JIS G3463 SUS430TB Stainless Steel Tube

JIS G3463 SUS430TB stainless steel tube (430 / UNS S43000), ferritic, Table 3 cast analysis, Rm min 412 N/mm² / proof min 245 N/mm², annealed. SHH STEEL can produce and supply seamless or welded routes with mill certificates.
Grade
SUS430TB (430 / UNS S43000 — body alias)
Standard
JIS G3463
Product form
Seamless and welded stainless steel boiler/HX tube, delivery annealed
Size
Typically OD 15.9–139.8 mm (Note 1); OD × wall (HX/boiler gauges) by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is JIS G3463 SUS430TB Stainless Steel Tube

JIS G3463 is the Japanese Industrial Standard for stainless steel tubes used in boiler and heat-exchanger service (superheater, HX, condenser, catalyser). Grade symbol SUS430TB sits in the ferritic set of Table 1. JIS G3463 SUS430TB is the classic 17Cr ferritic HX mark — useful when the water is mild and the budget refuses nickel.

SHH STEEL can produce and supply JIS G3463 SUS430TB as seamless or welded tube across the enquiry OD×wall band, solution-annealed or annealed as Table 2 requires, pickled or bright-finished, and documented on mill test certificates tied to cast analysis and tensile results. Duty focus: 17Cr ferritic workhorse for mild aqueous HX and condenser tube.

Shop language may still say “430 tube,” yet that commercial alias does not select Japanese cast limits, process symbols, or hydraulic/NDT rules. The purchase order has to name JIS G3463 and SUS430TB so the mill applies the correct analysis, heat treatment, mechanical floors, and marking. Design caution: weld grain growth and toughness limits; prefer stabilised L sisters for dense weld maps.

Scope discipline: SUS430TB is HX tube product under JIS G3463, not a piping product under JIS G3459 and not an ASTM A213 order by default. Sister marks often compared on the same RFQ include SUS430LXTB, SUS430J1LTB, SUS436LTB, SUS444TB. Role reminder: 17Cr ferritic workhorse for mild aqueous HX and condenser tube. Document the medium, design temperature, and weld map beside the SUS430TB line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Weld-shop note tied to SUS430TB: 430/ferritic fillers; low heat input; consider SUS430LXTB for welded corrosive-lean duty.

Inside this JIS G3463 series, compare SUS430LXTB, SUS430J1LTB, SUS436LTB, SUS444TB. Hub: JIS G3463. ASTM/ASME related product pages (not interchangeable by default): ASTM A213.

Chemical Composition of JIS G3463 SUS430TB

Cast analysis for JIS G3463 SUS430TB follows Table 3. Key windows on a typical certificate include C ≤0.12, Si ≤0.75, Mn ≤1.00, P ≤0.040, S ≤0.030, Cr 16.00–18.00. SHH STEEL ties the heat number on the tube marking to the same cast line on the MTC. Commercial alias 430 / UNS S43000 is body text only. Corrosion thread: 17Cr handles many fresh-water duties; chlorides and crevices push you to 436L/444 or austenitics.

Chemical limits for SUS430TB under JIS G3463 appear in the table underneath. Source priority is the 2021 Table 3 extract cross-checked to public Nikko / supplier tables. If your client specification cites a different edition footnote, send it before the heat is melted. Duty thread: 17Cr ferritic workhorse for mild aqueous HX and condenser tube.

Grade C Si Mn P S Cr
SUS430TB ≤0.12 ≤0.75 ≤1.00 ≤0.040 ≤0.030 16.00–18.00

Mechanical Properties of JIS G3463 SUS430TB

Ambient tensile floors for SUS430TB come from JIS G3463 Table 4: Rm min 412 N/mm², proof stress min 245 N/mm², elongation min 20% (OD ≥20 mm, No.11/12). These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: ferritic. Caution: weld grain growth and toughness limits; prefer stabilised L sisters for dense weld maps.

Grade Rm min (N/mm²) Proof stress min (N/mm²) A OD≥20 mm No.11/12 min (%) A 10≤OD<20 mm No.11 min (%) A OD<10 mm No.11 min (%)
SUS430TB 412 245 20 15 12

Ambient values from JIS G3463 Table 4 for SUS430TB. Heat treatment (Table 2): 720 °C min, air or slow cool. Elongation reductions apply for walls under 8 mm on No.12 pieces. For heat-exchanger tube the purchaser may designate an upper tensile limit (Table 4 min + 200 N/mm²) when necessary.

Manufacture of JIS G3463 SUS430TB Tube (Seamless and Welded)

JIS G3463 manufactures SUS430TB by seamless (symbol S) or welded routes — automatic arc (A), laser (L), or electric-resistance (E) — then applies the ordered finish: hot finish H, cold finish C, hot finish S-H or cold finish S-C / A-C / E-C as marked. SHH STEEL confirms the Table 1 symbol string on the acknowledgement before rolling or welding starts.

Ferritic heats are annealed (700 °C min, or 720 °C min for SUS430J1LTB) with rapid or slow cooling as Table 2 allows — not austenitic solution practice. Heat-treatment reference for SUS430TB: 720 °C min, air or slow cool. Pickling follows unless bright heat treatment leaves a scale-free surface. Duty thread: 17Cr ferritic workhorse for mild aqueous HX and condenser tube.

When dual documentation against ASTM A213 is requested for a related chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for SUS430TB: HX OD 15.9–38.1 mm common; ERW or seamless.

Dimensions and Tolerances for JIS G3463 SUS430TB

SHH STEEL aligns nominal diameter (A/B), outside diameter, schedule or wall, and length tolerance for SUS430TB before the mill slot is locked. Standard Note 1 frames typical OD from 15.9 mm to 139.8 mm (standard Note 1 general practice). Size hint: HX OD 15.9–38.1 mm common; ERW or seamless. Tolerance class follows the process route ordered for SUS430TB, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Weld-shop note tied to SUS430TB: 430/ferritic fillers; low heat input; consider SUS430LXTB for welded corrosive-lean duty.

Length supply may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against the packaging clause so pickled or polished finishes are not iron-stained in transit. Duty thread: 17Cr ferritic workhorse for mild aqueous HX and condenser tube. Fixed lengths and multiple cut lengths for SUS430TB are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Keep the SUS430TB caution visible here: weld grain growth and toughness limits; prefer stabilised L sisters for dense weld maps.

Equivalent Grades for JIS G3463 SUS430TB

Under JIS G3463, SUS430TB is the governing heat-exchanger and boiler tube grade on this page. Commercial talk often shortens it to 430 or UNS S43000, which is fine in body text and dual-cert conversations, but the purchase order and mill test certificate still have to carry the JIS G3463 SUS430TB line. Related ASTM tube pages in the 430 chemistry family are different product standards with their own wall bases, tensile tables, and NDT rules, so they are not interchangeable by default.

System Designation Notes
JIS G3463 SUS430TB Governing HX/boiler tube grade for this page
Commercial / UNS (body only) 430 / UNS S43000 Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A213 / A268 related TP430 family (ferritic tube practice) Related chemistry family — different product standard; not interchangeable by default
EN / other 1.4016 (X6Cr17) approximate wrought name Starting point for comparison only; no one-to-one tube product asserted here

Inside the G3463 ferritic band, compare sister grades SUS430LXTB, SUS430J1LTB, SUS436LTB, SUS444TB before you swap marks for weld density or chloride duty. Weld grain growth and toughness limits still apply on plain 430 tube, so dense weld maps usually prefer a stabilised L sister. Hub for the full series: JIS G3463.

Heat Treatment and Delivery Condition for JIS G3463 SUS430TB

SUS430TB is delivered annealed under JIS G3463. Table 2 reference: 720 °C min, air or slow cool. Fabricator heat treatment after hot bending should chase the same family practice. Weld thread: 430/ferritic fillers; low heat input; consider SUS430LXTB for welded corrosive-lean duty. Recorded furnace charts for SUS430TB should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Size practice for SUS430TB remains HX OD 15.9–38.1 mm common; ERW or seamless.

Cooling type matters — austenitic and duplex need rapid cool after solution treatment; ferritic anneal practice allows rapid or slow cool per Table 2. Duty thread: 17Cr ferritic workhorse for mild aqueous HX and condenser tube. Field heat treatment of SUS430TB after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Keep the SUS430TB caution visible here: weld grain growth and toughness limits; prefer stabilised L sisters for dense weld maps.

Corrosion Resistance of JIS G3463 SUS430TB

Corrosion behaviour of JIS G3463 SUS430TB tracks its ferritic balance: 17Cr handles many fresh-water duties; chlorides and crevices push you to 436L/444 or austenitics. Optional annex corrosion tests (oxalic, Strauss, Huey, etc.) are special quality items — order them when the duty needs coupon evidence. Design caution: weld grain growth and toughness limits; prefer stabilised L sisters for dense weld maps.

For heat-facing austenitics, oxidation resistance may dominate over aqueous IGC talk; for duplex and Mo austenitics, chlorides dominate; for ferritics, mild aqueous and weld practice dominate. SUS430TB is filed as ferritic. Caution: weld grain growth and toughness limits; prefer stabilised L sisters for dense weld maps. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for SUS430TB rather than relying on schedule thickness alone. Corrosion framing beside SUS430TB: 17Cr handles many fresh-water duties; chlorides and crevices push you to 436L/444 or austenitics.

Applications of JIS G3463 SUS430TB Tube

Applications of JIS G3463 SUS430TB tube centre on fresh-water coolers, HVAC exchangers, and mild chemical HX where nickel cost is unjustified. Role summary: 17Cr ferritic workhorse for mild aqueous HX and condenser tube. When a related chemistry is required under ASTM A213 or A269, open those sister pages — acceptance text is not automatic.

Downstream fabricators should inherit the same grade symbol on cut lists so informal alias substitutions do not creep in. Primary application sketch: fresh-water coolers, HVAC exchangers, and mild chemical HX where nickel cost is unjustified. Duty thread: 17Cr ferritic workhorse for mild aqueous HX and condenser tube. Commissioning teams benefit when the as-built dossier repeats SUS430TB beside heat numbers, linking isometric revisions to the same mill certificates. This paragraph is locked to SUS430TB duty: 17Cr ferritic workhorse for mild aqueous HX and condenser tube.

Weldability of JIS G3463 SUS430TB

SUS430TB is welded both as a mill product (A/L/E routes) and as fabricator joints on bundles. Shop guidance: 430/ferritic fillers; low heat input; consider SUS430LXTB for welded corrosive-lean duty. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Procedure qualification for SUS430TB should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. Corrosion framing beside SUS430TB: 17Cr handles many fresh-water duties; chlorides and crevices push you to 436L/444 or austenitics.

Filler selection should match or over-alloy the base chemistry as the WPS demands. Heat input, interpass temperature, and shielding follow the family — austenitic, duplex, or ferritic — not a single shop habit. Caution: weld grain growth and toughness limits; prefer stabilised L sisters for dense weld maps. Consumable lot control and shielding-gas notes for SUS430TB stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. This paragraph is locked to SUS430TB duty: 17Cr ferritic workhorse for mild aqueous HX and condenser tube.

Surface Finishes for JIS G3463 SUS430TB

For SUS430TB heat-exchanger supply, annealed and pickled after heat treatment is the usual mill finish: matte, scale-free, and ready for bundle assembly on fresh-water coolers and HVAC exchangers. Bright anneal or a ground/polished callout is available by agreement, but the order must name whether OD, ID, or both surfaces are in scope. Ambiguous “bright tube” wording is clarified before finishing slots are booked for this 17Cr workhorse grade.

Finish Typical supply Order note
Annealed and pickled Standard HX/boiler tube mill finish after anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts on coolers Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct anneal under G3463

Passivation restores the chromium-rich film after pickling or light fabrication work; it does not replace the anneal that sets SUS430TB mechanical properties. Keep carbon-steel tooling and strapping off finished bundles — free-iron stains show up later as rust blooms on 17Cr ferritic tube. Reject grinding burns, embedded free iron, and unrepaired weld undercut before packing closes.

Inspection and Testing for JIS G3463 SUS430TB

Inspection for JIS G3463 SUS430TB covers cast analysis, tensile tests, flattening or weld bend as applicable, hydrostatic test or NDT, dimensions, and appearance. Special quality annex items (IGC, grain size, etc.) apply only when ordered. Documents follow JIS G 0415 / purchaser-specified EN 10204 styles. Sampling plans for SUS430TB keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Corrosion framing beside SUS430TB: 17Cr handles many fresh-water duties; chlorides and crevices push you to 436L/444 or austenitics.

Marking includes SUS430TB, manufacture/finish symbols, manufacturer, and other mandatory marking-clause data. Traceability from stencil to MTC is part of supply, not an upgrade. Use: fresh-water coolers, HVAC exchangers, and mild chemical HX where nickel cost is unjustified. Non-conforming SUS430TB lengths are segregated and retested or rejected under retest clauses rather than reworked into unmarked stock. This paragraph is locked to SUS430TB duty: 17Cr ferritic workhorse for mild aqueous HX and condenser tube.

Packaging and Shipping for JIS G3463 SUS430TB

Packaging for SUS430TB uses wooden boxes, plywood cases, or bundled frames with waterproof wrapping as the OD and finish demand. Soft separators protect pickled and polished surfaces. Ends receive caps or bevel protectors when ordered. Bundle tickets for SUS430TB repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Weld-shop note tied to SUS430TB: 430/ferritic fillers; low heat input; consider SUS430LXTB for welded corrosive-lean duty.

Carbon-steel strapping never contacts the stainless OD without a barrier. Mixed-grade bundles are forbidden when chemistry integrity matters. Caution: weld grain growth and toughness limits; prefer stabilised L sisters for dense weld maps. Desiccant and wrap choices for SUS430TB follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Application context for SUS430TB stays fresh-water coolers, HVAC exchangers, and mild chemical HX where nickel cost is unjustified.

Shipping documents list JIS G3463, SUS430TB, sizes, quantities, heat numbers, and certificate type. SHH STEEL coordinates inland trucking and FOB/CIF packing scopes as the order states. Role: 17Cr ferritic workhorse for mild aqueous HX and condenser tube. Claims handling for SUS430TB starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Weld-shop note tied to SUS430TB: 430/ferritic fillers; low heat input; consider SUS430LXTB for welded corrosive-lean duty.

Why Choose SHH STEEL

SHH STEEL can produce and supply JIS G3463 SUS430TB with the process route, heat treatment, and tests named on your enquiry — not a bait-and-switch alias. Mill partners run stainless tube capacity that covers seamless and welded Table 1 symbols for this mark. Duty focus: 17Cr ferritic workhorse for mild aqueous HX and condenser tube.

Technical sales can map SUS430TB against sisters SUS430LXTB, SUS430J1LTB, SUS436LTB, SUS444TB and live ASTM pages without pretending standards are identical. Inspection coordination and export packing are in-house habits, not afterthoughts. Ask for a written acknowledgement that names SUS430TB, the manufacture process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS430TB to that written scope.

Supply Capability

SHH STEEL can produce and supply JIS G3463 SUS430TB across enquiry-oriented OD × wall bands, in seamless or welded routes, with certificates and optional annex tests as ordered. Summary capability follows in the table; stock language below is an RFQ map, not a frozen tonnage catalogue. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS430TB when the mill schedule allows.

Item Capability
Standard JIS G3463 stainless steel tubes for boilers and heat exchangers
Grade symbol SUS430TB
Product form Seamless (S) and welded (A / L / E) tube; finishes S-H / S-C / A / A-C / E-C as marked
Delivery condition annealed
Documents Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered)
Typical OD practice 15.9–139.8 mm per standard Note 1; other by agreement
Wall / gauge OD × wall / BWG-class HX gauges within Attached Tables; other by agreement

Stock / Available sizes

SHH STEEL can produce and supply JIS G3463 SUS430TB. Stock / Available sizes: enquiry band typically aligns with 15.9–139.8 mm OD practice under G3463 Note 1, with OD×wall HX gauges; schedule 5S–80 (and heavier by agreement) depending on grade family. For SUS430TB, practical fast-track sizes often sit in mid-bore process and utility ranges — send the OD × wall list for a firm acknowledgement. Context: HX OD 15.9–38.1 mm common; ERW or seamless.

Cut lengths, bevels, special NDT, and IGC annex tests add lead time — call them early. Sisters often quoted alongside: SUS430LXTB, SUS430J1LTB, SUS436LTB, SUS444TB. Email the size list to start. SHH STEEL can produce trial lengths of SUS430TB for procedure qualification before the bulk release when the project calendar needs it. SHH STEEL can produce trial lengths of SUS430TB for procedure qualification before bulk release when the project calendar needs it. Keep the SUS430TB caution visible here: weld grain growth and toughness limits; prefer stabilised L sisters for dense weld maps.

FAQ

What is JIS G3463 SUS430TB stainless steel tube used for?
JIS G3463 SUS430TB is stainless tube for boiler and heat-exchanger service (superheater, HX, condenser, catalyser) — fresh-water coolers, HVAC exchangers, and mild chemical HX where nickel cost is unjustified. Role summary: 17Cr ferritic workhorse for mild aqueous HX and condenser tube. It is a Japanese boiler/HX tube product standard mark, not an automatic ASTM A213 certificate.
Does JIS G3463 SUS430TB cover seamless and welded tube?
Yes. Manufacture allows seamless and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish marks such as S-H, S-C, A-C, or E-C. SHH STEEL can produce and supply either route for SUS430TB when the mill can meet the ordered size and tests. The title omits Seamless/Welded because JIS G3463 covers both manufacture routes — the PO must still name the process mark.
What heat treatment applies to SUS430TB?
SUS430TB is delivered annealed under JIS G3463. Table 2 reference: 720 °C min, air or slow cool. Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
How does SUS430TB compare with sister grades SUS430LXTB, SUS430J1LTB, SUS436LTB?
SUS430TB is filed as ferritic. Typical sisters on the same RFQ are SUS430LXTB, SUS430J1LTB, SUS436LTB. Design caution: weld grain growth and toughness limits; prefer stabilised L sisters for dense weld maps Pick the sister when the medium or strength floor outgrows this symbol rather than stretching wall alone.
What tests appear on the mill certificate for SUS430TB?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), flattening/flaring as applicable, dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
Is 430 / UNS S43000 the same as ordering SUS430TB?
No. 430 / UNS S43000 is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3463 and SUS430TB so cast limits, heat treatment, and process marks are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for JIS G3463 SUS430TB?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS430TB within the typical 15.9–139.8 mm OD practice, with measured walls by agreement. Size context: HX OD 15.9–38.1 mm common; ERW or seamless. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should SUS430TB be welded?
Shop guidance: 430/ferritic fillers; low heat input; consider SUS430LXTB for welded corrosive-lean duty. Mill heat treatment of seamless or welded tube does not replace a qualified WPS on fabricator joints or tube-to-tubesheet welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: weld grain growth and toughness limits; prefer stabilised L sisters for dense weld maps
When should I choose a duplex or higher-Mo grade instead of SUS430TB?
Move when chloride pitting, crevice attack, or SCC risk exceeds what ferritic practice can defend for the temperature and stress state. Caution for this mark: weld grain growth and toughness limits; prefer stabilised L sisters for dense weld maps Sister pointers: SUS430LXTB, SUS430J1LTB, SUS436LTB. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify JIS G3463 SUS430TB with ASTM A213 or ASME SA213?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3463 SUS430TB does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for SUS430TB?
Pickled after heat treatment is the usual HX tube supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS430TB when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

JIS G3463 SUS430TB is stainless steel tube for boiler and heat-exchanger service — 17Cr ferritic workhorse for mild aqueous HX and condenser tube. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS430LXTB, SUS430J1LTB, SUS436LTB. Related ASTM A213 pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process mark, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X