JIS G3463 SUS430J1LTB Stainless Steel Tube
What is JIS G3463 SUS430J1LTB Stainless Steel Tube
JIS G3463 is the Japanese Industrial Standard for stainless steel tubes used in boiler and heat-exchanger service (superheater, HX, condenser, catalyser). Grade symbol SUS430J1LTB sits in the ferritic set of Table 1. JIS G3463 SUS430J1LTB is ordered for Cu-Nb ferritic behaviour — not as a spelling variant of SUS430LXTB. Buyers working Japanese boiler and HX packages should treat SUS430J1LTB as a governed product symbol under G3463, with Table 3 chemistry and Table 4 tensile floors enforced on the same heat. Keep the SUS430J1LTB caution visible here: Cu and Nb windows are intentional — do not substitute SUS430LXTB without review.
SHH STEEL can produce and supply JIS G3463 SUS430J1LTB as seamless or welded tube across the enquiry OD×wall band, solution-annealed or annealed as Table 2 requires, pickled or bright-finished, and documented on mill test certificates tied to cast analysis and tensile results. Duty focus: Cu-Nb low-C ferritic for improved formability and mild corrosion HX tube.
Shop language may still say “Cu-Nb low-C ferritic (430J1L) tube,” yet that commercial alias does not select Japanese cast limits, process symbols, or hydraulic/NDT rules. The purchase order has to name JIS G3463 and SUS430J1LTB so the mill applies the correct analysis, heat treatment, mechanical floors, and marking. Design caution: Cu and Nb windows are intentional — do not substitute SUS430LXTB without review.
Scope discipline: SUS430J1LTB is HX tube product under JIS G3463, not a piping product under JIS G3459 and not an ASTM A213 order by default. Sister marks often compared on the same RFQ include SUS430LXTB, SUS430TB, SUS436LTB, SUS444TB. Role reminder: Cu-Nb low-C ferritic for improved formability and mild corrosion HX tube. Document the medium, design temperature, and weld map beside the SUS430J1LTB line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Corrosion framing beside SUS430J1LTB: Cu-Nb low-C balance targets formability plus mild aqueous resistance.
Inside this JIS G3463 series, compare SUS430LXTB, SUS430TB, SUS436LTB, SUS444TB. Hub: JIS G3463. ASTM/ASME related product pages (not interchangeable by default): ASTM A213.
Chemical Composition of JIS G3463 SUS430J1LTB
Cast analysis for JIS G3463 SUS430J1LTB follows Table 3. Key windows on a typical certificate include C ≤0.025, Si ≤1.00, Mn ≤1.00, P ≤0.040, S ≤0.030, Cr 16.00–20.00, Cu 0.30–0.80. SHH STEEL ties the heat number on the tube marking to the same cast line on the MTC. Commercial alias Cu-Nb low-C ferritic (430J1L) is body text only. Corrosion thread: Cu-Nb low-C balance targets formability plus mild aqueous resistance.
Chemical limits for SUS430J1LTB under JIS G3463 appear in the table underneath. Source priority is the 2021 Table 3 extract cross-checked to public Nikko / supplier tables. If your client specification cites a different edition footnote, send it before the heat is melted. Duty thread: Cu-Nb low-C ferritic for improved formability and mild corrosion HX tube.
| Grade | C | Si | Mn | P | S | Cr | Cu | N | Nb |
|---|---|---|---|---|---|---|---|---|---|
| SUS430J1LTB | ≤0.025 | ≤1.00 | ≤1.00 | ≤0.040 | ≤0.030 | 16.00–20.00 | 0.30–0.80 | ≤0.025 | 8×(C%+N%)–0.80 |
Mechanical Properties of JIS G3463 SUS430J1LTB
Ambient tensile floors for SUS430J1LTB come from JIS G3463 Table 4: Rm min 390 N/mm², proof stress min 205 N/mm², elongation min 20% (OD ≥20 mm, No.11/12). These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: ferritic. Caution: Cu and Nb windows are intentional — do not substitute SUS430LXTB without review.
| Grade | Rm min (N/mm²) | Proof stress min (N/mm²) | A OD≥20 mm No.11/12 min (%) | A 10≤OD<20 mm No.11 min (%) | A OD<10 mm No.11 min (%) |
|---|---|---|---|---|---|
| SUS430J1LTB | 390 | 205 | 20 | 15 | 12 |
Ambient values from JIS G3463 Table 4 for SUS430J1LTB. Heat treatment (Table 2): 720 °C min, air or slow cool. Elongation reductions apply for walls under 8 mm on No.12 pieces. For heat-exchanger tube the purchaser may designate an upper tensile limit (Table 4 min + 200 N/mm²) when necessary.
Manufacture of JIS G3463 SUS430J1LTB Tube (Seamless and Welded)
For SUS430J1LTB, the mill path is not “seamless only.” Table 1 explicitly pairs austenitic, duplex, and ferritic marks with seamless or A/L/E welded process symbols and S-H/S-C/A/A-C/E-C finishes. Order the combination that matches hydrostatic or NDT preference, not a habit from ASTM A213 alone. Seamless and welded options remain available for SUS430J1LTB; the acknowledgement repeats the Table 1 symbols so production cannot silently change route after the PO is firm. Weld-shop note tied to SUS430J1LTB: matching Cu-Nb ferritic practice; low heat input.
Ferritic heats are annealed (700 °C min, or 720 °C min for SUS430J1LTB) with rapid or slow cooling as Table 2 allows — not austenitic solution practice. Heat-treatment reference for SUS430J1LTB: 720 °C min, air or slow cool. Pickling follows unless bright heat treatment leaves a scale-free surface. Duty thread: Cu-Nb low-C ferritic for improved formability and mild corrosion HX tube.
When dual documentation against ASTM A213 is requested for a related chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for SUS430J1LTB: lighter walls for forming; annealed delivery at 720 °C min.
Dimensions and Tolerances for JIS G3463 SUS430J1LTB
SHH STEEL aligns nominal diameter (A/B), outside diameter, schedule or wall, and length tolerance for SUS430J1LTB before the mill slot is locked. Standard Note 1 frames typical OD from 15.9 mm to 139.8 mm (standard Note 1 general practice). Size hint: lighter walls for forming; annealed delivery at 720 °C min. Tolerance class follows the process route ordered for SUS430J1LTB, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Size practice for SUS430J1LTB remains lighter walls for forming; annealed delivery at 720 °C min.
Length supply may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against the packaging clause so pickled or polished finishes are not iron-stained in transit. Duty thread: Cu-Nb low-C ferritic for improved formability and mild corrosion HX tube. Fixed lengths and multiple cut lengths for SUS430J1LTB are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. This paragraph is locked to SUS430J1LTB duty: Cu-Nb low-C ferritic for improved formability and mild corrosion HX tube.
Equivalent Grades for JIS G3463 SUS430J1LTB
JIS G3463 SUS430J1LTB is the Cu-Nb low-carbon ferritic tube grade aimed at improved formability and mild corrosion heat-exchanger duty. Commercial shorthand “430J1L” is body-only language for catalogues and dual-cert talk; the order line stays on SUS430J1LTB. There is no clean one-to-one ASTM or EN tube product asserted here — chemistry kinship with other 17Cr ferritics is not acceptance kinship under G3463.
| System | Designation | Notes |
|---|---|---|
| JIS G3463 | SUS430J1LTB | Governing HX/boiler tube grade for this page |
| Commercial / UNS (body only) | 430J1L (Cu-Nb low-C ferritic) | Useful in dual-cert talk; Cu and Nb windows are intentional |
| ASTM A213 / A269 related | No one-to-one TP asserted | Related 17Cr ferritic family only — different product standard |
| EN / other | No one-to-one asserted | Starting point for comparison only; do not swap for SUS430LXTB without review |
Cu and Nb limits on SUS430J1LTB are deliberate — do not substitute SUS430LXTB or plain SUS430TB without engineering review. Other sisters in the band: SUS436LTB, SUS444TB. Series hub: JIS G3463.
Heat Treatment and Delivery Condition for JIS G3463 SUS430J1LTB
SUS430J1LTB is delivered annealed under JIS G3463. Table 2 reference: 720 °C min, air or slow cool. Fabricator heat treatment after hot bending should chase the same family practice. Weld thread: matching Cu-Nb ferritic practice; low heat input. Recorded furnace charts for SUS430J1LTB should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Weld-shop note tied to SUS430J1LTB: matching Cu-Nb ferritic practice; low heat input.
Cooling type matters — austenitic and duplex need rapid cool after solution treatment; ferritic anneal practice allows rapid or slow cool per Table 2. Duty thread: Cu-Nb low-C ferritic for improved formability and mild corrosion HX tube. Field heat treatment of SUS430J1LTB after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Weld-shop note tied to SUS430J1LTB: matching Cu-Nb ferritic practice; low heat input.
Corrosion Resistance of JIS G3463 SUS430J1LTB
Corrosion behaviour of JIS G3463 SUS430J1LTB tracks its ferritic balance: Cu-Nb low-C balance targets formability plus mild aqueous resistance. Optional annex corrosion tests (oxalic, Strauss, Huey, etc.) are special quality items — order them when the duty needs coupon evidence. Design caution: Cu and Nb windows are intentional — do not substitute SUS430LXTB without review.
For heat-facing austenitics, oxidation resistance may dominate over aqueous IGC talk; for duplex and Mo austenitics, chlorides dominate; for ferritics, mild aqueous and weld practice dominate. SUS430J1LTB is filed as ferritic. Caution: Cu and Nb windows are intentional — do not substitute SUS430LXTB without review. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for SUS430J1LTB rather than relying on schedule thickness alone. Size practice for SUS430J1LTB remains lighter walls for forming; annealed delivery at 720 °C min.
Applications of JIS G3463 SUS430J1LTB Tube
Applications of JIS G3463 SUS430J1LTB tube centre on formed ferritic HX, mild water coolers, and Japanese specs that name 430J1L. Role summary: Cu-Nb low-C ferritic for improved formability and mild corrosion HX tube. When a related chemistry is required under ASTM A213 or A269, open those sister pages — acceptance text is not automatic.
Downstream fabricators should inherit the same grade symbol on cut lists so informal alias substitutions do not creep in. Primary application sketch: formed ferritic HX, mild water coolers, and Japanese specs that name 430J1L. Duty thread: Cu-Nb low-C ferritic for improved formability and mild corrosion HX tube. Commissioning teams benefit when the as-built dossier repeats SUS430J1LTB beside heat numbers, linking isometric revisions to the same mill certificates. Size practice for SUS430J1LTB remains lighter walls for forming; annealed delivery at 720 °C min.
Weldability of JIS G3463 SUS430J1LTB
SUS430J1LTB is welded both as a mill product (A/L/E routes) and as fabricator joints on bundles. Shop guidance: matching Cu-Nb ferritic practice; low heat input. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Procedure qualification for SUS430J1LTB should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. This paragraph is locked to SUS430J1LTB duty: Cu-Nb low-C ferritic for improved formability and mild corrosion HX tube.
Filler selection should match or over-alloy the base chemistry as the WPS demands. Heat input, interpass temperature, and shielding follow the family — austenitic, duplex, or ferritic — not a single shop habit. Caution: Cu and Nb windows are intentional — do not substitute SUS430LXTB without review. Consumable lot control and shielding-gas notes for SUS430J1LTB stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Weld-shop note tied to SUS430J1LTB: matching Cu-Nb ferritic practice; low heat input.
Surface Finishes for JIS G3463 SUS430J1LTB
Surface supply for formed ferritic HX in SUS430J1LTB is typically annealed and pickled after heat treatment, giving a matte scale-free OD that still forms cleanly in mild water cooler work. Bright anneal or a named polish is by agreement when Japanese specs that call 430J1L also write an appearance or roughness line. Always state whether OD, ID, or both surfaces carry the finish — formed bends make ID scope especially easy to miss.
| Finish | Typical supply | Order note |
|---|---|---|
| Annealed and pickled | Standard mill finish for mild-corrosion HX tube | Matte, scale-free after pickling |
| Bright annealed | When scale-free appearance is written on the RFQ | State OD, ID, or both |
| Ground / polished | By agreement for formability or roughness callouts | Name Ra/grit and surface; avoid burn marks on Cu-Nb stock |
| Passivated | End-user A967-analogue requirements | Not a substitute for correct anneal or Cu/Nb chemistry |
Matching Cu-Nb ferritic welding practice and low heat input belong on the weld procedure, not on a polish note. Passivation after pickle or light dressing restores the passive film but never replaces heat treatment. Pack SUS430J1LTB away from carbon-steel strapping so free iron does not seed rust before the cooler ships.
Inspection and Testing for JIS G3463 SUS430J1LTB
Inspection for JIS G3463 SUS430J1LTB covers cast analysis, tensile tests, flattening or weld bend as applicable, hydrostatic test or NDT, dimensions, and appearance. Special quality annex items (IGC, grain size, etc.) apply only when ordered. Documents follow JIS G 0415 / purchaser-specified EN 10204 styles. Sampling plans for SUS430J1LTB keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Application context for SUS430J1LTB stays formed ferritic HX, mild water coolers, and Japanese specs that name 430J1L.
Marking includes SUS430J1LTB, manufacture/finish symbols, manufacturer, and other mandatory marking-clause data. Traceability from stencil to MTC is part of supply, not an upgrade. Use: formed ferritic HX, mild water coolers, and Japanese specs that name 430J1L. Non-conforming SUS430J1LTB lengths are segregated and retested or rejected under retest clauses rather than reworked into unmarked stock. Corrosion framing beside SUS430J1LTB: Cu-Nb low-C balance targets formability plus mild aqueous resistance.
Packaging and Shipping for JIS G3463 SUS430J1LTB
Packaging for SUS430J1LTB uses wooden boxes, plywood cases, or bundled frames with waterproof wrapping as the OD and finish demand. Soft separators protect pickled and polished surfaces. Ends receive caps or bevel protectors when ordered. Bundle tickets for SUS430J1LTB repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Size practice for SUS430J1LTB remains lighter walls for forming; annealed delivery at 720 °C min.
Carbon-steel strapping never contacts the stainless OD without a barrier. Mixed-grade bundles are forbidden when chemistry integrity matters. Caution: Cu and Nb windows are intentional — do not substitute SUS430LXTB without review. Desiccant and wrap choices for SUS430J1LTB follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Weld-shop note tied to SUS430J1LTB: matching Cu-Nb ferritic practice; low heat input.
Shipping documents list JIS G3463, SUS430J1LTB, sizes, quantities, heat numbers, and certificate type. SHH STEEL coordinates inland trucking and FOB/CIF packing scopes as the order states. Role: Cu-Nb low-C ferritic for improved formability and mild corrosion HX tube. Claims handling for SUS430J1LTB starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Weld-shop note tied to SUS430J1LTB: matching Cu-Nb ferritic practice; low heat input.
Why Choose SHH STEEL
SHH STEEL can produce and supply JIS G3463 SUS430J1LTB with the process route, heat treatment, and tests named on your enquiry — not a bait-and-switch alias. Mill partners run stainless tube capacity that covers seamless and welded Table 1 symbols for this mark. Duty focus: Cu-Nb low-C ferritic for improved formability and mild corrosion HX tube.
Technical sales can map SUS430J1LTB against sisters SUS430LXTB, SUS430TB, SUS436LTB, SUS444TB and live ASTM pages without pretending standards are identical. Inspection coordination and export packing are in-house habits, not afterthoughts. Ask for a written acknowledgement that names SUS430J1LTB, the manufacture process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS430J1LTB to that written scope.
Supply Capability
SHH STEEL can produce and supply JIS G3463 SUS430J1LTB across enquiry-oriented OD × wall bands, in seamless or welded routes, with certificates and optional annex tests as ordered. Summary capability follows in the table; stock language below is an RFQ map, not a frozen tonnage catalogue. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS430J1LTB when the mill schedule allows.
| Item | Capability |
|---|---|
| Standard | JIS G3463 stainless steel tubes for boilers and heat exchangers |
| Grade symbol | SUS430J1LTB |
| Product form | Seamless (S) and welded (A / L / E) tube; finishes S-H / S-C / A / A-C / E-C as marked |
| Delivery condition | annealed |
| Documents | Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered) |
| Typical OD practice | 15.9–139.8 mm per standard Note 1; other by agreement |
| Wall / gauge | OD × wall / BWG-class HX gauges within Attached Tables; other by agreement |
Stock / Available sizes
SHH STEEL can produce and supply JIS G3463 SUS430J1LTB. Stock / Available sizes: enquiry band typically aligns with 15.9–139.8 mm OD practice under G3463 Note 1, with OD×wall HX gauges; schedule 5S–80 (and heavier by agreement) depending on grade family. For SUS430J1LTB, practical fast-track sizes often sit in mid-bore process and utility ranges — send the OD × wall list for a firm acknowledgement. Context: lighter walls for forming; annealed delivery at 720 °C min.
Cut lengths, bevels, special NDT, and IGC annex tests add lead time — call them early. Sisters often quoted alongside: SUS430LXTB, SUS430TB, SUS436LTB, SUS444TB. Email the size list to start. SHH STEEL can produce trial lengths of SUS430J1LTB for procedure qualification before the bulk release when the project calendar needs it. SHH STEEL can produce trial lengths of SUS430J1LTB for procedure qualification before bulk release when the project calendar needs it. Corrosion framing beside SUS430J1LTB: Cu-Nb low-C balance targets formability plus mild aqueous resistance.
FAQ
-
What is JIS G3463 SUS430J1LTB stainless steel tube used for?
- JIS G3463 SUS430J1LTB is stainless tube for boiler and heat-exchanger service (superheater, HX, condenser, catalyser) — formed ferritic HX, mild water coolers, and Japanese specs that name 430J1L. Role summary: Cu-Nb low-C ferritic for improved formability and mild corrosion HX tube. It is a Japanese boiler/HX tube product standard mark, not an automatic ASTM A213 certificate.
-
Does JIS G3463 SUS430J1LTB cover seamless and welded tube?
- Yes. Manufacture allows seamless and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish marks such as S-H, S-C, A-C, or E-C. SHH STEEL can produce and supply either route for SUS430J1LTB when the mill can meet the ordered size and tests. The title omits Seamless/Welded because JIS G3463 covers both manufacture routes — the PO must still name the process mark.
-
What heat treatment applies to SUS430J1LTB?
- SUS430J1LTB is delivered annealed under JIS G3463. Table 2 reference: 720 °C min, air or slow cool. Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
-
How does SUS430J1LTB compare with sister grades SUS430LXTB, SUS430TB, SUS436LTB?
- SUS430J1LTB is filed as ferritic. Typical sisters on the same RFQ are SUS430LXTB, SUS430TB, SUS436LTB. Design caution: Cu and Nb windows are intentional — do not substitute SUS430LXTB without review Pick the sister when the medium or strength floor outgrows this symbol rather than stretching wall alone.
-
What tests appear on the mill certificate for SUS430J1LTB?
- Expect cast analysis (Table 3), room-temperature tensile results (Table 4), flattening/flaring as applicable, dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
-
Is Cu-Nb low-C ferritic (430J1L) the same as ordering SUS430J1LTB?
- No. Cu-Nb low-C ferritic (430J1L) is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3463 and SUS430J1LTB so cast limits, heat treatment, and process marks are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for JIS G3463 SUS430J1LTB?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS430J1LTB within the typical 15.9–139.8 mm OD practice, with measured walls by agreement. Size context: lighter walls for forming; annealed delivery at 720 °C min. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
How should SUS430J1LTB be welded?
- Shop guidance: matching Cu-Nb ferritic practice; low heat input. Mill heat treatment of seamless or welded tube does not replace a qualified WPS on fabricator joints or tube-to-tubesheet welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: Cu and Nb windows are intentional — do not substitute SUS430LXTB without review
-
When should I choose a duplex or higher-Mo grade instead of SUS430J1LTB?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what ferritic practice can defend for the temperature and stress state. Caution for this mark: Cu and Nb windows are intentional — do not substitute SUS430LXTB without review Sister pointers: SUS430LXTB, SUS430TB, SUS436LTB. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify JIS G3463 SUS430J1LTB with ASTM A213 or ASME SA213?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3463 SUS430J1LTB does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What surface finishes are available for SUS430J1LTB?
- Pickled after heat treatment is the usual HX tube supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS430J1LTB when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
JIS G3463 SUS430J1LTB is stainless steel tube for boiler and heat-exchanger service — Cu-Nb low-C ferritic for improved formability and mild corrosion HX tube. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS430LXTB, SUS430TB, SUS436LTB. Related ASTM A213 pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process mark, and medium notes to start the quote.