JIS G3463 SUS444TB Stainless Steel Tube | JIS G3463 Stainless Steel Tube - SHH STEEL

JIS G3463 SUS444TB Stainless Steel Tube

JIS G3463 SUS444TB stainless steel tube (444 / UNS S44400), ferritic, Table 3 cast analysis, Rm min 412 N/mm² / proof min 245 N/mm², annealed. SHH STEEL can produce and supply seamless or welded routes with mill certificates.
Grade
SUS444TB (444 / UNS S44400 — body alias)
Standard
JIS G3463
Product form
Seamless and welded stainless steel boiler/HX tube, delivery annealed
Size
Typically OD 15.9–139.8 mm (Note 1); OD × wall (HX/boiler gauges) by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is JIS G3463 SUS444TB Stainless Steel Tube

JIS G3463 covers both seamless and welded stainless tube for process, utility, condenser and heat-exchange duties. Inside that standard, SUS444TB is filed as ferritic. JIS G3463 SUS444TB is the nickel-saving Mo ferritic HX answer when 316L is overkill on alloy cost but 430 is not enough on chlorides. Buyers working Japanese boiler and HX packages should treat SUS444TB as a governed product symbol under G3463, with Table 3 chemistry and Table 4 tensile floors enforced on the same heat. Corrosion framing beside SUS444TB: ~2% Mo + stabilisation often rivals 316L in many fresh/mild chloride waters — coupon the real medium.

From pierce/draw or weld-and-anneal through marking and bundle protection, SHH STEEL can produce JIS G3463 SUS444TB for the sizes and tests on your RFQ. Application sketch: water heaters, mild chloride coolers, food/water exchangers, and nickel-saving HX bundles. Size and test clarity on the RFQ lets SHH STEEL lock the correct Table 1 symbols for SUS444TB before production starts. Corrosion framing beside SUS444TB: ~2% Mo + stabilisation often rivals 316L in many fresh/mild chloride waters — coupon the real medium.

On the floor people shorten marks; in QA they must not. SUS444TB under JIS G3463 carries specific Table 3 windows and Table 4 floors that a loose “444” note will not enforce. Caution: ferritic fabrication rules still apply; verify toughness and weld procedures; not automatic seawater duty. Keep isometric notes, tubesheet specs, and the mill acknowledgement aligned on SUS444TB so informal alias language cannot reopen the carbon or molybdenum window after melt. Keep the SUS444TB caution visible here: ferritic fabrication rules still apply; verify toughness and weld procedures; not automatic seawater duty.

Superheater, condenser and corrosive HX duties all sit in G3463’s scope statement; still match the alloy to the medium. For SUS444TB, that means: Mo-stabilised ferritic approaching 316L aqueous performance in many HX duties without nickel. Nearby marks: SUS436LTB, SUS430LXTB, SUS316LTB, SUS430J1LTB. Document the medium, design temperature, and weld map beside the SUS444TB line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Application context for SUS444TB stays water heaters, mild chloride coolers, food/water exchangers, and nickel-saving HX bundles.

Inside this JIS G3463 series, compare SUS436LTB, SUS430LXTB, SUS316LTB, SUS430J1LTB. Hub: JIS G3463. ASTM/ASME related product pages (not interchangeable by default): ASTM A213.

Chemical Composition of JIS G3463 SUS444TB

For SUS444TB, the melt ticket has to show Table 3 compliance — C ≤0.025, Si ≤0.75, Mn ≤1.00, P ≤0.040, S ≤0.030, Cr 17.00–20.00, Mo 1.75–2.50. Optional alloying footnotes in the standard still forbid blurring grade identity. Corrosion framing: ~2% Mo + stabilisation often rivals 316L in many fresh/mild chloride waters — coupon the real medium.

Where Mo, Cu, Ti, Nb or N appear, they are intentional levers for SUS444TB, not optional marketing. Confirm them on the MTC line-by-line. Role: Mo-stabilised ferritic approaching 316L aqueous performance in many HX duties without nickel. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for SUS444TB before the order is acknowledged. Keep the SUS444TB caution visible here: ferritic fabrication rules still apply; verify toughness and weld procedures; not automatic seawater duty.

Grade C Si Mn P S Cr Mo Ti/Nb/Zr
SUS444TB ≤0.025 ≤0.75 ≤1.00 ≤0.040 ≤0.030 17.00–20.00 1.75–2.50 8×(C%+N%)–0.80

Mechanical Properties of JIS G3463 SUS444TB

Do not confuse Table 4 tube tensile floors with plate or tube standards that share the 444 / UNS S44400 alias. For SUS444TB under G3463 expect Rm min 412 N/mm², proof stress min 245 N/mm², elongation min 20% (OD ≥20 mm, No.11/12), verified per heat/lot rules in tensile sampling clauses. Tensile sampling follows tensile sampling clauses for the ordered test unit of SUS444TB, and retests follow retest clauses when a result sits under the Table 4 floor. Application context for SUS444TB stays water heaters, mild chloride coolers, food/water exchangers, and nickel-saving HX bundles.

Grade Rm min (N/mm²) Proof stress min (N/mm²) A OD≥20 mm No.11/12 min (%) A 10≤OD<20 mm No.11 min (%) A OD<10 mm No.11 min (%)
SUS444TB 412 245 20 15 12

Ambient values from JIS G3463 Table 4 for SUS444TB. Heat treatment (Table 2): 700 °C min, air or slow cool. Elongation reductions apply for walls under 8 mm on No.12 pieces. For heat-exchanger tube the purchaser may designate an upper tensile limit (Table 4 min + 200 N/mm²) when necessary.

Manufacture of JIS G3463 SUS444TB Tube (Seamless and Welded)

JIS G3463 manufactures SUS444TB by seamless (symbol S) or welded routes — automatic arc (A), laser (L), or electric-resistance (E) — then applies the ordered finish: hot finish H, cold finish C, hot finish S-H or cold finish S-C / A-C / E-C as marked. SHH STEEL confirms the Table 1 symbol string on the acknowledgement before rolling or welding starts.

Welded SUS444TB needs weld-bead work or as-welded finish called out (as-welded vs cold-finished welded) so NDT and corrosion expectations match. Heat treatment: 700 °C min, air or slow cool. Ferritic heats are annealed (700 °C min, or 720 °C min for SUS430J1LTB) with rapid or slow cooling as Table 2 allows — not austenitic solution practice.

Hydrostatic testing or NDT (eddy current / ultrasonic per JIS G 0582/0583) replaces or accompanies pressure proof as the order states. Manufacture stays honest to the seamless or A/L/E welded choice. Size: common water-heater and cooler OD×wall bands; welded or seamless. Hydrostatic pressure or NDT class for SUS444TB is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. This paragraph is locked to SUS444TB duty: Mo-stabilised ferritic approaching 316L aqueous performance in many HX duties without nickel.

Dimensions and Tolerances for JIS G3463 SUS444TB

Out-of-table OD×wall combinations are by agreement — still under the same grade symbol SUS444TB. Duty: Mo-stabilised ferritic approaching 316L aqueous performance in many HX duties without nickel. Tolerance class follows the process route ordered for SUS444TB, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Corrosion framing beside SUS444TB: ~2% Mo + stabilisation often rivals 316L in many fresh/mild chloride waters — coupon the real medium.

Ovality, wall eccentricity (where applicable), and weld bead height limits are part of dimensional tolerance clauses — not optional cosmetics. Size reminder: common water-heater and cooler OD×wall bands; welded or seamless. Fixed lengths and multiple cut lengths for SUS444TB are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Application context for SUS444TB stays water heaters, mild chloride coolers, food/water exchangers, and nickel-saving HX bundles.

Equivalent Grades for JIS G3463 SUS444TB

JIS G3463 SUS444TB is the Mo-stabilised ferritic heat-exchanger tube grade that, in many aqueous duties, approaches 316L performance without the nickel bill. Commercial / UNS framing as 444 / UNS S44400 belongs in body text and dual-cert discussions only; the H1 and order line stay on SUS444TB. ASTM A268 TP444 and similar tube pages share chemistry kinship but remain different product standards — wall basis, mechanical table, and tests do not transfer by default.

System Designation Notes
JIS G3463 SUS444TB Governing HX/boiler tube grade for this page
Commercial / UNS (body only) 444 / UNS S44400 Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A268 related TP444 / S44400 ferritic tube family Related chemistry — different product standard; not interchangeable by default
EN / other 1.4521 (X2CrMoTi18-2) approximate wrought name Starting point for comparison only; no automatic tube dual-cert

Ferritic fabrication rules still apply: verify toughness and weld procedures, and do not treat SUS444TB as automatic seawater duty. Sisters: SUS436LTB, SUS430LXTB, SUS430J1LTB; austenitic neighbour often compared on price/performance: SUS316LTB. Series hub: JIS G3463.

Heat Treatment and Delivery Condition for JIS G3463 SUS444TB

Hot-finished seamless austenitics may use in-line rapid cool in lieu of a separate solution treatment under Table 2 note (a) unless the purchaser forbids it. Confirm for SUS444TB. Band: 700 °C min, air or slow cool. Recorded furnace charts for SUS444TB should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Application context for SUS444TB stays water heaters, mild chloride coolers, food/water exchangers, and nickel-saving HX bundles.

Grain-size testing applies where the standard requires it for specific H grades — state any extra metallographic demand on the PO for SUS444TB. Field heat treatment of SUS444TB after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Corrosion framing beside SUS444TB: ~2% Mo + stabilisation often rivals 316L in many fresh/mild chloride waters — coupon the real medium.

Corrosion Resistance of JIS G3463 SUS444TB

Medium, temperature, crevice geometry and weld condition decide whether SUS444TB is enough. Summary: ~2% Mo + stabilisation often rivals 316L in many fresh/mild chloride waters — coupon the real medium. Escalate via sisters SUS436LTB, SUS430LXTB, SUS316LTB, SUS430J1LTB when coupons fail. Coupon orientation, weld condition, and surface finish for SUS444TB belong in the corrosion test order so annex results can be compared to the installed bundle honestly. This paragraph is locked to SUS444TB duty: Mo-stabilised ferritic approaching 316L aqueous performance in many HX duties without nickel.

Surface finish and iron contamination control often matter as much as bulk chemistry on sanitary-lean duties for SUS444TB. Corrosion framing: ~2% Mo + stabilisation often rivals 316L in many fresh/mild chloride waters — coupon the real medium. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for SUS444TB rather than relying on schedule thickness alone. Weld-shop note tied to SUS444TB: 444/stabilised Mo ferritic fillers; strict heat-input control.

Applications of JIS G3463 SUS444TB Tube

From utility rooms to process racks, SUS444TB shows up wherever Japanese boiler/HX specs want ferritic behaviour. Use list: water heaters, mild chloride coolers, food/water exchangers, and nickel-saving HX bundles. Spool fabricators should copy SUS444TB onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Corrosion framing beside SUS444TB: ~2% Mo + stabilisation often rivals 316L in many fresh/mild chloride waters — coupon the real medium.

If the only reason for SUS444TB is “we always used this alias,” reopen the corrosion file before repeating the order. Caution: ferritic fabrication rules still apply; verify toughness and weld procedures; not automatic seawater duty. Commissioning teams benefit when the as-built dossier repeats SUS444TB beside heat numbers, linking isometric revisions to the same mill certificates. This paragraph is locked to SUS444TB duty: Mo-stabilised ferritic approaching 316L aqueous performance in many HX duties without nickel.

Weldability of JIS G3463 SUS444TB

Automatic mill welds and manual field welds need different procedure packs, but both must respect SUS444TB chemistry. Guidance: 444/stabilised Mo ferritic fillers; strict heat-input control. Procedure qualification for SUS444TB should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. Application context for SUS444TB stays water heaters, mild chloride coolers, food/water exchangers, and nickel-saving HX bundles.

Ferrite control on duplex SUS444TB and hot-crack control on high-Ni austenitics are procedure items, not afterthoughts. Guidance: 444/stabilised Mo ferritic fillers; strict heat-input control. Consumable lot control and shielding-gas notes for SUS444TB stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Corrosion framing beside SUS444TB: ~2% Mo + stabilisation often rivals 316L in many fresh/mild chloride waters — coupon the real medium.

Surface Finishes for JIS G3463 SUS444TB

SUS444TB for aqueous HX is normally annealed and pickled after heat treatment so the Mo-stabilised surface is scale-free before bundle assembly. Bright anneal is quoted when scale-free OD/ID appearance is written; ground or polished finishes follow agreed Ra or grit on the named surface. Because this grade is often picked as a nickel-saving alternative to 316L in coolers, finish scope (OD versus ID) should be as explicit as the chemistry line.

Finish Typical supply Order note
Annealed and pickled Standard HX/boiler tube mill finish Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface
Passivated When end-user chloride specs require it Not a substitute for correct anneal or Mo/Ti-Nb control

Passivation after pickle or fabrication welding is good practice in chloride-lean aqueous service, but it never replaces the anneal that qualifies SUS444TB under G3463. Reject grinding burns, embedded free iron, and unrepaired weld undercut; pack with iron-free materials so Mo ferritic OD does not leave stained.

Inspection and Testing for JIS G3463 SUS444TB

Third-party witness (SGS/TUV-style) is available when the project mandate requires it. Base acceptance still tracks G3463 for SUS444TB. Sampling plans for SUS444TB keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Weld-shop note tied to SUS444TB: 444/stabilised Mo ferritic fillers; strict heat-input control.

Dimensional inspection against dimensional tolerance clauses tolerances closes the lot. Failures retest per retest clauses — they are not silently shipped. Role: Mo-stabilised ferritic approaching 316L aqueous performance in many HX duties without nickel. Non-conforming SUS444TB lengths are segregated and retested or rejected under retest clauses rather than reworked into unmarked stock. Application context for SUS444TB stays water heaters, mild chloride coolers, food/water exchangers, and nickel-saving HX bundles.

Packaging and Shipping for JIS G3463 SUS444TB

Seaworthy packing is available for ocean legs — desiccant, VCI, and wrap specs by agreement. Grade mark SUS444TB stays visible on outer tags. Bundle tickets for SUS444TB repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Corrosion framing beside SUS444TB: ~2% Mo + stabilisation often rivals 316L in many fresh/mild chloride waters — coupon the real medium.

Container loading plans should keep heavy schedules from crushing thin-wall SUS444TB layers. Desiccant and wrap choices for SUS444TB follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Keep the SUS444TB caution visible here: ferritic fabrication rules still apply; verify toughness and weld procedures; not automatic seawater duty.

Shortages or transit damage claims need photos against the packing list before installation starts — tag identity must still read SUS444TB. Claims handling for SUS444TB starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Application context for SUS444TB stays water heaters, mild chloride coolers, food/water exchangers, and nickel-saving HX bundles.

Why Choose SHH STEEL

From RFQ clarification through MTC release, SHH STEEL treats SUS444TB as a governed product symbol, not a marketing synonym for 444 / UNS S44400. Role: Mo-stabilised ferritic approaching 316L aqueous performance in many HX duties without nickel. SHH STEEL can produce and supply SUS444TB against the OD × wall, process symbol, and test scope on your RFQ without swapping in an unstated sister grade.

Response time stays short because common SUS444TB enquiry sizes and document packs are already exercised on prior Japanese-spec orders. Use: water heaters, mild chloride coolers, food/water exchangers, and nickel-saving HX bundles. Ask for a written acknowledgement that names SUS444TB, the manufacture process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS444TB to that written scope.

Supply Capability

Capability framing for SUS444TB: Japanese-spec HX tube product, dual-route manufacture, documented heats. Caution remains: ferritic fabrication rules still apply; verify toughness and weld procedures; not automatic seawater duty. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS444TB when the mill schedule allows. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS444TB when the mill schedule allows. This paragraph is locked to SUS444TB duty: Mo-stabilised ferritic approaching 316L aqueous performance in many HX duties without nickel.

Item Capability
Standard JIS G3463 stainless steel tubes for boilers and heat exchangers
Grade symbol SUS444TB
Product form Seamless (S) and welded (A / L / E) tube; finishes S-H / S-C / A / A-C / E-C as marked
Delivery condition annealed
Documents Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered)
Typical OD practice 15.9–139.8 mm per standard Note 1; other by agreement
Wall / gauge OD × wall / BWG-class HX gauges within Attached Tables; other by agreement

Stock / Available sizes

Stock / Available sizes — treat published ranges as capability envelopes. Actual ex-stock pieces of SUS444TB change weekly; the reliable path is an OD × wall matrix on the enquiry. Duty: Mo-stabilised ferritic approaching 316L aqueous performance in many HX duties without nickel. SHH STEEL can supply alternate schedules and measured walls for SUS444TB once the design pressure and corrosion allowance are clear.

Repeat orders for SUS444TB go faster when prior heat records and accepted WPS numbers are referenced on the new RFQ. Role: Mo-stabilised ferritic approaching 316L aqueous performance in many HX duties without nickel. SHH STEEL can produce trial lengths of SUS444TB for procedure qualification before the bulk release when the project calendar needs it.

FAQ

What is JIS G3463 SUS444TB stainless steel tube used for?
JIS G3463 SUS444TB is stainless tube for boiler and heat-exchanger service (superheater, HX, condenser, catalyser) — water heaters, mild chloride coolers, food/water exchangers, and nickel-saving HX bundles. Role summary: Mo-stabilised ferritic approaching 316L aqueous performance in many HX duties without nickel. It is a Japanese boiler/HX tube product standard mark, not an automatic ASTM A213 certificate.
Does JIS G3463 SUS444TB cover seamless and welded tube?
Yes. Manufacture allows seamless and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish marks such as S-H, S-C, A-C, or E-C. SHH STEEL can produce and supply either route for SUS444TB when the mill can meet the ordered size and tests. The title omits Seamless/Welded because JIS G3463 covers both manufacture routes — the PO must still name the process mark.
What heat treatment applies to SUS444TB?
SUS444TB is delivered annealed under JIS G3463. Table 2 reference: 700 °C min, air or slow cool. Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
How does SUS444TB compare with sister grades SUS436LTB, SUS430LXTB, SUS316LTB?
SUS444TB is filed as ferritic. Typical sisters on the same RFQ are SUS436LTB, SUS430LXTB, SUS316LTB. Design caution: ferritic fabrication rules still apply; verify toughness and weld procedures; not automatic seawater duty Pick the sister when the medium or strength floor outgrows this symbol rather than stretching wall alone.
What tests appear on the mill certificate for SUS444TB?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), flattening/flaring as applicable, dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
Is 444 / UNS S44400 the same as ordering SUS444TB?
No. 444 / UNS S44400 is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3463 and SUS444TB so cast limits, heat treatment, and process marks are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for JIS G3463 SUS444TB?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS444TB within the typical 15.9–139.8 mm OD practice, with measured walls by agreement. Size context: common water-heater and cooler OD×wall bands; welded or seamless. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should SUS444TB be welded?
Shop guidance: 444/stabilised Mo ferritic fillers; strict heat-input control. Mill heat treatment of seamless or welded tube does not replace a qualified WPS on fabricator joints or tube-to-tubesheet welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: ferritic fabrication rules still apply; verify toughness and weld procedures; not automatic seawater duty
When should I choose a duplex or higher-Mo grade instead of SUS444TB?
Move when chloride pitting, crevice attack, or SCC risk exceeds what ferritic practice can defend for the temperature and stress state. Caution for this mark: ferritic fabrication rules still apply; verify toughness and weld procedures; not automatic seawater duty Sister pointers: SUS436LTB, SUS430LXTB, SUS316LTB. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify JIS G3463 SUS444TB with ASTM A213 or ASME SA213?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3463 SUS444TB does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for SUS444TB?
Pickled after heat treatment is the usual HX tube supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS444TB when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

JIS G3463 SUS444TB is stainless steel tube for boiler and heat-exchanger service — Mo-stabilised ferritic approaching 316L aqueous performance in many HX duties without nickel. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS436LTB, SUS430LXTB, SUS316LTB. Related ASTM A213 pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process mark, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X