JIS G3463 SUS409TB Stainless Steel Tube | JIS G3463 Stainless Steel Tube - SHH STEEL

JIS G3463 SUS409TB Stainless Steel Tube

JIS G3463 SUS409TB stainless steel tube (409 / UNS S40900), ferritic, Table 3 cast analysis, Rm min 412 N/mm² / proof min 206 N/mm², annealed. SHH STEEL can produce and supply seamless or welded routes with mill certificates.
Grade
SUS409TB (409 / UNS S40900 — body alias)
Standard
JIS G3463
Product form
Seamless and welded stainless steel boiler/HX tube, delivery annealed
Size
Typically OD 15.9–139.8 mm (Note 1); OD × wall (HX/boiler gauges) by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is JIS G3463 SUS409TB Stainless Steel Tube

JIS G3463 is the Japanese Industrial Standard for stainless steel tubes used in boiler and heat-exchanger service (superheater, HX, condenser, catalyser). Grade symbol SUS409TB sits in the ferritic set of Table 1. When the Japanese HX note says SUS409TB, expect 11Cr ferritic behaviour — not a bargain “304 tube”. Buyers working Japanese boiler and HX packages should treat SUS409TB as a governed product symbol under G3463, with Table 3 chemistry and Table 4 tensile floors enforced on the same heat. Corrosion framing beside SUS409TB: Ti stabilisation helps weld zones in mild service; not a seawater alloy.

SHH STEEL can produce and supply JIS G3463 SUS409TB as seamless or welded tube across the enquiry OD×wall band, solution-annealed or annealed as Table 2 requires, pickled or bright-finished, and documented on mill test certificates tied to cast analysis and tensile results. Duty focus: Ti-stabilised 11Cr ferritic for exhaust-adjacent and mild HX tube.

Shop language may still say “409 tube,” yet that commercial alias does not select Japanese cast limits, process symbols, or hydraulic/NDT rules. The purchase order has to name JIS G3463 and SUS409TB so the mill applies the correct analysis, heat treatment, mechanical floors, and marking. Design caution: limited chloride resistance; prefer SUS409LTB when weld carbon control matters.

Scope discipline: SUS409TB is HX tube product under JIS G3463, not a piping product under JIS G3459 and not an ASTM A213 order by default. Sister marks often compared on the same RFQ include SUS409LTB, SUS405TB, SUS410TiTB, SUS430TB. Role reminder: Ti-stabilised 11Cr ferritic for exhaust-adjacent and mild HX tube. Document the medium, design temperature, and weld map beside the SUS409TB line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Corrosion framing beside SUS409TB: Ti stabilisation helps weld zones in mild service; not a seawater alloy.

Inside this JIS G3463 series, compare SUS409LTB, SUS405TB, SUS410TiTB, SUS430TB. Hub: JIS G3463. ASTM/ASME related product pages (not interchangeable by default): ASTM A213.

Chemical Composition of JIS G3463 SUS409TB

Cast analysis for JIS G3463 SUS409TB follows Table 3. Key windows on a typical certificate include C ≤0.08, Si ≤1.00, Mn ≤1.00, P ≤0.040, S ≤0.030, Cr 10.50–11.75, Ti 6×C%–0.75. SHH STEEL ties the heat number on the tube marking to the same cast line on the MTC. Commercial alias 409 / UNS S40900 is body text only. Corrosion thread: Ti stabilisation helps weld zones in mild service; not a seawater alloy.

Chemical limits for SUS409TB under JIS G3463 appear in the table underneath. Source priority is the 2021 Table 3 extract cross-checked to public Nikko / supplier tables. If your client specification cites a different edition footnote, send it before the heat is melted. Duty thread: Ti-stabilised 11Cr ferritic for exhaust-adjacent and mild HX tube.

Grade C Si Mn P S Cr Ti
SUS409TB ≤0.08 ≤1.00 ≤1.00 ≤0.040 ≤0.030 10.50–11.75 6×C%–0.75

Mechanical Properties of JIS G3463 SUS409TB

Ambient tensile floors for SUS409TB come from JIS G3463 Table 4: Rm min 412 N/mm², proof stress min 206 N/mm², elongation min 20% (OD ≥20 mm, No.11/12). These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: ferritic. Caution: limited chloride resistance; prefer SUS409LTB when weld carbon control matters.

Grade Rm min (N/mm²) Proof stress min (N/mm²) A OD≥20 mm No.11/12 min (%) A 10≤OD<20 mm No.11 min (%) A OD<10 mm No.11 min (%)
SUS409TB 412 206 20 15 12

Ambient values from JIS G3463 Table 4 for SUS409TB. Heat treatment (Table 2): 700 °C min, air or slow cool. Elongation reductions apply for walls under 8 mm on No.12 pieces. For heat-exchanger tube the purchaser may designate an upper tensile limit (Table 4 min + 200 N/mm²) when necessary.

Manufacture of JIS G3463 SUS409TB Tube (Seamless and Welded)

JIS G3463 manufactures SUS409TB by seamless (symbol S) or welded routes — automatic arc (A), laser (L), or electric-resistance (E) — then applies the ordered finish: hot finish H, cold finish C, hot finish S-H or cold finish S-C / A-C / E-C as marked. SHH STEEL confirms the Table 1 symbol string on the acknowledgement before rolling or welding starts.

Ferritic heats are annealed (700 °C min, or 720 °C min for SUS430J1LTB) with rapid or slow cooling as Table 2 allows — not austenitic solution practice. Heat-treatment reference for SUS409TB: 700 °C min, air or slow cool. Pickling follows unless bright heat treatment leaves a scale-free surface. Duty thread: Ti-stabilised 11Cr ferritic for exhaust-adjacent and mild HX tube.

When dual documentation against ASTM A213 is requested for a related chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for SUS409TB: thin-wall HX OD; welded ERW common for commodity coolers.

Dimensions and Tolerances for JIS G3463 SUS409TB

SHH STEEL aligns nominal diameter (A/B), outside diameter, schedule or wall, and length tolerance for SUS409TB before the mill slot is locked. Standard Note 1 frames typical OD from 15.9 mm to 139.8 mm (standard Note 1 general practice). Size hint: thin-wall HX OD; welded ERW common for commodity coolers. Tolerance class follows the process route ordered for SUS409TB, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Corrosion framing beside SUS409TB: Ti stabilisation helps weld zones in mild service; not a seawater alloy.

Length supply may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against the packaging clause so pickled or polished finishes are not iron-stained in transit. Duty thread: Ti-stabilised 11Cr ferritic for exhaust-adjacent and mild HX tube. Fixed lengths and multiple cut lengths for SUS409TB are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Keep the SUS409TB caution visible here: limited chloride resistance; prefer SUS409LTB when weld carbon control matters.

Equivalent Grades for JIS G3463 SUS409TB

Equivalence talk for SUS409TB starts with 409 / UNS S40900: that commercial / UNS framing is useful in body text and dual-cert discussions, but the H1 and order line stay on JIS G3463 SUS409TB. ASTM A213 / A269 pages that share related chemistry are different product standards with different wall bases, mechanical tables, and tests. Sisters: SUS409LTB, SUS405TB, SUS410TiTB, SUS430TB. Caution: limited chloride resistance; prefer SUS409LTB when weld carbon control matters.

Heat Treatment and Delivery Condition for JIS G3463 SUS409TB

SUS409TB is delivered annealed under JIS G3463. Table 2 reference: 700 °C min, air or slow cool. Fabricator heat treatment after hot bending should chase the same family practice. Weld thread: 409/ferritic fillers; control heat input and grain growth. Recorded furnace charts for SUS409TB should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Corrosion framing beside SUS409TB: Ti stabilisation helps weld zones in mild service; not a seawater alloy.

Cooling type matters — austenitic and duplex need rapid cool after solution treatment; ferritic anneal practice allows rapid or slow cool per Table 2. Duty thread: Ti-stabilised 11Cr ferritic for exhaust-adjacent and mild HX tube. Field heat treatment of SUS409TB after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Keep the SUS409TB caution visible here: limited chloride resistance; prefer SUS409LTB when weld carbon control matters.

Corrosion Resistance of JIS G3463 SUS409TB

Corrosion behaviour of JIS G3463 SUS409TB tracks its ferritic balance: Ti stabilisation helps weld zones in mild service; not a seawater alloy. Optional annex corrosion tests (oxalic, Strauss, Huey, etc.) are special quality items — order them when the duty needs coupon evidence. Design caution: limited chloride resistance; prefer SUS409LTB when weld carbon control matters.

For heat-facing austenitics, oxidation resistance may dominate over aqueous IGC talk; for duplex and Mo austenitics, chlorides dominate; for ferritics, mild aqueous and weld practice dominate. SUS409TB is filed as ferritic. Caution: limited chloride resistance; prefer SUS409LTB when weld carbon control matters. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for SUS409TB rather than relying on schedule thickness alone. Application context for SUS409TB stays exhaust-gas coolers, automotive-adjacent heat exchangers, and mild aqueous ferritic bundles.

Applications of JIS G3463 SUS409TB Tube

Applications of JIS G3463 SUS409TB tube centre on exhaust-gas coolers, automotive-adjacent heat exchangers, and mild aqueous ferritic bundles. Role summary: Ti-stabilised 11Cr ferritic for exhaust-adjacent and mild HX tube. When a related chemistry is required under ASTM A213 or A269, open those sister pages — acceptance text is not automatic. Spool fabricators should copy SUS409TB onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Size practice for SUS409TB remains thin-wall HX OD; welded ERW common for commodity coolers.

Downstream fabricators should inherit the same grade symbol on cut lists so informal alias substitutions do not creep in. Primary application sketch: exhaust-gas coolers, automotive-adjacent heat exchangers, and mild aqueous ferritic bundles. Duty thread: Ti-stabilised 11Cr ferritic for exhaust-adjacent and mild HX tube. Commissioning teams benefit when the as-built dossier repeats SUS409TB beside heat numbers, linking isometric revisions to the same mill certificates. Corrosion framing beside SUS409TB: Ti stabilisation helps weld zones in mild service; not a seawater alloy.

Weldability of JIS G3463 SUS409TB

SUS409TB is welded both as a mill product (A/L/E routes) and as fabricator joints on bundles. Shop guidance: 409/ferritic fillers; control heat input and grain growth. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Procedure qualification for SUS409TB should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. Size practice for SUS409TB remains thin-wall HX OD; welded ERW common for commodity coolers.

Filler selection should match or over-alloy the base chemistry as the WPS demands. Heat input, interpass temperature, and shielding follow the family — austenitic, duplex, or ferritic — not a single shop habit. Caution: limited chloride resistance; prefer SUS409LTB when weld carbon control matters. Consumable lot control and shielding-gas notes for SUS409TB stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Application context for SUS409TB stays exhaust-gas coolers, automotive-adjacent heat exchangers, and mild aqueous ferritic bundles.

Surface Finishes for JIS G3463 SUS409TB

Surface supply for SUS409TB is typically pickled after heat treatment, or bright-annealed when scale-free OD/ID is ordered. Polished or special roughness finishes are by agreement and must state which surface (OD, ID, or both) is in scope. Duty: Ti-stabilised 11Cr ferritic for exhaust-adjacent and mild HX tube. Roughness or polish callouts for SUS409TB must name OD, ID, or both; ambiguous “bright tube” language is clarified before finishing slots are booked. This paragraph is locked to SUS409TB duty: Ti-stabilised 11Cr ferritic for exhaust-adjacent and mild HX tube.

Passivation treatments, when ordered, follow agreed ASTM A967 / JIS practice analogues — they are not a substitute for correct heat treatment. Caution: limited chloride resistance; prefer SUS409LTB when weld carbon control matters. Final visual standards for SUS409TB reject grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed. Size practice for SUS409TB remains thin-wall HX OD; welded ERW common for commodity coolers.

Inspection and Testing for JIS G3463 SUS409TB

Inspection for JIS G3463 SUS409TB covers cast analysis, tensile tests, flattening or weld bend as applicable, hydrostatic test or NDT, dimensions, and appearance. Special quality annex items (IGC, grain size, etc.) apply only when ordered. Documents follow JIS G 0415 / purchaser-specified EN 10204 styles. Sampling plans for SUS409TB keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. This paragraph is locked to SUS409TB duty: Ti-stabilised 11Cr ferritic for exhaust-adjacent and mild HX tube.

Marking includes SUS409TB, manufacture/finish symbols, manufacturer, and other mandatory marking-clause data. Traceability from stencil to MTC is part of supply, not an upgrade. Use: exhaust-gas coolers, automotive-adjacent heat exchangers, and mild aqueous ferritic bundles. Non-conforming SUS409TB lengths are segregated and retested or rejected under retest clauses rather than reworked into unmarked stock. Weld-shop note tied to SUS409TB: 409/ferritic fillers; control heat input and grain growth.

Packaging and Shipping for JIS G3463 SUS409TB

Packaging for SUS409TB uses wooden boxes, plywood cases, or bundled frames with waterproof wrapping as the OD and finish demand. Soft separators protect pickled and polished surfaces. Ends receive caps or bevel protectors when ordered. Bundle tickets for SUS409TB repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Size practice for SUS409TB remains thin-wall HX OD; welded ERW common for commodity coolers.

Carbon-steel strapping never contacts the stainless OD without a barrier. Mixed-grade bundles are forbidden when chemistry integrity matters. Caution: limited chloride resistance; prefer SUS409LTB when weld carbon control matters. Desiccant and wrap choices for SUS409TB follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Corrosion framing beside SUS409TB: Ti stabilisation helps weld zones in mild service; not a seawater alloy.

Shipping documents list JIS G3463, SUS409TB, sizes, quantities, heat numbers, and certificate type. SHH STEEL coordinates inland trucking and FOB/CIF packing scopes as the order states. Role: Ti-stabilised 11Cr ferritic for exhaust-adjacent and mild HX tube. Claims handling for SUS409TB starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Application context for SUS409TB stays exhaust-gas coolers, automotive-adjacent heat exchangers, and mild aqueous ferritic bundles.

Why Choose SHH STEEL

SHH STEEL can produce and supply JIS G3463 SUS409TB with the process route, heat treatment, and tests named on your enquiry — not a bait-and-switch alias. Mill partners run stainless tube capacity that covers seamless and welded Table 1 symbols for this mark. Duty focus: Ti-stabilised 11Cr ferritic for exhaust-adjacent and mild HX tube.

Technical sales can map SUS409TB against sisters SUS409LTB, SUS405TB, SUS410TiTB, SUS430TB and live ASTM pages without pretending standards are identical. Inspection coordination and export packing are in-house habits, not afterthoughts. Ask for a written acknowledgement that names SUS409TB, the manufacture process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS409TB to that written scope.

Supply Capability

SHH STEEL can produce and supply JIS G3463 SUS409TB across enquiry-oriented OD × wall bands, in seamless or welded routes, with certificates and optional annex tests as ordered. Summary capability follows in the table; stock language below is an RFQ map, not a frozen tonnage catalogue. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS409TB when the mill schedule allows.

Item Capability
Standard JIS G3463 stainless steel tubes for boilers and heat exchangers
Grade symbol SUS409TB
Product form Seamless (S) and welded (A / L / E) tube; finishes S-H / S-C / A / A-C / E-C as marked
Delivery condition annealed
Documents Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered)
Typical OD practice 15.9–139.8 mm per standard Note 1; other by agreement
Wall / gauge OD × wall / BWG-class HX gauges within Attached Tables; other by agreement

Stock / Available sizes

SHH STEEL can produce and supply JIS G3463 SUS409TB. Stock / Available sizes: enquiry band typically aligns with 15.9–139.8 mm OD practice under G3463 Note 1, with OD×wall HX gauges; schedule 5S–80 (and heavier by agreement) depending on grade family. For SUS409TB, practical fast-track sizes often sit in mid-bore process and utility ranges — send the OD × wall list for a firm acknowledgement. Context: thin-wall HX OD; welded ERW common for commodity coolers.

Cut lengths, bevels, special NDT, and IGC annex tests add lead time — call them early. Sisters often quoted alongside: SUS409LTB, SUS405TB, SUS410TiTB, SUS430TB. Email the size list to start. SHH STEEL can produce trial lengths of SUS409TB for procedure qualification before the bulk release when the project calendar needs it. SHH STEEL can produce trial lengths of SUS409TB for procedure qualification before bulk release when the project calendar needs it. Corrosion framing beside SUS409TB: Ti stabilisation helps weld zones in mild service; not a seawater alloy.

FAQ

What is JIS G3463 SUS409TB stainless steel tube used for?
JIS G3463 SUS409TB is stainless tube for boiler and heat-exchanger service (superheater, HX, condenser, catalyser) — exhaust-gas coolers, automotive-adjacent heat exchangers, and mild aqueous ferritic bundles. Role summary: Ti-stabilised 11Cr ferritic for exhaust-adjacent and mild HX tube. It is a Japanese boiler/HX tube product standard mark, not an automatic ASTM A213 certificate.
Does JIS G3463 SUS409TB cover seamless and welded tube?
Yes. Manufacture allows seamless and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish marks such as S-H, S-C, A-C, or E-C. SHH STEEL can produce and supply either route for SUS409TB when the mill can meet the ordered size and tests. The title omits Seamless/Welded because JIS G3463 covers both manufacture routes — the PO must still name the process mark.
What heat treatment applies to SUS409TB?
SUS409TB is delivered annealed under JIS G3463. Table 2 reference: 700 °C min, air or slow cool. Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
How does SUS409TB compare with sister grades SUS409LTB, SUS405TB, SUS410TiTB?
SUS409TB is filed as ferritic. Typical sisters on the same RFQ are SUS409LTB, SUS405TB, SUS410TiTB. Design caution: limited chloride resistance; prefer SUS409LTB when weld carbon control matters Pick the sister when the medium or strength floor outgrows this symbol rather than stretching wall alone.
What tests appear on the mill certificate for SUS409TB?
Expect cast analysis (Table 3), room-temperature tensile results (Table 4), flattening/flaring as applicable, dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
Is 409 / UNS S40900 the same as ordering SUS409TB?
No. 409 / UNS S40900 is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3463 and SUS409TB so cast limits, heat treatment, and process marks are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for JIS G3463 SUS409TB?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS409TB within the typical 15.9–139.8 mm OD practice, with measured walls by agreement. Size context: thin-wall HX OD; welded ERW common for commodity coolers. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should SUS409TB be welded?
Shop guidance: 409/ferritic fillers; control heat input and grain growth. Mill heat treatment of seamless or welded tube does not replace a qualified WPS on fabricator joints or tube-to-tubesheet welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: limited chloride resistance; prefer SUS409LTB when weld carbon control matters
When should I choose a duplex or higher-Mo grade instead of SUS409TB?
Move when chloride pitting, crevice attack, or SCC risk exceeds what ferritic practice can defend for the temperature and stress state. Caution for this mark: limited chloride resistance; prefer SUS409LTB when weld carbon control matters Sister pointers: SUS409LTB, SUS405TB, SUS410TiTB. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify JIS G3463 SUS409TB with ASTM A213 or ASME SA213?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3463 SUS409TB does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
What surface finishes are available for SUS409TB?
Pickled after heat treatment is the usual HX tube supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS409TB when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

JIS G3463 SUS409TB is stainless steel tube for boiler and heat-exchanger service — Ti-stabilised 11Cr ferritic for exhaust-adjacent and mild HX tube. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS409LTB, SUS405TB, SUS410TiTB. Related ASTM A213 pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process mark, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X