JIS G3463 SUS317LTB stainless steel tube (317L / UNS S31703), austenitic, Table 3 cast analysis, Rm min 481 N/mm² / proof min 177 N/mm², solution annealed. SHH STEEL can produce and supply seamless or welded routes with mill certificates.
Grade
SUS317LTB (317L / UNS S31703 — body alias)
Standard
JIS G3463
Product form
Seamless and welded stainless steel boiler/HX tube, delivery solution annealed
Size
Typically OD 15.9–139.8 mm (Note 1); OD × wall (HX/boiler gauges) by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is JIS G3463 SUS317LTB Stainless Steel Tube

Boiler and heat-exchanger packages that cite Japanese product standards look to JIS G3463 — Stainless steel boiler and heat exchanger tubes — rather than inventing a mill grade from AISI shorthand alone. SUS317LTB is the Table 1 symbol for this austenitic chemistry. JIS G3463 SUS317LTB is what you order when the corrosion file wants more molybdenum than 316L and the weld map forbids hoping carbon will stay low by accident.

Mill path for SUS317LTB: Table 1 manufacture/finish symbols, Table 2 heat treatment, Table 3 cast chemistry, Table 4 tensile floors. SHH STEEL can make and supply the grade to that stack with hydrostatic or NDT acceptance as ordered. Typical use: welded chemical condensers, seawater-lean coolers with careful design, and process HX needing Mo above 316L with as-welded stability.

Body text may mention 317L / UNS S31703 for cross-reference, but the H1 and order line stay on SUS317LTB. Silent alias swaps are how wrong carbon ceilings and wrong tensile tables enter the MTC. Keep this caution in view: lower tensile floors than SUS317TB; severe chlorides may still need SUS836LTB / SUS312LTB or duplex.

Order the standard the drawing and regulatory file actually require. Inside this G3463 series, compare SUS317TB, SUS316LTB, SUS890LTB, SUS836LTB before stretching surface finish or schedule alone. Duty thread: low-carbon higher-Mo austenitic for welded chemical and chloride HX tube. Document the medium, design temperature, and weld map beside the SUS317LTB line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Keep the SUS317LTB caution visible here: lower tensile floors than SUS317TB; severe chlorides may still need SUS836LTB / SUS312LTB or duplex.

Inside this JIS G3463 series, compare SUS317TB, SUS316LTB, SUS890LTB, SUS836LTB. Hub: JIS G3463. ASTM/ASME related product pages (not interchangeable by default): A213 TP317L, ASTM A213.

Chemical Composition of JIS G3463 SUS317LTB

Table 3 sets the melt limits for SUS317LTB. Highlight band: C ≤0.030, Si ≤1.00, Mn ≤2.00, P ≤0.040, S ≤0.030, Ni 11.00–15.00, Cr 18.00–20.00. Product analysis, when ordered, applies JIS G 0321 stainless product tolerances on top of Table 3. Alias note: 317L / UNS S31703. Every ladle analysis for SUS317LTB is checked against those windows before the heat is released to piercing, welding, or finishing, and the same numbers reappear on the inspection document. This paragraph is locked to SUS317LTB duty: low-carbon higher-Mo austenitic for welded chemical and chloride HX tube.

The composition table below is the cast window SHH STEEL quotes against for SUS317LTB. Edition framing is JIS G3463. Use thread: welded chemical condensers, seawater-lean coolers with careful design, and process HX needing Mo above 316L with as-welded stability. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for SUS317LTB before the order is acknowledged. Keep the SUS317LTB caution visible here: lower tensile floors than SUS317TB; severe chlorides may still need SUS836LTB / SUS312LTB or duplex.

Grade C Si Mn P S Ni Cr Mo
SUS317LTB ≤0.030 ≤1.00 ≤2.00 ≤0.040 ≤0.030 11.00–15.00 18.00–20.00 3.00–4.00

Mechanical Properties of JIS G3463 SUS317LTB

Table 4 mechanical acceptance for SUS317LTB: Rm min 481 N/mm², proof stress min 177 N/mm², elongation min 35% (OD ≥20 mm, No.11/12). Elongation rules change for walls under 8 mm and are not mandatory below 40 mm OD (record only unless agreed). Delivery framing: solution annealed. Tensile sampling follows tensile sampling clauses for the ordered test unit of SUS317LTB, and retests follow retest clauses when a result sits under the Table 4 floor. Application context for SUS317LTB stays welded chemical condensers, seawater-lean coolers with careful design, and process HX needing Mo above 316L with as-welded stability.

Grade Rm min (N/mm²) Proof stress min (N/mm²) A OD≥20 mm No.11/12 min (%) A 10≤OD<20 mm No.11 min (%) A OD<10 mm No.11 min (%)
SUS317LTB 481 177 35 30 27

Ambient values from JIS G3463 Table 4 for SUS317LTB. Heat treatment (Table 2): 1030 °C min, rapid cool. Elongation reductions apply for walls under 8 mm on No.12 pieces. For heat-exchanger tube the purchaser may designate an upper tensile limit (Table 4 min + 200 N/mm²) when necessary.

Manufacture of JIS G3463 SUS317LTB Tube (Seamless and Welded)

SHH STEEL can produce SUS317LTB as seamless S or as A/L/E welded tube, then heat-treat and pickle (or bright-anneal) per Table 2. Bevel ends are available by agreement; plain ends are the default when the PO is silent. Seamless and welded options remain available for SUS317LTB; the acknowledgement repeats the Table 1 symbols so production cannot silently change route after the PO is firm. This paragraph is locked to SUS317LTB duty: low-carbon higher-Mo austenitic for welded chemical and chloride HX tube.

After forming, SUS317LTB receives Table 2 treatment — 1030 °C min, rapid cool. Austenitic heats take solution annealing with rapid cooling; hot-finished seamless may omit separate solution treatment when hot-worked and rapidly cooled in-line under the Table 2 note, unless the purchaser forbids it. Use thread: welded chemical condensers, seawater-lean coolers with careful design, and process HX needing Mo above 316L with as-welded stability.

Marking carries the grade symbol SUS317LTB, process/finish marks, manufacturer ID, and other marking-clause items. Size hint: 19.0–50.8 mm OD typical enquiry band for process condensers. Weld thread: 317L fillers; purge ID; control interpass on multipass tubesheet welds. Hydrostatic pressure or NDT class for SUS317LTB is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Size practice for SUS317LTB remains 19.0–50.8 mm OD typical enquiry band for process condensers.

Dimensions and Tolerances for JIS G3463 SUS317LTB

Dimensional order lines for SUS317LTB should state OD × wall (or OD×wall HX gauges; schedule 5S/10S/20S/40/80/…), length type, and end finish. Tolerances follow dimensional tolerance clauses by process route. Use: welded chemical condensers, seawater-lean coolers with careful design, and process HX needing Mo above 316L with as-welded stability. Tolerance class follows the process route ordered for SUS317LTB, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Size practice for SUS317LTB remains 19.0–50.8 mm OD typical enquiry band for process condensers.

OD and wall tolerances differ for hot-finished seamless versus cold-finished / welded routes — quote the process symbol with the size. Caution: lower tensile floors than SUS317TB; severe chlorides may still need SUS836LTB / SUS312LTB or duplex. Fixed lengths and multiple cut lengths for SUS317LTB are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Application context for SUS317LTB stays welded chemical condensers, seawater-lean coolers with careful design, and process HX needing Mo above 316L with as-welded stability.

Equivalent Grades for JIS G3463 SUS317LTB

SUS317LTB is the JIS G3463 designation. Alias 317L / UNS S31703 appears only as a cross-walk. Compare sisters SUS317TB, SUS316LTB, SUS890LTB, SUS836LTB when the medium or temperature outgrows this mark. Hook: lock SUS317LTB on the PO. When a dual-cert path is required, list both JIS G3463 SUS317LTB and the ASTM mark with separate test scopes instead of assuming one chemistry line clears both files. This paragraph is locked to SUS317LTB duty: low-carbon higher-Mo austenitic for welded chemical and chloride HX tube.

Heat Treatment and Delivery Condition for JIS G3463 SUS317LTB

Mill heat treatment for SUS317LTB: 1030 °C min, rapid cool. Bright annealing may omit pickling when the surface is scale-free. Delivery label: solution annealed. Recorded furnace charts for SUS317LTB should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Weld-shop note tied to SUS317LTB: 317L fillers; purge ID; control interpass on multipass tubesheet welds.

Certificate wording for SUS317LTB should show the heat-treatment condition actually performed, not a generic “annealed” stamp that hides temperature. Use: welded chemical condensers, seawater-lean coolers with careful design, and process HX needing Mo above 316L with as-welded stability. Field heat treatment of SUS317LTB after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Application context for SUS317LTB stays welded chemical condensers, seawater-lean coolers with careful design, and process HX needing Mo above 316L with as-welded stability.

Corrosion Resistance of JIS G3463 SUS317LTB

low C + 3–4% Mo is a common Japanese chemical HX pick before jumping to 6Mo Special quality annex tests are available by agreement; they are not a blanket warranty for every process medium. Family filing: austenitic. Coupon orientation, weld condition, and surface finish for SUS317LTB belong in the corrosion test order so annex results can be compared to the installed bundle honestly. Size practice for SUS317LTB remains 19.0–50.8 mm OD typical enquiry band for process condensers.

Do not market invented PREN digits. Bring medium chemistry and SHH STEEL will map SUS317LTB honestly against SUS317TB, SUS316LTB, SUS890LTB, SUS836LTB. Role: low-carbon higher-Mo austenitic for welded chemical and chloride HX tube. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for SUS317LTB rather than relying on schedule thickness alone. This paragraph is locked to SUS317LTB duty: low-carbon higher-Mo austenitic for welded chemical and chloride HX tube.

Applications of JIS G3463 SUS317LTB Tube

Typical BOM language pairs JIS G3463 SUS317LTB with OD × wall (or schedule), manufacture/finish symbols, and heat-treatment condition. Primary sketch: welded chemical condensers, seawater-lean coolers with careful design, and process HX needing Mo above 316L with as-welded stability. Spool fabricators should copy SUS317LTB onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Keep the SUS317LTB caution visible here: lower tensile floors than SUS317TB; severe chlorides may still need SUS836LTB / SUS312LTB or duplex.

Spell SUS317LTB on tube-sheet drawings and bundle lists, bundle sheets and tubesheet specs alike. Sister options when the medium hardens: SUS317TB, SUS316LTB, SUS890LTB, SUS836LTB. Commissioning teams benefit when the as-built dossier repeats SUS317LTB beside heat numbers, linking isometric revisions to the same mill certificates. Application context for SUS317LTB stays welded chemical condensers, seawater-lean coolers with careful design, and process HX needing Mo above 316L with as-welded stability.

Weldability of JIS G3463 SUS317LTB

Weldability of SUS317LTB follows austenitic practice. Filler/shop note: 317L fillers; purge ID; control interpass on multipass tubesheet welds. Caution: lower tensile floors than SUS317TB; severe chlorides may still need SUS836LTB / SUS312LTB or duplex. Procedure qualification for SUS317LTB should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. Keep the SUS317LTB caution visible here: lower tensile floors than SUS317TB; severe chlorides may still need SUS836LTB / SUS312LTB or duplex.

For welded G3463 tube, confirm whether as-welded or cold-finished welded finish is acceptable to the corrosion owner. Shop note: 317L fillers; purge ID; control interpass on multipass tubesheet welds. Consumable lot control and shielding-gas notes for SUS317LTB stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Weld-shop note tied to SUS317LTB: 317L fillers; purge ID; control interpass on multipass tubesheet welds.

Surface Finishes for JIS G3463 SUS317LTB

Pickled mill finish covers most HX tube RFQs for SUS317LTB. Bright anneal, grind, or polish only when the enquiry writes a measurable target. Use: welded chemical condensers, seawater-lean coolers with careful design, and process HX needing Mo above 316L with as-welded stability. Roughness or polish callouts for SUS317LTB must name OD, ID, or both; ambiguous “bright tube” language is clarified before finishing slots are booked. Keep the SUS317LTB caution visible here: lower tensile floors than SUS317TB; severe chlorides may still need SUS836LTB / SUS312LTB or duplex.

Sanitary-lean duties may add ID polish; chemical lines may prefer a clean pickle only. State the need on the SUS317LTB order. Final visual standards for SUS317LTB reject grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed. Size practice for SUS317LTB remains 19.0–50.8 mm OD typical enquiry band for process condensers.

Inspection and Testing for JIS G3463 SUS317LTB

SHH STEEL reports the tests actually performed for SUS317LTB — no surrogate NDT lines. Hydrostatic vs eddy-current/ultrasonic choice belongs on the PO. Caution: lower tensile floors than SUS317TB; severe chlorides may still need SUS836LTB / SUS312LTB or duplex. Sampling plans for SUS317LTB keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Application context for SUS317LTB stays welded chemical condensers, seawater-lean coolers with careful design, and process HX needing Mo above 316L with as-welded stability.

NDT sensitivity levels and hydrostatic pressures follow the standard tables unless the purchaser specifies higher. Size context: 19.0–50.8 mm OD typical enquiry band for process condensers. Non-conforming SUS317LTB lengths are segregated and retested or rejected under retest clauses rather than reworked into unmarked stock. Weld-shop note tied to SUS317LTB: 317L fillers; purge ID; control interpass on multipass tubesheet welds.

Packaging and Shipping for JIS G3463 SUS317LTB

Export packing for JIS G3463 SUS317LTB is built around rust prevention and transit abrasion control. Bundle tickets repeat the grade symbol and heat number. Duty: low-carbon higher-Mo austenitic for welded chemical and chloride HX tube. Bundle tickets for SUS317LTB repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Weld-shop note tied to SUS317LTB: 317L fillers; purge ID; control interpass on multipass tubesheet welds.

Marking paint and ink stickers stay chloride-lean. Heat numbers on tags match the MTC for SUS317LTB. Desiccant and wrap choices for SUS317LTB follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Keep the SUS317LTB caution visible here: lower tensile floors than SUS317TB; severe chlorides may still need SUS836LTB / SUS312LTB or duplex.

Photographic packing records are available on request for project QA files on SUS317LTB. Claims handling for SUS317LTB starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Application context for SUS317LTB stays welded chemical condensers, seawater-lean coolers with careful design, and process HX needing Mo above 316L with as-welded stability.

Why Choose SHH STEEL

SHH STEEL can produce and supply JIS G3463 SUS317LTB. Buyers choose SHH STEEL for SUS317LTB because the paperwork matches the stencil: Table 3 chemistry, Table 4 tensile, Table 2 heat treatment, and honest seamless or A/L/E welded marking. Application fit: welded chemical condensers, seawater-lean coolers with careful design, and process HX needing Mo above 316L with as-welded stability.

SHH STEEL will not invent PREN posters or warehouse tonnages. Bring OD × wall, medium notes, and test scope — we will quote SUS317LTB cleanly. Ask for a written acknowledgement that names SUS317LTB, the manufacture process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS317LTB to that written scope.

Supply Capability

Supply capability for SUS317LTB covers manufacture/finish symbols in Table 1, heat treatment in Table 2, and mechanical acceptance in Table 4. SHH STEEL can make the sizes on your list when the mill slot fits. Role: low-carbon higher-Mo austenitic for welded chemical and chloride HX tube. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS317LTB when the mill schedule allows.

Item Capability
Standard JIS G3463 stainless steel tubes for boilers and heat exchangers
Grade symbol SUS317LTB
Product form Seamless (S) and welded (A / L / E) tube; finishes S-H / S-C / A / A-C / E-C as marked
Delivery condition solution annealed
Documents Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered)
Typical OD practice 15.9–139.8 mm per standard Note 1; other by agreement
Wall / gauge OD × wall / BWG-class HX gauges within Attached Tables; other by agreement

Stock / Available sizes

Stock / Available sizes for SUS317LTB: common A-number bores with schedule or measured wall as the project uses. Seamless and welded availability varies by diameter — confirm route with the RFQ. Hint: 19.0–50.8 mm OD typical enquiry band for process condensers. SHH STEEL can supply alternate schedules and measured walls for SUS317LTB once the design pressure and corrosion allowance are clear.

Mill certificates, packing photos, and third-party witness can be bundled into the SUS317LTB supply scope when the PO says so. Use: welded chemical condensers, seawater-lean coolers with careful design, and process HX needing Mo above 316L with as-welded stability. SHH STEEL can produce trial lengths of SUS317LTB for procedure qualification before the bulk release when the project calendar needs it.

FAQ

What is JIS G3463 SUS317LTB stainless steel tube used for?
JIS G3463 SUS317LTB is stainless tube for boiler and heat-exchanger service (superheater, HX, condenser, catalyser) — welded chemical condensers, seawater-lean coolers with careful design, and process HX needing Mo above 316L with as-welded stability. Role summary: low-carbon higher-Mo austenitic for welded chemical and chloride HX tube. It is a Japanese boiler/HX tube product standard mark, not an automatic ASTM A213 certificate.
Does JIS G3463 SUS317LTB cover seamless and welded tube?
Yes. Manufacture allows seamless and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish marks such as S-H, S-C, A-C, or E-C. SHH STEEL can produce and supply either route for SUS317LTB when the mill can meet the ordered size and tests. The title omits Seamless/Welded because JIS G3463 covers both manufacture routes — the PO must still name the process mark.
What heat treatment applies to SUS317LTB?
SUS317LTB is delivered solution annealed under JIS G3463. Table 2 reference: 1030 °C min, rapid cool. Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
How does SUS317LTB compare with sister grades SUS317TB, SUS316LTB, SUS890LTB?
SUS317LTB is filed as austenitic. Typical sisters on the same RFQ are SUS317TB, SUS316LTB, SUS890LTB. Design caution: lower tensile floors than SUS317TB; severe chlorides may still need SUS836LTB / SUS312LTB or duplex Pick the sister when the medium or strength floor outgrows this symbol rather than stretching wall alone.
What tests appear on the mill certificate for SUS317LTB?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), flattening/flaring as applicable, dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
Is 317L / UNS S31703 the same as ordering SUS317LTB?
No. 317L / UNS S31703 is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3463 and SUS317LTB so cast limits, heat treatment, and process marks are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for JIS G3463 SUS317LTB?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS317LTB within the typical 15.9–139.8 mm OD practice, with measured walls by agreement. Size context: 19.0–50.8 mm OD typical enquiry band for process condensers. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should SUS317LTB be welded?
Shop guidance: 317L fillers; purge ID; control interpass on multipass tubesheet welds. Mill heat treatment of seamless or welded tube does not replace a qualified WPS on fabricator joints or tube-to-tubesheet welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: lower tensile floors than SUS317TB; severe chlorides may still need SUS836LTB / SUS312LTB or duplex
When should I choose a duplex or higher-Mo grade instead of SUS317LTB?
Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: lower tensile floors than SUS317TB; severe chlorides may still need SUS836LTB / SUS312LTB or duplex Sister pointers: SUS317TB, SUS316LTB, SUS890LTB. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify JIS G3463 SUS317LTB with ASTM A213 or ASME SA213?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3463 SUS317LTB does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for SUS317LTB?
Pickled after heat treatment is the usual HX tube supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS317LTB when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

JIS G3463 SUS317LTB is stainless steel tube for boiler and heat-exchanger service — low-carbon higher-Mo austenitic for welded chemical and chloride HX tube. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS317TB, SUS316LTB, SUS890LTB. Related ASTM A213 pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process mark, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X