JIS G3463 SUS304TB Stainless Steel Tube
What is JIS G3463 SUS304TB Stainless Steel Tube
When the approved vendor list and tube-bundle notes say JIS G3463, the grade mark has to carry the TB suffix. SUS304TB is the full product symbol for this austenitic tube. When a Japanese boiler or heat-exchanger specification names JIS G3463 and “SUS304TB” rather than a vague “304 tube”, the purchase order finally locks cast chemistry, heat treatment, flattening/flaring, and hydraulic/NDT acceptance under one product standard.
SHH STEEL can supply SUS304TB tube in seamless S or welded A/L/E routes, with plain or bevelled ends, random or cut lengths, and EN 10204 / JIS G 0415 style inspection documents when specified. Role on the line: everyday 18-8 austenitic boiler and heat-exchanger tube where molybdenum is not justified. Size and test clarity on the RFQ lets SHH STEEL lock the correct Table 1 symbols for SUS304TB before production starts. Keep the SUS304TB caution visible here: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer SUS304LTB or a stabilised sister for corrosive welded HX bundles.
Equivalence talk to 304 / UNS S30400 belongs in engineering notes, not as a substitute for the JIS symbol. Lock JIS G3463 SUS304TB, OD × wall, manufacture/finish symbols, and any special quality annex items before melt. Watch-out: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer SUS304LTB or a stabilised sister for corrosive welded HX bundles.
Related ASTM tube pages share chemistry families but not Japanese acceptance text — confirm before dual-cert claims. Sisters on this hub: SUS304LTB, SUS316TB, SUS321TB, SUS304HTB. Use thread: utility condensers, low-pressure feedwater heaters, food/CIP heat exchangers, and general process coolers that still say “304 tube”. Document the medium, design temperature, and weld map beside the SUS304TB line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Size practice for SUS304TB remains HX OD×wall enquiries commonly sit in 15.9–38.1 mm with 1.2–3.2 mm wall; seamless S-C or welded A/E routes per manufacture symbols.
Inside this JIS G3463 series, compare SUS304LTB, SUS316TB, SUS321TB, SUS304HTB. Hub: JIS G3463. ASTM/ASME related product pages (not interchangeable by default): A213 TP304, A269 TP304, SA213 TP304, ASTM A213.
Chemical Composition of JIS G3463 SUS304TB
Chemistry control on SUS304TB starts at the ladle. Expect C ≤0.08, Si ≤1.00, Mn ≤2.00, P ≤0.040, S ≤0.030, Ni 8.00–11.00, Cr 18.00–20.00 within Table 3, reported on the inspection document against the heat. Body alias 304 / UNS S30400 does not widen those windows. Every ladle analysis for SUS304TB is checked against those windows before the heat is released to piercing, welding, or finishing, and the same numbers reappear on the inspection document. Application context for SUS304TB stays utility condensers, low-pressure feedwater heaters, food/CIP heat exchangers, and general process coolers that still say “304 tube”.
Read the table with the family in mind — austenitic — and with caution as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer SUS304LTB or a stabilised sister for corrosive welded HX bundles. Numbers without the matching heat-treatment row are incomplete purchase data. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for SUS304TB before the order is acknowledged. Application context for SUS304TB stays utility condensers, low-pressure feedwater heaters, food/CIP heat exchangers, and general process coolers that still say “304 tube”.
| Grade | C | Si | Mn | P | S | Ni | Cr |
|---|---|---|---|---|---|---|---|
| SUS304TB | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.040 | ≤0.030 | 8.00–11.00 | 18.00–20.00 |
Mechanical Properties of JIS G3463 SUS304TB
Proof stress and tensile minima for SUS304TB sit at Rm min 520 N/mm², proof stress min 206 N/mm², elongation min 35% (OD ≥20 mm, No.11/12). Flattening, flaring, and reverse-flattening (welded) testing backs ductility for the ordered process route. Watch-out: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer SUS304LTB or a stabilised sister for corrosive welded HX bundles.
| Grade | Rm min (N/mm²) | Proof stress min (N/mm²) | A OD≥20 mm No.11/12 min (%) | A 10≤OD<20 mm No.11 min (%) | A OD<10 mm No.11 min (%) |
|---|---|---|---|---|---|
| SUS304TB | 520 | 206 | 35 | 30 | 27 |
Ambient values from JIS G3463 Table 4 for SUS304TB. Heat treatment (Table 2): 1010 °C min, rapid cool. Elongation reductions apply for walls under 8 mm on No.12 pieces. For heat-exchanger tube the purchaser may designate an upper tensile limit (Table 4 min + 200 N/mm²) when necessary.
Manufacture of JIS G3463 SUS304TB Tube (Seamless and Welded)
JIS G3463 manufactures SUS304TB by seamless (symbol S) or welded routes — automatic arc (A), laser (L), or electric-resistance (E) — then applies the ordered finish: hot finish H, cold finish C, hot finish S-H or cold finish S-C / A-C / E-C as marked. SHH STEEL confirms the Table 1 symbol string on the acknowledgement before rolling or welding starts.
Process control for SUS304TB ends with verified heat treatment (1010 °C min, rapid cool) and surface conditioning. Austenitic heats take solution annealing with rapid cooling; hot-finished seamless may omit separate solution treatment when hot-worked and rapidly cooled in-line under the Table 2 note, unless the purchaser forbids it. Pickling or bright-anneal decisions for SUS304TB stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive duties. Weld-shop note tied to SUS304TB: 308/308L-class fillers for fabricator joints and U-bend returns; control heat input on non-L heats when the bundle stays in a corrosive medium.
Bevel geometry for walls ≤22 mm defaults to the standard figure when bevels are ordered without a drawing. Size practice: HX OD×wall enquiries commonly sit in 15.9–38.1 mm with 1.2–3.2 mm wall; seamless S-C or welded A/E routes per manufacture symbols. Hydrostatic pressure or NDT class for SUS304TB is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Size practice for SUS304TB remains HX OD×wall enquiries commonly sit in 15.9–38.1 mm with 1.2–3.2 mm wall; seamless S-C or welded A/E routes per manufacture symbols.
Dimensions and Tolerances for JIS G3463 SUS304TB
Mass tables in JIS G3463 support Attached Table mass/OD×wall ordering for common austenitic marks; for SUS304TB, confirm whether your project uses schedule or measured wall. Context: HX OD×wall enquiries commonly sit in 15.9–38.1 mm with 1.2–3.2 mm wall; seamless S-C or welded A/E routes per manufacture symbols. Tolerance class follows the process route ordered for SUS304TB, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Application context for SUS304TB stays utility condensers, low-pressure feedwater heaters, food/CIP heat exchangers, and general process coolers that still say “304 tube”.
For heat-exchange and building services, schedule tables often drive the BOM; for process plants, measured wall and corrosion allowance dominate. SUS304TB supports both conversations when the PO is clear. Fixed lengths and multiple cut lengths for SUS304TB are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Size practice for SUS304TB remains HX OD×wall enquiries commonly sit in 15.9–38.1 mm with 1.2–3.2 mm wall; seamless S-C or welded A/E routes per manufacture symbols.
Equivalent Grades for JIS G3463 SUS304TB
Do not treat 304 / UNS S30400 as interchangeable paperwork. Chemistry kinship is not acceptance kinship. Inside this series see SUS304LTB, SUS316TB, SUS321TB, SUS304HTB. Role: everyday 18-8 austenitic boiler and heat-exchanger tube where molybdenum is not justified. When a dual-cert path is required, list both JIS G3463 SUS304TB and the ASTM mark with separate test scopes instead of assuming one chemistry line clears both files. Size practice for SUS304TB remains HX OD×wall enquiries commonly sit in 15.9–38.1 mm with 1.2–3.2 mm wall; seamless S-C or welded A/E routes per manufacture symbols.
Heat Treatment and Delivery Condition for JIS G3463 SUS304TB
Stabilisation or special anneals, where the standard allows purchaser options (notably Ti/Nb grades), must be written on the order — silence means Table 2 defaults only. For SUS304TB: 1010 °C min, rapid cool. Recorded furnace charts for SUS304TB should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Size practice for SUS304TB remains HX OD×wall enquiries commonly sit in 15.9–38.1 mm with 1.2–3.2 mm wall; seamless S-C or welded A/E routes per manufacture symbols.
After local hot work in the field, restore solution annealed practice when the corrosion file demands it. Caution: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer SUS304LTB or a stabilised sister for corrosive welded HX bundles. Field heat treatment of SUS304TB after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. This paragraph is locked to SUS304TB duty: everyday 18-8 austenitic boiler and heat-exchanger tube where molybdenum is not justified.
Corrosion Resistance of JIS G3463 SUS304TB
Pick tests that match how SUS304TB is filed — austenitic. Corrosion thread: chromium-nickel passive film handles aqueous and mild chemical media on the tube OD/ID; outdoor chloride pitting and deposit crevices are the usual limiters. Caution: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer SUS304LTB or a stabilised sister for corrosive welded HX bundles.
Fire-protection and potable-adjacent lines still need the right alloy — G3463 scope does not make every mark equal. Use thread: utility condensers, low-pressure feedwater heaters, food/CIP heat exchangers, and general process coolers that still say “304 tube”. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for SUS304TB rather than relying on schedule thickness alone. Application context for SUS304TB stays utility condensers, low-pressure feedwater heaters, food/CIP heat exchangers, and general process coolers that still say “304 tube”.
Applications of JIS G3463 SUS304TB Tube
Project types that repeatedly call SUS304TB: utility condensers, low-pressure feedwater heaters, food/CIP heat exchangers, and general process coolers that still say “304 tube”. Duty: everyday 18-8 austenitic boiler and heat-exchanger tube where molybdenum is not justified. Caution still applies: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer SUS304LTB or a stabilised sister for corrosive welded HX bundles.
Superheater stubs, condenser bundles and corrosive process HX lines all appear in G3463’s scope — alloy choice still follows the medium. For this mark: everyday 18-8 austenitic boiler and heat-exchanger tube where molybdenum is not justified. Commissioning teams benefit when the as-built dossier repeats SUS304TB beside heat numbers, linking isometric revisions to the same mill certificates. Keep the SUS304TB caution visible here: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer SUS304LTB or a stabilised sister for corrosive welded HX bundles.
Weldability of JIS G3463 SUS304TB
Even seamless S tube of SUS304TB will see field welds. Use: 308/308L-class fillers for fabricator joints and U-bend returns; control heat input on non-L heats when the bundle stays in a corrosive medium. Restore heat treatment when the WPS and corrosion file require it. Procedure qualification for SUS304TB should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. Corrosion framing beside SUS304TB: chromium-nickel passive film handles aqueous and mild chemical media on the tube OD/ID; outdoor chloride pitting and deposit crevices are the usual limiters.
Dissimilar welds to carbon steel need buttering and dilution control — especially on heat-facing and Mo grades. Role context: everyday 18-8 austenitic boiler and heat-exchanger tube where molybdenum is not justified. Consumable lot control and shielding-gas notes for SUS304TB stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Application context for SUS304TB stays utility condensers, low-pressure feedwater heaters, food/CIP heat exchangers, and general process coolers that still say “304 tube”.
Surface Finishes for JIS G3463 SUS304TB
Iron-free handling after pickle matters — carbon-steel strapping stains show up later as rust blooms on SUS304TB. Finish thread tied to austenitic. Roughness or polish callouts for SUS304TB must name OD, ID, or both; ambiguous “bright tube” language is clarified before finishing slots are booked. Weld-shop note tied to SUS304TB: 308/308L-class fillers for fabricator joints and U-bend returns; control heat input on non-L heats when the bundle stays in a corrosive medium.
OD stencil ink and marking paint should be chloride-lean and removable where coating systems follow. Role: everyday 18-8 austenitic boiler and heat-exchanger tube where molybdenum is not justified. Final visual standards for SUS304TB reject grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed. Keep the SUS304TB caution visible here: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer SUS304LTB or a stabilised sister for corrosive welded HX bundles.
Inspection and Testing for JIS G3463 SUS304TB
Clause 13/14 define sampling and retests. For SUS304TB, keep the heat/lot identity unbroken from melt to bundle tag. Duty: everyday 18-8 austenitic boiler and heat-exchanger tube where molybdenum is not justified. Sampling plans for SUS304TB keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Keep the SUS304TB caution visible here: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer SUS304LTB or a stabilised sister for corrosive welded HX bundles.
Intergranular corrosion testing is annex/special — order it when polythionic or weld-decay risk is written into the duty file for SUS304TB. Non-conforming SUS304TB lengths are segregated and retested or rejected under retest clauses rather than reworked into unmarked stock. Keep the SUS304TB caution visible here: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer SUS304LTB or a stabilised sister for corrosive welded HX bundles.
Packaging and Shipping for JIS G3463 SUS304TB
Small-OD SUS304TB often ships in crates; large-OD in strapped bundles with OD pads. Confirm destination handling limits on the RFQ. Use: utility condensers, low-pressure feedwater heaters, food/CIP heat exchangers, and general process coolers that still say “304 tube”. Bundle tickets for SUS304TB repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Application context for SUS304TB stays utility condensers, low-pressure feedwater heaters, food/CIP heat exchangers, and general process coolers that still say “304 tube”.
Bevelled ends get protectors so landing edges survive trucking. Size hint: HX OD×wall enquiries commonly sit in 15.9–38.1 mm with 1.2–3.2 mm wall; seamless S-C or welded A/E routes per manufacture symbols. Desiccant and wrap choices for SUS304TB follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Corrosion framing beside SUS304TB: chromium-nickel passive film handles aqueous and mild chemical media on the tube OD/ID; outdoor chloride pitting and deposit crevices are the usual limiters.
Storage advice on arrival: keep bundles dry and off carbon-steel floors. Use thread: utility condensers, low-pressure feedwater heaters, food/CIP heat exchangers, and general process coolers that still say “304 tube”. Claims handling for SUS304TB starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Application context for SUS304TB stays utility condensers, low-pressure feedwater heaters, food/CIP heat exchangers, and general process coolers that still say “304 tube”.
Why Choose SHH STEEL
Project teams working to Japanese boiler/HX specs need a supplier that reads TB suffixes correctly. SHH STEEL can make SUS304TB to that discipline. Caution we keep visible: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer SUS304LTB or a stabilised sister for corrosive welded HX bundles.
Dual-cert discussions (JIS + ASTM) are handled with two acceptance regimes in view, not one certificate stretched by hope. Sisters: SUS304LTB, SUS316TB, SUS321TB, SUS304HTB. Ask for a written acknowledgement that names SUS304TB, the manufacture process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS304TB to that written scope.
Supply Capability
Whether you need prototype bundles or project tonnage of SUS304TB, SHH STEEL can supply against a clear OD × wall and test matrix. Duty: utility condensers, low-pressure feedwater heaters, food/CIP heat exchangers, and general process coolers that still say “304 tube”. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS304TB when the mill schedule allows.
| Item | Capability |
|---|---|
| Standard | JIS G3463 stainless steel tubes for boilers and heat exchangers |
| Grade symbol | SUS304TB |
| Product form | Seamless (S) and welded (A / L / E) tube; finishes S-H / S-C / A / A-C / E-C as marked |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered) |
| Typical OD practice | 15.9–139.8 mm per standard Note 1; other by agreement |
| Wall / gauge | OD × wall / BWG-class HX gauges within Attached Tables; other by agreement |
Stock / Available sizes
Stock / Available sizes: SHH STEEL quotes rolling/welding slots for SUS304TB rather than promising anonymous warehouse tons. Typical conversation starts around HX OD×wall enquiries commonly sit in 15.9–38.1 mm with 1.2–3.2 mm wall; seamless S-C or welded A/E routes per manufacture symbols. SHH STEEL can supply alternate schedules and measured walls for SUS304TB once the design pressure and corrosion allowance are clear.
If the project needs dual JIS G3463 + ASTM documentation, say so before melt. Caution: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer SUS304LTB or a stabilised sister for corrosive welded HX bundles. SHH STEEL can produce trial lengths of SUS304TB for procedure qualification before the bulk release when the project calendar needs it.
FAQ
-
What is JIS G3463 SUS304TB stainless steel tube used for?
- JIS G3463 SUS304TB is stainless tube for boiler and heat-exchanger service (superheater, HX, condenser, catalyser) — utility condensers, low-pressure feedwater heaters, food/CIP heat exchangers, and general process coolers that still say “304 tube”. Role summary: everyday 18-8 austenitic boiler and heat-exchanger tube where molybdenum is not justified. It is a Japanese boiler/HX tube product standard mark, not an automatic ASTM A213 certificate.
-
Does JIS G3463 SUS304TB cover seamless and welded tube?
- Yes. Manufacture allows seamless and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish marks such as S-H, S-C, A-C, or E-C. SHH STEEL can produce and supply either route for SUS304TB when the mill can meet the ordered size and tests. The title omits Seamless/Welded because JIS G3463 covers both manufacture routes — the PO must still name the process mark.
-
What heat treatment applies to SUS304TB?
- SUS304TB is delivered solution annealed under JIS G3463. Table 2 reference: 1010 °C min, rapid cool. Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
-
How does SUS304TB compare with sister grades SUS304LTB, SUS316TB, SUS321TB?
- SUS304TB is filed as austenitic. Typical sisters on the same RFQ are SUS304LTB, SUS316TB, SUS321TB. Design caution: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer SUS304LTB or a stabilised sister for corrosive welded HX bundles Pick the sister when the medium or strength floor outgrows this symbol rather than stretching wall alone.
-
What tests appear on the mill certificate for SUS304TB?
- Expect cast analysis (Table 3), room-temperature tensile results (Table 4), flattening/flaring as applicable, dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
-
Is 304 / UNS S30400 the same as ordering SUS304TB?
- No. 304 / UNS S30400 is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3463 and SUS304TB so cast limits, heat treatment, and process marks are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for JIS G3463 SUS304TB?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS304TB within the typical 15.9–139.8 mm OD practice, with measured walls by agreement. Size context: HX OD×wall enquiries commonly sit in 15.9–38.1 mm with 1.2–3.2 mm wall; seamless S-C or welded A/E routes per manufacture symbols. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
How should SUS304TB be welded?
- Shop guidance: 308/308L-class fillers for fabricator joints and U-bend returns; control heat input on non-L heats when the bundle stays in a corrosive medium. Mill heat treatment of seamless or welded tube does not replace a qualified WPS on fabricator joints or tube-to-tubesheet welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer SUS304LTB or a stabilised sister for corrosive welded HX bundles
-
When should I choose a duplex or higher-Mo grade instead of SUS304TB?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: as-welded intergranular attack risk rises when cast carbon sits near the 0.08% ceiling — prefer SUS304LTB or a stabilised sister for corrosive welded HX bundles Sister pointers: SUS304LTB, SUS316TB, SUS321TB. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify JIS G3463 SUS304TB with ASTM A213 or ASME SA213?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3463 SUS304TB does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What surface finishes are available for SUS304TB?
- Pickled after heat treatment is the usual HX tube supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS304TB when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
JIS G3463 SUS304TB is stainless steel tube for boiler and heat-exchanger service — everyday 18-8 austenitic boiler and heat-exchanger tube where molybdenum is not justified. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS304LTB, SUS316TB, SUS321TB. Related ASTM A213 pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process mark, and medium notes to start the quote.