JIS G3463 SUS316LTB Stainless Steel Tube

JIS G3463 SUS316LTB stainless steel tube (316L / UNS S31603), austenitic, Table 3 cast analysis, Rm min 481 N/mm² / proof min 177 N/mm², solution annealed. SHH STEEL can produce and supply seamless or welded routes with mill certificates.
Grade
SUS316LTB (316L / UNS S31603 — body alias)
Standard
JIS G3463
Product form
Seamless and welded stainless steel boiler/HX tube, delivery solution annealed
Size
Typically OD 15.9–139.8 mm (Note 1); OD × wall (HX/boiler gauges) by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is JIS G3463 SUS316LTB Stainless Steel Tube

Boiler and heat-exchanger packages that cite Japanese product standards look to JIS G3463 — Stainless steel boiler and heat exchanger tubes — rather than inventing a mill grade from AISI shorthand alone. SUS316LTB is the Table 1 symbol for this austenitic chemistry. If the PO says “316L exchanger tube” under a Japanese project, lock JIS G3463 SUS316LTB — alias talk alone will not enforce the 0.030% carbon ceiling.

Mill path for SUS316LTB: Table 1 manufacture/finish symbols, Table 2 heat treatment, Table 3 cast chemistry, Table 4 tensile floors. SHH STEEL can make and supply the grade to that stack with hydrostatic or NDT acceptance as ordered. Typical use: chemical condensers, food/pharma exchangers, desalination heaters, and U-tube bundles where field/shop welds stay in the medium.

Body text may mention 316L / UNS S31603 for cross-reference, but the H1 and order line stay on SUS316LTB. Silent alias swaps are how wrong carbon ceilings and wrong tensile tables enter the MTC. Keep this caution in view: lower Rm/proof floors than SUS316TB — engineer must accept Table 4 L values before substitution.

Order the standard the drawing and regulatory file actually require. Inside this G3463 series, compare SUS316TB, SUS317LTB, SUS316TiTB, SUS304LTB before stretching surface finish or schedule alone. Duty thread: low-carbon Mo austenitic HX / condenser tube for as-welded corrosive and chloride-lean process duty. Document the medium, design temperature, and weld map beside the SUS316LTB line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Keep the SUS316LTB caution visible here: lower Rm/proof floors than SUS316TB — engineer must accept Table 4 L values before substitution.

Inside this JIS G3463 series, compare SUS316TB, SUS317LTB, SUS316TiTB, SUS304LTB. Hub: JIS G3463. ASTM/ASME related product pages (not interchangeable by default): A213 TP316L, A269 TP316L, ASTM A213.

Chemical Composition of JIS G3463 SUS316LTB

Table 3 sets the melt limits for SUS316LTB. Highlight band: C ≤0.030, Si ≤1.00, Mn ≤2.00, P ≤0.040, S ≤0.030, Ni 12.00–16.00, Cr 16.00–18.00. Product analysis, when ordered, applies JIS G 0321 stainless product tolerances on top of Table 3. Alias note: 316L / UNS S31603. Every ladle analysis for SUS316LTB is checked against those windows before the heat is released to piercing, welding, or finishing, and the same numbers reappear on the inspection document. Application context for SUS316LTB stays chemical condensers, food/pharma exchangers, desalination heaters, and U-tube bundles where field/shop welds stay in the medium.

The composition table below is the cast window SHH STEEL quotes against for SUS316LTB. Edition framing is JIS G3463. Use thread: chemical condensers, food/pharma exchangers, desalination heaters, and U-tube bundles where field/shop welds stay in the medium. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for SUS316LTB before the order is acknowledged. Application context for SUS316LTB stays chemical condensers, food/pharma exchangers, desalination heaters, and U-tube bundles where field/shop welds stay in the medium.

Grade C Si Mn P S Ni Cr Mo
SUS316LTB ≤0.030 ≤1.00 ≤2.00 ≤0.040 ≤0.030 12.00–16.00 16.00–18.00 2.00–3.00

Mechanical Properties of JIS G3463 SUS316LTB

Table 4 mechanical acceptance for SUS316LTB: Rm min 481 N/mm², proof stress min 177 N/mm², elongation min 35% (OD ≥20 mm, No.11/12). Elongation rules change for walls under 8 mm and are not mandatory below 40 mm OD (record only unless agreed). Delivery framing: solution annealed. Tensile sampling follows tensile sampling clauses for the ordered test unit of SUS316LTB, and retests follow retest clauses when a result sits under the Table 4 floor. Corrosion framing beside SUS316LTB: low C plus Mo is the default Japanese answer for welded Mo austenitic HX; severe chlorides may still need 317L, duplex, or 6Mo.

Grade Rm min (N/mm²) Proof stress min (N/mm²) A OD≥20 mm No.11/12 min (%) A 10≤OD<20 mm No.11 min (%) A OD<10 mm No.11 min (%)
SUS316LTB 481 177 35 30 27

Ambient values from JIS G3463 Table 4 for SUS316LTB. Heat treatment (Table 2): 1010 °C min, rapid cool. Elongation reductions apply for walls under 8 mm on No.12 pieces. For heat-exchanger tube the purchaser may designate an upper tensile limit (Table 4 min + 200 N/mm²) when necessary.

Manufacture of JIS G3463 SUS316LTB Tube (Seamless and Welded)

JIS G3463 manufactures SUS316LTB by seamless (symbol S) or welded routes — automatic arc (A), laser (L), or electric-resistance (E) — then applies the ordered finish: hot finish H, cold finish C, hot finish S-H or cold finish S-C / A-C / E-C as marked. SHH STEEL confirms the Table 1 symbol string on the acknowledgement before rolling or welding starts.

After forming, SUS316LTB receives Table 2 treatment — 1010 °C min, rapid cool. Austenitic heats take solution annealing with rapid cooling; hot-finished seamless may omit separate solution treatment when hot-worked and rapidly cooled in-line under the Table 2 note, unless the purchaser forbids it. Use thread: chemical condensers, food/pharma exchangers, desalination heaters, and U-tube bundles where field/shop welds stay in the medium.

Marking carries the grade symbol SUS316LTB, process/finish marks, manufacturer ID, and other marking-clause items. Size hint: commodity HX OD 15.9–38.1 mm; welded or seamless per pressure and NDT plan. Weld thread: 316L fillers; thorough ID purge on tube-to-tubesheet and U-bend joints. Hydrostatic pressure or NDT class for SUS316LTB is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Size practice for SUS316LTB remains commodity HX OD 15.9–38.1 mm; welded or seamless per pressure and NDT plan.

Dimensions and Tolerances for JIS G3463 SUS316LTB

Dimensional order lines for SUS316LTB should state OD × wall (or OD×wall HX gauges; schedule 5S/10S/20S/40/80/…), length type, and end finish. Tolerances follow dimensional tolerance clauses by process route. Use: chemical condensers, food/pharma exchangers, desalination heaters, and U-tube bundles where field/shop welds stay in the medium. Tolerance class follows the process route ordered for SUS316LTB, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Application context for SUS316LTB stays chemical condensers, food/pharma exchangers, desalination heaters, and U-tube bundles where field/shop welds stay in the medium.

OD and wall tolerances differ for hot-finished seamless versus cold-finished / welded routes — quote the process symbol with the size. Caution: lower Rm/proof floors than SUS316TB — engineer must accept Table 4 L values before substitution. Fixed lengths and multiple cut lengths for SUS316LTB are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Corrosion framing beside SUS316LTB: low C plus Mo is the default Japanese answer for welded Mo austenitic HX; severe chlorides may still need 317L, duplex, or 6Mo.

Equivalent Grades for JIS G3463 SUS316LTB

SUS316LTB is the JIS G3463 designation. Alias 316L / UNS S31603 appears only as a cross-walk. Compare sisters SUS316TB, SUS317LTB, SUS316TiTB, SUS304LTB when the medium or temperature outgrows this mark. Hook: lock SUS316LTB on the PO. When a dual-cert path is required, list both JIS G3463 SUS316LTB and the ASTM mark with separate test scopes instead of assuming one chemistry line clears both files. Weld-shop note tied to SUS316LTB: 316L fillers; thorough ID purge on tube-to-tubesheet and U-bend joints.

Heat Treatment and Delivery Condition for JIS G3463 SUS316LTB

Mill heat treatment for SUS316LTB: 1010 °C min, rapid cool. Bright annealing may omit pickling when the surface is scale-free. Delivery label: solution annealed. Recorded furnace charts for SUS316LTB should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Application context for SUS316LTB stays chemical condensers, food/pharma exchangers, desalination heaters, and U-tube bundles where field/shop welds stay in the medium.

Certificate wording for SUS316LTB should show the heat-treatment condition actually performed, not a generic “annealed” stamp that hides temperature. Use: chemical condensers, food/pharma exchangers, desalination heaters, and U-tube bundles where field/shop welds stay in the medium. Field heat treatment of SUS316LTB after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. This paragraph is locked to SUS316LTB duty: low-carbon Mo austenitic HX / condenser tube for as-welded corrosive and chloride-lean process duty.

Corrosion Resistance of JIS G3463 SUS316LTB

low C plus Mo is the default Japanese answer for welded Mo austenitic HX; severe chlorides may still need 317L, duplex, or 6Mo Special quality annex tests are available by agreement; they are not a blanket warranty for every process medium. Family filing: austenitic. Coupon orientation, weld condition, and surface finish for SUS316LTB belong in the corrosion test order so annex results can be compared to the installed bundle honestly. Corrosion framing beside SUS316LTB: low C plus Mo is the default Japanese answer for welded Mo austenitic HX; severe chlorides may still need 317L, duplex, or 6Mo.

Do not market invented PREN digits. Bring medium chemistry and SHH STEEL will map SUS316LTB honestly against SUS316TB, SUS317LTB, SUS316TiTB, SUS304LTB. Role: low-carbon Mo austenitic HX / condenser tube for as-welded corrosive and chloride-lean process duty. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for SUS316LTB rather than relying on schedule thickness alone. This paragraph is locked to SUS316LTB duty: low-carbon Mo austenitic HX / condenser tube for as-welded corrosive and chloride-lean process duty.

Applications of JIS G3463 SUS316LTB Tube

Typical BOM language pairs JIS G3463 SUS316LTB with OD × wall (or schedule), manufacture/finish symbols, and heat-treatment condition. Primary sketch: chemical condensers, food/pharma exchangers, desalination heaters, and U-tube bundles where field/shop welds stay in the medium. Spool fabricators should copy SUS316LTB onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Application context for SUS316LTB stays chemical condensers, food/pharma exchangers, desalination heaters, and U-tube bundles where field/shop welds stay in the medium.

Spell SUS316LTB on tube-sheet drawings and bundle lists, bundle sheets and tubesheet specs alike. Sister options when the medium hardens: SUS316TB, SUS317LTB, SUS316TiTB, SUS304LTB. Commissioning teams benefit when the as-built dossier repeats SUS316LTB beside heat numbers, linking isometric revisions to the same mill certificates. Keep the SUS316LTB caution visible here: lower Rm/proof floors than SUS316TB — engineer must accept Table 4 L values before substitution.

Weldability of JIS G3463 SUS316LTB

Weldability of SUS316LTB follows austenitic practice. Filler/shop note: 316L fillers; thorough ID purge on tube-to-tubesheet and U-bend joints. Caution: lower Rm/proof floors than SUS316TB — engineer must accept Table 4 L values before substitution. Procedure qualification for SUS316LTB should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. Size practice for SUS316LTB remains commodity HX OD 15.9–38.1 mm; welded or seamless per pressure and NDT plan.

For welded G3463 tube, confirm whether as-welded or cold-finished welded finish is acceptable to the corrosion owner. Shop note: 316L fillers; thorough ID purge on tube-to-tubesheet and U-bend joints. Consumable lot control and shielding-gas notes for SUS316LTB stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Weld-shop note tied to SUS316LTB: 316L fillers; thorough ID purge on tube-to-tubesheet and U-bend joints.

Surface Finishes for JIS G3463 SUS316LTB

Pickled mill finish covers most HX tube RFQs for SUS316LTB. Bright anneal, grind, or polish only when the enquiry writes a measurable target. Use: chemical condensers, food/pharma exchangers, desalination heaters, and U-tube bundles where field/shop welds stay in the medium. Roughness or polish callouts for SUS316LTB must name OD, ID, or both; ambiguous “bright tube” language is clarified before finishing slots are booked. This paragraph is locked to SUS316LTB duty: low-carbon Mo austenitic HX / condenser tube for as-welded corrosive and chloride-lean process duty.

Sanitary-lean duties may add ID polish; chemical lines may prefer a clean pickle only. State the need on the SUS316LTB order. Final visual standards for SUS316LTB reject grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed. Corrosion framing beside SUS316LTB: low C plus Mo is the default Japanese answer for welded Mo austenitic HX; severe chlorides may still need 317L, duplex, or 6Mo.

Inspection and Testing for JIS G3463 SUS316LTB

SHH STEEL reports the tests actually performed for SUS316LTB — no surrogate NDT lines. Hydrostatic vs eddy-current/ultrasonic choice belongs on the PO. Caution: lower Rm/proof floors than SUS316TB — engineer must accept Table 4 L values before substitution. Sampling plans for SUS316LTB keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. This paragraph is locked to SUS316LTB duty: low-carbon Mo austenitic HX / condenser tube for as-welded corrosive and chloride-lean process duty.

NDT sensitivity levels and hydrostatic pressures follow the standard tables unless the purchaser specifies higher. Size context: commodity HX OD 15.9–38.1 mm; welded or seamless per pressure and NDT plan. Non-conforming SUS316LTB lengths are segregated and retested or rejected under retest clauses rather than reworked into unmarked stock. Size practice for SUS316LTB remains commodity HX OD 15.9–38.1 mm; welded or seamless per pressure and NDT plan.

Packaging and Shipping for JIS G3463 SUS316LTB

Export packing for JIS G3463 SUS316LTB is built around rust prevention and transit abrasion control. Bundle tickets repeat the grade symbol and heat number. Duty: low-carbon Mo austenitic HX / condenser tube for as-welded corrosive and chloride-lean process duty. Bundle tickets for SUS316LTB repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Keep the SUS316LTB caution visible here: lower Rm/proof floors than SUS316TB — engineer must accept Table 4 L values before substitution.

Marking paint and ink stickers stay chloride-lean. Heat numbers on tags match the MTC for SUS316LTB. Desiccant and wrap choices for SUS316LTB follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Corrosion framing beside SUS316LTB: low C plus Mo is the default Japanese answer for welded Mo austenitic HX; severe chlorides may still need 317L, duplex, or 6Mo.

Photographic packing records are available on request for project QA files on SUS316LTB. Claims handling for SUS316LTB starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. This paragraph is locked to SUS316LTB duty: low-carbon Mo austenitic HX / condenser tube for as-welded corrosive and chloride-lean process duty.

Why Choose SHH STEEL

Buyers choose SHH STEEL for SUS316LTB because the paperwork matches the stencil: Table 3 chemistry, Table 4 tensile, Table 2 heat treatment, and honest seamless or A/L/E welded marking. Application fit: chemical condensers, food/pharma exchangers, desalination heaters, and U-tube bundles where field/shop welds stay in the medium. SHH STEEL can produce and supply SUS316LTB against the OD × wall, process symbol, and test scope on your RFQ without swapping in an unstated sister grade.

SHH STEEL will not invent PREN posters or warehouse tonnages. Bring OD × wall, medium notes, and test scope — we will quote SUS316LTB cleanly. Ask for a written acknowledgement that names SUS316LTB, the manufacture process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS316LTB to that written scope.

Supply Capability

Supply capability for SUS316LTB covers manufacture/finish symbols in Table 1, heat treatment in Table 2, and mechanical acceptance in Table 4. SHH STEEL can make the sizes on your list when the mill slot fits. Role: low-carbon Mo austenitic HX / condenser tube for as-welded corrosive and chloride-lean process duty. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS316LTB when the mill schedule allows. Weld-shop note tied to SUS316LTB: 316L fillers; thorough ID purge on tube-to-tubesheet and U-bend joints.

Item Capability
Standard JIS G3463 stainless steel tubes for boilers and heat exchangers
Grade symbol SUS316LTB
Product form Seamless (S) and welded (A / L / E) tube; finishes S-H / S-C / A / A-C / E-C as marked
Delivery condition solution annealed
Documents Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered)
Typical OD practice 15.9–139.8 mm per standard Note 1; other by agreement
Wall / gauge OD × wall / BWG-class HX gauges within Attached Tables; other by agreement

Stock / Available sizes

Stock / Available sizes for SUS316LTB: common A-number bores with schedule or measured wall as the project uses. Seamless and welded availability varies by diameter — confirm route with the RFQ. Hint: commodity HX OD 15.9–38.1 mm; welded or seamless per pressure and NDT plan. SHH STEEL can supply alternate schedules and measured walls for SUS316LTB once the design pressure and corrosion allowance are clear.

Mill certificates, packing photos, and third-party witness can be bundled into the SUS316LTB supply scope when the PO says so. Use: chemical condensers, food/pharma exchangers, desalination heaters, and U-tube bundles where field/shop welds stay in the medium. SHH STEEL can produce trial lengths of SUS316LTB for procedure qualification before the bulk release when the project calendar needs it.

FAQ

What is JIS G3463 SUS316LTB stainless steel tube used for?
JIS G3463 SUS316LTB is stainless tube for boiler and heat-exchanger service (superheater, HX, condenser, catalyser) — chemical condensers, food/pharma exchangers, desalination heaters, and U-tube bundles where field/shop welds stay in the medium. Role summary: low-carbon Mo austenitic HX / condenser tube for as-welded corrosive and chloride-lean process duty. It is a Japanese boiler/HX tube product standard mark, not an automatic ASTM A213 certificate.
Does JIS G3463 SUS316LTB cover seamless and welded tube?
Yes. Manufacture allows seamless and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish marks such as S-H, S-C, A-C, or E-C. SHH STEEL can produce and supply either route for SUS316LTB when the mill can meet the ordered size and tests. The title omits Seamless/Welded because JIS G3463 covers both manufacture routes — the PO must still name the process mark.
What heat treatment applies to SUS316LTB?
SUS316LTB is delivered solution annealed under JIS G3463. Table 2 reference: 1010 °C min, rapid cool. Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
How does SUS316LTB compare with sister grades SUS316TB, SUS317LTB, SUS316TiTB?
SUS316LTB is filed as austenitic. Typical sisters on the same RFQ are SUS316TB, SUS317LTB, SUS316TiTB. Design caution: lower Rm/proof floors than SUS316TB — engineer must accept Table 4 L values before substitution Pick the sister when the medium or strength floor outgrows this symbol rather than stretching wall alone.
What tests appear on the mill certificate for SUS316LTB?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), flattening/flaring as applicable, dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
Is 316L / UNS S31603 the same as ordering SUS316LTB?
No. 316L / UNS S31603 is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3463 and SUS316LTB so cast limits, heat treatment, and process marks are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for JIS G3463 SUS316LTB?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS316LTB within the typical 15.9–139.8 mm OD practice, with measured walls by agreement. Size context: commodity HX OD 15.9–38.1 mm; welded or seamless per pressure and NDT plan. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should SUS316LTB be welded?
Shop guidance: 316L fillers; thorough ID purge on tube-to-tubesheet and U-bend joints. Mill heat treatment of seamless or welded tube does not replace a qualified WPS on fabricator joints or tube-to-tubesheet welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: lower Rm/proof floors than SUS316TB — engineer must accept Table 4 L values before substitution
When should I choose a duplex or higher-Mo grade instead of SUS316LTB?
Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: lower Rm/proof floors than SUS316TB — engineer must accept Table 4 L values before substitution Sister pointers: SUS316TB, SUS317LTB, SUS316TiTB. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify JIS G3463 SUS316LTB with ASTM A213 or ASME SA213?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3463 SUS316LTB does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for SUS316LTB?
Pickled after heat treatment is the usual HX tube supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS316LTB when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

JIS G3463 SUS316LTB is stainless steel tube for boiler and heat-exchanger service — low-carbon Mo austenitic HX / condenser tube for as-welded corrosive and chloride-lean process duty. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS316TB, SUS317LTB, SUS316TiTB. Related ASTM A213 pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process mark, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response