JIS G3463 SUS836LTB Stainless Steel Tube | JIS G3463 Stainless Steel Tube - SHH STEEL

JIS G3463 SUS836LTB Stainless Steel Tube

JIS G3463 SUS836LTB stainless steel tube (~6Mo / high-Mo Ni austenitic (JIS SUS836L)), austenitic, Table 3 cast analysis, Rm min 520 N/mm² / proof min 206 N/mm², solution annealed. SHH STEEL can produce and supply seamless or welded routes with mill certificates.
Grade
SUS836LTB (~6Mo / high-Mo Ni austenitic (JIS SUS836L) — body alias)
Standard
JIS G3463
Product form
Seamless and welded stainless steel boiler/HX tube, delivery solution annealed
Size
Typically OD 15.9–139.8 mm (Note 1); OD × wall (HX/boiler gauges) by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is JIS G3463 SUS836LTB Stainless Steel Tube

When the approved vendor list and tube-bundle notes say JIS G3463, the grade mark has to carry the TB suffix. SUS836LTB is the full product symbol for this austenitic tube. When 317L fails the crevice mock-up and the project still wants austenitic tube, JIS G3463 SUS836LTB is the Japanese 6Mo-class HX mark to put on the PO.

SHH STEEL can supply SUS836LTB tube in seamless S or welded A/L/E routes, with plain or bevelled ends, random or cut lengths, and EN 10204 / JIS G 0415 style inspection documents when specified. Role on the line: high-Mo Ni austenitic (~6Mo class) for aggressive chloride and chemical HX tube. Size and test clarity on the RFQ lets SHH STEEL lock the correct Table 1 symbols for SUS836LTB before production starts. Size practice for SUS836LTB remains seamless cold-finished HX OD; NDT class often elevated by purchaser.

Equivalence talk to ~6Mo / high-Mo Ni austenitic (JIS SUS836L) belongs in engineering notes, not as a substitute for the JIS symbol. Lock JIS G3463 SUS836LTB, OD × wall, manufacture/finish symbols, and any special quality annex items before melt. Watch-out: do not invent PREN posters; bring medium data — duplex may still win on strength or cost.

Related ASTM tube pages share chemistry families but not Japanese acceptance text — confirm before dual-cert claims. Sisters on this hub: SUS890LTB, SUS312LTB, SUS317LTB, SUS316LTB. Use thread: severe chloride condensers, bleach chemical coolers, and high-PREN austenitic tube bundles. Document the medium, design temperature, and weld map beside the SUS836LTB line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Application context for SUS836LTB stays severe chloride condensers, bleach chemical coolers, and high-PREN austenitic tube bundles.

Inside this JIS G3463 series, compare SUS890LTB, SUS312LTB, SUS317LTB, SUS316LTB. Hub: JIS G3463. ASTM/ASME related product pages (not interchangeable by default): ASTM A213.

Chemical Composition of JIS G3463 SUS836LTB

Chemistry control on SUS836LTB starts at the ladle. Expect C ≤0.030, Si ≤1.00, Mn ≤2.00, P ≤0.040, S ≤0.030, Ni 24.00–26.00, Cr 19.00–24.00 within Table 3, reported on the inspection document against the heat. Body alias ~6Mo / high-Mo Ni austenitic (JIS SUS836L) does not widen those windows. Every ladle analysis for SUS836LTB is checked against those windows before the heat is released to piercing, welding, or finishing, and the same numbers reappear on the inspection document. This paragraph is locked to SUS836LTB duty: high-Mo Ni austenitic (~6Mo class) for aggressive chloride and chemical HX tube.

Read the table with the family in mind — austenitic — and with caution do not invent PREN posters; bring medium data — duplex may still win on strength or cost. Numbers without the matching heat-treatment row are incomplete purchase data. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for SUS836LTB before the order is acknowledged. Size practice for SUS836LTB remains seamless cold-finished HX OD; NDT class often elevated by purchaser.

Grade C Si Mn P S Ni Cr Mo N
SUS836LTB ≤0.030 ≤1.00 ≤2.00 ≤0.040 ≤0.030 24.00–26.00 19.00–24.00 5.00–7.00 ≤0.25

Mechanical Properties of JIS G3463 SUS836LTB

Proof stress and tensile minima for SUS836LTB sit at Rm min 520 N/mm², proof stress min 206 N/mm², elongation min 35% (OD ≥20 mm, No.11/12). Flattening, flaring, and reverse-flattening (welded) testing backs ductility for the ordered process route. Watch-out: do not invent PREN posters; bring medium data — duplex may still win on strength or cost.

Grade Rm min (N/mm²) Proof stress min (N/mm²) A OD≥20 mm No.11/12 min (%) A 10≤OD<20 mm No.11 min (%) A OD<10 mm No.11 min (%)
SUS836LTB 520 206 35 30 27

Ambient values from JIS G3463 Table 4 for SUS836LTB. Heat treatment (Table 2): 1010 °C min, rapid cool. Elongation reductions apply for walls under 8 mm on No.12 pieces. For heat-exchanger tube the purchaser may designate an upper tensile limit (Table 4 min + 200 N/mm²) when necessary.

Manufacture of JIS G3463 SUS836LTB Tube (Seamless and Welded)

Both seamless and welded SUS836LTB are legitimate under JIS G3463. Pick S when the design pressure, wall, or NDT plan favours a pierced/drawn route; pick A, L, or E when welded economics fit and the weld procedure is qualified. Finish symbols S-H/S-C/A/A-C/E-C ride with the process mark on the tube stencil. Seamless and welded options remain available for SUS836LTB; the acknowledgement repeats the Table 1 symbols so production cannot silently change route after the PO is firm. Weld-shop note tied to SUS836LTB: 6Mo / high-Ni Mo fillers; strict purge and heat-input control.

Process control for SUS836LTB ends with verified heat treatment (1010 °C min, rapid cool) and surface conditioning. Austenitic heats take solution annealing with rapid cooling; hot-finished seamless may omit separate solution treatment when hot-worked and rapidly cooled in-line under the Table 2 note, unless the purchaser forbids it. Pickling or bright-anneal decisions for SUS836LTB stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive duties. Weld-shop note tied to SUS836LTB: 6Mo / high-Ni Mo fillers; strict purge and heat-input control.

Bevel geometry for walls ≤22 mm defaults to the standard figure when bevels are ordered without a drawing. Size practice: seamless cold-finished HX OD; NDT class often elevated by purchaser. Hydrostatic pressure or NDT class for SUS836LTB is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Corrosion framing beside SUS836LTB: 5–7% Mo plus N targets aggressive pitting/crevice service beyond 317L.

Dimensions and Tolerances for JIS G3463 SUS836LTB

Mass tables in JIS G3463 support Attached Table mass/OD×wall ordering for common austenitic marks; for SUS836LTB, confirm whether your project uses schedule or measured wall. Context: seamless cold-finished HX OD; NDT class often elevated by purchaser. Tolerance class follows the process route ordered for SUS836LTB, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Size practice for SUS836LTB remains seamless cold-finished HX OD; NDT class often elevated by purchaser.

For heat-exchange and building services, schedule tables often drive the BOM; for process plants, measured wall and corrosion allowance dominate. SUS836LTB supports both conversations when the PO is clear. Fixed lengths and multiple cut lengths for SUS836LTB are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Keep the SUS836LTB caution visible here: do not invent PREN posters; bring medium data — duplex may still win on strength or cost.

Equivalent Grades for JIS G3463 SUS836LTB

SUS836LTB is the JIS G3463 high-Mo nickel austenitic tube grade aimed at aggressive chloride and chemical heat-exchanger duty — roughly a 6Mo-class chemistry family in commercial talk. Alias language such as “~6Mo / high-Mo Ni austenitic (JIS SUS836L)” is body-only; the governing product mark on this page is SUS836LTB. Do not invent a one-to-one ASTM or EN substitute from a 6Mo brochure — related UNS marks (for example S31254-class talk) sit under different product standards and mechanical tables.

System Designation Notes
JIS G3463 SUS836LTB Governing HX/boiler tube grade for this page
Commercial / UNS (body only) ~6Mo / high-Mo Ni austenitic (JIS SUS836L) Useful in dual-cert talk; confirm Mo/Ni/N on the cast analysis
ASTM A213 / A269 related 6Mo-class austenitic tube family (no single TP asserted as identical) Related chemistry family — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local 6Mo tube specs

When the medium outgrows this mark, compare SUS890LTB, SUS312LTB, SUS317LTB, SUS316LTB rather than stretching a dual-cert claim. Confirm every alloying window on the MTC for SUS836LTB — brochure “6Mo” labels are not chemistry. Hub: JIS G3463.

Heat Treatment and Delivery Condition for JIS G3463 SUS836LTB

Stabilisation or special anneals, where the standard allows purchaser options (notably Ti/Nb grades), must be written on the order — silence means Table 2 defaults only. For SUS836LTB: 1010 °C min, rapid cool. Recorded furnace charts for SUS836LTB should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Keep the SUS836LTB caution visible here: do not invent PREN posters; bring medium data — duplex may still win on strength or cost.

After local hot work in the field, restore solution annealed practice when the corrosion file demands it. Caution: do not invent PREN posters; bring medium data — duplex may still win on strength or cost. Field heat treatment of SUS836LTB after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Application context for SUS836LTB stays severe chloride condensers, bleach chemical coolers, and high-PREN austenitic tube bundles.

Corrosion Resistance of JIS G3463 SUS836LTB

Pick tests that match how SUS836LTB is filed — austenitic. Corrosion thread: 5–7% Mo plus N targets aggressive pitting/crevice service beyond 317L. Caution: do not invent PREN posters; bring medium data — duplex may still win on strength or cost. Coupon orientation, weld condition, and surface finish for SUS836LTB belong in the corrosion test order so annex results can be compared to the installed bundle honestly. Corrosion framing beside SUS836LTB: 5–7% Mo plus N targets aggressive pitting/crevice service beyond 317L.

Fire-protection and potable-adjacent lines still need the right alloy — G3463 scope does not make every mark equal. Use thread: severe chloride condensers, bleach chemical coolers, and high-PREN austenitic tube bundles. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for SUS836LTB rather than relying on schedule thickness alone. Size practice for SUS836LTB remains seamless cold-finished HX OD; NDT class often elevated by purchaser.

Applications of JIS G3463 SUS836LTB Tube

Project types that repeatedly call SUS836LTB: severe chloride condensers, bleach chemical coolers, and high-PREN austenitic tube bundles. Duty: high-Mo Ni austenitic (~6Mo class) for aggressive chloride and chemical HX tube. Caution still applies: do not invent PREN posters; bring medium data — duplex may still win on strength or cost. Spool fabricators should copy SUS836LTB onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Size practice for SUS836LTB remains seamless cold-finished HX OD; NDT class often elevated by purchaser.

Superheater stubs, condenser bundles and corrosive process HX lines all appear in G3463’s scope — alloy choice still follows the medium. For this mark: high-Mo Ni austenitic (~6Mo class) for aggressive chloride and chemical HX tube. Commissioning teams benefit when the as-built dossier repeats SUS836LTB beside heat numbers, linking isometric revisions to the same mill certificates. Corrosion framing beside SUS836LTB: 5–7% Mo plus N targets aggressive pitting/crevice service beyond 317L.

Weldability of JIS G3463 SUS836LTB

Even seamless S tube of SUS836LTB will see field welds. Use: 6Mo / high-Ni Mo fillers; strict purge and heat-input control. Restore heat treatment when the WPS and corrosion file require it. Procedure qualification for SUS836LTB should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. Weld-shop note tied to SUS836LTB: 6Mo / high-Ni Mo fillers; strict purge and heat-input control.

Dissimilar welds to carbon steel need buttering and dilution control — especially on heat-facing and Mo grades. Role context: high-Mo Ni austenitic (~6Mo class) for aggressive chloride and chemical HX tube. Consumable lot control and shielding-gas notes for SUS836LTB stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Corrosion framing beside SUS836LTB: 5–7% Mo plus N targets aggressive pitting/crevice service beyond 317L.

Surface Finishes for JIS G3463 SUS836LTB

Aggressive chloride and chemical HX tube in SUS836LTB is typically solution annealed and pickled so scale and heat tint are gone before the exchanger is built. Bright anneal is ordered when both appearance and a clean bore matter; ground or polished finishes are by agreement with OD/ID scope named. Because PREN and Mo windows are the reason this mark is chosen, finish language should never distract from verifying solution anneal on the certificate.

Finish Typical supply Order note
Solution annealed and pickled Standard chemical-service HX mill finish Matte, scale-free after pickle; anneal on MTC
Bright annealed Scale-free OD/ID when appearance is specified State OD, ID, or both
Ground / polished By agreement for roughness or hygienic-lean callouts Name Ra/grit and surface; polish after correct anneal
Passivated Common when chloride end-user specs require it Not a substitute for solution anneal or Mo chemistry

Passivation after pickling or after fabrication welding is good practice in chloride service; it still does not replace solution annealing for SUS836LTB. Keep free-iron and carbon-steel contamination off the OD/ID, and use packing that will not leave chloride films on high-Mo austenitic tube.

Inspection and Testing for JIS G3463 SUS836LTB

Clause 13/14 define sampling and retests. For SUS836LTB, keep the heat/lot identity unbroken from melt to bundle tag. Duty: high-Mo Ni austenitic (~6Mo class) for aggressive chloride and chemical HX tube. Sampling plans for SUS836LTB keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Size practice for SUS836LTB remains seamless cold-finished HX OD; NDT class often elevated by purchaser.

Intergranular corrosion testing is annex/special — order it when polythionic or weld-decay risk is written into the duty file for SUS836LTB. Non-conforming SUS836LTB lengths are segregated and retested or rejected under retest clauses rather than reworked into unmarked stock. Keep the SUS836LTB caution visible here: do not invent PREN posters; bring medium data — duplex may still win on strength or cost.

Packaging and Shipping for JIS G3463 SUS836LTB

Small-OD SUS836LTB often ships in crates; large-OD in strapped bundles with OD pads. Confirm destination handling limits on the RFQ. Use: severe chloride condensers, bleach chemical coolers, and high-PREN austenitic tube bundles. Bundle tickets for SUS836LTB repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Size practice for SUS836LTB remains seamless cold-finished HX OD; NDT class often elevated by purchaser.

Bevelled ends get protectors so landing edges survive trucking. Size hint: seamless cold-finished HX OD; NDT class often elevated by purchaser. Desiccant and wrap choices for SUS836LTB follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Weld-shop note tied to SUS836LTB: 6Mo / high-Ni Mo fillers; strict purge and heat-input control.

Storage advice on arrival: keep bundles dry and off carbon-steel floors. Use thread: severe chloride condensers, bleach chemical coolers, and high-PREN austenitic tube bundles. Claims handling for SUS836LTB starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Weld-shop note tied to SUS836LTB: 6Mo / high-Ni Mo fillers; strict purge and heat-input control.

Why Choose SHH STEEL

Project teams working to Japanese boiler/HX specs need a supplier that reads TB suffixes correctly. SHH STEEL can make SUS836LTB to that discipline. Caution we keep visible: do not invent PREN posters; bring medium data — duplex may still win on strength or cost. SHH STEEL can produce and supply SUS836LTB against the OD × wall, process symbol, and test scope on your RFQ without swapping in an unstated sister grade.

Dual-cert discussions (JIS + ASTM) are handled with two acceptance regimes in view, not one certificate stretched by hope. Sisters: SUS890LTB, SUS312LTB, SUS317LTB, SUS316LTB. Ask for a written acknowledgement that names SUS836LTB, the manufacture process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS836LTB to that written scope.

Supply Capability

Whether you need prototype bundles or project tonnage of SUS836LTB, SHH STEEL can supply against a clear OD × wall and test matrix. Duty: severe chloride condensers, bleach chemical coolers, and high-PREN austenitic tube bundles. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS836LTB when the mill schedule allows.

Item Capability
Standard JIS G3463 stainless steel tubes for boilers and heat exchangers
Grade symbol SUS836LTB
Product form Seamless (S) and welded (A / L / E) tube; finishes S-H / S-C / A / A-C / E-C as marked
Delivery condition solution annealed
Documents Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered)
Typical OD practice 15.9–139.8 mm per standard Note 1; other by agreement
Wall / gauge OD × wall / BWG-class HX gauges within Attached Tables; other by agreement

Stock / Available sizes

Stock / Available sizes: SHH STEEL quotes rolling/welding slots for SUS836LTB rather than promising anonymous warehouse tons. Typical conversation starts around seamless cold-finished HX OD; NDT class often elevated by purchaser. SHH STEEL can supply alternate schedules and measured walls for SUS836LTB once the design pressure and corrosion allowance are clear. SHH STEEL can supply alternate schedules and measured walls for SUS836LTB once design pressure and corrosion allowance are clear. Keep the SUS836LTB caution visible here: do not invent PREN posters; bring medium data — duplex may still win on strength or cost.

If the project needs dual JIS G3463 + ASTM documentation, say so before melt. Caution: do not invent PREN posters; bring medium data — duplex may still win on strength or cost. SHH STEEL can produce trial lengths of SUS836LTB for procedure qualification before the bulk release when the project calendar needs it.

FAQ

What is JIS G3463 SUS836LTB stainless steel tube used for?
JIS G3463 SUS836LTB is stainless tube for boiler and heat-exchanger service (superheater, HX, condenser, catalyser) — severe chloride condensers, bleach chemical coolers, and high-PREN austenitic tube bundles. Role summary: high-Mo Ni austenitic (~6Mo class) for aggressive chloride and chemical HX tube. It is a Japanese boiler/HX tube product standard mark, not an automatic ASTM A213 certificate.
Does JIS G3463 SUS836LTB cover seamless and welded tube?
Yes. Manufacture allows seamless and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish marks such as S-H, S-C, A-C, or E-C. SHH STEEL can produce and supply either route for SUS836LTB when the mill can meet the ordered size and tests. The title omits Seamless/Welded because JIS G3463 covers both manufacture routes — the PO must still name the process mark.
What heat treatment applies to SUS836LTB?
SUS836LTB is delivered solution annealed under JIS G3463. Table 2 reference: 1010 °C min, rapid cool. Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
How does SUS836LTB compare with sister grades SUS890LTB, SUS312LTB, SUS317LTB?
SUS836LTB is filed as austenitic. Typical sisters on the same RFQ are SUS890LTB, SUS312LTB, SUS317LTB. Design caution: do not invent PREN posters; bring medium data — duplex may still win on strength or cost Pick the sister when the medium or strength floor outgrows this symbol rather than stretching wall alone.
What tests appear on the mill certificate for SUS836LTB?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), flattening/flaring as applicable, dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
Is ~6Mo / high-Mo Ni austenitic (JIS SUS836L) the same as ordering SUS836LTB?
No. ~6Mo / high-Mo Ni austenitic (JIS SUS836L) is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3463 and SUS836LTB so cast limits, heat treatment, and process marks are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for JIS G3463 SUS836LTB?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS836LTB within the typical 15.9–139.8 mm OD practice, with measured walls by agreement. Size context: seamless cold-finished HX OD; NDT class often elevated by purchaser. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should SUS836LTB be welded?
Shop guidance: 6Mo / high-Ni Mo fillers; strict purge and heat-input control. Mill heat treatment of seamless or welded tube does not replace a qualified WPS on fabricator joints or tube-to-tubesheet welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: do not invent PREN posters; bring medium data — duplex may still win on strength or cost
When should I choose a duplex or higher-Mo grade instead of SUS836LTB?
Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: do not invent PREN posters; bring medium data — duplex may still win on strength or cost Sister pointers: SUS890LTB, SUS312LTB, SUS317LTB. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify JIS G3463 SUS836LTB with ASTM A213 or ASME SA213?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3463 SUS836LTB does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for SUS836LTB?
Pickled after heat treatment is the usual HX tube supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS836LTB when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

JIS G3463 SUS836LTB is stainless steel tube for boiler and heat-exchanger service — high-Mo Ni austenitic (~6Mo class) for aggressive chloride and chemical HX tube. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS890LTB, SUS312LTB, SUS317LTB. Related ASTM A213 pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process mark, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X