JIS G3463 SUS347TB Stainless Steel Tube
What is JIS G3463 SUS347TB Stainless Steel Tube
When the approved vendor list and tube-bundle notes say JIS G3463, the grade mark has to carry the TB suffix. SUS347TB is the full product symbol for this austenitic tube. JIS G3463 SUS347TB is ordered when niobium stabilisation — not titanium marketing — is written into the corrosion file. Buyers working Japanese boiler and HX packages should treat SUS347TB as a governed product symbol under G3463, with Table 3 chemistry and Table 4 tensile floors enforced on the same heat. Weld-shop note tied to SUS347TB: 347-class fillers; optional stabilisation 850–930 °C by agreement.
SHH STEEL can supply SUS347TB tube in seamless S or welded A/L/E routes, with plain or bevelled ends, random or cut lengths, and EN 10204 / JIS G 0415 style inspection documents when specified. Role on the line: Nb-stabilised 18-8 HX / superheater tube for polythionic and weld-decay service. Size and test clarity on the RFQ lets SHH STEEL lock the correct Table 1 symbols for SUS347TB before production starts. Weld-shop note tied to SUS347TB: 347-class fillers; optional stabilisation 850–930 °C by agreement.
Equivalence talk to 347 / UNS S34700 belongs in engineering notes, not as a substitute for the JIS symbol. Lock JIS G3463 SUS347TB, OD × wall, manufacture/finish symbols, and any special quality annex items before melt. Watch-out: Nb ≥10×C must show on the cast line; not a Mo substitute for chloride pitting.
Related ASTM tube pages share chemistry families but not Japanese acceptance text — confirm before dual-cert claims. Sisters on this hub: SUS347HTB, SUS321TB, SUS304TB, SUS321HTB. Use thread: refinery HX, sulphur-plant coolers, and welded steam/process bundles in the sensitising band. Document the medium, design temperature, and weld map beside the SUS347TB line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Corrosion framing beside SUS347TB: Nb stabilisation fights intergranular attack; chloride ranking remains 18-8 class.
Inside this JIS G3463 series, compare SUS347HTB, SUS321TB, SUS304TB, SUS321HTB. Hub: JIS G3463. ASTM/ASME related product pages (not interchangeable by default): A213 TP347, ASTM A213.
Chemical Composition of JIS G3463 SUS347TB
Chemistry control on SUS347TB starts at the ladle. Expect C ≤0.08, Si ≤1.00, Mn ≤2.00, P ≤0.040, S ≤0.030, Ni 9.00–13.00, Cr 17.00–19.00 within Table 3, reported on the inspection document against the heat. Body alias 347 / UNS S34700 does not widen those windows. Every ladle analysis for SUS347TB is checked against those windows before the heat is released to piercing, welding, or finishing, and the same numbers reappear on the inspection document. Corrosion framing beside SUS347TB: Nb stabilisation fights intergranular attack; chloride ranking remains 18-8 class.
Read the table with the family in mind — austenitic — and with caution Nb ≥10×C must show on the cast line; not a Mo substitute for chloride pitting. Numbers without the matching heat-treatment row are incomplete purchase data. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for SUS347TB before the order is acknowledged. This paragraph is locked to SUS347TB duty: Nb-stabilised 18-8 HX / superheater tube for polythionic and weld-decay service.
| Grade | C | Si | Mn | P | S | Ni | Cr | Nb |
|---|---|---|---|---|---|---|---|---|
| SUS347TB | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.040 | ≤0.030 | 9.00–13.00 | 17.00–19.00 | ≥10×C% |
Mechanical Properties of JIS G3463 SUS347TB
Proof stress and tensile minima for SUS347TB sit at Rm min 520 N/mm², proof stress min 206 N/mm², elongation min 35% (OD ≥20 mm, No.11/12). Flattening, flaring, and reverse-flattening (welded) testing backs ductility for the ordered process route. Watch-out: Nb ≥10×C must show on the cast line; not a Mo substitute for chloride pitting.
| Grade | Rm min (N/mm²) | Proof stress min (N/mm²) | A OD≥20 mm No.11/12 min (%) | A 10≤OD<20 mm No.11 min (%) | A OD<10 mm No.11 min (%) |
|---|---|---|---|---|---|
| SUS347TB | 520 | 206 | 35 | 30 | 27 |
Ambient values from JIS G3463 Table 4 for SUS347TB. Heat treatment (Table 2): 980 °C min, rapid cool (stabilisation 850–930 °C may be ordered). Elongation reductions apply for walls under 8 mm on No.12 pieces. For heat-exchanger tube the purchaser may designate an upper tensile limit (Table 4 min + 200 N/mm²) when necessary.
Manufacture of JIS G3463 SUS347TB Tube (Seamless and Welded)
For SUS347TB, the mill path is not “seamless only.” Table 1 explicitly pairs austenitic, duplex, and ferritic marks with seamless or A/L/E welded process symbols and S-H/S-C/A/A-C/E-C finishes. Order the combination that matches hydrostatic or NDT preference, not a habit from ASTM A213 alone. Seamless and welded options remain available for SUS347TB; the acknowledgement repeats the Table 1 symbols so production cannot silently change route after the PO is firm. This paragraph is locked to SUS347TB duty: Nb-stabilised 18-8 HX / superheater tube for polythionic and weld-decay service.
Process control for SUS347TB ends with verified heat treatment (980 °C min, rapid cool (stabilisation 850–930 °C may be ordered)) and surface conditioning. Austenitic heats take solution annealing with rapid cooling; hot-finished seamless may omit separate solution treatment when hot-worked and rapidly cooled in-line under the Table 2 note, unless the purchaser forbids it.
Bevel geometry for walls ≤22 mm defaults to the standard figure when bevels are ordered without a drawing. Size practice: seamless HX/superheater gauges; U-bend annex when ordered. Hydrostatic pressure or NDT class for SUS347TB is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Size practice for SUS347TB remains seamless HX/superheater gauges; U-bend annex when ordered.
Dimensions and Tolerances for JIS G3463 SUS347TB
Mass tables in JIS G3463 support Attached Table mass/OD×wall ordering for common austenitic marks; for SUS347TB, confirm whether your project uses schedule or measured wall. Context: seamless HX/superheater gauges; U-bend annex when ordered. Tolerance class follows the process route ordered for SUS347TB, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Keep the SUS347TB caution visible here: Nb ≥10×C must show on the cast line; not a Mo substitute for chloride pitting.
For heat-exchange and building services, schedule tables often drive the BOM; for process plants, measured wall and corrosion allowance dominate. SUS347TB supports both conversations when the PO is clear. Fixed lengths and multiple cut lengths for SUS347TB are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Weld-shop note tied to SUS347TB: 347-class fillers; optional stabilisation 850–930 °C by agreement.
Equivalent Grades for JIS G3463 SUS347TB
Do not treat 347 / UNS S34700 as interchangeable paperwork. Chemistry kinship is not acceptance kinship. Inside this series see SUS347HTB, SUS321TB, SUS304TB, SUS321HTB. Role: Nb-stabilised 18-8 HX / superheater tube for polythionic and weld-decay service. When a dual-cert path is required, list both JIS G3463 SUS347TB and the ASTM mark with separate test scopes instead of assuming one chemistry line clears both files. Weld-shop note tied to SUS347TB: 347-class fillers; optional stabilisation 850–930 °C by agreement.
Heat Treatment and Delivery Condition for JIS G3463 SUS347TB
Stabilisation or special anneals, where the standard allows purchaser options (notably Ti/Nb grades), must be written on the order — silence means Table 2 defaults only. For SUS347TB: 980 °C min, rapid cool (stabilisation 850–930 °C may be ordered). Recorded furnace charts for SUS347TB should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. This paragraph is locked to SUS347TB duty: Nb-stabilised 18-8 HX / superheater tube for polythionic and weld-decay service.
After local hot work in the field, restore solution annealed practice when the corrosion file demands it. Caution: Nb ≥10×C must show on the cast line; not a Mo substitute for chloride pitting. Field heat treatment of SUS347TB after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Keep the SUS347TB caution visible here: Nb ≥10×C must show on the cast line; not a Mo substitute for chloride pitting.
Corrosion Resistance of JIS G3463 SUS347TB
Pick tests that match how SUS347TB is filed — austenitic. Corrosion thread: Nb stabilisation fights intergranular attack; chloride ranking remains 18-8 class. Caution: Nb ≥10×C must show on the cast line; not a Mo substitute for chloride pitting. Coupon orientation, weld condition, and surface finish for SUS347TB belong in the corrosion test order so annex results can be compared to the installed bundle honestly. Application context for SUS347TB stays refinery HX, sulphur-plant coolers, and welded steam/process bundles in the sensitising band.
Fire-protection and potable-adjacent lines still need the right alloy — G3463 scope does not make every mark equal. Use thread: refinery HX, sulphur-plant coolers, and welded steam/process bundles in the sensitising band. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for SUS347TB rather than relying on schedule thickness alone. Keep the SUS347TB caution visible here: Nb ≥10×C must show on the cast line; not a Mo substitute for chloride pitting.
Applications of JIS G3463 SUS347TB Tube
Project types that repeatedly call SUS347TB: refinery HX, sulphur-plant coolers, and welded steam/process bundles in the sensitising band. Duty: Nb-stabilised 18-8 HX / superheater tube for polythionic and weld-decay service. Caution still applies: Nb ≥10×C must show on the cast line; not a Mo substitute for chloride pitting. Spool fabricators should copy SUS347TB onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Weld-shop note tied to SUS347TB: 347-class fillers; optional stabilisation 850–930 °C by agreement.
Superheater stubs, condenser bundles and corrosive process HX lines all appear in G3463’s scope — alloy choice still follows the medium. For this mark: Nb-stabilised 18-8 HX / superheater tube for polythionic and weld-decay service. Commissioning teams benefit when the as-built dossier repeats SUS347TB beside heat numbers, linking isometric revisions to the same mill certificates. Size practice for SUS347TB remains seamless HX/superheater gauges; U-bend annex when ordered.
Weldability of JIS G3463 SUS347TB
Even seamless S tube of SUS347TB will see field welds. Use: 347-class fillers; optional stabilisation 850–930 °C by agreement. Restore heat treatment when the WPS and corrosion file require it. Procedure qualification for SUS347TB should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. Corrosion framing beside SUS347TB: Nb stabilisation fights intergranular attack; chloride ranking remains 18-8 class.
Dissimilar welds to carbon steel need buttering and dilution control — especially on heat-facing and Mo grades. Role context: Nb-stabilised 18-8 HX / superheater tube for polythionic and weld-decay service. Consumable lot control and shielding-gas notes for SUS347TB stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Size practice for SUS347TB remains seamless HX/superheater gauges; U-bend annex when ordered.
Surface Finishes for JIS G3463 SUS347TB
Iron-free handling after pickle matters — carbon-steel strapping stains show up later as rust blooms on SUS347TB. Finish thread tied to austenitic. Roughness or polish callouts for SUS347TB must name OD, ID, or both; ambiguous “bright tube” language is clarified before finishing slots are booked. This paragraph is locked to SUS347TB duty: Nb-stabilised 18-8 HX / superheater tube for polythionic and weld-decay service.
OD stencil ink and marking paint should be chloride-lean and removable where coating systems follow. Role: Nb-stabilised 18-8 HX / superheater tube for polythionic and weld-decay service. Final visual standards for SUS347TB reject grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed. Application context for SUS347TB stays refinery HX, sulphur-plant coolers, and welded steam/process bundles in the sensitising band.
Inspection and Testing for JIS G3463 SUS347TB
Clause 13/14 define sampling and retests. For SUS347TB, keep the heat/lot identity unbroken from melt to bundle tag. Duty: Nb-stabilised 18-8 HX / superheater tube for polythionic and weld-decay service. Sampling plans for SUS347TB keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Application context for SUS347TB stays refinery HX, sulphur-plant coolers, and welded steam/process bundles in the sensitising band.
Intergranular corrosion testing is annex/special — order it when polythionic or weld-decay risk is written into the duty file for SUS347TB. Non-conforming SUS347TB lengths are segregated and retested or rejected under retest clauses rather than reworked into unmarked stock. Weld-shop note tied to SUS347TB: 347-class fillers; optional stabilisation 850–930 °C by agreement.
Packaging and Shipping for JIS G3463 SUS347TB
Small-OD SUS347TB often ships in crates; large-OD in strapped bundles with OD pads. Confirm destination handling limits on the RFQ. Use: refinery HX, sulphur-plant coolers, and welded steam/process bundles in the sensitising band. Bundle tickets for SUS347TB repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Application context for SUS347TB stays refinery HX, sulphur-plant coolers, and welded steam/process bundles in the sensitising band.
Bevelled ends get protectors so landing edges survive trucking. Size hint: seamless HX/superheater gauges; U-bend annex when ordered. Desiccant and wrap choices for SUS347TB follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Application context for SUS347TB stays refinery HX, sulphur-plant coolers, and welded steam/process bundles in the sensitising band.
Storage advice on arrival: keep bundles dry and off carbon-steel floors. Use thread: refinery HX, sulphur-plant coolers, and welded steam/process bundles in the sensitising band. Claims handling for SUS347TB starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Weld-shop note tied to SUS347TB: 347-class fillers; optional stabilisation 850–930 °C by agreement.
Why Choose SHH STEEL
Project teams working to Japanese boiler/HX specs need a supplier that reads TB suffixes correctly. SHH STEEL can make SUS347TB to that discipline. Caution we keep visible: Nb ≥10×C must show on the cast line; not a Mo substitute for chloride pitting. SHH STEEL can produce and supply SUS347TB against the OD × wall, process symbol, and test scope on your RFQ without swapping in an unstated sister grade.
Dual-cert discussions (JIS + ASTM) are handled with two acceptance regimes in view, not one certificate stretched by hope. Sisters: SUS347HTB, SUS321TB, SUS304TB, SUS321HTB. Ask for a written acknowledgement that names SUS347TB, the manufacture process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS347TB to that written scope.
Supply Capability
Whether you need prototype bundles or project tonnage of SUS347TB, SHH STEEL can supply against a clear OD × wall and test matrix. Duty: refinery HX, sulphur-plant coolers, and welded steam/process bundles in the sensitising band. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS347TB when the mill schedule allows.
| Item | Capability |
|---|---|
| Standard | JIS G3463 stainless steel tubes for boilers and heat exchangers |
| Grade symbol | SUS347TB |
| Product form | Seamless (S) and welded (A / L / E) tube; finishes S-H / S-C / A / A-C / E-C as marked |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered) |
| Typical OD practice | 15.9–139.8 mm per standard Note 1; other by agreement |
| Wall / gauge | OD × wall / BWG-class HX gauges within Attached Tables; other by agreement |
Stock / Available sizes
Stock / Available sizes: SHH STEEL quotes rolling/welding slots for SUS347TB rather than promising anonymous warehouse tons. Typical conversation starts around seamless HX/superheater gauges; U-bend annex when ordered. SHH STEEL can supply alternate schedules and measured walls for SUS347TB once the design pressure and corrosion allowance are clear. SHH STEEL can supply alternate schedules and measured walls for SUS347TB once design pressure and corrosion allowance are clear. This paragraph is locked to SUS347TB duty: Nb-stabilised 18-8 HX / superheater tube for polythionic and weld-decay service.
If the project needs dual JIS G3463 + ASTM documentation, say so before melt. Caution: Nb ≥10×C must show on the cast line; not a Mo substitute for chloride pitting. SHH STEEL can produce trial lengths of SUS347TB for procedure qualification before the bulk release when the project calendar needs it. SHH STEEL can produce trial lengths of SUS347TB for procedure qualification before bulk release when the project calendar needs it. Application context for SUS347TB stays refinery HX, sulphur-plant coolers, and welded steam/process bundles in the sensitising band.
FAQ
-
What is JIS G3463 SUS347TB stainless steel tube used for?
- JIS G3463 SUS347TB is stainless tube for boiler and heat-exchanger service (superheater, HX, condenser, catalyser) — refinery HX, sulphur-plant coolers, and welded steam/process bundles in the sensitising band. Role summary: Nb-stabilised 18-8 HX / superheater tube for polythionic and weld-decay service. It is a Japanese boiler/HX tube product standard mark, not an automatic ASTM A213 certificate.
-
Does JIS G3463 SUS347TB cover seamless and welded tube?
- Yes. Manufacture allows seamless and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish marks such as S-H, S-C, A-C, or E-C. SHH STEEL can produce and supply either route for SUS347TB when the mill can meet the ordered size and tests. The title omits Seamless/Welded because JIS G3463 covers both manufacture routes — the PO must still name the process mark.
-
What heat treatment applies to SUS347TB?
- SUS347TB is delivered solution annealed under JIS G3463. Table 2 reference: 980 °C min, rapid cool (stabilisation 850–930 °C may be ordered). Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
-
How does SUS347TB compare with sister grades SUS347HTB, SUS321TB, SUS304TB?
- SUS347TB is filed as austenitic. Typical sisters on the same RFQ are SUS347HTB, SUS321TB, SUS304TB. Design caution: Nb ≥10×C must show on the cast line; not a Mo substitute for chloride pitting Pick the sister when the medium or strength floor outgrows this symbol rather than stretching wall alone.
-
What tests appear on the mill certificate for SUS347TB?
- Expect cast analysis (Table 3), room-temperature tensile results (Table 4), flattening/flaring as applicable, dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
-
Is 347 / UNS S34700 the same as ordering SUS347TB?
- No. 347 / UNS S34700 is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3463 and SUS347TB so cast limits, heat treatment, and process marks are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for JIS G3463 SUS347TB?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS347TB within the typical 15.9–139.8 mm OD practice, with measured walls by agreement. Size context: seamless HX/superheater gauges; U-bend annex when ordered. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
How should SUS347TB be welded?
- Shop guidance: 347-class fillers; optional stabilisation 850–930 °C by agreement. Mill heat treatment of seamless or welded tube does not replace a qualified WPS on fabricator joints or tube-to-tubesheet welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: Nb ≥10×C must show on the cast line; not a Mo substitute for chloride pitting
-
When should I choose a duplex or higher-Mo grade instead of SUS347TB?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: Nb ≥10×C must show on the cast line; not a Mo substitute for chloride pitting Sister pointers: SUS347HTB, SUS321TB, SUS304TB. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify JIS G3463 SUS347TB with ASTM A213 or ASME SA213?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3463 SUS347TB does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What surface finishes are available for SUS347TB?
- Pickled after heat treatment is the usual HX tube supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS347TB when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
JIS G3463 SUS347TB is stainless steel tube for boiler and heat-exchanger service — Nb-stabilised 18-8 HX / superheater tube for polythionic and weld-decay service. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS347HTB, SUS321TB, SUS304TB. Related ASTM A213 pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process mark, and medium notes to start the quote.