JIS G3463 SUS316HTB Stainless Steel Tube
What is JIS G3463 SUS316HTB Stainless Steel Tube
JIS G3463 is the Japanese Industrial Standard for stainless steel tubes used in boiler and heat-exchanger service (superheater, HX, condenser, catalyser). Grade symbol SUS316HTB sits in the austenitic set of Table 1. Order JIS G3463 SUS316HTB when the temperature file wants a carbon floor and the medium still wants molybdenum — not when someone only typed “316H” from habit.
SHH STEEL can produce and supply JIS G3463 SUS316HTB as seamless or welded tube across the enquiry OD×wall band, solution-annealed or annealed as Table 2 requires, pickled or bright-finished, and documented on mill test certificates tied to cast analysis and tensile results. Duty focus: controlled-carbon Mo austenitic for elevated-temperature HX tube where hot strength and molybdenum both matter.
Shop language may still say “316H tube,” yet that commercial alias does not select Japanese cast limits, process symbols, or hydraulic/NDT rules. The purchase order has to name JIS G3463 and SUS316HTB so the mill applies the correct analysis, heat treatment, mechanical floors, and marking. Design caution: 0.04–0.10% C window forbids silent L dual-certs; aqueous welded duty still reviews L or stabilised options.
Scope discipline: SUS316HTB is HX tube product under JIS G3463, not a piping product under JIS G3459 and not an ASTM A213 order by default. Sister marks often compared on the same RFQ include SUS316TB, SUS316LTB, SUS321HTB, SUS347HTB. Role reminder: controlled-carbon Mo austenitic for elevated-temperature HX tube where hot strength and molybdenum both matter.
Inside this JIS G3463 series, compare SUS316TB, SUS316LTB, SUS321HTB, SUS347HTB. Hub: JIS G3463. ASTM/ASME related product pages (not interchangeable by default): A213 TP316H, ASTM A213.
Chemical Composition of JIS G3463 SUS316HTB
Cast analysis for JIS G3463 SUS316HTB follows Table 3. Key windows on a typical certificate include C 0.04–0.10, Si ≤0.75, Mn ≤2.00, P ≤0.030, S ≤0.030, Ni 11.00–14.00, Cr 16.00–18.00. SHH STEEL ties the heat number on the tube marking to the same cast line on the MTC. Commercial alias 316H / UNS S31609 is body text only. Corrosion thread: Mo helps aqueous pitting relative to 304H; oxidation behaviour is still austenitic Mo-family, not 310-class.
Chemical limits for SUS316HTB under JIS G3463 appear in the table underneath. Source priority is the 2021 Table 3 extract cross-checked to public Nikko / supplier tables. If your client specification cites a different edition footnote, send it before the heat is melted. Duty thread: controlled-carbon Mo austenitic for elevated-temperature HX tube where hot strength and molybdenum both matter.
| Grade | C | Si | Mn | P | S | Ni | Cr | Mo |
|---|---|---|---|---|---|---|---|---|
| SUS316HTB | 0.04–0.10 | ≤0.75 | ≤2.00 | ≤0.030 | ≤0.030 | 11.00–14.00 | 16.00–18.00 | 2.00–3.00 |
Mechanical Properties of JIS G3463 SUS316HTB
Ambient tensile floors for SUS316HTB come from JIS G3463 Table 4: Rm min 520 N/mm², proof stress min 206 N/mm², elongation min 35% (OD ≥20 mm, No.11/12). These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: austenitic. Caution: 0.04–0.10% C window forbids silent L dual-certs; aqueous welded duty still reviews L or stabilised options.
| Grade | Rm min (N/mm²) | Proof stress min (N/mm²) | A OD≥20 mm No.11/12 min (%) | A 10≤OD<20 mm No.11 min (%) | A OD<10 mm No.11 min (%) |
|---|---|---|---|---|---|
| SUS316HTB | 520 | 206 | 35 | 30 | 27 |
Ambient values from JIS G3463 Table 4 for SUS316HTB. Heat treatment (Table 2): 1040 °C min, rapid cool. Elongation reductions apply for walls under 8 mm on No.12 pieces. For heat-exchanger tube the purchaser may designate an upper tensile limit (Table 4 min + 200 N/mm²) when necessary.
Manufacture of JIS G3463 SUS316HTB Tube (Seamless and Welded)
SHH STEEL can produce SUS316HTB as seamless S or as A/L/E welded tube, then heat-treat and pickle (or bright-anneal) per Table 2. Bevel ends are available by agreement; plain ends are the default when the PO is silent. Seamless and welded options remain available for SUS316HTB; the acknowledgement repeats the Table 1 symbols so production cannot silently change route after the PO is firm. Corrosion framing beside SUS316HTB: Mo helps aqueous pitting relative to 304H; oxidation behaviour is still austenitic Mo-family, not 310-class.
Austenitic heats take solution annealing with rapid cooling; hot-finished seamless may omit separate solution treatment when hot-worked and rapidly cooled in-line under the Table 2 note, unless the purchaser forbids it. Heat-treatment reference for SUS316HTB: 1040 °C min, rapid cool. Pickling follows unless bright heat treatment leaves a scale-free surface. Duty thread: controlled-carbon Mo austenitic for elevated-temperature HX tube where hot strength and molybdenum both matter.
When dual documentation against ASTM A213 is requested for a related chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for SUS316HTB: seamless S-H for heavier hot walls; S-C for thinner precision HX.
Dimensions and Tolerances for JIS G3463 SUS316HTB
SHH STEEL aligns nominal diameter (A/B), outside diameter, schedule or wall, and length tolerance for SUS316HTB before the mill slot is locked. Standard Note 1 frames typical OD from 15.9 mm to 139.8 mm (standard Note 1 general practice). Size hint: seamless S-H for heavier hot walls; S-C for thinner precision HX.
Length supply may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against the packaging clause so pickled or polished finishes are not iron-stained in transit. Duty thread: controlled-carbon Mo austenitic for elevated-temperature HX tube where hot strength and molybdenum both matter. Fixed lengths and multiple cut lengths for SUS316HTB are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Weld-shop note tied to SUS316HTB: 316H-class fillers when matching hot strength; purge and heat-input control on returns.
Equivalent Grades for JIS G3463 SUS316HTB
Equivalence talk for SUS316HTB starts with 316H / UNS S31609: that commercial / UNS framing is useful in body text and dual-cert discussions, but the H1 and order line stay on JIS G3463 SUS316HTB. ASTM A213 / A269 pages that share related chemistry are different product standards with different wall bases, mechanical tables, and tests. Sisters: SUS316TB, SUS316LTB, SUS321HTB, SUS347HTB. Caution: 0.04–0.10% C window forbids silent L dual-certs; aqueous welded duty still reviews L or stabilised options.
Heat Treatment and Delivery Condition for JIS G3463 SUS316HTB
SUS316HTB is delivered solution annealed under JIS G3463. Table 2 reference: 1040 °C min, rapid cool. Fabricator heat treatment after hot bending should chase the same family practice. Weld thread: 316H-class fillers when matching hot strength; purge and heat-input control on returns. Recorded furnace charts for SUS316HTB should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. This paragraph is locked to SUS316HTB duty: controlled-carbon Mo austenitic for elevated-temperature HX tube where hot strength and molybdenum both matter.
Cooling type matters — austenitic and duplex need rapid cool after solution treatment; ferritic anneal practice allows rapid or slow cool per Table 2. Duty thread: controlled-carbon Mo austenitic for elevated-temperature HX tube where hot strength and molybdenum both matter. Field heat treatment of SUS316HTB after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Size practice for SUS316HTB remains seamless S-H for heavier hot walls; S-C for thinner precision HX.
Corrosion Resistance of JIS G3463 SUS316HTB
Corrosion behaviour of JIS G3463 SUS316HTB tracks its austenitic balance: Mo helps aqueous pitting relative to 304H; oxidation behaviour is still austenitic Mo-family, not 310-class. Optional annex corrosion tests (oxalic, Strauss, Huey, etc.) are special quality items — order them when the duty needs coupon evidence. Design caution: 0.04–0.10% C window forbids silent L dual-certs; aqueous welded duty still reviews L or stabilised options.
For heat-facing austenitics, oxidation resistance may dominate over aqueous IGC talk; for duplex and Mo austenitics, chlorides dominate; for ferritics, mild aqueous and weld practice dominate. SUS316HTB is filed as austenitic. Caution: 0.04–0.10% C window forbids silent L dual-certs; aqueous welded duty still reviews L or stabilised options. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for SUS316HTB rather than relying on schedule thickness alone. This paragraph is locked to SUS316HTB duty: controlled-carbon Mo austenitic for elevated-temperature HX tube where hot strength and molybdenum both matter.
Applications of JIS G3463 SUS316HTB Tube
Applications of JIS G3463 SUS316HTB tube centre on high-temperature process steam exchangers, superheater-adjacent Mo tube, and heat-recovery bundles needing Mo plus a carbon floor. Role summary: controlled-carbon Mo austenitic for elevated-temperature HX tube where hot strength and molybdenum both matter. When a related chemistry is required under ASTM A213 or A269, open those sister pages — acceptance text is not automatic.
Downstream fabricators should inherit the same grade symbol on cut lists so informal alias substitutions do not creep in. Primary application sketch: high-temperature process steam exchangers, superheater-adjacent Mo tube, and heat-recovery bundles needing Mo plus a carbon floor. Duty thread: controlled-carbon Mo austenitic for elevated-temperature HX tube where hot strength and molybdenum both matter.
Weldability of JIS G3463 SUS316HTB
SUS316HTB is welded both as a mill product (A/L/E routes) and as fabricator joints on bundles. Shop guidance: 316H-class fillers when matching hot strength; purge and heat-input control on returns. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Procedure qualification for SUS316HTB should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. Size practice for SUS316HTB remains seamless S-H for heavier hot walls; S-C for thinner precision HX.
Filler selection should match or over-alloy the base chemistry as the WPS demands. Heat input, interpass temperature, and shielding follow the family — austenitic, duplex, or ferritic — not a single shop habit. Caution: 0.04–0.10% C window forbids silent L dual-certs; aqueous welded duty still reviews L or stabilised options. Consumable lot control and shielding-gas notes for SUS316HTB stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Weld-shop note tied to SUS316HTB: 316H-class fillers when matching hot strength; purge and heat-input control on returns.
Surface Finishes for JIS G3463 SUS316HTB
Surface supply for SUS316HTB is typically pickled after heat treatment, or bright-annealed when scale-free OD/ID is ordered. Polished or special roughness finishes are by agreement and must state which surface (OD, ID, or both) is in scope. Duty: controlled-carbon Mo austenitic for elevated-temperature HX tube where hot strength and molybdenum both matter.
Passivation treatments, when ordered, follow agreed ASTM A967 / JIS practice analogues — they are not a substitute for correct heat treatment. Caution: 0.04–0.10% C window forbids silent L dual-certs; aqueous welded duty still reviews L or stabilised options. Final visual standards for SUS316HTB reject grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed. Weld-shop note tied to SUS316HTB: 316H-class fillers when matching hot strength; purge and heat-input control on returns.
Inspection and Testing for JIS G3463 SUS316HTB
Inspection for JIS G3463 SUS316HTB covers cast analysis, tensile tests, flattening or weld bend as applicable, hydrostatic test or NDT, dimensions, and appearance. Special quality annex items (IGC, grain size, etc.) apply only when ordered. Documents follow JIS G 0415 / purchaser-specified EN 10204 styles. Sampling plans for SUS316HTB keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Weld-shop note tied to SUS316HTB: 316H-class fillers when matching hot strength; purge and heat-input control on returns.
Marking includes SUS316HTB, manufacture/finish symbols, manufacturer, and other mandatory marking-clause data. Traceability from stencil to MTC is part of supply, not an upgrade. Use: high-temperature process steam exchangers, superheater-adjacent Mo tube, and heat-recovery bundles needing Mo plus a carbon floor. Non-conforming SUS316HTB lengths are segregated and retested or rejected under retest clauses rather than reworked into unmarked stock. Corrosion framing beside SUS316HTB: Mo helps aqueous pitting relative to 304H; oxidation behaviour is still austenitic Mo-family, not 310-class.
Packaging and Shipping for JIS G3463 SUS316HTB
Packaging for SUS316HTB uses wooden boxes, plywood cases, or bundled frames with waterproof wrapping as the OD and finish demand. Soft separators protect pickled and polished surfaces. Ends receive caps or bevel protectors when ordered. Bundle tickets for SUS316HTB repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Keep the SUS316HTB caution visible here: 0.04–0.10% C window forbids silent L dual-certs; aqueous welded duty still reviews L or stabilised options.
Carbon-steel strapping never contacts the stainless OD without a barrier. Mixed-grade bundles are forbidden when chemistry integrity matters. Caution: 0.04–0.10% C window forbids silent L dual-certs; aqueous welded duty still reviews L or stabilised options. Desiccant and wrap choices for SUS316HTB follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Application context for SUS316HTB stays high-temperature process steam exchangers, superheater-adjacent Mo tube, and heat-recovery bundles needing Mo plus a carbon floor.
Shipping documents list JIS G3463, SUS316HTB, sizes, quantities, heat numbers, and certificate type. SHH STEEL coordinates inland trucking and FOB/CIF packing scopes as the order states. Role: controlled-carbon Mo austenitic for elevated-temperature HX tube where hot strength and molybdenum both matter. Claims handling for SUS316HTB starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Corrosion framing beside SUS316HTB: Mo helps aqueous pitting relative to 304H; oxidation behaviour is still austenitic Mo-family, not 310-class.
Why Choose SHH STEEL
SHH STEEL can produce and supply JIS G3463 SUS316HTB with the process route, heat treatment, and tests named on your enquiry — not a bait-and-switch alias. Mill partners run stainless tube capacity that covers seamless and welded Table 1 symbols for this mark. Duty focus: controlled-carbon Mo austenitic for elevated-temperature HX tube where hot strength and molybdenum both matter.
Technical sales can map SUS316HTB against sisters SUS316TB, SUS316LTB, SUS321HTB, SUS347HTB and live ASTM pages without pretending standards are identical. Inspection coordination and export packing are in-house habits, not afterthoughts. Ask for a written acknowledgement that names SUS316HTB, the manufacture process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS316HTB to that written scope.
Supply Capability
SHH STEEL can produce and supply JIS G3463 SUS316HTB across enquiry-oriented OD × wall bands, in seamless or welded routes, with certificates and optional annex tests as ordered. Summary capability follows in the table; stock language below is an RFQ map, not a frozen tonnage catalogue. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS316HTB when the mill schedule allows.
| Item | Capability |
|---|---|
| Standard | JIS G3463 stainless steel tubes for boilers and heat exchangers |
| Grade symbol | SUS316HTB |
| Product form | Seamless (S) and welded (A / L / E) tube; finishes S-H / S-C / A / A-C / E-C as marked |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered) |
| Typical OD practice | 15.9–139.8 mm per standard Note 1; other by agreement |
| Wall / gauge | OD × wall / BWG-class HX gauges within Attached Tables; other by agreement |
Stock / Available sizes
SHH STEEL can produce and supply JIS G3463 SUS316HTB. Stock / Available sizes: enquiry band typically aligns with 15.9–139.8 mm OD practice under G3463 Note 1, with OD×wall HX gauges; schedule 5S–80 (and heavier by agreement) depending on grade family. For SUS316HTB, practical fast-track sizes often sit in mid-bore process and utility ranges — send the OD × wall list for a firm acknowledgement. Context: seamless S-H for heavier hot walls; S-C for thinner precision HX.
Cut lengths, bevels, special NDT, and IGC annex tests add lead time — call them early. Sisters often quoted alongside: SUS316TB, SUS316LTB, SUS321HTB, SUS347HTB. Email the size list to start. SHH STEEL can produce trial lengths of SUS316HTB for procedure qualification before the bulk release when the project calendar needs it. SHH STEEL can produce trial lengths of SUS316HTB for procedure qualification before bulk release when the project calendar needs it. Weld-shop note tied to SUS316HTB: 316H-class fillers when matching hot strength; purge and heat-input control on returns.
FAQ
-
What is JIS G3463 SUS316HTB stainless steel tube used for?
- JIS G3463 SUS316HTB is stainless tube for boiler and heat-exchanger service (superheater, HX, condenser, catalyser) — high-temperature process steam exchangers, superheater-adjacent Mo tube, and heat-recovery bundles needing Mo plus a carbon floor. Role summary: controlled-carbon Mo austenitic for elevated-temperature HX tube where hot strength and molybdenum both matter. It is a Japanese boiler/HX tube product standard mark, not an automatic ASTM A213 certificate.
-
Does JIS G3463 SUS316HTB cover seamless and welded tube?
- Yes. Manufacture allows seamless and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish marks such as S-H, S-C, A-C, or E-C. SHH STEEL can produce and supply either route for SUS316HTB when the mill can meet the ordered size and tests. The title omits Seamless/Welded because JIS G3463 covers both manufacture routes — the PO must still name the process mark.
-
What heat treatment applies to SUS316HTB?
- SUS316HTB is delivered solution annealed under JIS G3463. Table 2 reference: 1040 °C min, rapid cool. Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
-
How does SUS316HTB compare with sister grades SUS316TB, SUS316LTB, SUS321HTB?
- SUS316HTB is filed as austenitic. Typical sisters on the same RFQ are SUS316TB, SUS316LTB, SUS321HTB. Design caution: 0.04–0.10% C window forbids silent L dual-certs; aqueous welded duty still reviews L or stabilised options Pick the sister when the medium or strength floor outgrows this symbol rather than stretching wall alone.
-
What tests appear on the mill certificate for SUS316HTB?
- Expect cast analysis (Table 3), room-temperature tensile results (Table 4), flattening/flaring as applicable, dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
-
Is 316H / UNS S31609 the same as ordering SUS316HTB?
- No. 316H / UNS S31609 is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3463 and SUS316HTB so cast limits, heat treatment, and process marks are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for JIS G3463 SUS316HTB?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS316HTB within the typical 15.9–139.8 mm OD practice, with measured walls by agreement. Size context: seamless S-H for heavier hot walls; S-C for thinner precision HX. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
How should SUS316HTB be welded?
- Shop guidance: 316H-class fillers when matching hot strength; purge and heat-input control on returns. Mill heat treatment of seamless or welded tube does not replace a qualified WPS on fabricator joints or tube-to-tubesheet welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: 0.04–0.10% C window forbids silent L dual-certs; aqueous welded duty still reviews L or stabilised options
-
When should I choose a duplex or higher-Mo grade instead of SUS316HTB?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: 0.04–0.10% C window forbids silent L dual-certs; aqueous welded duty still reviews L or stabilised options Sister pointers: SUS316TB, SUS316LTB, SUS321HTB. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify JIS G3463 SUS316HTB with ASTM A213 or ASME SA213?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3463 SUS316HTB does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What surface finishes are available for SUS316HTB?
- Pickled after heat treatment is the usual HX tube supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS316HTB when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
JIS G3463 SUS316HTB is stainless steel tube for boiler and heat-exchanger service — controlled-carbon Mo austenitic for elevated-temperature HX tube where hot strength and molybdenum both matter. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS316TB, SUS316LTB, SUS321HTB. Related ASTM A213 pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process mark, and medium notes to start the quote.