JIS G3463 SUS304HTB Stainless Steel Tube | JIS G3463 Stainless Steel Tube - SHH STEEL

JIS G3463 SUS304HTB Stainless Steel Tube

JIS G3463 SUS304HTB stainless steel tube (304H / UNS S30409), austenitic, Table 3 cast analysis, Rm min 520 N/mm² / proof min 206 N/mm², solution annealed. SHH STEEL can produce and supply seamless or welded routes with mill certificates.
Grade
SUS304HTB (304H / UNS S30409 — body alias)
Standard
JIS G3463
Product form
Seamless and welded stainless steel boiler/HX tube, delivery solution annealed
Size
Typically OD 15.9–139.8 mm (Note 1); OD × wall (HX/boiler gauges) by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is JIS G3463 SUS304HTB Stainless Steel Tube

JIS G3463 is the Japanese Industrial Standard for stainless steel tubes used in boiler and heat-exchanger service (superheater, HX, condenser, catalyser). Grade symbol SUS304HTB sits in the austenitic set of Table 1. JIS G3463 SUS304HTB exists so buyers stop pretending ordinary SUS304TB meets a written elevated-temperature carbon floor on boiler tube. Buyers working Japanese boiler and HX packages should treat SUS304HTB as a governed product symbol under G3463, with Table 3 chemistry and Table 4 tensile floors enforced on the same heat. Size practice for SUS304HTB remains hot-finished seamless S-H is common for heavier walls; cold-finished S-C for thinner HX gauges.

SHH STEEL can produce and supply JIS G3463 SUS304HTB as seamless or welded tube across the enquiry OD×wall band, solution-annealed or annealed as Table 2 requires, pickled or bright-finished, and documented on mill test certificates tied to cast analysis and tensile results. Duty focus: controlled-carbon 18-8 austenitic tube aimed at elevated-temperature HX and superheater-adjacent duty where a minimum carbon floor supports hot strength.

Shop language may still say “304H tube,” yet that commercial alias does not select Japanese cast limits, process symbols, or hydraulic/NDT rules. The purchase order has to name JIS G3463 and SUS304HTB so the mill applies the correct analysis, heat treatment, mechanical floors, and marking. Design caution: the 0.04–0.10% carbon window is intentional — do not dual-certify as SUS304LTB; welded corrosive aqueous duty still prefers an L or stabilised grade.

Scope discipline: SUS304HTB is HX tube product under JIS G3463, not a piping product under JIS G3459 and not an ASTM A213 order by default. Sister marks often compared on the same RFQ include SUS304TB, SUS321HTB, SUS347HTB, SUS316HTB. Role reminder: controlled-carbon 18-8 austenitic tube aimed at elevated-temperature HX and superheater-adjacent duty where a minimum carbon floor supports hot strength.

Inside this JIS G3463 series, compare SUS304TB, SUS321HTB, SUS347HTB, SUS316HTB. Hub: JIS G3463. ASTM/ASME related product pages (not interchangeable by default): A213 TP304H, ASTM A213.

Chemical Composition of JIS G3463 SUS304HTB

Cast analysis for JIS G3463 SUS304HTB follows Table 3. Key windows on a typical certificate include C 0.04–0.10, Si ≤0.75, Mn ≤2.00, P ≤0.040, S ≤0.030, Ni 8.00–11.00, Cr 18.00–20.00. SHH STEEL ties the heat number on the tube marking to the same cast line on the MTC. Commercial alias 304H / UNS S30409 is body text only. Corrosion thread: oxidation resistance is adequate for many hot-gas HX duties, but aqueous chloride pitting remains similar to standard 304.

Chemical limits for SUS304HTB under JIS G3463 appear in the table underneath. Source priority is the 2021 Table 3 extract cross-checked to public Nikko / supplier tables. If your client specification cites a different edition footnote, send it before the heat is melted. Duty thread: controlled-carbon 18-8 austenitic tube aimed at elevated-temperature HX and superheater-adjacent duty where a minimum carbon floor supports hot strength.

Grade C Si Mn P S Ni Cr
SUS304HTB 0.04–0.10 ≤0.75 ≤2.00 ≤0.040 ≤0.030 8.00–11.00 18.00–20.00

Mechanical Properties of JIS G3463 SUS304HTB

Ambient tensile floors for SUS304HTB come from JIS G3463 Table 4: Rm min 520 N/mm², proof stress min 206 N/mm², elongation min 35% (OD ≥20 mm, No.11/12). These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: austenitic. Caution: the 0.04–0.10% carbon window is intentional — do not dual-certify as SUS304LTB; welded corrosive aqueous duty still prefers an L or stabilised grade.

Grade Rm min (N/mm²) Proof stress min (N/mm²) A OD≥20 mm No.11/12 min (%) A 10≤OD<20 mm No.11 min (%) A OD<10 mm No.11 min (%)
SUS304HTB 520 206 35 30 27

Ambient values from JIS G3463 Table 4 for SUS304HTB. Heat treatment (Table 2): 1040 °C min, rapid cool. Elongation reductions apply for walls under 8 mm on No.12 pieces. For heat-exchanger tube the purchaser may designate an upper tensile limit (Table 4 min + 200 N/mm²) when necessary.

Manufacture of JIS G3463 SUS304HTB Tube (Seamless and Welded)

Both seamless and welded SUS304HTB are legitimate under JIS G3463. Pick S when the design pressure, wall, or NDT plan favours a pierced/drawn route; pick A, L, or E when welded economics fit and the weld procedure is qualified. Finish symbols S-H/S-C/A/A-C/E-C ride with the process mark on the tube stencil. Seamless and welded options remain available for SUS304HTB; the acknowledgement repeats the Table 1 symbols so production cannot silently change route after the PO is firm. This paragraph is locked to SUS304HTB duty: controlled-carbon 18-8 austenitic tube aimed at elevated-temperature HX and superheater-adjacent duty where a minimum carbon floor supports hot strength.

Austenitic heats take solution annealing with rapid cooling; hot-finished seamless may omit separate solution treatment when hot-worked and rapidly cooled in-line under the Table 2 note, unless the purchaser forbids it. Heat-treatment reference for SUS304HTB: 1040 °C min, rapid cool. Pickling follows unless bright heat treatment leaves a scale-free surface. Duty thread: controlled-carbon 18-8 austenitic tube aimed at elevated-temperature HX and superheater-adjacent duty where a minimum carbon floor supports hot strength.

When dual documentation against ASTM A213 is requested for a related chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for SUS304HTB: hot-finished seamless S-H is common for heavier walls; cold-finished S-C for thinner HX gauges.

Dimensions and Tolerances for JIS G3463 SUS304HTB

SHH STEEL aligns nominal diameter (A/B), outside diameter, schedule or wall, and length tolerance for SUS304HTB before the mill slot is locked. Standard Note 1 frames typical OD from 15.9 mm to 139.8 mm (standard Note 1 general practice). Size hint: hot-finished seamless S-H is common for heavier walls; cold-finished S-C for thinner HX gauges.

Length supply may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against the packaging clause so pickled or polished finishes are not iron-stained in transit. Duty thread: controlled-carbon 18-8 austenitic tube aimed at elevated-temperature HX and superheater-adjacent duty where a minimum carbon floor supports hot strength.

Equivalent Grades for JIS G3463 SUS304HTB

Equivalence talk for SUS304HTB starts with 304H / UNS S30409: that commercial / UNS framing is useful in body text and dual-cert discussions, but the H1 and order line stay on JIS G3463 SUS304HTB. ASTM A213 / A269 pages that share related chemistry are different product standards with different wall bases, mechanical tables, and tests. Sisters: SUS304TB, SUS321HTB, SUS347HTB, SUS316HTB. Caution: the 0.04–0.10% carbon window is intentional — do not dual-certify as SUS304LTB; welded corrosive aqueous duty still prefers an L or stabilised grade.

Heat Treatment and Delivery Condition for JIS G3463 SUS304HTB

SUS304HTB is delivered solution annealed under JIS G3463. Table 2 reference: 1040 °C min, rapid cool. Fabricator heat treatment after hot bending should chase the same family practice. Weld thread: 308H-class fillers when matching hot strength; avoid treating the joint like a low-carbon L weld without procedure review. Recorded furnace charts for SUS304HTB should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Corrosion framing beside SUS304HTB: oxidation resistance is adequate for many hot-gas HX duties, but aqueous chloride pitting remains similar to standard 304.

Cooling type matters — austenitic and duplex need rapid cool after solution treatment; ferritic anneal practice allows rapid or slow cool per Table 2. Duty thread: controlled-carbon 18-8 austenitic tube aimed at elevated-temperature HX and superheater-adjacent duty where a minimum carbon floor supports hot strength. Field heat treatment of SUS304HTB after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. This paragraph is locked to SUS304HTB duty: controlled-carbon 18-8 austenitic tube aimed at elevated-temperature HX and superheater-adjacent duty where a minimum carbon floor supports hot strength.

Corrosion Resistance of JIS G3463 SUS304HTB

Corrosion behaviour of JIS G3463 SUS304HTB tracks its austenitic balance: oxidation resistance is adequate for many hot-gas HX duties, but aqueous chloride pitting remains similar to standard 304. Optional annex corrosion tests (oxalic, Strauss, Huey, etc.) are special quality items — order them when the duty needs coupon evidence. Design caution: the 0.04–0.10% carbon window is intentional — do not dual-certify as SUS304LTB; welded corrosive aqueous duty still prefers an L or stabilised grade.

For heat-facing austenitics, oxidation resistance may dominate over aqueous IGC talk; for duplex and Mo austenitics, chlorides dominate; for ferritics, mild aqueous and weld practice dominate. SUS304HTB is filed as austenitic. Caution: the 0.04–0.10% carbon window is intentional — do not dual-certify as SUS304LTB; welded corrosive aqueous duty still prefers an L or stabilised grade.

Applications of JIS G3463 SUS304HTB Tube

Applications of JIS G3463 SUS304HTB tube centre on superheater stubs, high-temperature process steam exchangers, reformer waste-heat coolers, and heat-recovery bundles that still want an 18-8 alloy. Role summary: controlled-carbon 18-8 austenitic tube aimed at elevated-temperature HX and superheater-adjacent duty where a minimum carbon floor supports hot strength. When a related chemistry is required under ASTM A213 or A269, open those sister pages — acceptance text is not automatic.

Downstream fabricators should inherit the same grade symbol on cut lists so informal alias substitutions do not creep in. Primary application sketch: superheater stubs, high-temperature process steam exchangers, reformer waste-heat coolers, and heat-recovery bundles that still want an 18-8 alloy. Duty thread: controlled-carbon 18-8 austenitic tube aimed at elevated-temperature HX and superheater-adjacent duty where a minimum carbon floor supports hot strength.

Weldability of JIS G3463 SUS304HTB

SUS304HTB is welded both as a mill product (A/L/E routes) and as fabricator joints on bundles. Shop guidance: 308H-class fillers when matching hot strength; avoid treating the joint like a low-carbon L weld without procedure review. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Procedure qualification for SUS304HTB should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. Application context for SUS304HTB stays superheater stubs, high-temperature process steam exchangers, reformer waste-heat coolers, and heat-recovery bundles that still want an 18-8 alloy.

Filler selection should match or over-alloy the base chemistry as the WPS demands. Heat input, interpass temperature, and shielding follow the family — austenitic, duplex, or ferritic — not a single shop habit. Caution: the 0.04–0.10% carbon window is intentional — do not dual-certify as SUS304LTB; welded corrosive aqueous duty still prefers an L or stabilised grade.

Surface Finishes for JIS G3463 SUS304HTB

Surface supply for SUS304HTB is typically pickled after heat treatment, or bright-annealed when scale-free OD/ID is ordered. Polished or special roughness finishes are by agreement and must state which surface (OD, ID, or both) is in scope. Duty: controlled-carbon 18-8 austenitic tube aimed at elevated-temperature HX and superheater-adjacent duty where a minimum carbon floor supports hot strength.

Passivation treatments, when ordered, follow agreed ASTM A967 / JIS practice analogues — they are not a substitute for correct heat treatment. Caution: the 0.04–0.10% carbon window is intentional — do not dual-certify as SUS304LTB; welded corrosive aqueous duty still prefers an L or stabilised grade. Final visual standards for SUS304HTB reject grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed. This paragraph is locked to SUS304HTB duty: controlled-carbon 18-8 austenitic tube aimed at elevated-temperature HX and superheater-adjacent duty where a minimum carbon floor supports hot strength.

Inspection and Testing for JIS G3463 SUS304HTB

Inspection for JIS G3463 SUS304HTB covers cast analysis, tensile tests, flattening or weld bend as applicable, hydrostatic test or NDT, dimensions, and appearance. Special quality annex items (IGC, grain size, etc.) apply only when ordered. Documents follow JIS G 0415 / purchaser-specified EN 10204 styles. Sampling plans for SUS304HTB keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. This paragraph is locked to SUS304HTB duty: controlled-carbon 18-8 austenitic tube aimed at elevated-temperature HX and superheater-adjacent duty where a minimum carbon floor supports hot strength.

Marking includes SUS304HTB, manufacture/finish symbols, manufacturer, and other mandatory marking-clause data. Traceability from stencil to MTC is part of supply, not an upgrade. Use: superheater stubs, high-temperature process steam exchangers, reformer waste-heat coolers, and heat-recovery bundles that still want an 18-8 alloy. Non-conforming SUS304HTB lengths are segregated and retested or rejected under retest clauses rather than reworked into unmarked stock. Keep the SUS304HTB caution visible here: the 0.04–0.10% carbon window is intentional — do not dual-certify as SUS304LTB; welded corrosive aqueous duty still prefers an L or stabilised grade.

Packaging and Shipping for JIS G3463 SUS304HTB

Packaging for SUS304HTB uses wooden boxes, plywood cases, or bundled frames with waterproof wrapping as the OD and finish demand. Soft separators protect pickled and polished surfaces. Ends receive caps or bevel protectors when ordered. Bundle tickets for SUS304HTB repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Keep the SUS304HTB caution visible here: the 0.04–0.10% carbon window is intentional — do not dual-certify as SUS304LTB; welded corrosive aqueous duty still prefers an L or stabilised grade.

Carbon-steel strapping never contacts the stainless OD without a barrier. Mixed-grade bundles are forbidden when chemistry integrity matters. Caution: the 0.04–0.10% carbon window is intentional — do not dual-certify as SUS304LTB; welded corrosive aqueous duty still prefers an L or stabilised grade. Desiccant and wrap choices for SUS304HTB follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Application context for SUS304HTB stays superheater stubs, high-temperature process steam exchangers, reformer waste-heat coolers, and heat-recovery bundles that still want an 18-8 alloy.

Shipping documents list JIS G3463, SUS304HTB, sizes, quantities, heat numbers, and certificate type. SHH STEEL coordinates inland trucking and FOB/CIF packing scopes as the order states. Role: controlled-carbon 18-8 austenitic tube aimed at elevated-temperature HX and superheater-adjacent duty where a minimum carbon floor supports hot strength. Claims handling for SUS304HTB starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. This paragraph is locked to SUS304HTB duty: controlled-carbon 18-8 austenitic tube aimed at elevated-temperature HX and superheater-adjacent duty where a minimum carbon floor supports hot strength.

Why Choose SHH STEEL

SHH STEEL can produce and supply JIS G3463 SUS304HTB with the process route, heat treatment, and tests named on your enquiry — not a bait-and-switch alias. Mill partners run stainless tube capacity that covers seamless and welded Table 1 symbols for this mark. Duty focus: controlled-carbon 18-8 austenitic tube aimed at elevated-temperature HX and superheater-adjacent duty where a minimum carbon floor supports hot strength.

Technical sales can map SUS304HTB against sisters SUS304TB, SUS321HTB, SUS347HTB, SUS316HTB and live ASTM pages without pretending standards are identical. Inspection coordination and export packing are in-house habits, not afterthoughts. Ask for a written acknowledgement that names SUS304HTB, the manufacture process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS304HTB to that written scope.

Supply Capability

SHH STEEL can produce and supply JIS G3463 SUS304HTB across enquiry-oriented OD × wall bands, in seamless or welded routes, with certificates and optional annex tests as ordered. Summary capability follows in the table; stock language below is an RFQ map, not a frozen tonnage catalogue. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS304HTB when the mill schedule allows.

Item Capability
Standard JIS G3463 stainless steel tubes for boilers and heat exchangers
Grade symbol SUS304HTB
Product form Seamless (S) and welded (A / L / E) tube; finishes S-H / S-C / A / A-C / E-C as marked
Delivery condition solution annealed
Documents Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered)
Typical OD practice 15.9–139.8 mm per standard Note 1; other by agreement
Wall / gauge OD × wall / BWG-class HX gauges within Attached Tables; other by agreement

Stock / Available sizes

SHH STEEL can produce and supply JIS G3463 SUS304HTB. Stock / Available sizes: enquiry band typically aligns with 15.9–139.8 mm OD practice under G3463 Note 1, with OD×wall HX gauges; schedule 5S–80 (and heavier by agreement) depending on grade family. For SUS304HTB, practical fast-track sizes often sit in mid-bore process and utility ranges — send the OD × wall list for a firm acknowledgement. Context: hot-finished seamless S-H is common for heavier walls; cold-finished S-C for thinner HX gauges.

Cut lengths, bevels, special NDT, and IGC annex tests add lead time — call them early. Sisters often quoted alongside: SUS304TB, SUS321HTB, SUS347HTB, SUS316HTB. Email the size list to start. SHH STEEL can produce trial lengths of SUS304HTB for procedure qualification before the bulk release when the project calendar needs it. SHH STEEL can produce trial lengths of SUS304HTB for procedure qualification before bulk release when the project calendar needs it. Weld-shop note tied to SUS304HTB: 308H-class fillers when matching hot strength; avoid treating the joint like a low-carbon L weld without procedure review.

FAQ

What is JIS G3463 SUS304HTB stainless steel tube used for?
JIS G3463 SUS304HTB is stainless tube for boiler and heat-exchanger service (superheater, HX, condenser, catalyser) — superheater stubs, high-temperature process steam exchangers, reformer waste-heat coolers, and heat-recovery bundles that still want an 18-8 alloy. Role summary: controlled-carbon 18-8 austenitic tube aimed at elevated-temperature HX and superheater-adjacent duty where a minimum carbon floor supports hot strength. It is a Japanese boiler/HX tube product standard mark, not an automatic ASTM A213 certificate.
Does JIS G3463 SUS304HTB cover seamless and welded tube?
Yes. Manufacture allows seamless and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish marks such as S-H, S-C, A-C, or E-C. SHH STEEL can produce and supply either route for SUS304HTB when the mill can meet the ordered size and tests. The title omits Seamless/Welded because JIS G3463 covers both manufacture routes — the PO must still name the process mark.
What heat treatment applies to SUS304HTB?
SUS304HTB is delivered solution annealed under JIS G3463. Table 2 reference: 1040 °C min, rapid cool. Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
How does SUS304HTB compare with sister grades SUS304TB, SUS321HTB, SUS347HTB?
SUS304HTB is filed as austenitic. Typical sisters on the same RFQ are SUS304TB, SUS321HTB, SUS347HTB. Design caution: the 0.04–0.10% carbon window is intentional — do not dual-certify as SUS304LTB; welded corrosive aqueous duty still prefers an L or stabilised grade Pick the sister when the medium or strength floor outgrows this symbol rather than stretching wall alone.
What tests appear on the mill certificate for SUS304HTB?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), flattening/flaring as applicable, dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
Is 304H / UNS S30409 the same as ordering SUS304HTB?
No. 304H / UNS S30409 is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3463 and SUS304HTB so cast limits, heat treatment, and process marks are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for JIS G3463 SUS304HTB?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS304HTB within the typical 15.9–139.8 mm OD practice, with measured walls by agreement. Size context: hot-finished seamless S-H is common for heavier walls; cold-finished S-C for thinner HX gauges. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should SUS304HTB be welded?
Shop guidance: 308H-class fillers when matching hot strength; avoid treating the joint like a low-carbon L weld without procedure review. Mill heat treatment of seamless or welded tube does not replace a qualified WPS on fabricator joints or tube-to-tubesheet welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: the 0.04–0.10% carbon window is intentional — do not dual-certify as SUS304LTB; welded corrosive aqueous duty still prefers an L or stabilised grade
When should I choose a duplex or higher-Mo grade instead of SUS304HTB?
Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: the 0.04–0.10% carbon window is intentional — do not dual-certify as SUS304LTB; welded corrosive aqueous duty still prefers an L or stabilised grade Sister pointers: SUS304TB, SUS321HTB, SUS347HTB. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify JIS G3463 SUS304HTB with ASTM A213 or ASME SA213?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3463 SUS304HTB does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for SUS304HTB?
Pickled after heat treatment is the usual HX tube supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS304HTB when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

JIS G3463 SUS304HTB is stainless steel tube for boiler and heat-exchanger service — controlled-carbon 18-8 austenitic tube aimed at elevated-temperature HX and superheater-adjacent duty where a minimum carbon floor supports hot strength. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS304TB, SUS321HTB, SUS347HTB. Related ASTM A213 pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process mark, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *