JIS G3463 SUS321TB Stainless Steel Tube
What is JIS G3463 SUS321TB Stainless Steel Tube
Boiler and heat-exchanger packages that cite Japanese product standards look to JIS G3463 — Stainless steel boiler and heat exchanger tubes — rather than inventing a mill grade from AISI shorthand alone. SUS321TB is the Table 1 symbol for this austenitic chemistry. JIS G3463 SUS321TB is the Ti-stabilised boiler/HX answer when the project refuses molybdenum but still fears weld decay.
Mill path for SUS321TB: Table 1 manufacture/finish symbols, Table 2 heat treatment, Table 3 cast chemistry, Table 4 tensile floors. SHH STEEL can make and supply the grade to that stack with hydrostatic or NDT acceptance as ordered. Typical use: refinery HX, steam reformers’ waste-heat exchangers, and welded 18-8 bundles in the sensitising range.
Body text may mention 321 / UNS S32100 for cross-reference, but the H1 and order line stay on SUS321TB. Silent alias swaps are how wrong carbon ceilings and wrong tensile tables enter the MTC. Keep this caution in view: Ti must meet the 5×C rule on the MTC; not a chloride upgrade over 304 — use Mo grades when pitting governs.
Order the standard the drawing and regulatory file actually require. Inside this G3463 series, compare SUS321HTB, SUS347TB, SUS304TB, SUS304LTB before stretching surface finish or schedule alone. Duty thread: Ti-stabilised 18-8 HX / superheater tube for weld-decay and polythionic-lean resistance without molybdenum. Document the medium, design temperature, and weld map beside the SUS321TB line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Size practice for SUS321TB remains superheater and HX OD within 15.9–76.2 mm common; seamless dominant for pressure parts.
Inside this JIS G3463 series, compare SUS321HTB, SUS347TB, SUS304TB, SUS304LTB. Hub: JIS G3463. ASTM/ASME related product pages (not interchangeable by default): A213 TP321, ASTM A213.
Chemical Composition of JIS G3463 SUS321TB
Table 3 sets the melt limits for SUS321TB. Highlight band: C ≤0.08, Si ≤1.00, Mn ≤2.00, P ≤0.040, S ≤0.030, Ni 9.00–13.00, Cr 17.00–19.00. Product analysis, when ordered, applies JIS G 0321 stainless product tolerances on top of Table 3. Alias note: 321 / UNS S32100. Every ladle analysis for SUS321TB is checked against those windows before the heat is released to piercing, welding, or finishing, and the same numbers reappear on the inspection document. Size practice for SUS321TB remains superheater and HX OD within 15.9–76.2 mm common; seamless dominant for pressure parts.
The composition table below is the cast window SHH STEEL quotes against for SUS321TB. Edition framing is JIS G3463. Use thread: refinery HX, steam reformers’ waste-heat exchangers, and welded 18-8 bundles in the sensitising range. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for SUS321TB before the order is acknowledged. Weld-shop note tied to SUS321TB: 321/347-class fillers; optional stabilisation anneal 850–930 °C when ordered.
| Grade | C | Si | Mn | P | S | Ni | Cr | Ti |
|---|---|---|---|---|---|---|---|---|
| SUS321TB | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.040 | ≤0.030 | 9.00–13.00 | 17.00–19.00 | ≥5×C% |
Mechanical Properties of JIS G3463 SUS321TB
Table 4 mechanical acceptance for SUS321TB: Rm min 520 N/mm², proof stress min 206 N/mm², elongation min 35% (OD ≥20 mm, No.11/12). Elongation rules change for walls under 8 mm and are not mandatory below 40 mm OD (record only unless agreed). Delivery framing: solution annealed. Tensile sampling follows tensile sampling clauses for the ordered test unit of SUS321TB, and retests follow retest clauses when a result sits under the Table 4 floor. This paragraph is locked to SUS321TB duty: Ti-stabilised 18-8 HX / superheater tube for weld-decay and polythionic-lean resistance without molybdenum.
| Grade | Rm min (N/mm²) | Proof stress min (N/mm²) | A OD≥20 mm No.11/12 min (%) | A 10≤OD<20 mm No.11 min (%) | A OD<10 mm No.11 min (%) |
|---|---|---|---|---|---|
| SUS321TB | 520 | 206 | 35 | 30 | 27 |
Ambient values from JIS G3463 Table 4 for SUS321TB. Heat treatment (Table 2): 920 °C min, rapid cool (stabilisation 850–930 °C may be ordered). Elongation reductions apply for walls under 8 mm on No.12 pieces. For heat-exchanger tube the purchaser may designate an upper tensile limit (Table 4 min + 200 N/mm²) when necessary.
Manufacture of JIS G3463 SUS321TB Tube (Seamless and Welded)
JIS G3463 manufactures SUS321TB by seamless (symbol S) or welded routes — automatic arc (A), laser (L), or electric-resistance (E) — then applies the ordered finish: hot finish H, cold finish C, hot finish S-H or cold finish S-C / A-C / E-C as marked. SHH STEEL confirms the Table 1 symbol string on the acknowledgement before rolling or welding starts.
After forming, SUS321TB receives Table 2 treatment — 920 °C min, rapid cool (stabilisation 850–930 °C may be ordered). Austenitic heats take solution annealing with rapid cooling; hot-finished seamless may omit separate solution treatment when hot-worked and rapidly cooled in-line under the Table 2 note, unless the purchaser forbids it. Use thread: refinery HX, steam reformers’ waste-heat exchangers, and welded 18-8 bundles in the sensitising range.
Marking carries the grade symbol SUS321TB, process/finish marks, manufacturer ID, and other marking-clause items. Size hint: superheater and HX OD within 15.9–76.2 mm common; seamless dominant for pressure parts. Weld thread: 321/347-class fillers; optional stabilisation anneal 850–930 °C when ordered. Hydrostatic pressure or NDT class for SUS321TB is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Weld-shop note tied to SUS321TB: 321/347-class fillers; optional stabilisation anneal 850–930 °C when ordered.
Dimensions and Tolerances for JIS G3463 SUS321TB
Dimensional order lines for SUS321TB should state OD × wall (or OD×wall HX gauges; schedule 5S/10S/20S/40/80/…), length type, and end finish. Tolerances follow dimensional tolerance clauses by process route. Use: refinery HX, steam reformers’ waste-heat exchangers, and welded 18-8 bundles in the sensitising range. Tolerance class follows the process route ordered for SUS321TB, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Keep the SUS321TB caution visible here: Ti must meet the 5×C rule on the MTC; not a chloride upgrade over 304 — use Mo grades when pitting governs.
OD and wall tolerances differ for hot-finished seamless versus cold-finished / welded routes — quote the process symbol with the size. Caution: Ti must meet the 5×C rule on the MTC; not a chloride upgrade over 304 — use Mo grades when pitting governs. Fixed lengths and multiple cut lengths for SUS321TB are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Keep the SUS321TB caution visible here: Ti must meet the 5×C rule on the MTC; not a chloride upgrade over 304 — use Mo grades when pitting governs.
Equivalent Grades for JIS G3463 SUS321TB
SUS321TB is the JIS G3463 designation. Alias 321 / UNS S32100 appears only as a cross-walk. Compare sisters SUS321HTB, SUS347TB, SUS304TB, SUS304LTB when the medium or temperature outgrows this mark. Hook: lock SUS321TB on the PO. When a dual-cert path is required, list both JIS G3463 SUS321TB and the ASTM mark with separate test scopes instead of assuming one chemistry line clears both files. Keep the SUS321TB caution visible here: Ti must meet the 5×C rule on the MTC; not a chloride upgrade over 304 — use Mo grades when pitting governs.
Heat Treatment and Delivery Condition for JIS G3463 SUS321TB
Mill heat treatment for SUS321TB: 920 °C min, rapid cool (stabilisation 850–930 °C may be ordered). Bright annealing may omit pickling when the surface is scale-free. Delivery label: solution annealed. Recorded furnace charts for SUS321TB should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. This paragraph is locked to SUS321TB duty: Ti-stabilised 18-8 HX / superheater tube for weld-decay and polythionic-lean resistance without molybdenum.
Certificate wording for SUS321TB should show the heat-treatment condition actually performed, not a generic “annealed” stamp that hides temperature. Use: refinery HX, steam reformers’ waste-heat exchangers, and welded 18-8 bundles in the sensitising range. Field heat treatment of SUS321TB after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Size practice for SUS321TB remains superheater and HX OD within 15.9–76.2 mm common; seamless dominant for pressure parts.
Corrosion Resistance of JIS G3463 SUS321TB
stabilisation protects weld HAZ; aqueous chloride ranking stays near 304 Special quality annex tests are available by agreement; they are not a blanket warranty for every process medium. Family filing: austenitic. Coupon orientation, weld condition, and surface finish for SUS321TB belong in the corrosion test order so annex results can be compared to the installed bundle honestly. Size practice for SUS321TB remains superheater and HX OD within 15.9–76.2 mm common; seamless dominant for pressure parts.
Do not market invented PREN digits. Bring medium chemistry and SHH STEEL will map SUS321TB honestly against SUS321HTB, SUS347TB, SUS304TB, SUS304LTB. Role: Ti-stabilised 18-8 HX / superheater tube for weld-decay and polythionic-lean resistance without molybdenum. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for SUS321TB rather than relying on schedule thickness alone. Size practice for SUS321TB remains superheater and HX OD within 15.9–76.2 mm common; seamless dominant for pressure parts.
Applications of JIS G3463 SUS321TB Tube
Typical BOM language pairs JIS G3463 SUS321TB with OD × wall (or schedule), manufacture/finish symbols, and heat-treatment condition. Primary sketch: refinery HX, steam reformers’ waste-heat exchangers, and welded 18-8 bundles in the sensitising range. Spool fabricators should copy SUS321TB onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Weld-shop note tied to SUS321TB: 321/347-class fillers; optional stabilisation anneal 850–930 °C when ordered.
Spell SUS321TB on tube-sheet drawings and bundle lists, bundle sheets and tubesheet specs alike. Sister options when the medium hardens: SUS321HTB, SUS347TB, SUS304TB, SUS304LTB. Commissioning teams benefit when the as-built dossier repeats SUS321TB beside heat numbers, linking isometric revisions to the same mill certificates. Keep the SUS321TB caution visible here: Ti must meet the 5×C rule on the MTC; not a chloride upgrade over 304 — use Mo grades when pitting governs.
Weldability of JIS G3463 SUS321TB
Weldability of SUS321TB follows austenitic practice. Filler/shop note: 321/347-class fillers; optional stabilisation anneal 850–930 °C when ordered. Caution: Ti must meet the 5×C rule on the MTC; not a chloride upgrade over 304 — use Mo grades when pitting governs. Procedure qualification for SUS321TB should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. Corrosion framing beside SUS321TB: stabilisation protects weld HAZ; aqueous chloride ranking stays near 304.
For welded G3463 tube, confirm whether as-welded or cold-finished welded finish is acceptable to the corrosion owner. Shop note: 321/347-class fillers; optional stabilisation anneal 850–930 °C when ordered. Consumable lot control and shielding-gas notes for SUS321TB stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Weld-shop note tied to SUS321TB: 321/347-class fillers; optional stabilisation anneal 850–930 °C when ordered.
Surface Finishes for JIS G3463 SUS321TB
Pickled mill finish covers most HX tube RFQs for SUS321TB. Bright anneal, grind, or polish only when the enquiry writes a measurable target. Use: refinery HX, steam reformers’ waste-heat exchangers, and welded 18-8 bundles in the sensitising range. Roughness or polish callouts for SUS321TB must name OD, ID, or both; ambiguous “bright tube” language is clarified before finishing slots are booked. Keep the SUS321TB caution visible here: Ti must meet the 5×C rule on the MTC; not a chloride upgrade over 304 — use Mo grades when pitting governs.
Sanitary-lean duties may add ID polish; chemical lines may prefer a clean pickle only. State the need on the SUS321TB order. Final visual standards for SUS321TB reject grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed. Weld-shop note tied to SUS321TB: 321/347-class fillers; optional stabilisation anneal 850–930 °C when ordered.
Inspection and Testing for JIS G3463 SUS321TB
SHH STEEL reports the tests actually performed for SUS321TB — no surrogate NDT lines. Hydrostatic vs eddy-current/ultrasonic choice belongs on the PO. Caution: Ti must meet the 5×C rule on the MTC; not a chloride upgrade over 304 — use Mo grades when pitting governs. Sampling plans for SUS321TB keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Application context for SUS321TB stays refinery HX, steam reformers’ waste-heat exchangers, and welded 18-8 bundles in the sensitising range.
NDT sensitivity levels and hydrostatic pressures follow the standard tables unless the purchaser specifies higher. Size context: superheater and HX OD within 15.9–76.2 mm common; seamless dominant for pressure parts. Non-conforming SUS321TB lengths are segregated and retested or rejected under retest clauses rather than reworked into unmarked stock. Application context for SUS321TB stays refinery HX, steam reformers’ waste-heat exchangers, and welded 18-8 bundles in the sensitising range.
Packaging and Shipping for JIS G3463 SUS321TB
Export packing for JIS G3463 SUS321TB is built around rust prevention and transit abrasion control. Bundle tickets repeat the grade symbol and heat number. Duty: Ti-stabilised 18-8 HX / superheater tube for weld-decay and polythionic-lean resistance without molybdenum. Bundle tickets for SUS321TB repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. This paragraph is locked to SUS321TB duty: Ti-stabilised 18-8 HX / superheater tube for weld-decay and polythionic-lean resistance without molybdenum.
Marking paint and ink stickers stay chloride-lean. Heat numbers on tags match the MTC for SUS321TB. Desiccant and wrap choices for SUS321TB follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Weld-shop note tied to SUS321TB: 321/347-class fillers; optional stabilisation anneal 850–930 °C when ordered.
Photographic packing records are available on request for project QA files on SUS321TB. Claims handling for SUS321TB starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Weld-shop note tied to SUS321TB: 321/347-class fillers; optional stabilisation anneal 850–930 °C when ordered Claims handling for SUS321TB starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Order-line discipline for SUS321TB still points at role: Ti-stabilised 18-8 HX / superheater tube for weld-decay and polythionic-lean resistance without molybdenum.
Why Choose SHH STEEL
Buyers choose SHH STEEL for SUS321TB because the paperwork matches the stencil: Table 3 chemistry, Table 4 tensile, Table 2 heat treatment, and honest seamless or A/L/E welded marking. Application fit: refinery HX, steam reformers’ waste-heat exchangers, and welded 18-8 bundles in the sensitising range. SHH STEEL can produce and supply SUS321TB against the OD × wall, process symbol, and test scope on your RFQ without swapping in an unstated sister grade.
SHH STEEL will not invent PREN posters or warehouse tonnages. Bring OD × wall, medium notes, and test scope — we will quote SUS321TB cleanly. Ask for a written acknowledgement that names SUS321TB, the manufacture process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS321TB to that written scope.
Supply Capability
Supply capability for SUS321TB covers manufacture/finish symbols in Table 1, heat treatment in Table 2, and mechanical acceptance in Table 4. SHH STEEL can make the sizes on your list when the mill slot fits. Role: Ti-stabilised 18-8 HX / superheater tube for weld-decay and polythionic-lean resistance without molybdenum. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS321TB when the mill schedule allows. Keep the SUS321TB caution visible here: Ti must meet the 5×C rule on the MTC; not a chloride upgrade over 304 — use Mo grades when pitting governs.
| Item | Capability |
|---|---|
| Standard | JIS G3463 stainless steel tubes for boilers and heat exchangers |
| Grade symbol | SUS321TB |
| Product form | Seamless (S) and welded (A / L / E) tube; finishes S-H / S-C / A / A-C / E-C as marked |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered) |
| Typical OD practice | 15.9–139.8 mm per standard Note 1; other by agreement |
| Wall / gauge | OD × wall / BWG-class HX gauges within Attached Tables; other by agreement |
Stock / Available sizes
Stock / Available sizes for SUS321TB: common A-number bores with schedule or measured wall as the project uses. Seamless and welded availability varies by diameter — confirm route with the RFQ. Hint: superheater and HX OD within 15.9–76.2 mm common; seamless dominant for pressure parts. SHH STEEL can supply alternate schedules and measured walls for SUS321TB once the design pressure and corrosion allowance are clear.
Mill certificates, packing photos, and third-party witness can be bundled into the SUS321TB supply scope when the PO says so. Use: refinery HX, steam reformers’ waste-heat exchangers, and welded 18-8 bundles in the sensitising range. SHH STEEL can produce trial lengths of SUS321TB for procedure qualification before the bulk release when the project calendar needs it.
FAQ
-
What is JIS G3463 SUS321TB stainless steel tube used for?
- JIS G3463 SUS321TB is stainless tube for boiler and heat-exchanger service (superheater, HX, condenser, catalyser) — refinery HX, steam reformers’ waste-heat exchangers, and welded 18-8 bundles in the sensitising range. Role summary: Ti-stabilised 18-8 HX / superheater tube for weld-decay and polythionic-lean resistance without molybdenum. It is a Japanese boiler/HX tube product standard mark, not an automatic ASTM A213 certificate.
-
Does JIS G3463 SUS321TB cover seamless and welded tube?
- Yes. Manufacture allows seamless and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish marks such as S-H, S-C, A-C, or E-C. SHH STEEL can produce and supply either route for SUS321TB when the mill can meet the ordered size and tests. The title omits Seamless/Welded because JIS G3463 covers both manufacture routes — the PO must still name the process mark.
-
What heat treatment applies to SUS321TB?
- SUS321TB is delivered solution annealed under JIS G3463. Table 2 reference: 920 °C min, rapid cool (stabilisation 850–930 °C may be ordered). Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
-
How does SUS321TB compare with sister grades SUS321HTB, SUS347TB, SUS304TB?
- SUS321TB is filed as austenitic. Typical sisters on the same RFQ are SUS321HTB, SUS347TB, SUS304TB. Design caution: Ti must meet the 5×C rule on the MTC; not a chloride upgrade over 304 — use Mo grades when pitting governs Pick the sister when the medium or strength floor outgrows this symbol rather than stretching wall alone.
-
What tests appear on the mill certificate for SUS321TB?
- Expect cast analysis (Table 3), room-temperature tensile results (Table 4), flattening/flaring as applicable, dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
-
Is 321 / UNS S32100 the same as ordering SUS321TB?
- No. 321 / UNS S32100 is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3463 and SUS321TB so cast limits, heat treatment, and process marks are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for JIS G3463 SUS321TB?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS321TB within the typical 15.9–139.8 mm OD practice, with measured walls by agreement. Size context: superheater and HX OD within 15.9–76.2 mm common; seamless dominant for pressure parts. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
How should SUS321TB be welded?
- Shop guidance: 321/347-class fillers; optional stabilisation anneal 850–930 °C when ordered. Mill heat treatment of seamless or welded tube does not replace a qualified WPS on fabricator joints or tube-to-tubesheet welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: Ti must meet the 5×C rule on the MTC; not a chloride upgrade over 304 — use Mo grades when pitting governs
-
When should I choose a duplex or higher-Mo grade instead of SUS321TB?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: Ti must meet the 5×C rule on the MTC; not a chloride upgrade over 304 — use Mo grades when pitting governs Sister pointers: SUS321HTB, SUS347TB, SUS304TB. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify JIS G3463 SUS321TB with ASTM A213 or ASME SA213?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3463 SUS321TB does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What surface finishes are available for SUS321TB?
- Pickled after heat treatment is the usual HX tube supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS321TB when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
JIS G3463 SUS321TB is stainless steel tube for boiler and heat-exchanger service — Ti-stabilised 18-8 HX / superheater tube for weld-decay and polythionic-lean resistance without molybdenum. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS321HTB, SUS347TB, SUS304TB. Related ASTM A213 pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process mark, and medium notes to start the quote.