JIS G3463 SUS430LXTB Stainless Steel Tube

JIS G3463 SUS430LXTB stainless steel tube (430LX Ti/Nb-stabilised), ferritic, Table 3 cast analysis, Rm min 360 N/mm² / proof min 175 N/mm², annealed. SHH STEEL can produce and supply seamless or welded routes with mill certificates.
Grade
SUS430LXTB (430LX Ti/Nb-stabilised — body alias)
Standard
JIS G3463
Product form
Seamless and welded stainless steel boiler/HX tube, delivery annealed
Size
Typically OD 15.9–139.8 mm (Note 1); OD × wall (HX/boiler gauges) by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is JIS G3463 SUS430LXTB Stainless Steel Tube

JIS G3463 covers both seamless and welded stainless tube for process, utility, condenser and heat-exchange duties. Inside that standard, SUS430LXTB is filed as ferritic. When the cooler will be welded throughout, JIS G3463 SUS430LXTB is usually the safer 17Cr choice than plain SUS430TB. Buyers working Japanese boiler and HX packages should treat SUS430LXTB as a governed product symbol under G3463, with Table 3 chemistry and Table 4 tensile floors enforced on the same heat. Weld-shop note tied to SUS430LXTB: stabilised ferritic fillers; control heat input.

From pierce/draw or weld-and-anneal through marking and bundle protection, SHH STEEL can produce JIS G3463 SUS430LXTB for the sizes and tests on your RFQ. Application sketch: welded fresh-water coolers, HVAC exchangers, and ferritic condensers needing stabilisation. Size and test clarity on the RFQ lets SHH STEEL lock the correct Table 1 symbols for SUS430LXTB before production starts. Weld-shop note tied to SUS430LXTB: stabilised ferritic fillers; control heat input.

On the floor people shorten marks; in QA they must not. SUS430LXTB under JIS G3463 carries specific Table 3 windows and Table 4 floors that a loose “430LX Ti” note will not enforce. Caution: lower tensile floors than SUS430TB; confirm stabilising elements on the MTC. Keep isometric notes, tubesheet specs, and the mill acknowledgement aligned on SUS430LXTB so informal alias language cannot reopen the carbon or molybdenum window after melt. This paragraph is locked to SUS430LXTB duty: stabilised low-C 17Cr ferritic for welded mild HX tube.

Superheater, condenser and corrosive HX duties all sit in G3463’s scope statement; still match the alloy to the medium. For SUS430LXTB, that means: stabilised low-C 17Cr ferritic for welded mild HX tube. Nearby marks: SUS430TB, SUS430J1LTB, SUS436LTB, SUS444TB. Document the medium, design temperature, and weld map beside the SUS430LXTB line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Weld-shop note tied to SUS430LXTB: stabilised ferritic fillers; control heat input.

Inside this JIS G3463 series, compare SUS430TB, SUS430J1LTB, SUS436LTB, SUS444TB. Hub: JIS G3463. ASTM/ASME related product pages (not interchangeable by default): ASTM A213.

Chemical Composition of JIS G3463 SUS430LXTB

For SUS430LXTB, the melt ticket has to show Table 3 compliance — C ≤0.030, Si ≤0.75, Mn ≤1.00, P ≤0.040, S ≤0.030, Cr 16.00–19.00, Ti or Nb per standard footnote. Optional alloying footnotes in the standard still forbid blurring grade identity. Corrosion framing: stabilisation + low C improves welded mild aqueous behaviour versus plain 430.

Where Mo, Cu, Ti, Nb or N appear, they are intentional levers for SUS430LXTB, not optional marketing. Confirm them on the MTC line-by-line. Role: stabilised low-C 17Cr ferritic for welded mild HX tube. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for SUS430LXTB before the order is acknowledged. Application context for SUS430LXTB stays welded fresh-water coolers, HVAC exchangers, and ferritic condensers needing stabilisation.

Grade C Si Mn P S Cr Ti or Nb
SUS430LXTB ≤0.030 ≤0.75 ≤1.00 ≤0.040 ≤0.030 16.00–19.00 per standard footnote

Mechanical Properties of JIS G3463 SUS430LXTB

Do not confuse Table 4 tube tensile floors with plate or tube standards that share the 430LX Ti/Nb-stabilised alias. For SUS430LXTB under G3463 expect Rm min 360 N/mm², proof stress min 175 N/mm², elongation min 20% (OD ≥20 mm, No.11/12), verified per heat/lot rules in tensile sampling clauses. Tensile sampling follows tensile sampling clauses for the ordered test unit of SUS430LXTB, and retests follow retest clauses when a result sits under the Table 4 floor. Corrosion framing beside SUS430LXTB: stabilisation + low C improves welded mild aqueous behaviour versus plain 430.

Grade Rm min (N/mm²) Proof stress min (N/mm²) A OD≥20 mm No.11/12 min (%) A 10≤OD<20 mm No.11 min (%) A OD<10 mm No.11 min (%)
SUS430LXTB 360 175 20 15 12

Ambient values from JIS G3463 Table 4 for SUS430LXTB. Heat treatment (Table 2): 720 °C min, air or slow cool. Elongation reductions apply for walls under 8 mm on No.12 pieces. For heat-exchanger tube the purchaser may designate an upper tensile limit (Table 4 min + 200 N/mm²) when necessary.

Manufacture of JIS G3463 SUS430LXTB Tube (Seamless and Welded)

Both seamless and welded SUS430LXTB are legitimate under JIS G3463. Pick S when the design pressure, wall, or NDT plan favours a pierced/drawn route; pick A, L, or E when welded economics fit and the weld procedure is qualified. Finish symbols S-H/S-C/A/A-C/E-C ride with the process mark on the tube stencil. Seamless and welded options remain available for SUS430LXTB; the acknowledgement repeats the Table 1 symbols so production cannot silently change route after the PO is firm. Application context for SUS430LXTB stays welded fresh-water coolers, HVAC exchangers, and ferritic condensers needing stabilisation.

Welded SUS430LXTB needs weld-bead work or as-welded finish called out (as-welded vs cold-finished welded) so NDT and corrosion expectations match. Heat treatment: 720 °C min, air or slow cool. Ferritic heats are annealed (700 °C min, or 720 °C min for SUS430J1LTB) with rapid or slow cooling as Table 2 allows — not austenitic solution practice.

Hydrostatic testing or NDT (eddy current / ultrasonic per JIS G 0582/0583) replaces or accompanies pressure proof as the order states. Manufacture stays honest to the seamless or A/L/E welded choice. Size: commodity HX OD; welded routes common. Hydrostatic pressure or NDT class for SUS430LXTB is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Corrosion framing beside SUS430LXTB: stabilisation + low C improves welded mild aqueous behaviour versus plain 430.

Dimensions and Tolerances for JIS G3463 SUS430LXTB

Out-of-table OD×wall combinations are by agreement — still under the same grade symbol SUS430LXTB. Duty: stabilised low-C 17Cr ferritic for welded mild HX tube. Tolerance class follows the process route ordered for SUS430LXTB, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Corrosion framing beside SUS430LXTB: stabilisation + low C improves welded mild aqueous behaviour versus plain 430.

Ovality, wall eccentricity (where applicable), and weld bead height limits are part of dimensional tolerance clauses — not optional cosmetics. Size reminder: commodity HX OD; welded routes common. Fixed lengths and multiple cut lengths for SUS430LXTB are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Size practice for SUS430LXTB remains commodity HX OD; welded routes common.

Equivalent Grades for JIS G3463 SUS430LXTB

SUS430LXTB is the stabilised low-carbon 17Cr ferritic tube mark under JIS G3463, written for welded mild heat-exchanger duty where plain SUS430TB grain growth would be a concern. The body-only alias “430LX Ti/Nb-stabilised” helps buyers in dual-cert talk, but it is not a substitute designation on the PO or MTC. European or ASTM marks that sit near the same chemistry still carry different hydrostatic, NDT, and heat-treatment text, so keep SUS430LXTB as the governing symbol unless a written dual-cert plan exists.

System Designation Notes
JIS G3463 SUS430LXTB Governing HX/boiler tube grade for this page
Commercial / UNS (body only) 430LX (Ti/Nb-stabilised) Useful in dual-cert talk; confirm Ti/Nb on the cast analysis
ASTM A213 / A269 related Stabilised 430-family tube practice (no single TP asserted) Related chemistry family — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local ferritic tube specs

Tensile floors on SUS430LXTB sit lower than SUS430TB in typical G3463 practice, so do not assume the plain-430 mechanical table. Sisters worth reading beside this page: SUS430TB, SUS430J1LTB, SUS436LTB, SUS444TB. Full series hub: JIS G3463.

Heat Treatment and Delivery Condition for JIS G3463 SUS430LXTB

Hot-finished seamless austenitics may use in-line rapid cool in lieu of a separate solution treatment under Table 2 note (a) unless the purchaser forbids it. Confirm for SUS430LXTB. Band: 720 °C min, air or slow cool. Recorded furnace charts for SUS430LXTB should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Size practice for SUS430LXTB remains commodity HX OD; welded routes common.

Grain-size testing applies where the standard requires it for specific H grades — state any extra metallographic demand on the PO for SUS430LXTB. Field heat treatment of SUS430LXTB after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Corrosion framing beside SUS430LXTB: stabilisation + low C improves welded mild aqueous behaviour versus plain 430.

Corrosion Resistance of JIS G3463 SUS430LXTB

Medium, temperature, crevice geometry and weld condition decide whether SUS430LXTB is enough. Summary: stabilisation + low C improves welded mild aqueous behaviour versus plain 430. Escalate via sisters SUS430TB, SUS430J1LTB, SUS436LTB, SUS444TB when coupons fail. Coupon orientation, weld condition, and surface finish for SUS430LXTB belong in the corrosion test order so annex results can be compared to the installed bundle honestly. This paragraph is locked to SUS430LXTB duty: stabilised low-C 17Cr ferritic for welded mild HX tube.

Surface finish and iron contamination control often matter as much as bulk chemistry on sanitary-lean duties for SUS430LXTB. Corrosion framing: stabilisation + low C improves welded mild aqueous behaviour versus plain 430. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for SUS430LXTB rather than relying on schedule thickness alone. Application context for SUS430LXTB stays welded fresh-water coolers, HVAC exchangers, and ferritic condensers needing stabilisation.

Applications of JIS G3463 SUS430LXTB Tube

From utility rooms to process racks, SUS430LXTB shows up wherever Japanese boiler/HX specs want ferritic behaviour. Use list: welded fresh-water coolers, HVAC exchangers, and ferritic condensers needing stabilisation. Spool fabricators should copy SUS430LXTB onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. This paragraph is locked to SUS430LXTB duty: stabilised low-C 17Cr ferritic for welded mild HX tube.

If the only reason for SUS430LXTB is “we always used this alias,” reopen the corrosion file before repeating the order. Caution: lower tensile floors than SUS430TB; confirm stabilising elements on the MTC. Commissioning teams benefit when the as-built dossier repeats SUS430LXTB beside heat numbers, linking isometric revisions to the same mill certificates. Size practice for SUS430LXTB remains commodity HX OD; welded routes common.

Weldability of JIS G3463 SUS430LXTB

Automatic mill welds and manual field welds need different procedure packs, but both must respect SUS430LXTB chemistry. Guidance: stabilised ferritic fillers; control heat input. Procedure qualification for SUS430LXTB should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. This paragraph is locked to SUS430LXTB duty: stabilised low-C 17Cr ferritic for welded mild HX tube.

Ferrite control on duplex SUS430LXTB and hot-crack control on high-Ni austenitics are procedure items, not afterthoughts. Guidance: stabilised ferritic fillers; control heat input. Consumable lot control and shielding-gas notes for SUS430LXTB stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Keep the SUS430LXTB caution visible here: lower tensile floors than SUS430TB; confirm stabilising elements on the MTC.

Surface Finishes for JIS G3463 SUS430LXTB

Welded SUS430LXTB tube is commonly supplied annealed and pickled, with bead dressing called out when flow or inspection needs a flush ID/OD. Bright anneal is ordered when scale-free appearance matters on commodity HX OD; polish or special roughness is by agreement and must name the surface. Because this mark is chosen for welded fresh-water coolers and HVAC exchangers that need stabilisation, finish language should stay measurable rather than relying on mill habit.

Finish Typical supply Order note
Annealed and pickled Usual welded HX mill finish after anneal Matte, scale-free; confirm stabilisers already on MTC
Bright annealed Scale-free OD/ID when appearance is specified State OD, ID, or both
Ground / polished / bead dressed By agreement for flow or inspection callouts Name Ra/grit and which surface; dress welds before polish
Passivated When the end-user file requires it Not a substitute for correct anneal or Ti/Nb control

Do not polish over unresolved weld defects — inspection comes before cosmetics on SUS430LXTB. Passivation is an add-on film treatment, not a fix for missed heat treatment. Use iron-free packing and chloride-lean stencil practice so finished stabilised ferritic tube does not leave the yard with free-iron blooms.

Inspection and Testing for JIS G3463 SUS430LXTB

Third-party witness (SGS/TUV-style) is available when the project mandate requires it. Base acceptance still tracks G3463 for SUS430LXTB. Sampling plans for SUS430LXTB keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Corrosion framing beside SUS430LXTB: stabilisation + low C improves welded mild aqueous behaviour versus plain 430.

Dimensional inspection against dimensional tolerance clauses tolerances closes the lot. Failures retest per retest clauses — they are not silently shipped. Role: stabilised low-C 17Cr ferritic for welded mild HX tube. Non-conforming SUS430LXTB lengths are segregated and retested or rejected under retest clauses rather than reworked into unmarked stock. Keep the SUS430LXTB caution visible here: lower tensile floors than SUS430TB; confirm stabilising elements on the MTC.

Packaging and Shipping for JIS G3463 SUS430LXTB

Seaworthy packing is available for ocean legs — desiccant, VCI, and wrap specs by agreement. Grade mark SUS430LXTB stays visible on outer tags. Bundle tickets for SUS430LXTB repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Corrosion framing beside SUS430LXTB: stabilisation + low C improves welded mild aqueous behaviour versus plain 430.

Container loading plans should keep heavy schedules from crushing thin-wall SUS430LXTB layers. Desiccant and wrap choices for SUS430LXTB follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Weld-shop note tied to SUS430LXTB: stabilised ferritic fillers; control heat input Desiccant and wrap choices for SUS430LXTB follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Medium risk note for SUS430LXTB: lower tensile floors than SUS430TB; confirm stabilising elements on the MTC.

Shortages or transit damage claims need photos against the packing list before installation starts — tag identity must still read SUS430LXTB. Claims handling for SUS430LXTB starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Keep the SUS430LXTB caution visible here: lower tensile floors than SUS430TB; confirm stabilising elements on the MTC.

Why Choose SHH STEEL

From RFQ clarification through MTC release, SHH STEEL treats SUS430LXTB as a governed product symbol, not a marketing synonym for 430LX Ti/Nb-stabilised. Role: stabilised low-C 17Cr ferritic for welded mild HX tube. SHH STEEL can produce and supply SUS430LXTB against the OD × wall, process symbol, and test scope on your RFQ without swapping in an unstated sister grade.

Response time stays short because common SUS430LXTB enquiry sizes and document packs are already exercised on prior Japanese-spec orders. Use: welded fresh-water coolers, HVAC exchangers, and ferritic condensers needing stabilisation. Ask for a written acknowledgement that names SUS430LXTB, the manufacture process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS430LXTB to that written scope.

Supply Capability

Capability framing for SUS430LXTB: Japanese-spec HX tube product, dual-route manufacture, documented heats. Caution remains: lower tensile floors than SUS430TB; confirm stabilising elements on the MTC. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS430LXTB when the mill schedule allows. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS430LXTB when the mill schedule allows. This paragraph is locked to SUS430LXTB duty: stabilised low-C 17Cr ferritic for welded mild HX tube.

Item Capability
Standard JIS G3463 stainless steel tubes for boilers and heat exchangers
Grade symbol SUS430LXTB
Product form Seamless (S) and welded (A / L / E) tube; finishes S-H / S-C / A / A-C / E-C as marked
Delivery condition annealed
Documents Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered)
Typical OD practice 15.9–139.8 mm per standard Note 1; other by agreement
Wall / gauge OD × wall / BWG-class HX gauges within Attached Tables; other by agreement

Stock / Available sizes

Stock / Available sizes — treat published ranges as capability envelopes. Actual ex-stock pieces of SUS430LXTB change weekly; the reliable path is an OD × wall matrix on the enquiry. Duty: stabilised low-C 17Cr ferritic for welded mild HX tube. SHH STEEL can supply alternate schedules and measured walls for SUS430LXTB once the design pressure and corrosion allowance are clear.

Repeat orders for SUS430LXTB go faster when prior heat records and accepted WPS numbers are referenced on the new RFQ. Role: stabilised low-C 17Cr ferritic for welded mild HX tube. SHH STEEL can produce trial lengths of SUS430LXTB for procedure qualification before the bulk release when the project calendar needs it. SHH STEEL can produce trial lengths of SUS430LXTB for procedure qualification before bulk release when the project calendar needs it. Weld-shop note tied to SUS430LXTB: stabilised ferritic fillers; control heat input.

FAQ

What is JIS G3463 SUS430LXTB stainless steel tube used for?
JIS G3463 SUS430LXTB is stainless tube for boiler and heat-exchanger service (superheater, HX, condenser, catalyser) — welded fresh-water coolers, HVAC exchangers, and ferritic condensers needing stabilisation. Role summary: stabilised low-C 17Cr ferritic for welded mild HX tube. It is a Japanese boiler/HX tube product standard mark, not an automatic ASTM A213 certificate.
Does JIS G3463 SUS430LXTB cover seamless and welded tube?
Yes. Manufacture allows seamless and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish marks such as S-H, S-C, A-C, or E-C. SHH STEEL can produce and supply either route for SUS430LXTB when the mill can meet the ordered size and tests. The title omits Seamless/Welded because JIS G3463 covers both manufacture routes — the PO must still name the process mark.
What heat treatment applies to SUS430LXTB?
SUS430LXTB is delivered annealed under JIS G3463. Table 2 reference: 720 °C min, air or slow cool. Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
How does SUS430LXTB compare with sister grades SUS430TB, SUS430J1LTB, SUS436LTB?
SUS430LXTB is filed as ferritic. Typical sisters on the same RFQ are SUS430TB, SUS430J1LTB, SUS436LTB. Design caution: lower tensile floors than SUS430TB; confirm stabilising elements on the MTC Pick the sister when the medium or strength floor outgrows this symbol rather than stretching wall alone.
What tests appear on the mill certificate for SUS430LXTB?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), flattening/flaring as applicable, dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
Is 430LX Ti/Nb-stabilised the same as ordering SUS430LXTB?
No. 430LX Ti/Nb-stabilised is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3463 and SUS430LXTB so cast limits, heat treatment, and process marks are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for JIS G3463 SUS430LXTB?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS430LXTB within the typical 15.9–139.8 mm OD practice, with measured walls by agreement. Size context: commodity HX OD; welded routes common. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should SUS430LXTB be welded?
Shop guidance: stabilised ferritic fillers; control heat input. Mill heat treatment of seamless or welded tube does not replace a qualified WPS on fabricator joints or tube-to-tubesheet welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: lower tensile floors than SUS430TB; confirm stabilising elements on the MTC
When should I choose a duplex or higher-Mo grade instead of SUS430LXTB?
Move when chloride pitting, crevice attack, or SCC risk exceeds what ferritic practice can defend for the temperature and stress state. Caution for this mark: lower tensile floors than SUS430TB; confirm stabilising elements on the MTC Sister pointers: SUS430TB, SUS430J1LTB, SUS436LTB. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify JIS G3463 SUS430LXTB with ASTM A213 or ASME SA213?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3463 SUS430LXTB does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for SUS430LXTB?
Pickled after heat treatment is the usual HX tube supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS430LXTB when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

JIS G3463 SUS430LXTB is stainless steel tube for boiler and heat-exchanger service — stabilised low-C 17Cr ferritic for welded mild HX tube. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS430TB, SUS430J1LTB, SUS436LTB. Related ASTM A213 pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process mark, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X