JIS G3463 SUS329J3LTB Stainless Steel Tube
What is JIS G3463 SUS329J3LTB Stainless Steel Tube
Boiler and heat-exchanger packages that cite Japanese product standards look to JIS G3463 — Stainless steel boiler and heat exchanger tubes — rather than inventing a mill grade from AISI shorthand alone. SUS329J3LTB is the Table 1 symbol for this austenitic-ferritic (duplex) chemistry. When the cooler needs duplex strength and chloride resistance under a Japanese HX standard, JIS G3463 SUS329J3LTB is the 2205-class mark to lock — not “duplex 316”.
Mill path for SUS329J3LTB: Table 1 manufacture/finish symbols, Table 2 heat treatment, Table 3 cast chemistry, Table 4 tensile floors. SHH STEEL can make and supply the grade to that stack with hydrostatic or NDT acceptance as ordered. Typical use: seawater-lean coolers, chemical condensers, oil & gas process HX, and high-strength chloride tube bundles.
Body text may mention ~2205 / UNS S31803–S32205 class for cross-reference, but the H1 and order line stay on SUS329J3LTB. Silent alias swaps are how wrong carbon ceilings and wrong tensile tables enter the MTC. Keep this caution in view: respect duplex temperature and sour-service limits; solution anneal after hot bends; not a silent swap for 316L.
Order the standard the drawing and regulatory file actually require. Inside this G3463 series, compare SUS329J4LTB, SUS329J1TB, SUS316LTB, SUS317LTB before stretching surface finish or schedule alone. Duty thread: standard duplex (~2205 class) HX tube for chloride process condensers and coolers. Document the medium, design temperature, and weld map beside the SUS329J3LTB line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Corrosion framing beside SUS329J3LTB: PREN and strength both beat 316L in many chloride waters; crevice design and biofouling still matter.
Inside this JIS G3463 series, compare SUS329J4LTB, SUS329J1TB, SUS316LTB, SUS317LTB. Hub: JIS G3463. ASTM/ASME related product pages (not interchangeable by default): ASTM A213.
Chemical Composition of JIS G3463 SUS329J3LTB
Table 3 sets the melt limits for SUS329J3LTB. Highlight band: C ≤0.030, Si ≤1.00, Mn ≤1.50, P ≤0.040, S ≤0.030, Ni 4.50–7.50, Cr 21.00–26.00. Product analysis, when ordered, applies JIS G 0321 stainless product tolerances on top of Table 3. Alias note: ~2205 / UNS S31803–S32205 class. Every ladle analysis for SUS329J3LTB is checked against those windows before the heat is released to piercing, welding, or finishing, and the same numbers reappear on the inspection document. This paragraph is locked to SUS329J3LTB duty: standard duplex (~2205 class) HX tube for chloride process condensers and coolers.
The composition table below is the cast window SHH STEEL quotes against for SUS329J3LTB. Edition framing is JIS G3463. Use thread: seawater-lean coolers, chemical condensers, oil & gas process HX, and high-strength chloride tube bundles. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for SUS329J3LTB before the order is acknowledged. Application context for SUS329J3LTB stays seawater-lean coolers, chemical condensers, oil & gas process HX, and high-strength chloride tube bundles.
| Grade | C | Si | Mn | P | S | Ni | Cr | Mo | N |
|---|---|---|---|---|---|---|---|---|---|
| SUS329J3LTB | ≤0.030 | ≤1.00 | ≤1.50 | ≤0.040 | ≤0.030 | 4.50–7.50 | 21.00–26.00 | 2.50–4.00 | 0.08–0.30 |
Mechanical Properties of JIS G3463 SUS329J3LTB
Table 4 mechanical acceptance for SUS329J3LTB: Rm min 618 N/mm², proof stress min 441 N/mm², elongation min 18% (OD ≥20 mm, No.11/12). Elongation rules change for walls under 8 mm and are not mandatory below 40 mm OD (record only unless agreed). Delivery framing: solution annealed. Tensile sampling follows tensile sampling clauses for the ordered test unit of SUS329J3LTB, and retests follow retest clauses when a result sits under the Table 4 floor. Application context for SUS329J3LTB stays seawater-lean coolers, chemical condensers, oil & gas process HX, and high-strength chloride tube bundles.
| Grade | Rm min (N/mm²) | Proof stress min (N/mm²) | A OD≥20 mm No.11/12 min (%) | A 10≤OD<20 mm No.11 min (%) | A OD<10 mm No.11 min (%) |
|---|---|---|---|---|---|
| SUS329J3LTB | 618 | 441 | 18 | 13 | 10 |
Ambient values from JIS G3463 Table 4 for SUS329J3LTB. Heat treatment (Table 2): 950 °C min, rapid cool. Elongation reductions apply for walls under 8 mm on No.12 pieces. For heat-exchanger tube the purchaser may designate an upper tensile limit (Table 4 min + 200 N/mm²) when necessary.
Manufacture of JIS G3463 SUS329J3LTB Tube (Seamless and Welded)
Both seamless and welded SUS329J3LTB are legitimate under JIS G3463. Pick S when the design pressure, wall, or NDT plan favours a pierced/drawn route; pick A, L, or E when welded economics fit and the weld procedure is qualified. Finish symbols S-H/S-C/A/A-C/E-C ride with the process mark on the tube stencil. Seamless and welded options remain available for SUS329J3LTB; the acknowledgement repeats the Table 1 symbols so production cannot silently change route after the PO is firm. Corrosion framing beside SUS329J3LTB: PREN and strength both beat 316L in many chloride waters; crevice design and biofouling still matter.
After forming, SUS329J3LTB receives Table 2 treatment — 950 °C min, rapid cool. Duplex heats need solution annealing with rapid cooling to restore phase balance — do not skip Table 2 temperatures after hot forming. Use thread: seawater-lean coolers, chemical condensers, oil & gas process HX, and high-strength chloride tube bundles. Pickling or bright-anneal decisions for SUS329J3LTB stay tied to the ordered surface quality rather than to a generic mill habit that ignores chloride-sensitive duties. Keep the SUS329J3LTB caution visible here: respect duplex temperature and sour-service limits; solution anneal after hot bends; not a silent swap for 316L.
Marking carries the grade symbol SUS329J3LTB, process/finish marks, manufacturer ID, and other marking-clause items. Size hint: HX OD 19.0–50.8 mm common; U-bend annex with care for duplex springback. Weld thread: 22Cr duplex fillers; heat input, interpass, and ferrite window per WPS; purge ID. Hydrostatic pressure or NDT class for SUS329J3LTB is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Corrosion framing beside SUS329J3LTB: PREN and strength both beat 316L in many chloride waters; crevice design and biofouling still matter.
Dimensions and Tolerances for JIS G3463 SUS329J3LTB
Dimensional order lines for SUS329J3LTB should state OD × wall (or OD×wall HX gauges; schedule 5S/10S/20S/40/80/…), length type, and end finish. Tolerances follow dimensional tolerance clauses by process route. Use: seawater-lean coolers, chemical condensers, oil & gas process HX, and high-strength chloride tube bundles. Tolerance class follows the process route ordered for SUS329J3LTB, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Corrosion framing beside SUS329J3LTB: PREN and strength both beat 316L in many chloride waters; crevice design and biofouling still matter.
OD and wall tolerances differ for hot-finished seamless versus cold-finished / welded routes — quote the process symbol with the size. Caution: respect duplex temperature and sour-service limits; solution anneal after hot bends; not a silent swap for 316L. Fixed lengths and multiple cut lengths for SUS329J3LTB are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Keep the SUS329J3LTB caution visible here: respect duplex temperature and sour-service limits; solution anneal after hot bends; not a silent swap for 316L.
Equivalent Grades for JIS G3463 SUS329J3LTB
SUS329J3LTB is the JIS G3463 designation. Alias ~2205 / UNS S31803–S32205 class appears only as a cross-walk. Compare sisters SUS329J4LTB, SUS329J1TB, SUS316LTB, SUS317LTB when the medium or temperature outgrows this mark. Hook: lock SUS329J3LTB on the PO. When a dual-cert path is required, list both JIS G3463 SUS329J3LTB and the ASTM mark with separate test scopes instead of assuming one chemistry line clears both files. Application context for SUS329J3LTB stays seawater-lean coolers, chemical condensers, oil & gas process HX, and high-strength chloride tube bundles.
Heat Treatment and Delivery Condition for JIS G3463 SUS329J3LTB
Mill heat treatment for SUS329J3LTB: 950 °C min, rapid cool. Bright annealing may omit pickling when the surface is scale-free. Delivery label: solution annealed. Recorded furnace charts for SUS329J3LTB should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Application context for SUS329J3LTB stays seawater-lean coolers, chemical condensers, oil & gas process HX, and high-strength chloride tube bundles.
Certificate wording for SUS329J3LTB should show the heat-treatment condition actually performed, not a generic “annealed” stamp that hides temperature. Use: seawater-lean coolers, chemical condensers, oil & gas process HX, and high-strength chloride tube bundles. Field heat treatment of SUS329J3LTB after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Application context for SUS329J3LTB stays seawater-lean coolers, chemical condensers, oil & gas process HX, and high-strength chloride tube bundles.
Corrosion Resistance of JIS G3463 SUS329J3LTB
PREN and strength both beat 316L in many chloride waters; crevice design and biofouling still matter Special quality annex tests are available by agreement; they are not a blanket warranty for every process medium. Family filing: austenitic-ferritic (duplex). Coupon orientation, weld condition, and surface finish for SUS329J3LTB belong in the corrosion test order so annex results can be compared to the installed bundle honestly. Keep the SUS329J3LTB caution visible here: respect duplex temperature and sour-service limits; solution anneal after hot bends; not a silent swap for 316L.
Do not market invented PREN digits. Bring medium chemistry and SHH STEEL will map SUS329J3LTB honestly against SUS329J4LTB, SUS329J1TB, SUS316LTB, SUS317LTB. Role: standard duplex (~2205 class) HX tube for chloride process condensers and coolers. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for SUS329J3LTB rather than relying on schedule thickness alone. Size practice for SUS329J3LTB remains HX OD 19.0–50.8 mm common; U-bend annex with care for duplex springback.
Applications of JIS G3463 SUS329J3LTB Tube
Typical BOM language pairs JIS G3463 SUS329J3LTB with OD × wall (or schedule), manufacture/finish symbols, and heat-treatment condition. Primary sketch: seawater-lean coolers, chemical condensers, oil & gas process HX, and high-strength chloride tube bundles. Spool fabricators should copy SUS329J3LTB onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Size practice for SUS329J3LTB remains HX OD 19.0–50.8 mm common; U-bend annex with care for duplex springback.
Spell SUS329J3LTB on tube-sheet drawings and bundle lists, bundle sheets and tubesheet specs alike. Sister options when the medium hardens: SUS329J4LTB, SUS329J1TB, SUS316LTB, SUS317LTB. Commissioning teams benefit when the as-built dossier repeats SUS329J3LTB beside heat numbers, linking isometric revisions to the same mill certificates. Size practice for SUS329J3LTB remains HX OD 19.0–50.8 mm common; U-bend annex with care for duplex springback.
Weldability of JIS G3463 SUS329J3LTB
Weldability of SUS329J3LTB follows austenitic-ferritic (duplex) practice. Filler/shop note: 22Cr duplex fillers; heat input, interpass, and ferrite window per WPS; purge ID. Caution: respect duplex temperature and sour-service limits; solution anneal after hot bends; not a silent swap for 316L. Procedure qualification for SUS329J3LTB should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. Keep the SUS329J3LTB caution visible here: respect duplex temperature and sour-service limits; solution anneal after hot bends; not a silent swap for 316L.
For welded G3463 tube, confirm whether as-welded or cold-finished welded finish is acceptable to the corrosion owner. Shop note: 22Cr duplex fillers; heat input, interpass, and ferrite window per WPS; purge ID. Consumable lot control and shielding-gas notes for SUS329J3LTB stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Size practice for SUS329J3LTB remains HX OD 19.0–50.8 mm common; U-bend annex with care for duplex springback.
Surface Finishes for JIS G3463 SUS329J3LTB
Pickled mill finish covers most HX tube RFQs for SUS329J3LTB. Bright anneal, grind, or polish only when the enquiry writes a measurable target. Use: seawater-lean coolers, chemical condensers, oil & gas process HX, and high-strength chloride tube bundles. Roughness or polish callouts for SUS329J3LTB must name OD, ID, or both; ambiguous “bright tube” language is clarified before finishing slots are booked. Weld-shop note tied to SUS329J3LTB: 22Cr duplex fillers; heat input, interpass, and ferrite window per WPS; purge ID.
Sanitary-lean duties may add ID polish; chemical lines may prefer a clean pickle only. State the need on the SUS329J3LTB order. Final visual standards for SUS329J3LTB reject grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed. Application context for SUS329J3LTB stays seawater-lean coolers, chemical condensers, oil & gas process HX, and high-strength chloride tube bundles.
Inspection and Testing for JIS G3463 SUS329J3LTB
SHH STEEL reports the tests actually performed for SUS329J3LTB — no surrogate NDT lines. Hydrostatic vs eddy-current/ultrasonic choice belongs on the PO. Caution: respect duplex temperature and sour-service limits; solution anneal after hot bends; not a silent swap for 316L. Sampling plans for SUS329J3LTB keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Corrosion framing beside SUS329J3LTB: PREN and strength both beat 316L in many chloride waters; crevice design and biofouling still matter.
NDT sensitivity levels and hydrostatic pressures follow the standard tables unless the purchaser specifies higher. Size context: HX OD 19.0–50.8 mm common; U-bend annex with care for duplex springback. Non-conforming SUS329J3LTB lengths are segregated and retested or rejected under retest clauses rather than reworked into unmarked stock. Application context for SUS329J3LTB stays seawater-lean coolers, chemical condensers, oil & gas process HX, and high-strength chloride tube bundles.
Packaging and Shipping for JIS G3463 SUS329J3LTB
Export packing for JIS G3463 SUS329J3LTB is built around rust prevention and transit abrasion control. Bundle tickets repeat the grade symbol and heat number. Duty: standard duplex (~2205 class) HX tube for chloride process condensers and coolers. Bundle tickets for SUS329J3LTB repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Application context for SUS329J3LTB stays seawater-lean coolers, chemical condensers, oil & gas process HX, and high-strength chloride tube bundles.
Marking paint and ink stickers stay chloride-lean. Heat numbers on tags match the MTC for SUS329J3LTB. Desiccant and wrap choices for SUS329J3LTB follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Size practice for SUS329J3LTB remains HX OD 19.0–50.8 mm common; U-bend annex with care for duplex springback.
Photographic packing records are available on request for project QA files on SUS329J3LTB. Claims handling for SUS329J3LTB starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Keep the SUS329J3LTB caution visible here: respect duplex temperature and sour-service limits; solution anneal after hot bends; not a silent swap for 316L.
Why Choose SHH STEEL
Buyers choose SHH STEEL for SUS329J3LTB because the paperwork matches the stencil: Table 3 chemistry, Table 4 tensile, Table 2 heat treatment, and honest seamless or A/L/E welded marking. Application fit: seawater-lean coolers, chemical condensers, oil & gas process HX, and high-strength chloride tube bundles. SHH STEEL can produce and supply SUS329J3LTB against the OD × wall, process symbol, and test scope on your RFQ without swapping in an unstated sister grade.
SHH STEEL will not invent PREN posters or warehouse tonnages. Bring OD × wall, medium notes, and test scope — we will quote SUS329J3LTB cleanly. Ask for a written acknowledgement that names SUS329J3LTB, the manufacture process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS329J3LTB to that written scope.
Supply Capability
Supply capability for SUS329J3LTB covers manufacture/finish symbols in Table 1, heat treatment in Table 2, and mechanical acceptance in Table 4. SHH STEEL can make the sizes on your list when the mill slot fits. Role: standard duplex (~2205 class) HX tube for chloride process condensers and coolers. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS329J3LTB when the mill schedule allows. This paragraph is locked to SUS329J3LTB duty: standard duplex (~2205 class) HX tube for chloride process condensers and coolers.
| Item | Capability |
|---|---|
| Standard | JIS G3463 stainless steel tubes for boilers and heat exchangers |
| Grade symbol | SUS329J3LTB |
| Product form | Seamless (S) and welded (A / L / E) tube; finishes S-H / S-C / A / A-C / E-C as marked |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered) |
| Typical OD practice | 15.9–139.8 mm per standard Note 1; other by agreement |
| Wall / gauge | OD × wall / BWG-class HX gauges within Attached Tables; other by agreement |
Stock / Available sizes
Stock / Available sizes for SUS329J3LTB: common A-number bores with schedule or measured wall as the project uses. Seamless and welded availability varies by diameter — confirm route with the RFQ. Hint: HX OD 19.0–50.8 mm common; U-bend annex with care for duplex springback. SHH STEEL can supply alternate schedules and measured walls for SUS329J3LTB once the design pressure and corrosion allowance are clear.
Mill certificates, packing photos, and third-party witness can be bundled into the SUS329J3LTB supply scope when the PO says so. Use: seawater-lean coolers, chemical condensers, oil & gas process HX, and high-strength chloride tube bundles. SHH STEEL can produce trial lengths of SUS329J3LTB for procedure qualification before the bulk release when the project calendar needs it.
FAQ
-
What is JIS G3463 SUS329J3LTB stainless steel tube used for?
- JIS G3463 SUS329J3LTB is stainless tube for boiler and heat-exchanger service (superheater, HX, condenser, catalyser) — seawater-lean coolers, chemical condensers, oil & gas process HX, and high-strength chloride tube bundles. Role summary: standard duplex (~2205 class) HX tube for chloride process condensers and coolers. It is a Japanese boiler/HX tube product standard mark, not an automatic ASTM A213 certificate.
-
Does JIS G3463 SUS329J3LTB cover seamless and welded tube?
- Yes. Manufacture allows seamless and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish marks such as S-H, S-C, A-C, or E-C. SHH STEEL can produce and supply either route for SUS329J3LTB when the mill can meet the ordered size and tests. The title omits Seamless/Welded because JIS G3463 covers both manufacture routes — the PO must still name the process mark.
-
What heat treatment applies to SUS329J3LTB?
- SUS329J3LTB is delivered solution annealed under JIS G3463. Table 2 reference: 950 °C min, rapid cool. Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
-
How does SUS329J3LTB compare with sister grades SUS329J4LTB, SUS329J1TB, SUS316LTB?
- SUS329J3LTB is filed as austenitic-ferritic (duplex). Typical sisters on the same RFQ are SUS329J4LTB, SUS329J1TB, SUS316LTB. Design caution: respect duplex temperature and sour-service limits; solution anneal after hot bends; not a silent swap for 316L Pick the sister when the medium or strength floor outgrows this symbol rather than stretching wall alone.
-
What tests appear on the mill certificate for SUS329J3LTB?
- Expect cast analysis (Table 3), room-temperature tensile results (Table 4), flattening/flaring as applicable, dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
-
Is ~2205 / UNS S31803–S32205 class the same as ordering SUS329J3LTB?
- No. ~2205 / UNS S31803–S32205 class is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3463 and SUS329J3LTB so cast limits, heat treatment, and process marks are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for JIS G3463 SUS329J3LTB?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS329J3LTB within the typical 15.9–139.8 mm OD practice, with measured walls by agreement. Size context: HX OD 19.0–50.8 mm common; U-bend annex with care for duplex springback. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
How should SUS329J3LTB be welded?
- Shop guidance: 22Cr duplex fillers; heat input, interpass, and ferrite window per WPS; purge ID. Mill heat treatment of seamless or welded tube does not replace a qualified WPS on fabricator joints or tube-to-tubesheet welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: respect duplex temperature and sour-service limits; solution anneal after hot bends; not a silent swap for 316L
-
When should I choose a duplex or higher-Mo grade instead of SUS329J3LTB?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic-ferritic (duplex) practice can defend for the temperature and stress state. Caution for this mark: respect duplex temperature and sour-service limits; solution anneal after hot bends; not a silent swap for 316L Sister pointers: SUS329J4LTB, SUS329J1TB, SUS316LTB. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify JIS G3463 SUS329J3LTB with ASTM A213 or ASME SA213?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3463 SUS329J3LTB does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What surface finishes are available for SUS329J3LTB?
- Pickled after heat treatment is the usual HX tube supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS329J3LTB when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
JIS G3463 SUS329J3LTB is stainless steel tube for boiler and heat-exchanger service — standard duplex (~2205 class) HX tube for chloride process condensers and coolers. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS329J4LTB, SUS329J1TB, SUS316LTB. Related ASTM A213 pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process mark, and medium notes to start the quote.