JIS G3463 SUS329J4LTB Stainless Steel Tube
What is JIS G3463 SUS329J4LTB Stainless Steel Tube
JIS G3463 is the Japanese Industrial Standard for stainless steel tubes used in boiler and heat-exchanger service (superheater, HX, condenser, catalyser). Grade symbol SUS329J4LTB sits in the austenitic-ferritic (duplex) set of Table 1. JIS G3463 SUS329J4LTB is the step-up duplex HX symbol when 329J3L coupons are marginal — not a thicker wall of austenitic 317L.
SHH STEEL can produce and supply JIS G3463 SUS329J4LTB as seamless or welded tube across the enquiry OD×wall band, solution-annealed or annealed as Table 2 requires, pickled or bright-finished, and documented on mill test certificates tied to cast analysis and tensile results. Duty focus: higher-Cr duplex sister for tougher chloride HX / cooler duty than 329J3L.
Shop language may still say “higher-Cr duplex (329J4L) tube,” yet that commercial alias does not select Japanese cast limits, process symbols, or hydraulic/NDT rules. The purchase order has to name JIS G3463 and SUS329J4LTB so the mill applies the correct analysis, heat treatment, mechanical floors, and marking. Design caution: still duplex — confirm temperature, sour, and fabrication limits; do not treat as superduplex without checking chemistry.
Scope discipline: SUS329J4LTB is HX tube product under JIS G3463, not a piping product under JIS G3459 and not an ASTM A213 order by default. Sister marks often compared on the same RFQ include SUS329J3LTB, SUS329J1TB, SUS836LTB, SUS317LTB. Role reminder: higher-Cr duplex sister for tougher chloride HX / cooler duty than 329J3L.
Inside this JIS G3463 series, compare SUS329J3LTB, SUS329J1TB, SUS836LTB, SUS317LTB. Hub: JIS G3463. ASTM/ASME related product pages (not interchangeable by default): ASTM A213.
Chemical Composition of JIS G3463 SUS329J4LTB
Cast analysis for JIS G3463 SUS329J4LTB follows Table 3. Key windows on a typical certificate include C ≤0.030, Si ≤1.00, Mn ≤1.50, P ≤0.040, S ≤0.030, Ni 5.50–7.50, Cr 24.00–26.00. SHH STEEL ties the heat number on the tube marking to the same cast line on the MTC. Commercial alias higher-Cr duplex (329J4L) is body text only. Corrosion thread: higher Cr vs 329J3L targets tougher chloride media; coupon the crevice geometry.
Chemical limits for SUS329J4LTB under JIS G3463 appear in the table underneath. Source priority is the 2021 Table 3 extract cross-checked to public Nikko / supplier tables. If your client specification cites a different edition footnote, send it before the heat is melted. Duty thread: higher-Cr duplex sister for tougher chloride HX / cooler duty than 329J3L.
| Grade | C | Si | Mn | P | S | Ni | Cr | Mo | N |
|---|---|---|---|---|---|---|---|---|---|
| SUS329J4LTB | ≤0.030 | ≤1.00 | ≤1.50 | ≤0.040 | ≤0.030 | 5.50–7.50 | 24.00–26.00 | 2.50–3.50 | 0.08–0.30 |
Mechanical Properties of JIS G3463 SUS329J4LTB
Ambient tensile floors for SUS329J4LTB come from JIS G3463 Table 4: Rm min 618 N/mm², proof stress min 441 N/mm², elongation min 18% (OD ≥20 mm, No.11/12). These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: austenitic-ferritic (duplex). Caution: still duplex — confirm temperature, sour, and fabrication limits; do not treat as superduplex without checking chemistry.
| Grade | Rm min (N/mm²) | Proof stress min (N/mm²) | A OD≥20 mm No.11/12 min (%) | A 10≤OD<20 mm No.11 min (%) | A OD<10 mm No.11 min (%) |
|---|---|---|---|---|---|
| SUS329J4LTB | 618 | 441 | 18 | 13 | 10 |
Ambient values from JIS G3463 Table 4 for SUS329J4LTB. Heat treatment (Table 2): 950 °C min, rapid cool. Elongation reductions apply for walls under 8 mm on No.12 pieces. For heat-exchanger tube the purchaser may designate an upper tensile limit (Table 4 min + 200 N/mm²) when necessary.
Manufacture of JIS G3463 SUS329J4LTB Tube (Seamless and Welded)
For SUS329J4LTB, the mill path is not “seamless only.” Table 1 explicitly pairs austenitic, duplex, and ferritic marks with seamless or A/L/E welded process symbols and S-H/S-C/A/A-C/E-C finishes. Order the combination that matches hydrostatic or NDT preference, not a habit from ASTM A213 alone. Seamless and welded options remain available for SUS329J4LTB; the acknowledgement repeats the Table 1 symbols so production cannot silently change route after the PO is firm. Corrosion framing beside SUS329J4LTB: higher Cr vs 329J3L targets tougher chloride media; coupon the crevice geometry.
Duplex heats need solution annealing with rapid cooling to restore phase balance — do not skip Table 2 temperatures after hot forming. Heat-treatment reference for SUS329J4LTB: 950 °C min, rapid cool. Pickling follows unless bright heat treatment leaves a scale-free surface. Duty thread: higher-Cr duplex sister for tougher chloride HX / cooler duty than 329J3L.
When dual documentation against ASTM A213 is requested for a related chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for SUS329J4LTB: seamless preferred for critical chloride coolers; NDT often upgraded.
Dimensions and Tolerances for JIS G3463 SUS329J4LTB
SHH STEEL aligns nominal diameter (A/B), outside diameter, schedule or wall, and length tolerance for SUS329J4LTB before the mill slot is locked. Standard Note 1 frames typical OD from 15.9 mm to 139.8 mm (standard Note 1 general practice). Size hint: seamless preferred for critical chloride coolers; NDT often upgraded. Tolerance class follows the process route ordered for SUS329J4LTB, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Size practice for SUS329J4LTB remains seamless preferred for critical chloride coolers; NDT often upgraded.
Length supply may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against the packaging clause so pickled or polished finishes are not iron-stained in transit. Duty thread: higher-Cr duplex sister for tougher chloride HX / cooler duty than 329J3L. Fixed lengths and multiple cut lengths for SUS329J4LTB are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Corrosion framing beside SUS329J4LTB: higher Cr vs 329J3L targets tougher chloride media; coupon the crevice geometry.
Equivalent Grades for JIS G3463 SUS329J4LTB
Equivalence talk for SUS329J4LTB starts with higher-Cr duplex (329J4L): that commercial / UNS framing is useful in body text and dual-cert discussions, but the H1 and order line stay on JIS G3463 SUS329J4LTB. ASTM A213 / A269 pages that share related chemistry are different product standards with different wall bases, mechanical tables, and tests. Sisters: SUS329J3LTB, SUS329J1TB, SUS836LTB, SUS317LTB. Caution: still duplex — confirm temperature, sour, and fabrication limits; do not treat as superduplex without checking chemistry.
Heat Treatment and Delivery Condition for JIS G3463 SUS329J4LTB
SUS329J4LTB is delivered solution annealed under JIS G3463. Table 2 reference: 950 °C min, rapid cool. Fabricator heat treatment after hot bending should chase the same family practice. Weld thread: matching higher-Cr duplex fillers; strict thermal control on tubesheet welds. Recorded furnace charts for SUS329J4LTB should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. This paragraph is locked to SUS329J4LTB duty: higher-Cr duplex sister for tougher chloride HX / cooler duty than 329J3L.
Cooling type matters — austenitic and duplex need rapid cool after solution treatment; ferritic anneal practice allows rapid or slow cool per Table 2. Duty thread: higher-Cr duplex sister for tougher chloride HX / cooler duty than 329J3L. Field heat treatment of SUS329J4LTB after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Size practice for SUS329J4LTB remains seamless preferred for critical chloride coolers; NDT often upgraded.
Corrosion Resistance of JIS G3463 SUS329J4LTB
Corrosion behaviour of JIS G3463 SUS329J4LTB tracks its austenitic-ferritic (duplex) balance: higher Cr vs 329J3L targets tougher chloride media; coupon the crevice geometry. Optional annex corrosion tests (oxalic, Strauss, Huey, etc.) are special quality items — order them when the duty needs coupon evidence. Design caution: still duplex — confirm temperature, sour, and fabrication limits; do not treat as superduplex without checking chemistry.
For heat-facing austenitics, oxidation resistance may dominate over aqueous IGC talk; for duplex and Mo austenitics, chlorides dominate; for ferritics, mild aqueous and weld practice dominate. SUS329J4LTB is filed as austenitic-ferritic (duplex). Caution: still duplex — confirm temperature, sour, and fabrication limits; do not treat as superduplex without checking chemistry. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for SUS329J4LTB rather than relying on schedule thickness alone. Keep the SUS329J4LTB caution visible here: still duplex — confirm temperature, sour, and fabrication limits; do not treat as superduplex without checking chemistry.
Applications of JIS G3463 SUS329J4LTB Tube
Applications of JIS G3463 SUS329J4LTB tube centre on more aggressive chloride condensers, process coolers, and Japanese duplex HX that specify 329J4L. Role summary: higher-Cr duplex sister for tougher chloride HX / cooler duty than 329J3L. When a related chemistry is required under ASTM A213 or A269, open those sister pages — acceptance text is not automatic.
Downstream fabricators should inherit the same grade symbol on cut lists so informal alias substitutions do not creep in. Primary application sketch: more aggressive chloride condensers, process coolers, and Japanese duplex HX that specify 329J4L. Duty thread: higher-Cr duplex sister for tougher chloride HX / cooler duty than 329J3L. Commissioning teams benefit when the as-built dossier repeats SUS329J4LTB beside heat numbers, linking isometric revisions to the same mill certificates. Corrosion framing beside SUS329J4LTB: higher Cr vs 329J3L targets tougher chloride media; coupon the crevice geometry.
Weldability of JIS G3463 SUS329J4LTB
SUS329J4LTB is welded both as a mill product (A/L/E routes) and as fabricator joints on bundles. Shop guidance: matching higher-Cr duplex fillers; strict thermal control on tubesheet welds. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Procedure qualification for SUS329J4LTB should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. Corrosion framing beside SUS329J4LTB: higher Cr vs 329J3L targets tougher chloride media; coupon the crevice geometry.
Filler selection should match or over-alloy the base chemistry as the WPS demands. Heat input, interpass temperature, and shielding follow the family — austenitic, duplex, or ferritic — not a single shop habit. Caution: still duplex — confirm temperature, sour, and fabrication limits; do not treat as superduplex without checking chemistry. Consumable lot control and shielding-gas notes for SUS329J4LTB stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Corrosion framing beside SUS329J4LTB: higher Cr vs 329J3L targets tougher chloride media; coupon the crevice geometry.
Surface Finishes for JIS G3463 SUS329J4LTB
Surface supply for SUS329J4LTB is typically pickled after heat treatment, or bright-annealed when scale-free OD/ID is ordered. Polished or special roughness finishes are by agreement and must state which surface (OD, ID, or both) is in scope. Duty: higher-Cr duplex sister for tougher chloride HX / cooler duty than 329J3L. Roughness or polish callouts for SUS329J4LTB must name OD, ID, or both; ambiguous “bright tube” language is clarified before finishing slots are booked. Keep the SUS329J4LTB caution visible here: still duplex — confirm temperature, sour, and fabrication limits; do not treat as superduplex without checking chemistry.
Passivation treatments, when ordered, follow agreed ASTM A967 / JIS practice analogues — they are not a substitute for correct heat treatment. Caution: still duplex — confirm temperature, sour, and fabrication limits; do not treat as superduplex without checking chemistry. Final visual standards for SUS329J4LTB reject grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed. Size practice for SUS329J4LTB remains seamless preferred for critical chloride coolers; NDT often upgraded.
Inspection and Testing for JIS G3463 SUS329J4LTB
Inspection for JIS G3463 SUS329J4LTB covers cast analysis, tensile tests, flattening or weld bend as applicable, hydrostatic test or NDT, dimensions, and appearance. Special quality annex items (IGC, grain size, etc.) apply only when ordered. Documents follow JIS G 0415 / purchaser-specified EN 10204 styles. Sampling plans for SUS329J4LTB keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Keep the SUS329J4LTB caution visible here: still duplex — confirm temperature, sour, and fabrication limits; do not treat as superduplex without checking chemistry.
Marking includes SUS329J4LTB, manufacture/finish symbols, manufacturer, and other mandatory marking-clause data. Traceability from stencil to MTC is part of supply, not an upgrade. Use: more aggressive chloride condensers, process coolers, and Japanese duplex HX that specify 329J4L. Non-conforming SUS329J4LTB lengths are segregated and retested or rejected under retest clauses rather than reworked into unmarked stock. Weld-shop note tied to SUS329J4LTB: matching higher-Cr duplex fillers; strict thermal control on tubesheet welds.
Packaging and Shipping for JIS G3463 SUS329J4LTB
Packaging for SUS329J4LTB uses wooden boxes, plywood cases, or bundled frames with waterproof wrapping as the OD and finish demand. Soft separators protect pickled and polished surfaces. Ends receive caps or bevel protectors when ordered. Bundle tickets for SUS329J4LTB repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Keep the SUS329J4LTB caution visible here: still duplex — confirm temperature, sour, and fabrication limits; do not treat as superduplex without checking chemistry.
Carbon-steel strapping never contacts the stainless OD without a barrier. Mixed-grade bundles are forbidden when chemistry integrity matters. Caution: still duplex — confirm temperature, sour, and fabrication limits; do not treat as superduplex without checking chemistry. Desiccant and wrap choices for SUS329J4LTB follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Weld-shop note tied to SUS329J4LTB: matching higher-Cr duplex fillers; strict thermal control on tubesheet welds.
Shipping documents list JIS G3463, SUS329J4LTB, sizes, quantities, heat numbers, and certificate type. SHH STEEL coordinates inland trucking and FOB/CIF packing scopes as the order states. Role: higher-Cr duplex sister for tougher chloride HX / cooler duty than 329J3L. Claims handling for SUS329J4LTB starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Size practice for SUS329J4LTB remains seamless preferred for critical chloride coolers; NDT often upgraded.
Why Choose SHH STEEL
SHH STEEL can produce and supply JIS G3463 SUS329J4LTB with the process route, heat treatment, and tests named on your enquiry — not a bait-and-switch alias. Mill partners run stainless tube capacity that covers seamless and welded Table 1 symbols for this mark. Duty focus: higher-Cr duplex sister for tougher chloride HX / cooler duty than 329J3L.
Technical sales can map SUS329J4LTB against sisters SUS329J3LTB, SUS329J1TB, SUS836LTB, SUS317LTB and live ASTM pages without pretending standards are identical. Inspection coordination and export packing are in-house habits, not afterthoughts. Ask for a written acknowledgement that names SUS329J4LTB, the manufacture process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS329J4LTB to that written scope.
Supply Capability
SHH STEEL can produce and supply JIS G3463 SUS329J4LTB across enquiry-oriented OD × wall bands, in seamless or welded routes, with certificates and optional annex tests as ordered. Summary capability follows in the table; stock language below is an RFQ map, not a frozen tonnage catalogue. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS329J4LTB when the mill schedule allows.
| Item | Capability |
|---|---|
| Standard | JIS G3463 stainless steel tubes for boilers and heat exchangers |
| Grade symbol | SUS329J4LTB |
| Product form | Seamless (S) and welded (A / L / E) tube; finishes S-H / S-C / A / A-C / E-C as marked |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered) |
| Typical OD practice | 15.9–139.8 mm per standard Note 1; other by agreement |
| Wall / gauge | OD × wall / BWG-class HX gauges within Attached Tables; other by agreement |
Stock / Available sizes
SHH STEEL can produce and supply JIS G3463 SUS329J4LTB. Stock / Available sizes: enquiry band typically aligns with 15.9–139.8 mm OD practice under G3463 Note 1, with OD×wall HX gauges; schedule 5S–80 (and heavier by agreement) depending on grade family. For SUS329J4LTB, practical fast-track sizes often sit in mid-bore process and utility ranges — send the OD × wall list for a firm acknowledgement. Context: seamless preferred for critical chloride coolers; NDT often upgraded.
Cut lengths, bevels, special NDT, and IGC annex tests add lead time — call them early. Sisters often quoted alongside: SUS329J3LTB, SUS329J1TB, SUS836LTB, SUS317LTB. Email the size list to start. SHH STEEL can produce trial lengths of SUS329J4LTB for procedure qualification before the bulk release when the project calendar needs it. SHH STEEL can produce trial lengths of SUS329J4LTB for procedure qualification before bulk release when the project calendar needs it. This paragraph is locked to SUS329J4LTB duty: higher-Cr duplex sister for tougher chloride HX / cooler duty than 329J3L.
FAQ
-
What is JIS G3463 SUS329J4LTB stainless steel tube used for?
- JIS G3463 SUS329J4LTB is stainless tube for boiler and heat-exchanger service (superheater, HX, condenser, catalyser) — more aggressive chloride condensers, process coolers, and Japanese duplex HX that specify 329J4L. Role summary: higher-Cr duplex sister for tougher chloride HX / cooler duty than 329J3L. It is a Japanese boiler/HX tube product standard mark, not an automatic ASTM A213 certificate.
-
Does JIS G3463 SUS329J4LTB cover seamless and welded tube?
- Yes. Manufacture allows seamless and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish marks such as S-H, S-C, A-C, or E-C. SHH STEEL can produce and supply either route for SUS329J4LTB when the mill can meet the ordered size and tests. The title omits Seamless/Welded because JIS G3463 covers both manufacture routes — the PO must still name the process mark.
-
What heat treatment applies to SUS329J4LTB?
- SUS329J4LTB is delivered solution annealed under JIS G3463. Table 2 reference: 950 °C min, rapid cool. Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
-
How does SUS329J4LTB compare with sister grades SUS329J3LTB, SUS329J1TB, SUS836LTB?
- SUS329J4LTB is filed as austenitic-ferritic (duplex). Typical sisters on the same RFQ are SUS329J3LTB, SUS329J1TB, SUS836LTB. Design caution: still duplex — confirm temperature, sour, and fabrication limits; do not treat as superduplex without checking chemistry Pick the sister when the medium or strength floor outgrows this symbol rather than stretching wall alone.
-
What tests appear on the mill certificate for SUS329J4LTB?
- Expect cast analysis (Table 3), room-temperature tensile results (Table 4), flattening/flaring as applicable, dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
-
Is higher-Cr duplex (329J4L) the same as ordering SUS329J4LTB?
- No. higher-Cr duplex (329J4L) is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3463 and SUS329J4LTB so cast limits, heat treatment, and process marks are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for JIS G3463 SUS329J4LTB?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS329J4LTB within the typical 15.9–139.8 mm OD practice, with measured walls by agreement. Size context: seamless preferred for critical chloride coolers; NDT often upgraded. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
How should SUS329J4LTB be welded?
- Shop guidance: matching higher-Cr duplex fillers; strict thermal control on tubesheet welds. Mill heat treatment of seamless or welded tube does not replace a qualified WPS on fabricator joints or tube-to-tubesheet welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: still duplex — confirm temperature, sour, and fabrication limits; do not treat as superduplex without checking chemistry
-
When should I choose a duplex or higher-Mo grade instead of SUS329J4LTB?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic-ferritic (duplex) practice can defend for the temperature and stress state. Caution for this mark: still duplex — confirm temperature, sour, and fabrication limits; do not treat as superduplex without checking chemistry Sister pointers: SUS329J3LTB, SUS329J1TB, SUS836LTB. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify JIS G3463 SUS329J4LTB with ASTM A213 or ASME SA213?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3463 SUS329J4LTB does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What surface finishes are available for SUS329J4LTB?
- Pickled after heat treatment is the usual HX tube supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS329J4LTB when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
JIS G3463 SUS329J4LTB is stainless steel tube for boiler and heat-exchanger service — higher-Cr duplex sister for tougher chloride HX / cooler duty than 329J3L. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS329J3LTB, SUS329J1TB, SUS836LTB. Related ASTM A213 pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process mark, and medium notes to start the quote.