JIS G3463 SUS310TB Stainless Steel Tube
What is JIS G3463 SUS310TB Stainless Steel Tube
JIS G3463 is the Japanese Industrial Standard for stainless steel tubes used in boiler and heat-exchanger service (superheater, HX, condenser, catalyser). Grade symbol SUS310TB sits in the austenitic set of Table 1. JIS G3463 SUS310TB is ordered when the gas temperature outgrows 309 and the project still wants an austenitic HX tube — not a vague “310 pipe” alias.
SHH STEEL can produce and supply JIS G3463 SUS310TB as seamless or welded tube across the enquiry OD×wall band, solution-annealed or annealed as Table 2 requires, pickled or bright-finished, and documented on mill test certificates tied to cast analysis and tensile results. Duty focus: 25Cr-20Ni austenitic tube for severe oxidation and carburising-lean hot-gas heat exchange.
Shop language may still say “310 tube,” yet that commercial alias does not select Japanese cast limits, process symbols, or hydraulic/NDT rules. The purchase order has to name JIS G3463 and SUS310TB so the mill applies the correct analysis, heat treatment, mechanical floors, and marking. Design caution: carbon up to 0.15% — aqueous as-welded duty is not this grade’s mission; prefer SUS310STB when weld IGC matters; fired-heater tubes are outside G3463 scope.
Scope discipline: SUS310TB is HX tube product under JIS G3463, not a piping product under JIS G3459 and not an ASTM A213 order by default. Sister marks often compared on the same RFQ include SUS310STB, SUS309TB, SUS309STB, SUS304HTB. Role reminder: 25Cr-20Ni austenitic tube for severe oxidation and carburising-lean hot-gas heat exchange. Document the medium, design temperature, and weld map beside the SUS310TB line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. This paragraph is locked to SUS310TB duty: 25Cr-20Ni austenitic tube for severe oxidation and carburising-lean hot-gas heat exchange.
Inside this JIS G3463 series, compare SUS310STB, SUS309TB, SUS309STB, SUS304HTB. Hub: JIS G3463. ASTM/ASME related product pages (not interchangeable by default): ASTM A213.
Chemical Composition of JIS G3463 SUS310TB
Cast analysis for JIS G3463 SUS310TB follows Table 3. Key windows on a typical certificate include C ≤0.15, Si ≤1.50, Mn ≤2.00, P ≤0.040, S ≤0.030, Ni 19.00–22.00, Cr 24.00–26.00. SHH STEEL ties the heat number on the tube marking to the same cast line on the MTC. Commercial alias 310 / UNS S31000 class is body text only. Corrosion thread: excellent hot oxidation resistance from the 25Cr-20Ni balance; aqueous chloride ranking is secondary.
Chemical limits for SUS310TB under JIS G3463 appear in the table underneath. Source priority is the 2021 Table 3 extract cross-checked to public Nikko / supplier tables. If your client specification cites a different edition footnote, send it before the heat is melted. Duty thread: 25Cr-20Ni austenitic tube for severe oxidation and carburising-lean hot-gas heat exchange.
| Grade | C | Si | Mn | P | S | Ni | Cr |
|---|---|---|---|---|---|---|---|
| SUS310TB | ≤0.15 | ≤1.50 | ≤2.00 | ≤0.040 | ≤0.030 | 19.00–22.00 | 24.00–26.00 |
Mechanical Properties of JIS G3463 SUS310TB
Ambient tensile floors for SUS310TB come from JIS G3463 Table 4: Rm min 520 N/mm², proof stress min 206 N/mm², elongation min 35% (OD ≥20 mm, No.11/12). These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: austenitic. Caution: carbon up to 0.15% — aqueous as-welded duty is not this grade’s mission; prefer SUS310STB when weld IGC matters; fired-heater tubes are outside G3463 scope.
| Grade | Rm min (N/mm²) | Proof stress min (N/mm²) | A OD≥20 mm No.11/12 min (%) | A 10≤OD<20 mm No.11 min (%) | A OD<10 mm No.11 min (%) |
|---|---|---|---|---|---|
| SUS310TB | 520 | 206 | 35 | 30 | 27 |
Ambient values from JIS G3463 Table 4 for SUS310TB. Heat treatment (Table 2): 1030 °C min, rapid cool. Elongation reductions apply for walls under 8 mm on No.12 pieces. For heat-exchanger tube the purchaser may designate an upper tensile limit (Table 4 min + 200 N/mm²) when necessary.
Manufacture of JIS G3463 SUS310TB Tube (Seamless and Welded)
Both seamless and welded SUS310TB are legitimate under JIS G3463. Pick S when the design pressure, wall, or NDT plan favours a pierced/drawn route; pick A, L, or E when welded economics fit and the weld procedure is qualified. Finish symbols S-H/S-C/A/A-C/E-C ride with the process mark on the tube stencil. Seamless and welded options remain available for SUS310TB; the acknowledgement repeats the Table 1 symbols so production cannot silently change route after the PO is firm. Application context for SUS310TB stays radiant-adjacent coolers, sulphur-bearing hot gas exchangers, cement kiln waste-heat tubes, and high-temperature process heaters (not fired-heater tubes under this standard’s exclusion).
Austenitic heats take solution annealing with rapid cooling; hot-finished seamless may omit separate solution treatment when hot-worked and rapidly cooled in-line under the Table 2 note, unless the purchaser forbids it. Heat-treatment reference for SUS310TB: 1030 °C min, rapid cool. Pickling follows unless bright heat treatment leaves a scale-free surface. Duty thread: 25Cr-20Ni austenitic tube for severe oxidation and carburising-lean hot-gas heat exchange.
When dual documentation against ASTM A213 is requested for a related chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for SUS310TB: seamless S-H/S-C dominate heat-service walls; confirm OD within the 15.9–139.8 mm general practice.
Dimensions and Tolerances for JIS G3463 SUS310TB
SHH STEEL aligns nominal diameter (A/B), outside diameter, schedule or wall, and length tolerance for SUS310TB before the mill slot is locked. Standard Note 1 frames typical OD from 15.9 mm to 139.8 mm (standard Note 1 general practice). Size hint: seamless S-H/S-C dominate heat-service walls; confirm OD within the 15.9–139.8 mm general practice.
Length supply may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against the packaging clause so pickled or polished finishes are not iron-stained in transit. Duty thread: 25Cr-20Ni austenitic tube for severe oxidation and carburising-lean hot-gas heat exchange. Fixed lengths and multiple cut lengths for SUS310TB are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Weld-shop note tied to SUS310TB: 310/310S-class fillers; control hot cracking on high-Ni welds; aqueous joints prefer the S sister.
Equivalent Grades for JIS G3463 SUS310TB
Equivalence talk for SUS310TB starts with 310 / UNS S31000 class: that commercial / UNS framing is useful in body text and dual-cert discussions, but the H1 and order line stay on JIS G3463 SUS310TB. ASTM A213 / A269 pages that share related chemistry are different product standards with different wall bases, mechanical tables, and tests. Sisters: SUS310STB, SUS309TB, SUS309STB, SUS304HTB. Caution: carbon up to 0.15% — aqueous as-welded duty is not this grade’s mission; prefer SUS310STB when weld IGC matters; fired-heater tubes are outside G3463 scope.
Heat Treatment and Delivery Condition for JIS G3463 SUS310TB
SUS310TB is delivered solution annealed under JIS G3463. Table 2 reference: 1030 °C min, rapid cool. Fabricator heat treatment after hot bending should chase the same family practice. Weld thread: 310/310S-class fillers; control hot cracking on high-Ni welds; aqueous joints prefer the S sister. Recorded furnace charts for SUS310TB should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Weld-shop note tied to SUS310TB: 310/310S-class fillers; control hot cracking on high-Ni welds; aqueous joints prefer the S sister.
Cooling type matters — austenitic and duplex need rapid cool after solution treatment; ferritic anneal practice allows rapid or slow cool per Table 2. Duty thread: 25Cr-20Ni austenitic tube for severe oxidation and carburising-lean hot-gas heat exchange. Field heat treatment of SUS310TB after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. This paragraph is locked to SUS310TB duty: 25Cr-20Ni austenitic tube for severe oxidation and carburising-lean hot-gas heat exchange.
Corrosion Resistance of JIS G3463 SUS310TB
Corrosion behaviour of JIS G3463 SUS310TB tracks its austenitic balance: excellent hot oxidation resistance from the 25Cr-20Ni balance; aqueous chloride ranking is secondary. Optional annex corrosion tests (oxalic, Strauss, Huey, etc.) are special quality items — order them when the duty needs coupon evidence. Design caution: carbon up to 0.15% — aqueous as-welded duty is not this grade’s mission; prefer SUS310STB when weld IGC matters; fired-heater tubes are outside G3463 scope.
For heat-facing austenitics, oxidation resistance may dominate over aqueous IGC talk; for duplex and Mo austenitics, chlorides dominate; for ferritics, mild aqueous and weld practice dominate. SUS310TB is filed as austenitic. Caution: carbon up to 0.15% — aqueous as-welded duty is not this grade’s mission; prefer SUS310STB when weld IGC matters; fired-heater tubes are outside G3463 scope.
Applications of JIS G3463 SUS310TB Tube
Applications of JIS G3463 SUS310TB tube centre on radiant-adjacent coolers, sulphur-bearing hot gas exchangers, cement kiln waste-heat tubes, and high-temperature process heaters (not fired-heater tubes under this standard’s exclusion). Role summary: 25Cr-20Ni austenitic tube for severe oxidation and carburising-lean hot-gas heat exchange. When a related chemistry is required under ASTM A213 or A269, open those sister pages — acceptance text is not automatic.
Downstream fabricators should inherit the same grade symbol on cut lists so informal alias substitutions do not creep in. Primary application sketch: radiant-adjacent coolers, sulphur-bearing hot gas exchangers, cement kiln waste-heat tubes, and high-temperature process heaters (not fired-heater tubes under this standard’s exclusion). Duty thread: 25Cr-20Ni austenitic tube for severe oxidation and carburising-lean hot-gas heat exchange.
Weldability of JIS G3463 SUS310TB
SUS310TB is welded both as a mill product (A/L/E routes) and as fabricator joints on bundles. Shop guidance: 310/310S-class fillers; control hot cracking on high-Ni welds; aqueous joints prefer the S sister. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Procedure qualification for SUS310TB should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. Size practice for SUS310TB remains seamless S-H/S-C dominate heat-service walls; confirm OD within the 15.9–139.8 mm general practice.
Filler selection should match or over-alloy the base chemistry as the WPS demands. Heat input, interpass temperature, and shielding follow the family — austenitic, duplex, or ferritic — not a single shop habit. Caution: carbon up to 0.15% — aqueous as-welded duty is not this grade’s mission; prefer SUS310STB when weld IGC matters; fired-heater tubes are outside G3463 scope.
Surface Finishes for JIS G3463 SUS310TB
Surface supply for SUS310TB is typically pickled after heat treatment, or bright-annealed when scale-free OD/ID is ordered. Polished or special roughness finishes are by agreement and must state which surface (OD, ID, or both) is in scope. Duty: 25Cr-20Ni austenitic tube for severe oxidation and carburising-lean hot-gas heat exchange. Roughness or polish callouts for SUS310TB must name OD, ID, or both; ambiguous “bright tube” language is clarified before finishing slots are booked. Size practice for SUS310TB remains seamless S-H/S-C dominate heat-service walls; confirm OD within the 15.9–139.8 mm general practice.
Passivation treatments, when ordered, follow agreed ASTM A967 / JIS practice analogues — they are not a substitute for correct heat treatment. Caution: carbon up to 0.15% — aqueous as-welded duty is not this grade’s mission; prefer SUS310STB when weld IGC matters; fired-heater tubes are outside G3463 scope. Final visual standards for SUS310TB reject grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed. Size practice for SUS310TB remains seamless S-H/S-C dominate heat-service walls; confirm OD within the 15.9–139.8 mm general practice.
Inspection and Testing for JIS G3463 SUS310TB
Inspection for JIS G3463 SUS310TB covers cast analysis, tensile tests, flattening or weld bend as applicable, hydrostatic test or NDT, dimensions, and appearance. Special quality annex items (IGC, grain size, etc.) apply only when ordered. Documents follow JIS G 0415 / purchaser-specified EN 10204 styles. Sampling plans for SUS310TB keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Corrosion framing beside SUS310TB: excellent hot oxidation resistance from the 25Cr-20Ni balance; aqueous chloride ranking is secondary.
Marking includes SUS310TB, manufacture/finish symbols, manufacturer, and other mandatory marking-clause data. Traceability from stencil to MTC is part of supply, not an upgrade. Use: radiant-adjacent coolers, sulphur-bearing hot gas exchangers, cement kiln waste-heat tubes, and high-temperature process heaters (not fired-heater tubes under this standard’s exclusion). Non-conforming SUS310TB lengths are segregated and retested or rejected under retest clauses rather than reworked into unmarked stock. Size practice for SUS310TB remains seamless S-H/S-C dominate heat-service walls; confirm OD within the 15.9–139.8 mm general practice.
Packaging and Shipping for JIS G3463 SUS310TB
Packaging for SUS310TB uses wooden boxes, plywood cases, or bundled frames with waterproof wrapping as the OD and finish demand. Soft separators protect pickled and polished surfaces. Ends receive caps or bevel protectors when ordered. Bundle tickets for SUS310TB repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Size practice for SUS310TB remains seamless S-H/S-C dominate heat-service walls; confirm OD within the 15.9–139.8 mm general practice.
Carbon-steel strapping never contacts the stainless OD without a barrier. Mixed-grade bundles are forbidden when chemistry integrity matters. Caution: carbon up to 0.15% — aqueous as-welded duty is not this grade’s mission; prefer SUS310STB when weld IGC matters; fired-heater tubes are outside G3463 scope. Desiccant and wrap choices for SUS310TB follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Corrosion framing beside SUS310TB: excellent hot oxidation resistance from the 25Cr-20Ni balance; aqueous chloride ranking is secondary.
Shipping documents list JIS G3463, SUS310TB, sizes, quantities, heat numbers, and certificate type. SHH STEEL coordinates inland trucking and FOB/CIF packing scopes as the order states. Role: 25Cr-20Ni austenitic tube for severe oxidation and carburising-lean hot-gas heat exchange. Claims handling for SUS310TB starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Size practice for SUS310TB remains seamless S-H/S-C dominate heat-service walls; confirm OD within the 15.9–139.8 mm general practice.
Why Choose SHH STEEL
SHH STEEL can produce and supply JIS G3463 SUS310TB with the process route, heat treatment, and tests named on your enquiry — not a bait-and-switch alias. Mill partners run stainless tube capacity that covers seamless and welded Table 1 symbols for this mark. Duty focus: 25Cr-20Ni austenitic tube for severe oxidation and carburising-lean hot-gas heat exchange.
Technical sales can map SUS310TB against sisters SUS310STB, SUS309TB, SUS309STB, SUS304HTB and live ASTM pages without pretending standards are identical. Inspection coordination and export packing are in-house habits, not afterthoughts. Ask for a written acknowledgement that names SUS310TB, the manufacture process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS310TB to that written scope.
Supply Capability
SHH STEEL can produce and supply JIS G3463 SUS310TB across enquiry-oriented OD × wall bands, in seamless or welded routes, with certificates and optional annex tests as ordered. Summary capability follows in the table; stock language below is an RFQ map, not a frozen tonnage catalogue. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS310TB when the mill schedule allows.
| Item | Capability |
|---|---|
| Standard | JIS G3463 stainless steel tubes for boilers and heat exchangers |
| Grade symbol | SUS310TB |
| Product form | Seamless (S) and welded (A / L / E) tube; finishes S-H / S-C / A / A-C / E-C as marked |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered) |
| Typical OD practice | 15.9–139.8 mm per standard Note 1; other by agreement |
| Wall / gauge | OD × wall / BWG-class HX gauges within Attached Tables; other by agreement |
Stock / Available sizes
SHH STEEL can produce and supply JIS G3463 SUS310TB. Stock / Available sizes: enquiry band typically aligns with 15.9–139.8 mm OD practice under G3463 Note 1, with OD×wall HX gauges; schedule 5S–80 (and heavier by agreement) depending on grade family. For SUS310TB, practical fast-track sizes often sit in mid-bore process and utility ranges — send the OD × wall list for a firm acknowledgement. Context: seamless S-H/S-C dominate heat-service walls; confirm OD within the 15.9–139.8 mm general practice.
Cut lengths, bevels, special NDT, and IGC annex tests add lead time — call them early. Sisters often quoted alongside: SUS310STB, SUS309TB, SUS309STB, SUS304HTB. Email the size list to start. SHH STEEL can produce trial lengths of SUS310TB for procedure qualification before the bulk release when the project calendar needs it. SHH STEEL can produce trial lengths of SUS310TB for procedure qualification before bulk release when the project calendar needs it. This paragraph is locked to SUS310TB duty: 25Cr-20Ni austenitic tube for severe oxidation and carburising-lean hot-gas heat exchange.
FAQ
-
What is JIS G3463 SUS310TB stainless steel tube used for?
- JIS G3463 SUS310TB is stainless tube for boiler and heat-exchanger service (superheater, HX, condenser, catalyser) — radiant-adjacent coolers, sulphur-bearing hot gas exchangers, cement kiln waste-heat tubes, and high-temperature process heaters (not fired-heater tubes under this standard’s exclusion). Role summary: 25Cr-20Ni austenitic tube for severe oxidation and carburising-lean hot-gas heat exchange. It is a Japanese boiler/HX tube product standard mark, not an automatic ASTM A213 certificate.
-
Does JIS G3463 SUS310TB cover seamless and welded tube?
- Yes. Manufacture allows seamless and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish marks such as S-H, S-C, A-C, or E-C. SHH STEEL can produce and supply either route for SUS310TB when the mill can meet the ordered size and tests. The title omits Seamless/Welded because JIS G3463 covers both manufacture routes — the PO must still name the process mark.
-
What heat treatment applies to SUS310TB?
- SUS310TB is delivered solution annealed under JIS G3463. Table 2 reference: 1030 °C min, rapid cool. Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
-
How does SUS310TB compare with sister grades SUS310STB, SUS309TB, SUS309STB?
- SUS310TB is filed as austenitic. Typical sisters on the same RFQ are SUS310STB, SUS309TB, SUS309STB. Design caution: carbon up to 0.15% — aqueous as-welded duty is not this grade’s mission; prefer SUS310STB when weld IGC matters; fired-heater tubes are outside G3463 scope Pick the sister when the medium or strength floor outgrows this symbol rather than stretching wall alone.
-
What tests appear on the mill certificate for SUS310TB?
- Expect cast analysis (Table 3), room-temperature tensile results (Table 4), flattening/flaring as applicable, dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
-
Is 310 / UNS S31000 class the same as ordering SUS310TB?
- No. 310 / UNS S31000 class is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3463 and SUS310TB so cast limits, heat treatment, and process marks are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for JIS G3463 SUS310TB?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS310TB within the typical 15.9–139.8 mm OD practice, with measured walls by agreement. Size context: seamless S-H/S-C dominate heat-service walls; confirm OD within the 15.9–139.8 mm general practice. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
How should SUS310TB be welded?
- Shop guidance: 310/310S-class fillers; control hot cracking on high-Ni welds; aqueous joints prefer the S sister. Mill heat treatment of seamless or welded tube does not replace a qualified WPS on fabricator joints or tube-to-tubesheet welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: carbon up to 0.15% — aqueous as-welded duty is not this grade’s mission; prefer SUS310STB when weld IGC matters; fired-heater tubes are outside G3463 scope
-
When should I choose a duplex or higher-Mo grade instead of SUS310TB?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: carbon up to 0.15% — aqueous as-welded duty is not this grade’s mission; prefer SUS310STB when weld IGC matters; fired-heater tubes are outside G3463 scope Sister pointers: SUS310STB, SUS309TB, SUS309STB. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify JIS G3463 SUS310TB with ASTM A213 or ASME SA213?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3463 SUS310TB does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What surface finishes are available for SUS310TB?
- Pickled after heat treatment is the usual HX tube supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS310TB when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
JIS G3463 SUS310TB is stainless steel tube for boiler and heat-exchanger service — 25Cr-20Ni austenitic tube for severe oxidation and carburising-lean hot-gas heat exchange. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS310STB, SUS309TB, SUS309STB. Related ASTM A213 pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process mark, and medium notes to start the quote.