JIS G3463 SUS347HTB Stainless Steel Tube
What is JIS G3463 SUS347HTB Stainless Steel Tube
When the approved vendor list and tube-bundle notes say JIS G3463, the grade mark has to carry the TB suffix. SUS347HTB is the full product symbol for this austenitic tube. SUS347HTB under JIS G3463 is the Nb-stabilised hot-strength sister — not a warehouse rename of SUS347TB. Buyers working Japanese boiler and HX packages should treat SUS347HTB as a governed product symbol under G3463, with Table 3 chemistry and Table 4 tensile floors enforced on the same heat. Keep the SUS347HTB caution visible here: carbon window 0.04–0.10%; confirm Nb 8×C–1.00 on MTC; different solution temperatures for cold vs hot finish.
SHH STEEL can supply SUS347HTB tube in seamless S or welded A/L/E routes, with plain or bevelled ends, random or cut lengths, and EN 10204 / JIS G 0415 style inspection documents when specified. Role on the line: controlled-carbon Nb-stabilised tube for elevated-temperature HX / superheater duty. Size and test clarity on the RFQ lets SHH STEEL lock the correct Table 1 symbols for SUS347HTB before production starts. Weld-shop note tied to SUS347HTB: 347H fillers; match heat treatment to cold-finished 1095 °C or hot-finished 1050 °C practice.
Equivalence talk to 347H / UNS S34709 belongs in engineering notes, not as a substitute for the JIS symbol. Lock JIS G3463 SUS347HTB, OD × wall, manufacture/finish symbols, and any special quality annex items before melt. Watch-out: carbon window 0.04–0.10%; confirm Nb 8×C–1.00 on MTC; different solution temperatures for cold vs hot finish.
Related ASTM tube pages share chemistry families but not Japanese acceptance text — confirm before dual-cert claims. Sisters on this hub: SUS347TB, SUS321HTB, SUS304HTB, SUS316HTB. Use thread: high-temperature superheater stainless tube, hot process HX, and heat-recovery bundles needing Nb plus carbon floor. Document the medium, design temperature, and weld map beside the SUS347HTB line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Keep the SUS347HTB caution visible here: carbon window 0.04–0.10%; confirm Nb 8×C–1.00 on MTC; different solution temperatures for cold vs hot finish.
Inside this JIS G3463 series, compare SUS347TB, SUS321HTB, SUS304HTB, SUS316HTB. Hub: JIS G3463. ASTM/ASME related product pages (not interchangeable by default): A213 TP347H, ASTM A213.
Chemical Composition of JIS G3463 SUS347HTB
Chemistry control on SUS347HTB starts at the ladle. Expect C 0.04–0.10, Si ≤1.00, Mn ≤2.00, P ≤0.030, S ≤0.030, Ni 9.00–13.00, Cr 17.00–20.00 within Table 3, reported on the inspection document against the heat. Body alias 347H / UNS S34709 does not widen those windows. Every ladle analysis for SUS347HTB is checked against those windows before the heat is released to piercing, welding, or finishing, and the same numbers reappear on the inspection document. Application context for SUS347HTB stays high-temperature superheater stainless tube, hot process HX, and heat-recovery bundles needing Nb plus carbon floor.
Read the table with the family in mind — austenitic — and with caution carbon window 0.04–0.10%; confirm Nb 8×C–1.00 on MTC; different solution temperatures for cold vs hot finish. Numbers without the matching heat-treatment row are incomplete purchase data. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for SUS347HTB before the order is acknowledged. This paragraph is locked to SUS347HTB duty: controlled-carbon Nb-stabilised tube for elevated-temperature HX / superheater duty.
| Grade | C | Si | Mn | P | S | Ni | Cr | Nb |
|---|---|---|---|---|---|---|---|---|
| SUS347HTB | 0.04–0.10 | ≤1.00 | ≤2.00 | ≤0.030 | ≤0.030 | 9.00–13.00 | 17.00–20.00 | 8×C%–1.00 |
Mechanical Properties of JIS G3463 SUS347HTB
Proof stress and tensile minima for SUS347HTB sit at Rm min 520 N/mm², proof stress min 206 N/mm², elongation min 35% (OD ≥20 mm, No.11/12). Flattening, flaring, and reverse-flattening (welded) testing backs ductility for the ordered process route. Watch-out: carbon window 0.04–0.10%; confirm Nb 8×C–1.00 on MTC; different solution temperatures for cold vs hot finish.
| Grade | Rm min (N/mm²) | Proof stress min (N/mm²) | A OD≥20 mm No.11/12 min (%) | A 10≤OD<20 mm No.11 min (%) | A OD<10 mm No.11 min (%) |
|---|---|---|---|---|---|
| SUS347HTB | 520 | 206 | 35 | 30 | 27 |
Ambient values from JIS G3463 Table 4 for SUS347HTB. Heat treatment (Table 2): Cold finished 1095 °C rapid cool; hot finished 1050 °C rapid cool. Elongation reductions apply for walls under 8 mm on No.12 pieces. For heat-exchanger tube the purchaser may designate an upper tensile limit (Table 4 min + 200 N/mm²) when necessary.
Manufacture of JIS G3463 SUS347HTB Tube (Seamless and Welded)
SHH STEEL can produce SUS347HTB as seamless S or as A/L/E welded tube, then heat-treat and pickle (or bright-anneal) per Table 2. Bevel ends are available by agreement; plain ends are the default when the PO is silent. Seamless and welded options remain available for SUS347HTB; the acknowledgement repeats the Table 1 symbols so production cannot silently change route after the PO is firm. Size practice for SUS347HTB remains seamless dominant; OD×wall from thermal/mechanical boiler design.
Process control for SUS347HTB ends with verified heat treatment (Cold finished 1095 °C rapid cool; hot finished 1050 °C rapid cool) and surface conditioning. Austenitic heats take solution annealing with rapid cooling; hot-finished seamless may omit separate solution treatment when hot-worked and rapidly cooled in-line under the Table 2 note, unless the purchaser forbids it.
Bevel geometry for walls ≤22 mm defaults to the standard figure when bevels are ordered without a drawing. Size practice: seamless dominant; OD×wall from thermal/mechanical boiler design. Hydrostatic pressure or NDT class for SUS347HTB is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. This paragraph is locked to SUS347HTB duty: controlled-carbon Nb-stabilised tube for elevated-temperature HX / superheater duty.
Dimensions and Tolerances for JIS G3463 SUS347HTB
Mass tables in JIS G3463 support Attached Table mass/OD×wall ordering for common austenitic marks; for SUS347HTB, confirm whether your project uses schedule or measured wall. Context: seamless dominant; OD×wall from thermal/mechanical boiler design. Tolerance class follows the process route ordered for SUS347HTB, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. This paragraph is locked to SUS347HTB duty: controlled-carbon Nb-stabilised tube for elevated-temperature HX / superheater duty.
For heat-exchange and building services, schedule tables often drive the BOM; for process plants, measured wall and corrosion allowance dominate. SUS347HTB supports both conversations when the PO is clear. Fixed lengths and multiple cut lengths for SUS347HTB are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. This paragraph is locked to SUS347HTB duty: controlled-carbon Nb-stabilised tube for elevated-temperature HX / superheater duty.
Equivalent Grades for JIS G3463 SUS347HTB
Do not treat 347H / UNS S34709 as interchangeable paperwork. Chemistry kinship is not acceptance kinship. Inside this series see SUS347TB, SUS321HTB, SUS304HTB, SUS316HTB. Role: controlled-carbon Nb-stabilised tube for elevated-temperature HX / superheater duty. When a dual-cert path is required, list both JIS G3463 SUS347HTB and the ASTM mark with separate test scopes instead of assuming one chemistry line clears both files. Weld-shop note tied to SUS347HTB: 347H fillers; match heat treatment to cold-finished 1095 °C or hot-finished 1050 °C practice.
Heat Treatment and Delivery Condition for JIS G3463 SUS347HTB
Stabilisation or special anneals, where the standard allows purchaser options (notably Ti/Nb grades), must be written on the order — silence means Table 2 defaults only. For SUS347HTB: Cold finished 1095 °C rapid cool; hot finished 1050 °C rapid cool. Recorded furnace charts for SUS347HTB should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Weld-shop note tied to SUS347HTB: 347H fillers; match heat treatment to cold-finished 1095 °C or hot-finished 1050 °C practice.
After local hot work in the field, restore solution annealed practice when the corrosion file demands it. Caution: carbon window 0.04–0.10%; confirm Nb 8×C–1.00 on MTC; different solution temperatures for cold vs hot finish. Field heat treatment of SUS347HTB after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Weld-shop note tied to SUS347HTB: 347H fillers; match heat treatment to cold-finished 1095 °C or hot-finished 1050 °C practice.
Corrosion Resistance of JIS G3463 SUS347HTB
Pick tests that match how SUS347HTB is filed — austenitic. Corrosion thread: elevated-temperature stability is the mission; aqueous chlorides still need separate alloy logic. Caution: carbon window 0.04–0.10%; confirm Nb 8×C–1.00 on MTC; different solution temperatures for cold vs hot finish. Coupon orientation, weld condition, and surface finish for SUS347HTB belong in the corrosion test order so annex results can be compared to the installed bundle honestly. Application context for SUS347HTB stays high-temperature superheater stainless tube, hot process HX, and heat-recovery bundles needing Nb plus carbon floor.
Fire-protection and potable-adjacent lines still need the right alloy — G3463 scope does not make every mark equal. Use thread: high-temperature superheater stainless tube, hot process HX, and heat-recovery bundles needing Nb plus carbon floor. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for SUS347HTB rather than relying on schedule thickness alone. Corrosion framing beside SUS347HTB: elevated-temperature stability is the mission; aqueous chlorides still need separate alloy logic.
Applications of JIS G3463 SUS347HTB Tube
Project types that repeatedly call SUS347HTB: high-temperature superheater stainless tube, hot process HX, and heat-recovery bundles needing Nb plus carbon floor. Duty: controlled-carbon Nb-stabilised tube for elevated-temperature HX / superheater duty. Caution still applies: carbon window 0.04–0.10%; confirm Nb 8×C–1.00 on MTC; different solution temperatures for cold vs hot finish. Spool fabricators should copy SUS347HTB onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Corrosion framing beside SUS347HTB: elevated-temperature stability is the mission; aqueous chlorides still need separate alloy logic.
Superheater stubs, condenser bundles and corrosive process HX lines all appear in G3463’s scope — alloy choice still follows the medium. For this mark: controlled-carbon Nb-stabilised tube for elevated-temperature HX / superheater duty. Commissioning teams benefit when the as-built dossier repeats SUS347HTB beside heat numbers, linking isometric revisions to the same mill certificates. Size practice for SUS347HTB remains seamless dominant; OD×wall from thermal/mechanical boiler design.
Weldability of JIS G3463 SUS347HTB
Even seamless S tube of SUS347HTB will see field welds. Use: 347H fillers; match heat treatment to cold-finished 1095 °C or hot-finished 1050 °C practice. Restore heat treatment when the WPS and corrosion file require it. Procedure qualification for SUS347HTB should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. Keep the SUS347HTB caution visible here: carbon window 0.04–0.10%; confirm Nb 8×C–1.00 on MTC; different solution temperatures for cold vs hot finish.
Dissimilar welds to carbon steel need buttering and dilution control — especially on heat-facing and Mo grades. Role context: controlled-carbon Nb-stabilised tube for elevated-temperature HX / superheater duty. Consumable lot control and shielding-gas notes for SUS347HTB stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Corrosion framing beside SUS347HTB: elevated-temperature stability is the mission; aqueous chlorides still need separate alloy logic.
Surface Finishes for JIS G3463 SUS347HTB
Iron-free handling after pickle matters — carbon-steel strapping stains show up later as rust blooms on SUS347HTB. Finish thread tied to austenitic. Roughness or polish callouts for SUS347HTB must name OD, ID, or both; ambiguous “bright tube” language is clarified before finishing slots are booked. Application context for SUS347HTB stays high-temperature superheater stainless tube, hot process HX, and heat-recovery bundles needing Nb plus carbon floor.
OD stencil ink and marking paint should be chloride-lean and removable where coating systems follow. Role: controlled-carbon Nb-stabilised tube for elevated-temperature HX / superheater duty. Final visual standards for SUS347HTB reject grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed. Weld-shop note tied to SUS347HTB: 347H fillers; match heat treatment to cold-finished 1095 °C or hot-finished 1050 °C practice.
Inspection and Testing for JIS G3463 SUS347HTB
Clause 13/14 define sampling and retests. For SUS347HTB, keep the heat/lot identity unbroken from melt to bundle tag. Duty: controlled-carbon Nb-stabilised tube for elevated-temperature HX / superheater duty. Sampling plans for SUS347HTB keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Keep the SUS347HTB caution visible here: carbon window 0.04–0.10%; confirm Nb 8×C–1.00 on MTC; different solution temperatures for cold vs hot finish.
Intergranular corrosion testing is annex/special — order it when polythionic or weld-decay risk is written into the duty file for SUS347HTB. Non-conforming SUS347HTB lengths are segregated and retested or rejected under retest clauses rather than reworked into unmarked stock. Corrosion framing beside SUS347HTB: elevated-temperature stability is the mission; aqueous chlorides still need separate alloy logic.
Packaging and Shipping for JIS G3463 SUS347HTB
Small-OD SUS347HTB often ships in crates; large-OD in strapped bundles with OD pads. Confirm destination handling limits on the RFQ. Use: high-temperature superheater stainless tube, hot process HX, and heat-recovery bundles needing Nb plus carbon floor. Bundle tickets for SUS347HTB repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Corrosion framing beside SUS347HTB: elevated-temperature stability is the mission; aqueous chlorides still need separate alloy logic.
Bevelled ends get protectors so landing edges survive trucking. Size hint: seamless dominant; OD×wall from thermal/mechanical boiler design. Desiccant and wrap choices for SUS347HTB follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. This paragraph is locked to SUS347HTB duty: controlled-carbon Nb-stabilised tube for elevated-temperature HX / superheater duty.
Storage advice on arrival: keep bundles dry and off carbon-steel floors. Use thread: high-temperature superheater stainless tube, hot process HX, and heat-recovery bundles needing Nb plus carbon floor. Claims handling for SUS347HTB starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Application context for SUS347HTB stays high-temperature superheater stainless tube, hot process HX, and heat-recovery bundles needing Nb plus carbon floor.
Why Choose SHH STEEL
Project teams working to Japanese boiler/HX specs need a supplier that reads TB suffixes correctly. SHH STEEL can make SUS347HTB to that discipline. Caution we keep visible: carbon window 0.04–0.10%; confirm Nb 8×C–1.00 on MTC; different solution temperatures for cold vs hot finish. SHH STEEL can produce and supply SUS347HTB against the OD × wall, process symbol, and test scope on your RFQ without swapping in an unstated sister grade.
Dual-cert discussions (JIS + ASTM) are handled with two acceptance regimes in view, not one certificate stretched by hope. Sisters: SUS347TB, SUS321HTB, SUS304HTB, SUS316HTB. Ask for a written acknowledgement that names SUS347HTB, the manufacture process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS347HTB to that written scope.
Supply Capability
Whether you need prototype bundles or project tonnage of SUS347HTB, SHH STEEL can supply against a clear OD × wall and test matrix. Duty: high-temperature superheater stainless tube, hot process HX, and heat-recovery bundles needing Nb plus carbon floor. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS347HTB when the mill schedule allows.
| Item | Capability |
|---|---|
| Standard | JIS G3463 stainless steel tubes for boilers and heat exchangers |
| Grade symbol | SUS347HTB |
| Product form | Seamless (S) and welded (A / L / E) tube; finishes S-H / S-C / A / A-C / E-C as marked |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered) |
| Typical OD practice | 15.9–139.8 mm per standard Note 1; other by agreement |
| Wall / gauge | OD × wall / BWG-class HX gauges within Attached Tables; other by agreement |
Stock / Available sizes
Stock / Available sizes: SHH STEEL quotes rolling/welding slots for SUS347HTB rather than promising anonymous warehouse tons. Typical conversation starts around seamless dominant; OD×wall from thermal/mechanical boiler design. SHH STEEL can supply alternate schedules and measured walls for SUS347HTB once the design pressure and corrosion allowance are clear. SHH STEEL can supply alternate schedules and measured walls for SUS347HTB once design pressure and corrosion allowance are clear. Keep the SUS347HTB caution visible here: carbon window 0.04–0.10%; confirm Nb 8×C–1.00 on MTC; different solution temperatures for cold vs hot finish.
If the project needs dual JIS G3463 + ASTM documentation, say so before melt. Caution: carbon window 0.04–0.10%; confirm Nb 8×C–1.00 on MTC; different solution temperatures for cold vs hot finish. SHH STEEL can produce trial lengths of SUS347HTB for procedure qualification before the bulk release when the project calendar needs it.
FAQ
-
What is JIS G3463 SUS347HTB stainless steel tube used for?
- JIS G3463 SUS347HTB is stainless tube for boiler and heat-exchanger service (superheater, HX, condenser, catalyser) — high-temperature superheater stainless tube, hot process HX, and heat-recovery bundles needing Nb plus carbon floor. Role summary: controlled-carbon Nb-stabilised tube for elevated-temperature HX / superheater duty. It is a Japanese boiler/HX tube product standard mark, not an automatic ASTM A213 certificate.
-
Does JIS G3463 SUS347HTB cover seamless and welded tube?
- Yes. Manufacture allows seamless and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish marks such as S-H, S-C, A-C, or E-C. SHH STEEL can produce and supply either route for SUS347HTB when the mill can meet the ordered size and tests. The title omits Seamless/Welded because JIS G3463 covers both manufacture routes — the PO must still name the process mark.
-
What heat treatment applies to SUS347HTB?
- SUS347HTB is delivered solution annealed under JIS G3463. Table 2 reference: Cold finished 1095 °C rapid cool; hot finished 1050 °C rapid cool. Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
-
How does SUS347HTB compare with sister grades SUS347TB, SUS321HTB, SUS304HTB?
- SUS347HTB is filed as austenitic. Typical sisters on the same RFQ are SUS347TB, SUS321HTB, SUS304HTB. Design caution: carbon window 0.04–0.10%; confirm Nb 8×C–1.00 on MTC; different solution temperatures for cold vs hot finish Pick the sister when the medium or strength floor outgrows this symbol rather than stretching wall alone.
-
What tests appear on the mill certificate for SUS347HTB?
- Expect cast analysis (Table 3), room-temperature tensile results (Table 4), flattening/flaring as applicable, dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
-
Is 347H / UNS S34709 the same as ordering SUS347HTB?
- No. 347H / UNS S34709 is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3463 and SUS347HTB so cast limits, heat treatment, and process marks are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for JIS G3463 SUS347HTB?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS347HTB within the typical 15.9–139.8 mm OD practice, with measured walls by agreement. Size context: seamless dominant; OD×wall from thermal/mechanical boiler design. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
How should SUS347HTB be welded?
- Shop guidance: 347H fillers; match heat treatment to cold-finished 1095 °C or hot-finished 1050 °C practice. Mill heat treatment of seamless or welded tube does not replace a qualified WPS on fabricator joints or tube-to-tubesheet welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: carbon window 0.04–0.10%; confirm Nb 8×C–1.00 on MTC; different solution temperatures for cold vs hot finish
-
When should I choose a duplex or higher-Mo grade instead of SUS347HTB?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: carbon window 0.04–0.10%; confirm Nb 8×C–1.00 on MTC; different solution temperatures for cold vs hot finish Sister pointers: SUS347TB, SUS321HTB, SUS304HTB. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify JIS G3463 SUS347HTB with ASTM A213 or ASME SA213?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3463 SUS347HTB does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What surface finishes are available for SUS347HTB?
- Pickled after heat treatment is the usual HX tube supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS347HTB when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
JIS G3463 SUS347HTB is stainless steel tube for boiler and heat-exchanger service — controlled-carbon Nb-stabilised tube for elevated-temperature HX / superheater duty. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS347TB, SUS321HTB, SUS304HTB. Related ASTM A213 pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process mark, and medium notes to start the quote.