JIS G3463 SUS309STB Stainless Steel Tube
What is JIS G3463 SUS309STB Stainless Steel Tube
JIS G3463 covers both seamless and welded stainless tube for process, utility, condenser and heat-exchange duties. Inside that standard, SUS309STB is filed as austenitic. When the drawing says 309 but the shop will weld extensively, JIS G3463 SUS309STB is usually the safer product symbol than SUS309TB. Buyers working Japanese boiler and HX packages should treat SUS309STB as a governed product symbol under G3463, with Table 3 chemistry and Table 4 tensile floors enforced on the same heat. Corrosion framing beside SUS309STB: retains 309-class oxidation resistance with a tighter carbon ceiling that helps weld-zone stability on U-bends.
From pierce/draw or weld-and-anneal through marking and bundle protection, SHH STEEL can produce JIS G3463 SUS309STB for the sizes and tests on your RFQ. Application sketch: heat-treatment furnace coolers, incinerator interconnect exchangers, hot-gas transfer HX, and welded heat-facing bundles that also see condensate. Size and test clarity on the RFQ lets SHH STEEL lock the correct Table 1 symbols for SUS309STB before production starts. Size practice for SUS309STB remains both seamless S and automatic-arc A are common; specify finish H or C with the enquiry OD×wall.
On the floor people shorten marks; in QA they must not. SUS309STB under JIS G3463 carries specific Table 3 windows and Table 4 floors that a loose “309S” note will not enforce. Caution: still not a chloride-process first choice — move to Mo austenitic or duplex when pitting governs. Keep isometric notes, tubesheet specs, and the mill acknowledgement aligned on SUS309STB so informal alias language cannot reopen the carbon or molybdenum window after melt. Size practice for SUS309STB remains both seamless S and automatic-arc A are common; specify finish H or C with the enquiry OD×wall.
Superheater, condenser and corrosive HX duties all sit in G3463’s scope statement; still match the alloy to the medium. For SUS309STB, that means: lower-carbon 309S austenitic HX tube for oxidation service with better as-welded aqueous behaviour than high-C 309. Nearby marks: SUS309TB, SUS310STB, SUS304TB, SUS321TB. Document the medium, design temperature, and weld map beside the SUS309STB line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Corrosion framing beside SUS309STB: retains 309-class oxidation resistance with a tighter carbon ceiling that helps weld-zone stability on U-bends.
Inside this JIS G3463 series, compare SUS309TB, SUS310STB, SUS304TB, SUS321TB. Hub: JIS G3463. ASTM/ASME related product pages (not interchangeable by default): A213 TP309S, ASTM A213.
Chemical Composition of JIS G3463 SUS309STB
For SUS309STB, the melt ticket has to show Table 3 compliance — C ≤0.08, Si ≤1.00, Mn ≤2.00, P ≤0.040, S ≤0.030, Ni 12.00–15.00, Cr 22.00–24.00. Optional alloying footnotes in the standard still forbid blurring grade identity. Corrosion framing: retains 309-class oxidation resistance with a tighter carbon ceiling that helps weld-zone stability on U-bends.
Where Mo, Cu, Ti, Nb or N appear, they are intentional levers for SUS309STB, not optional marketing. Confirm them on the MTC line-by-line. Role: lower-carbon 309S austenitic HX tube for oxidation service with better as-welded aqueous behaviour than high-C 309. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for SUS309STB before the order is acknowledged. Weld-shop note tied to SUS309STB: 309L fillers preferred; verify ferrite balance on heavy sections before production welding.
| Grade | C | Si | Mn | P | S | Ni | Cr |
|---|---|---|---|---|---|---|---|
| SUS309STB | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.040 | ≤0.030 | 12.00–15.00 | 22.00–24.00 |
Mechanical Properties of JIS G3463 SUS309STB
Do not confuse Table 4 tube tensile floors with plate or tube standards that share the 309S / UNS S30908 alias. For SUS309STB under G3463 expect Rm min 520 N/mm², proof stress min 206 N/mm², elongation min 35% (OD ≥20 mm, No.11/12), verified per heat/lot rules in tensile sampling clauses. Tensile sampling follows tensile sampling clauses for the ordered test unit of SUS309STB, and retests follow retest clauses when a result sits under the Table 4 floor. Application context for SUS309STB stays heat-treatment furnace coolers, incinerator interconnect exchangers, hot-gas transfer HX, and welded heat-facing bundles that also see condensate.
| Grade | Rm min (N/mm²) | Proof stress min (N/mm²) | A OD≥20 mm No.11/12 min (%) | A 10≤OD<20 mm No.11 min (%) | A OD<10 mm No.11 min (%) |
|---|---|---|---|---|---|
| SUS309STB | 520 | 206 | 35 | 30 | 27 |
Ambient values from JIS G3463 Table 4 for SUS309STB. Heat treatment (Table 2): 1030 °C min, rapid cool. Elongation reductions apply for walls under 8 mm on No.12 pieces. For heat-exchanger tube the purchaser may designate an upper tensile limit (Table 4 min + 200 N/mm²) when necessary.
Manufacture of JIS G3463 SUS309STB Tube (Seamless and Welded)
JIS G3463 manufactures SUS309STB by seamless (symbol S) or welded routes — automatic arc (A), laser (L), or electric-resistance (E) — then applies the ordered finish: hot finish H, cold finish C, hot finish S-H or cold finish S-C / A-C / E-C as marked. SHH STEEL confirms the Table 1 symbol string on the acknowledgement before rolling or welding starts.
Welded SUS309STB needs weld-bead work or as-welded finish called out (as-welded vs cold-finished welded) so NDT and corrosion expectations match. Heat treatment: 1030 °C min, rapid cool. Austenitic heats take solution annealing with rapid cooling; hot-finished seamless may omit separate solution treatment when hot-worked and rapidly cooled in-line under the Table 2 note, unless the purchaser forbids it.
Hydrostatic testing or NDT (eddy current / ultrasonic per JIS G 0582/0583) replaces or accompanies pressure proof as the order states. Manufacture stays honest to the seamless or A/L/E welded choice. Size: both seamless S and automatic-arc A are common; specify finish H or C with the enquiry OD×wall. Hydrostatic pressure or NDT class for SUS309STB is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Size practice for SUS309STB remains both seamless S and automatic-arc A are common; specify finish H or C with the enquiry OD×wall.
Dimensions and Tolerances for JIS G3463 SUS309STB
Out-of-table OD×wall combinations are by agreement — still under the same grade symbol SUS309STB. Duty: lower-carbon 309S austenitic HX tube for oxidation service with better as-welded aqueous behaviour than high-C 309. Tolerance class follows the process route ordered for SUS309STB, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Keep the SUS309STB caution visible here: still not a chloride-process first choice — move to Mo austenitic or duplex when pitting governs.
Ovality, wall eccentricity (where applicable), and weld bead height limits are part of dimensional tolerance clauses — not optional cosmetics. Size reminder: both seamless S and automatic-arc A are common; specify finish H or C with the enquiry OD×wall. Fixed lengths and multiple cut lengths for SUS309STB are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Keep the SUS309STB caution visible here: still not a chloride-process first choice — move to Mo austenitic or duplex when pitting governs.
Equivalent Grades for JIS G3463 SUS309STB
European EN tube/tube numbers and ASTM marks may sit near 309S / UNS S30908, yet hydrostatic, NDT and heat-treatment text diverge. Keep SUS309STB as the governing symbol unless a written dual-cert plan exists. Caution: still not a chloride-process first choice — move to Mo austenitic or duplex when pitting governs. When a dual-cert path is required, list both JIS G3463 SUS309STB and the ASTM mark with separate test scopes instead of assuming one chemistry line clears both files. Weld-shop note tied to SUS309STB: 309L fillers preferred; verify ferrite balance on heavy sections before production welding.
Heat Treatment and Delivery Condition for JIS G3463 SUS309STB
Hot-finished seamless austenitics may use in-line rapid cool in lieu of a separate solution treatment under Table 2 note (a) unless the purchaser forbids it. Confirm for SUS309STB. Band: 1030 °C min, rapid cool. Recorded furnace charts for SUS309STB should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Size practice for SUS309STB remains both seamless S and automatic-arc A are common; specify finish H or C with the enquiry OD×wall.
Grain-size testing applies where the standard requires it for specific H grades — state any extra metallographic demand on the PO for SUS309STB. Field heat treatment of SUS309STB after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Corrosion framing beside SUS309STB: retains 309-class oxidation resistance with a tighter carbon ceiling that helps weld-zone stability on U-bends.
Corrosion Resistance of JIS G3463 SUS309STB
Medium, temperature, crevice geometry and weld condition decide whether SUS309STB is enough. Summary: retains 309-class oxidation resistance with a tighter carbon ceiling that helps weld-zone stability on U-bends. Escalate via sisters SUS309TB, SUS310STB, SUS304TB, SUS321TB when coupons fail. Coupon orientation, weld condition, and surface finish for SUS309STB belong in the corrosion test order so annex results can be compared to the installed bundle honestly. Corrosion framing beside SUS309STB: retains 309-class oxidation resistance with a tighter carbon ceiling that helps weld-zone stability on U-bends.
Surface finish and iron contamination control often matter as much as bulk chemistry on sanitary-lean duties for SUS309STB. Corrosion framing: retains 309-class oxidation resistance with a tighter carbon ceiling that helps weld-zone stability on U-bends. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for SUS309STB rather than relying on schedule thickness alone. This paragraph is locked to SUS309STB duty: lower-carbon 309S austenitic HX tube for oxidation service with better as-welded aqueous behaviour than high-C 309.
Applications of JIS G3463 SUS309STB Tube
From utility rooms to process racks, SUS309STB shows up wherever Japanese boiler/HX specs want austenitic behaviour. Use list: heat-treatment furnace coolers, incinerator interconnect exchangers, hot-gas transfer HX, and welded heat-facing bundles that also see condensate. Spool fabricators should copy SUS309STB onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Application context for SUS309STB stays heat-treatment furnace coolers, incinerator interconnect exchangers, hot-gas transfer HX, and welded heat-facing bundles that also see condensate.
If the only reason for SUS309STB is “we always used this alias,” reopen the corrosion file before repeating the order. Caution: still not a chloride-process first choice — move to Mo austenitic or duplex when pitting governs. Commissioning teams benefit when the as-built dossier repeats SUS309STB beside heat numbers, linking isometric revisions to the same mill certificates. Application context for SUS309STB stays heat-treatment furnace coolers, incinerator interconnect exchangers, hot-gas transfer HX, and welded heat-facing bundles that also see condensate.
Weldability of JIS G3463 SUS309STB
Automatic mill welds and manual field welds need different procedure packs, but both must respect SUS309STB chemistry. Guidance: 309L fillers preferred; verify ferrite balance on heavy sections before production welding. Procedure qualification for SUS309STB should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. Weld-shop note tied to SUS309STB: 309L fillers preferred; verify ferrite balance on heavy sections before production welding.
Ferrite control on duplex SUS309STB and hot-crack control on high-Ni austenitics are procedure items, not afterthoughts. Guidance: 309L fillers preferred; verify ferrite balance on heavy sections before production welding. Consumable lot control and shielding-gas notes for SUS309STB stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Keep the SUS309STB caution visible here: still not a chloride-process first choice — move to Mo austenitic or duplex when pitting governs.
Surface Finishes for JIS G3463 SUS309STB
Welded tube may need bead dressing for flow or inspection; call that out rather than assuming mill habit. Size/finish context: both seamless S and automatic-arc A are common; specify finish H or C with the enquiry OD×wall. Roughness or polish callouts for SUS309STB must name OD, ID, or both; ambiguous “bright tube” language is clarified before finishing slots are booked. Application context for SUS309STB stays heat-treatment furnace coolers, incinerator interconnect exchangers, hot-gas transfer HX, and welded heat-facing bundles that also see condensate.
Do not polish over unresolved weld defects — inspection comes before cosmetics on SUS309STB. Final visual standards for SUS309STB reject grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed. This paragraph is locked to SUS309STB duty: lower-carbon 309S austenitic HX tube for oxidation service with better as-welded aqueous behaviour than high-C 309.
Inspection and Testing for JIS G3463 SUS309STB
Third-party witness (SGS/TUV-style) is available when the project mandate requires it. Base acceptance still tracks G3463 for SUS309STB. Sampling plans for SUS309STB keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Corrosion framing beside SUS309STB: retains 309-class oxidation resistance with a tighter carbon ceiling that helps weld-zone stability on U-bends.
Dimensional inspection against dimensional tolerance clauses tolerances closes the lot. Failures retest per retest clauses — they are not silently shipped. Role: lower-carbon 309S austenitic HX tube for oxidation service with better as-welded aqueous behaviour than high-C 309. Non-conforming SUS309STB lengths are segregated and retested or rejected under retest clauses rather than reworked into unmarked stock. Weld-shop note tied to SUS309STB: 309L fillers preferred; verify ferrite balance on heavy sections before production welding.
Packaging and Shipping for JIS G3463 SUS309STB
Seaworthy packing is available for ocean legs — desiccant, VCI, and wrap specs by agreement. Grade mark SUS309STB stays visible on outer tags. Bundle tickets for SUS309STB repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. This paragraph is locked to SUS309STB duty: lower-carbon 309S austenitic HX tube for oxidation service with better as-welded aqueous behaviour than high-C 309.
Container loading plans should keep heavy schedules from crushing thin-wall SUS309STB layers. Desiccant and wrap choices for SUS309STB follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Weld-shop note tied to SUS309STB: 309L fillers preferred; verify ferrite balance on heavy sections before production welding.
Shortages or transit damage claims need photos against the packing list before installation starts — tag identity must still read SUS309STB. Claims handling for SUS309STB starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. This paragraph is locked to SUS309STB duty: lower-carbon 309S austenitic HX tube for oxidation service with better as-welded aqueous behaviour than high-C 309.
Why Choose SHH STEEL
From RFQ clarification through MTC release, SHH STEEL treats SUS309STB as a governed product symbol, not a marketing synonym for 309S / UNS S30908. Role: lower-carbon 309S austenitic HX tube for oxidation service with better as-welded aqueous behaviour than high-C 309. SHH STEEL can produce and supply SUS309STB against the OD × wall, process symbol, and test scope on your RFQ without swapping in an unstated sister grade.
Response time stays short because common SUS309STB enquiry sizes and document packs are already exercised on prior Japanese-spec orders. Use: heat-treatment furnace coolers, incinerator interconnect exchangers, hot-gas transfer HX, and welded heat-facing bundles that also see condensate. Ask for a written acknowledgement that names SUS309STB, the manufacture process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS309STB to that written scope.
Supply Capability
Capability framing for SUS309STB: Japanese-spec HX tube product, dual-route manufacture, documented heats. Caution remains: still not a chloride-process first choice — move to Mo austenitic or duplex when pitting governs. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS309STB when the mill schedule allows. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS309STB when the mill schedule allows. Size practice for SUS309STB remains both seamless S and automatic-arc A are common; specify finish H or C with the enquiry OD×wall.
| Item | Capability |
|---|---|
| Standard | JIS G3463 stainless steel tubes for boilers and heat exchangers |
| Grade symbol | SUS309STB |
| Product form | Seamless (S) and welded (A / L / E) tube; finishes S-H / S-C / A / A-C / E-C as marked |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered) |
| Typical OD practice | 15.9–139.8 mm per standard Note 1; other by agreement |
| Wall / gauge | OD × wall / BWG-class HX gauges within Attached Tables; other by agreement |
Stock / Available sizes
Stock / Available sizes — treat published ranges as capability envelopes. Actual ex-stock pieces of SUS309STB change weekly; the reliable path is an OD × wall matrix on the enquiry. Duty: lower-carbon 309S austenitic HX tube for oxidation service with better as-welded aqueous behaviour than high-C 309. SHH STEEL can supply alternate schedules and measured walls for SUS309STB once the design pressure and corrosion allowance are clear.
Repeat orders for SUS309STB go faster when prior heat records and accepted WPS numbers are referenced on the new RFQ. Role: lower-carbon 309S austenitic HX tube for oxidation service with better as-welded aqueous behaviour than high-C 309. SHH STEEL can produce trial lengths of SUS309STB for procedure qualification before the bulk release when the project calendar needs it.
FAQ
-
What is JIS G3463 SUS309STB stainless steel tube used for?
- JIS G3463 SUS309STB is stainless tube for boiler and heat-exchanger service (superheater, HX, condenser, catalyser) — heat-treatment furnace coolers, incinerator interconnect exchangers, hot-gas transfer HX, and welded heat-facing bundles that also see condensate. Role summary: lower-carbon 309S austenitic HX tube for oxidation service with better as-welded aqueous behaviour than high-C 309. It is a Japanese boiler/HX tube product standard mark, not an automatic ASTM A213 certificate.
-
Does JIS G3463 SUS309STB cover seamless and welded tube?
- Yes. Manufacture allows seamless and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish marks such as S-H, S-C, A-C, or E-C. SHH STEEL can produce and supply either route for SUS309STB when the mill can meet the ordered size and tests. The title omits Seamless/Welded because JIS G3463 covers both manufacture routes — the PO must still name the process mark.
-
What heat treatment applies to SUS309STB?
- SUS309STB is delivered solution annealed under JIS G3463. Table 2 reference: 1030 °C min, rapid cool. Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
-
How does SUS309STB compare with sister grades SUS309TB, SUS310STB, SUS304TB?
- SUS309STB is filed as austenitic. Typical sisters on the same RFQ are SUS309TB, SUS310STB, SUS304TB. Design caution: still not a chloride-process first choice — move to Mo austenitic or duplex when pitting governs Pick the sister when the medium or strength floor outgrows this symbol rather than stretching wall alone.
-
What tests appear on the mill certificate for SUS309STB?
- Expect cast analysis (Table 3), room-temperature tensile results (Table 4), flattening/flaring as applicable, dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
-
Is 309S / UNS S30908 the same as ordering SUS309STB?
- No. 309S / UNS S30908 is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3463 and SUS309STB so cast limits, heat treatment, and process marks are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for JIS G3463 SUS309STB?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS309STB within the typical 15.9–139.8 mm OD practice, with measured walls by agreement. Size context: both seamless S and automatic-arc A are common; specify finish H or C with the enquiry OD×wall. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
How should SUS309STB be welded?
- Shop guidance: 309L fillers preferred; verify ferrite balance on heavy sections before production welding. Mill heat treatment of seamless or welded tube does not replace a qualified WPS on fabricator joints or tube-to-tubesheet welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: still not a chloride-process first choice — move to Mo austenitic or duplex when pitting governs
-
When should I choose a duplex or higher-Mo grade instead of SUS309STB?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: still not a chloride-process first choice — move to Mo austenitic or duplex when pitting governs Sister pointers: SUS309TB, SUS310STB, SUS304TB. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify JIS G3463 SUS309STB with ASTM A213 or ASME SA213?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3463 SUS309STB does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What surface finishes are available for SUS309STB?
- Pickled after heat treatment is the usual HX tube supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS309STB when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
JIS G3463 SUS309STB is stainless steel tube for boiler and heat-exchanger service — lower-carbon 309S austenitic HX tube for oxidation service with better as-welded aqueous behaviour than high-C 309. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS309TB, SUS310STB, SUS304TB. Related ASTM A213 pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process mark, and medium notes to start the quote.