings and bundle lists, bundle sheets and tubesheet specs alike. Sister options when the medium hardens: SUS836LTB, SUS317LTB, SUS312LTB, SUS316LTB. Commissioning teams benefit when the as-built dossier repeats SUS890LTB beside heat numbers, linking isometric revisions to the same mill certificates. Size practice for SUS890LTB remains seamless HX gauges; welded only with qualified high-alloy procedures.
Weldability of JIS G3463 SUS890LTB
Weldability of SUS890LTB follows austenitic practice. Filler/shop note: 904L-class / high-Ni Cu-Mo fillers; control segregation and heat input. Caution: lower Rm/proof floors than many 6Mo marks; confirm Cu 1–2% on the cast line. Procedure qualification for SUS890LTB should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. Keep the SUS890LTB caution visible here: lower Rm/proof floors than many 6Mo marks; confirm Cu 1–2% on the cast line.
For welded G3463 tube, confirm whether as-welded or cold-finished welded finish is acceptable to the corrosion owner. Shop note: 904L-class / high-Ni Cu-Mo fillers; control segregation and heat input. Consumable lot control and shielding-gas notes for SUS890LTB stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Keep the SUS890LTB caution visible here: lower Rm/proof floors than many 6Mo marks; confirm Cu 1–2% on the cast line.
Surface Finishes for JIS G3463 SUS890LTB
Pickled mill finish after solution anneal covers most SUS890LTB RFQs for sulphuric coolers and chemical condensers. Bright anneal, grind, or polish only when the enquiry writes a measurable target and names OD, ID, or both. Sanitary-lean duties may add ID polish; many chemical lines prefer a clean pickle only — state the need on the order so finishing slots match the process, not a catalogue default.
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Usual chemical HX mill finish | Matte, scale-free; Cu confirmed on MTC |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement (often ID for sanitary-lean lines) | Name Ra/grit and which surface |
| Passivated | When end-user chemical specs require it | Not a substitute for solution anneal or Cu-Mo chemistry |
Passivation is a film treatment after correct heat treatment — it will not raise tensile floors or fix a cast that missed copper. Final visual standards reject grinding burns, embedded free iron, and unrepaired undercut; pack SUS890LTB with iron-free, chloride-aware materials before chemical-plant shipment.
Inspection and Testing for JIS G3463 SUS890LTB
SHH STEEL reports the tests actually performed for SUS890LTB — no surrogate NDT lines. Hydrostatic vs eddy-current/ultrasonic choice belongs on the PO. Caution: lower Rm/proof floors than many 6Mo marks; confirm Cu 1–2% on the cast line. Sampling plans for SUS890LTB keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Application context for SUS890LTB stays sulphuric coolers, chemical condensers, and process HX written around 904L-family chemistry.
NDT sensitivity levels and hydrostatic pressures follow the standard tables unless the purchaser specifies higher. Size context: seamless HX gauges; welded only with qualified high-alloy procedures. Non-conforming SUS890LTB lengths are segregated and retested or rejected under retest clauses rather than reworked into unmarked stock. Keep the SUS890LTB caution visible here: lower Rm/proof floors than many 6Mo marks; confirm Cu 1–2% on the cast line.
Packaging and Shipping for JIS G3463 SUS890LTB
Export packing for JIS G3463 SUS890LTB is built around rust prevention and transit abrasion control. Bundle tickets repeat the grade symbol and heat number. Duty: Cu-Mo high-Ni austenitic (~904L class) for sulphuric and chloride chemical HX tube. Bundle tickets for SUS890LTB repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Size practice for SUS890LTB remains seamless HX gauges; welded only with qualified high-alloy procedures.
Marking paint and ink stickers stay chloride-lean. Heat numbers on tags match the MTC for SUS890LTB. Desiccant and wrap choices for SUS890LTB follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Application context for SUS890LTB stays sulphuric coolers, chemical condensers, and process HX written around 904L-family chemistry.
Photographic packing records are available on request for project QA files on SUS890LTB. Claims handling for SUS890LTB starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Keep the SUS890LTB caution visible here: lower Rm/proof floors than many 6Mo marks; confirm Cu 1–2% on the cast line.
Why Choose SHH STEEL
Buyers choose SHH STEEL for SUS890LTB because the paperwork matches the stencil: Table 3 chemistry, Table 4 tensile, Table 2 heat treatment, and honest seamless or A/L/E welded marking. Application fit: sulphuric coolers, chemical condensers, and process HX written around 904L-family chemistry. SHH STEEL can produce and supply SUS890LTB against the OD × wall, process symbol, and test scope on your RFQ without swapping in an unstated sister grade.
SHH STEEL will not invent PREN posters or warehouse tonnages. Bring OD × wall, medium notes, and test scope — we will quote SUS890LTB cleanly. Ask for a written acknowledgement that names SUS890LTB, the manufacture process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS890LTB to that written scope.
Supply Capability
Supply capability for SUS890LTB covers manufacture/finish symbols in Table 1, heat treatment in Table 2, and mechanical acceptance in Table 4. SHH STEEL can make the sizes on your list when the mill slot fits. Role: Cu-Mo high-Ni austenitic (~904L class) for sulphuric and chloride chemical HX tube. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS890LTB when the mill schedule allows. Corrosion framing beside SUS890LTB: Cu + Mo + high Ni helps in reducing acids and many chloride duties; verify temperature limits.
| Item | Capability |
|---|---|
| Standard | JIS G3463 stainless steel tubes for boilers and heat exchangers |
| Grade symbol | SUS890LTB |
| Product form | Seamless (S) and welded (A / L / E) tube; finishes S-H / S-C / A / A-C / E-C as marked |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered) |
| Typical OD practice | 15.9–139.8 mm per standard Note 1; other by agreement |
| Wall / gauge | OD × wall / BWG-class HX gauges within Attached Tables; other by agreement |
Stock / Available sizes
Stock / Available sizes for SUS890LTB: common A-number bores with schedule or measured wall as the project uses. Seamless and welded availability varies by diameter — confirm route with the RFQ. Hint: seamless HX gauges; welded only with qualified high-alloy procedures. SHH STEEL can supply alternate schedules and measured walls for SUS890LTB once the design pressure and corrosion allowance are clear.
Mill certificates, packing photos, and third-party witness can be bundled into the SUS890LTB supply scope when the PO says so. Use: sulphuric coolers, chemical condensers, and process HX written around 904L-family chemistry. SHH STEEL can produce trial lengths of SUS890LTB for procedure qualification before the bulk release when the project calendar needs it.
FAQ
-
What is JIS G3463 SUS890LTB stainless steel tube used for?
- JIS G3463 SUS890LTB is stainless tube for boiler and heat-exchanger service (superheater, HX, condenser, catalyser) — sulphuric coolers, chemical condensers, and process HX written around 904L-family chemistry. Role summary: Cu-Mo high-Ni austenitic (~904L class) for sulphuric and chloride chemical HX tube. It is a Japanese boiler/HX tube product standard mark, not an automatic ASTM A213 certificate.
-
Does JIS G3463 SUS890LTB cover seamless and welded tube?
- Yes. Manufacture allows seamless and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish marks such as S-H, S-C, A-C, or E-C. SHH STEEL can produce and supply either route for SUS890LTB when the mill can meet the ordered size and tests. The title omits Seamless/Welded because JIS G3463 covers both manufacture routes — the PO must still name the process mark.
-
What heat treatment applies to SUS890LTB?
- SUS890LTB is delivered solution annealed under JIS G3463. Table 2 reference: 1030 °C min, rapid cool. Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
-
How does SUS890LTB compare with sister grades SUS836LTB, SUS317LTB, SUS312LTB?
- SUS890LTB is filed as austenitic. Typical sisters on the same RFQ are SUS836LTB, SUS317LTB, SUS312LTB. Design caution: lower Rm/proof floors than many 6Mo marks; confirm Cu 1–2% on the cast line Pick the sister when the medium or strength floor outgrows this symbol rather than stretching wall alone.
-
What tests appear on the mill certificate for SUS890LTB?
- Expect cast analysis (Table 3), room-temperature tensile results (Table 4), flattening/flaring as applicable, dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
-
Is ~904L-class Cu-Mo austenitic (JIS SUS890L) the same as ordering SUS890LTB?
- No. ~904L-class Cu-Mo austenitic (JIS SUS890L) is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3463 and SUS890LTB so cast limits, heat treatment, and process marks are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for JIS G3463 SUS890LTB?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS890LTB within the typical 15.9–139.8 mm OD practice, with measured walls by agreement. Size context: seamless HX gauges; welded only with qualified high-alloy procedures. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
How should SUS890LTB be welded?
- Shop guidance: 904L-class / high-Ni Cu-Mo fillers; control segregation and heat input. Mill heat treatment of seamless or welded tube does not replace a qualified WPS on fabricator joints or tube-to-tubesheet welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: lower Rm/proof floors than many 6Mo marks; confirm Cu 1–2% on the cast line
-
When should I choose a duplex or higher-Mo grade instead of SUS890LTB?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: lower Rm/proof floors than many 6Mo marks; confirm Cu 1–2% on the cast line Sister pointers: SUS836LTB, SUS317LTB, SUS312LTB. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify JIS G3463 SUS890LTB with ASTM A213 or ASME SA213?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3463 SUS890LTB does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What surface finishes are available for SUS890LTB?
- Pickled after heat treatment is the usual HX tube supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS890LTB when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
JIS G3463 SUS890LTB is stainless steel tube for boiler and heat-exchanger service — Cu-Mo high-Ni austenitic (~904L class) for sulphuric and chloride chemical HX tube. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS836LTB, SUS317LTB, SUS312LTB. Related ASTM A213 pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process mark, and medium notes to start the quote.