JIS G3463 SUS329J1TB Stainless Steel Tube
What is JIS G3463 SUS329J1TB Stainless Steel Tube
JIS G3463 is the Japanese Industrial Standard for stainless steel tubes used in boiler and heat-exchanger service (superheater, HX, condenser, catalyser). Grade symbol SUS329J1TB sits in the austenitic-ferritic (duplex) set of Table 1. JIS G3463 SUS329J1TB is the early duplex HX mark — check whether the project actually wants the newer low-carbon 329J3L/J4L sisters before melting.
SHH STEEL can produce and supply JIS G3463 SUS329J1TB as seamless or welded tube across the enquiry OD×wall band, solution-annealed or annealed as Table 2 requires, pickled or bright-finished, and documented on mill test certificates tied to cast analysis and tensile results. Duty focus: legacy duplex HX tube for chloride-lean process coolers with higher strength than austenitics.
Shop language may still say “early JIS duplex (329J1) tube,” yet that commercial alias does not select Japanese cast limits, process symbols, or hydraulic/NDT rules. The purchase order has to name JIS G3463 and SUS329J1TB so the mill applies the correct analysis, heat treatment, mechanical floors, and marking. Design caution: higher carbon than modern L duplex — prefer SUS329J3LTB / SUS329J4LTB for welded chloride duty when the spec allows.
Scope discipline: SUS329J1TB is HX tube product under JIS G3463, not a piping product under JIS G3459 and not an ASTM A213 order by default. Sister marks often compared on the same RFQ include SUS329J3LTB, SUS329J4LTB, SUS316LTB, SUS317LTB. Role reminder: legacy duplex HX tube for chloride-lean process coolers with higher strength than austenitics.
Inside this JIS G3463 series, compare SUS329J3LTB, SUS329J4LTB, SUS316LTB, SUS317LTB. Hub: JIS G3463. ASTM/ASME related product pages (not interchangeable by default): ASTM A213.
Chemical Composition of JIS G3463 SUS329J1TB
Cast analysis for JIS G3463 SUS329J1TB follows Table 3. Key windows on a typical certificate include C ≤0.08, Si ≤1.00, Mn ≤1.50, P ≤0.040, S ≤0.030, Ni 3.00–6.00, Cr 23.00–28.00. SHH STEEL ties the heat number on the tube marking to the same cast line on the MTC. Commercial alias early JIS duplex (329J1) is body text only. Corrosion thread: duplex phase balance gives strength and improved chloride resistance vs 316 in many waters; verify temperature and sour limits.
Chemical limits for SUS329J1TB under JIS G3463 appear in the table underneath. Source priority is the 2021 Table 3 extract cross-checked to public Nikko / supplier tables. If your client specification cites a different edition footnote, send it before the heat is melted. Duty thread: legacy duplex HX tube for chloride-lean process coolers with higher strength than austenitics.
| Grade | C | Si | Mn | P | S | Ni | Cr | Mo |
|---|---|---|---|---|---|---|---|---|
| SUS329J1TB | ≤0.08 | ≤1.00 | ≤1.50 | ≤0.040 | ≤0.030 | 3.00–6.00 | 23.00–28.00 | 1.00–3.00 |
Mechanical Properties of JIS G3463 SUS329J1TB
Ambient tensile floors for SUS329J1TB come from JIS G3463 Table 4: Rm min 588 N/mm², proof stress min 392 N/mm², elongation min 18% (OD ≥20 mm, No.11/12). These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: austenitic-ferritic (duplex). Caution: higher carbon than modern L duplex — prefer SUS329J3LTB / SUS329J4LTB for welded chloride duty when the spec allows.
| Grade | Rm min (N/mm²) | Proof stress min (N/mm²) | A OD≥20 mm No.11/12 min (%) | A 10≤OD<20 mm No.11 min (%) | A OD<10 mm No.11 min (%) |
|---|---|---|---|---|---|
| SUS329J1TB | 588 | 392 | 18 | 13 | 10 |
Ambient values from JIS G3463 Table 4 for SUS329J1TB. Heat treatment (Table 2): 950 °C min, rapid cool. Elongation reductions apply for walls under 8 mm on No.12 pieces. For heat-exchanger tube the purchaser may designate an upper tensile limit (Table 4 min + 200 N/mm²) when necessary.
Manufacture of JIS G3463 SUS329J1TB Tube (Seamless and Welded)
JIS G3463 manufactures SUS329J1TB by seamless (symbol S) or welded routes — automatic arc (A), laser (L), or electric-resistance (E) — then applies the ordered finish: hot finish H, cold finish C, hot finish S-H or cold finish S-C / A-C / E-C as marked. SHH STEEL confirms the Table 1 symbol string on the acknowledgement before rolling or welding starts.
Duplex heats need solution annealing with rapid cooling to restore phase balance — do not skip Table 2 temperatures after hot forming. Heat-treatment reference for SUS329J1TB: 950 °C min, rapid cool. Pickling follows unless bright heat treatment leaves a scale-free surface. Duty thread: legacy duplex HX tube for chloride-lean process coolers with higher strength than austenitics.
When dual documentation against ASTM A213 is requested for a related chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for SUS329J1TB: seamless or welded; keep OD in HX practice and respect duplex bend radii.
Dimensions and Tolerances for JIS G3463 SUS329J1TB
SHH STEEL aligns nominal diameter (A/B), outside diameter, schedule or wall, and length tolerance for SUS329J1TB before the mill slot is locked. Standard Note 1 frames typical OD from 15.9 mm to 139.8 mm (standard Note 1 general practice). Size hint: seamless or welded; keep OD in HX practice and respect duplex bend radii.
Length supply may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against the packaging clause so pickled or polished finishes are not iron-stained in transit. Duty thread: legacy duplex HX tube for chloride-lean process coolers with higher strength than austenitics. Fixed lengths and multiple cut lengths for SUS329J1TB are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Weld-shop note tied to SUS329J1TB: duplex fillers with controlled heat input and ferrite targets; solution anneal after hot forming.
Equivalent Grades for JIS G3463 SUS329J1TB
Equivalence talk for SUS329J1TB starts with early JIS duplex (329J1): that commercial / UNS framing is useful in body text and dual-cert discussions, but the H1 and order line stay on JIS G3463 SUS329J1TB. ASTM A213 / A269 pages that share related chemistry are different product standards with different wall bases, mechanical tables, and tests. Sisters: SUS329J3LTB, SUS329J4LTB, SUS316LTB, SUS317LTB. Caution: higher carbon than modern L duplex — prefer SUS329J3LTB / SUS329J4LTB for welded chloride duty when the spec allows.
Heat Treatment and Delivery Condition for JIS G3463 SUS329J1TB
SUS329J1TB is delivered solution annealed under JIS G3463. Table 2 reference: 950 °C min, rapid cool. Fabricator heat treatment after hot bending should chase the same family practice. Weld thread: duplex fillers with controlled heat input and ferrite targets; solution anneal after hot forming. Recorded furnace charts for SUS329J1TB should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Weld-shop note tied to SUS329J1TB: duplex fillers with controlled heat input and ferrite targets; solution anneal after hot forming.
Cooling type matters — austenitic and duplex need rapid cool after solution treatment; ferritic anneal practice allows rapid or slow cool per Table 2. Duty thread: legacy duplex HX tube for chloride-lean process coolers with higher strength than austenitics. Field heat treatment of SUS329J1TB after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Size practice for SUS329J1TB remains seamless or welded; keep OD in HX practice and respect duplex bend radii.
Corrosion Resistance of JIS G3463 SUS329J1TB
Corrosion behaviour of JIS G3463 SUS329J1TB tracks its austenitic-ferritic (duplex) balance: duplex phase balance gives strength and improved chloride resistance vs 316 in many waters; verify temperature and sour limits. Optional annex corrosion tests (oxalic, Strauss, Huey, etc.) are special quality items — order them when the duty needs coupon evidence. Design caution: higher carbon than modern L duplex — prefer SUS329J3LTB / SUS329J4LTB for welded chloride duty when the spec allows.
For heat-facing austenitics, oxidation resistance may dominate over aqueous IGC talk; for duplex and Mo austenitics, chlorides dominate; for ferritics, mild aqueous and weld practice dominate. SUS329J1TB is filed as austenitic-ferritic (duplex). Caution: higher carbon than modern L duplex — prefer SUS329J3LTB / SUS329J4LTB for welded chloride duty when the spec allows.
Applications of JIS G3463 SUS329J1TB Tube
Applications of JIS G3463 SUS329J1TB tube centre on process coolers, water exchangers, and older Japanese duplex HX specs that still name 329J1. Role summary: legacy duplex HX tube for chloride-lean process coolers with higher strength than austenitics. When a related chemistry is required under ASTM A213 or A269, open those sister pages — acceptance text is not automatic.
Downstream fabricators should inherit the same grade symbol on cut lists so informal alias substitutions do not creep in. Primary application sketch: process coolers, water exchangers, and older Japanese duplex HX specs that still name 329J1. Duty thread: legacy duplex HX tube for chloride-lean process coolers with higher strength than austenitics. Commissioning teams benefit when the as-built dossier repeats SUS329J1TB beside heat numbers, linking isometric revisions to the same mill certificates. Corrosion framing beside SUS329J1TB: duplex phase balance gives strength and improved chloride resistance vs 316 in many waters; verify temperature and sour limits.
Weldability of JIS G3463 SUS329J1TB
SUS329J1TB is welded both as a mill product (A/L/E routes) and as fabricator joints on bundles. Shop guidance: duplex fillers with controlled heat input and ferrite targets; solution anneal after hot forming. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Procedure qualification for SUS329J1TB should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. Weld-shop note tied to SUS329J1TB: duplex fillers with controlled heat input and ferrite targets; solution anneal after hot forming.
Filler selection should match or over-alloy the base chemistry as the WPS demands. Heat input, interpass temperature, and shielding follow the family — austenitic, duplex, or ferritic — not a single shop habit. Caution: higher carbon than modern L duplex — prefer SUS329J3LTB / SUS329J4LTB for welded chloride duty when the spec allows.
Surface Finishes for JIS G3463 SUS329J1TB
Surface supply for SUS329J1TB is typically pickled after heat treatment, or bright-annealed when scale-free OD/ID is ordered. Polished or special roughness finishes are by agreement and must state which surface (OD, ID, or both) is in scope. Duty: legacy duplex HX tube for chloride-lean process coolers with higher strength than austenitics. Roughness or polish callouts for SUS329J1TB must name OD, ID, or both; ambiguous “bright tube” language is clarified before finishing slots are booked. Corrosion framing beside SUS329J1TB: duplex phase balance gives strength and improved chloride resistance vs 316 in many waters; verify temperature and sour limits.
Passivation treatments, when ordered, follow agreed ASTM A967 / JIS practice analogues — they are not a substitute for correct heat treatment. Caution: higher carbon than modern L duplex — prefer SUS329J3LTB / SUS329J4LTB for welded chloride duty when the spec allows. Final visual standards for SUS329J1TB reject grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed. Keep the SUS329J1TB caution visible here: higher carbon than modern L duplex — prefer SUS329J3LTB / SUS329J4LTB for welded chloride duty when the spec allows.
Inspection and Testing for JIS G3463 SUS329J1TB
Inspection for JIS G3463 SUS329J1TB covers cast analysis, tensile tests, flattening or weld bend as applicable, hydrostatic test or NDT, dimensions, and appearance. Special quality annex items (IGC, grain size, etc.) apply only when ordered. Documents follow JIS G 0415 / purchaser-specified EN 10204 styles. Sampling plans for SUS329J1TB keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. This paragraph is locked to SUS329J1TB duty: legacy duplex HX tube for chloride-lean process coolers with higher strength than austenitics.
Marking includes SUS329J1TB, manufacture/finish symbols, manufacturer, and other mandatory marking-clause data. Traceability from stencil to MTC is part of supply, not an upgrade. Use: process coolers, water exchangers, and older Japanese duplex HX specs that still name 329J1. Non-conforming SUS329J1TB lengths are segregated and retested or rejected under retest clauses rather than reworked into unmarked stock. Keep the SUS329J1TB caution visible here: higher carbon than modern L duplex — prefer SUS329J3LTB / SUS329J4LTB for welded chloride duty when the spec allows.
Packaging and Shipping for JIS G3463 SUS329J1TB
Packaging for SUS329J1TB uses wooden boxes, plywood cases, or bundled frames with waterproof wrapping as the OD and finish demand. Soft separators protect pickled and polished surfaces. Ends receive caps or bevel protectors when ordered. Bundle tickets for SUS329J1TB repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Corrosion framing beside SUS329J1TB: duplex phase balance gives strength and improved chloride resistance vs 316 in many waters; verify temperature and sour limits.
Carbon-steel strapping never contacts the stainless OD without a barrier. Mixed-grade bundles are forbidden when chemistry integrity matters. Caution: higher carbon than modern L duplex — prefer SUS329J3LTB / SUS329J4LTB for welded chloride duty when the spec allows. Desiccant and wrap choices for SUS329J1TB follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Weld-shop note tied to SUS329J1TB: duplex fillers with controlled heat input and ferrite targets; solution anneal after hot forming.
Shipping documents list JIS G3463, SUS329J1TB, sizes, quantities, heat numbers, and certificate type. SHH STEEL coordinates inland trucking and FOB/CIF packing scopes as the order states. Role: legacy duplex HX tube for chloride-lean process coolers with higher strength than austenitics. Claims handling for SUS329J1TB starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Corrosion framing beside SUS329J1TB: duplex phase balance gives strength and improved chloride resistance vs 316 in many waters; verify temperature and sour limits.
Why Choose SHH STEEL
SHH STEEL can produce and supply JIS G3463 SUS329J1TB with the process route, heat treatment, and tests named on your enquiry — not a bait-and-switch alias. Mill partners run stainless tube capacity that covers seamless and welded Table 1 symbols for this mark. Duty focus: legacy duplex HX tube for chloride-lean process coolers with higher strength than austenitics.
Technical sales can map SUS329J1TB against sisters SUS329J3LTB, SUS329J4LTB, SUS316LTB, SUS317LTB and live ASTM pages without pretending standards are identical. Inspection coordination and export packing are in-house habits, not afterthoughts. Ask for a written acknowledgement that names SUS329J1TB, the manufacture process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS329J1TB to that written scope.
Supply Capability
SHH STEEL can produce and supply JIS G3463 SUS329J1TB across enquiry-oriented OD × wall bands, in seamless or welded routes, with certificates and optional annex tests as ordered. Summary capability follows in the table; stock language below is an RFQ map, not a frozen tonnage catalogue. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS329J1TB when the mill schedule allows.
| Item | Capability |
|---|---|
| Standard | JIS G3463 stainless steel tubes for boilers and heat exchangers |
| Grade symbol | SUS329J1TB |
| Product form | Seamless (S) and welded (A / L / E) tube; finishes S-H / S-C / A / A-C / E-C as marked |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered) |
| Typical OD practice | 15.9–139.8 mm per standard Note 1; other by agreement |
| Wall / gauge | OD × wall / BWG-class HX gauges within Attached Tables; other by agreement |
Stock / Available sizes
SHH STEEL can produce and supply JIS G3463 SUS329J1TB. Stock / Available sizes: enquiry band typically aligns with 15.9–139.8 mm OD practice under G3463 Note 1, with OD×wall HX gauges; schedule 5S–80 (and heavier by agreement) depending on grade family. For SUS329J1TB, practical fast-track sizes often sit in mid-bore process and utility ranges — send the OD × wall list for a firm acknowledgement. Context: seamless or welded; keep OD in HX practice and respect duplex bend radii.
Cut lengths, bevels, special NDT, and IGC annex tests add lead time — call them early. Sisters often quoted alongside: SUS329J3LTB, SUS329J4LTB, SUS316LTB, SUS317LTB. Email the size list to start. SHH STEEL can produce trial lengths of SUS329J1TB for procedure qualification before the bulk release when the project calendar needs it. SHH STEEL can produce trial lengths of SUS329J1TB for procedure qualification before bulk release when the project calendar needs it. This paragraph is locked to SUS329J1TB duty: legacy duplex HX tube for chloride-lean process coolers with higher strength than austenitics.
FAQ
-
What is JIS G3463 SUS329J1TB stainless steel tube used for?
- JIS G3463 SUS329J1TB is stainless tube for boiler and heat-exchanger service (superheater, HX, condenser, catalyser) — process coolers, water exchangers, and older Japanese duplex HX specs that still name 329J1. Role summary: legacy duplex HX tube for chloride-lean process coolers with higher strength than austenitics. It is a Japanese boiler/HX tube product standard mark, not an automatic ASTM A213 certificate.
-
Does JIS G3463 SUS329J1TB cover seamless and welded tube?
- Yes. Manufacture allows seamless and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish marks such as S-H, S-C, A-C, or E-C. SHH STEEL can produce and supply either route for SUS329J1TB when the mill can meet the ordered size and tests. The title omits Seamless/Welded because JIS G3463 covers both manufacture routes — the PO must still name the process mark.
-
What heat treatment applies to SUS329J1TB?
- SUS329J1TB is delivered solution annealed under JIS G3463. Table 2 reference: 950 °C min, rapid cool. Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
-
How does SUS329J1TB compare with sister grades SUS329J3LTB, SUS329J4LTB, SUS316LTB?
- SUS329J1TB is filed as austenitic-ferritic (duplex). Typical sisters on the same RFQ are SUS329J3LTB, SUS329J4LTB, SUS316LTB. Design caution: higher carbon than modern L duplex — prefer SUS329J3LTB / SUS329J4LTB for welded chloride duty when the spec allows Pick the sister when the medium or strength floor outgrows this symbol rather than stretching wall alone.
-
What tests appear on the mill certificate for SUS329J1TB?
- Expect cast analysis (Table 3), room-temperature tensile results (Table 4), flattening/flaring as applicable, dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
-
Is early JIS duplex (329J1) the same as ordering SUS329J1TB?
- No. early JIS duplex (329J1) is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3463 and SUS329J1TB so cast limits, heat treatment, and process marks are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for JIS G3463 SUS329J1TB?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS329J1TB within the typical 15.9–139.8 mm OD practice, with measured walls by agreement. Size context: seamless or welded; keep OD in HX practice and respect duplex bend radii. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
How should SUS329J1TB be welded?
- Shop guidance: duplex fillers with controlled heat input and ferrite targets; solution anneal after hot forming. Mill heat treatment of seamless or welded tube does not replace a qualified WPS on fabricator joints or tube-to-tubesheet welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: higher carbon than modern L duplex — prefer SUS329J3LTB / SUS329J4LTB for welded chloride duty when the spec allows
-
When should I choose a duplex or higher-Mo grade instead of SUS329J1TB?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic-ferritic (duplex) practice can defend for the temperature and stress state. Caution for this mark: higher carbon than modern L duplex — prefer SUS329J3LTB / SUS329J4LTB for welded chloride duty when the spec allows Sister pointers: SUS329J3LTB, SUS329J4LTB, SUS316LTB. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify JIS G3463 SUS329J1TB with ASTM A213 or ASME SA213?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3463 SUS329J1TB does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What surface finishes are available for SUS329J1TB?
- Pickled after heat treatment is the usual HX tube supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS329J1TB when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
JIS G3463 SUS329J1TB is stainless steel tube for boiler and heat-exchanger service — legacy duplex HX tube for chloride-lean process coolers with higher strength than austenitics. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS329J3LTB, SUS329J4LTB, SUS316LTB. Related ASTM A213 pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process mark, and medium notes to start the quote.