JIS G3463 SUS304LTB Stainless Steel Tube
What is JIS G3463 SUS304LTB Stainless Steel Tube
Boiler and heat-exchanger packages that cite Japanese product standards look to JIS G3463 — Stainless steel boiler and heat exchanger tubes — rather than inventing a mill grade from AISI shorthand alone. SUS304LTB is the Table 1 symbol for this austenitic chemistry. If the bundle is full of U-bends and the medium is aqueous, JIS G3463 SUS304LTB is usually the honest 18-8 answer — not a hope that SUS304TB “will be fine”.
Mill path for SUS304LTB: Table 1 manufacture/finish symbols, Table 2 heat treatment, Table 3 cast chemistry, Table 4 tensile floors. SHH STEEL can make and supply the grade to that stack with hydrostatic or NDT acceptance as ordered. Typical use: chemical coolers, food CIP exchangers, pharmaceutical utilities, desalination brine heaters, and U-bend bundles where post-weld anneal is impractical.
Body text may mention 304L / UNS S30403 for cross-reference, but the H1 and order line stay on SUS304LTB. Silent alias swaps are how wrong carbon ceilings and wrong tensile tables enter the MTC. Keep this caution in view: Rm and proof floors sit below SUS304TB — do not swap L stock into a drawing that needs the higher tensile table without engineer sign-off.
Order the standard the drawing and regulatory file actually require. Inside this G3463 series, compare SUS304TB, SUS316LTB, SUS321TB, SUS347TB before stretching surface finish or schedule alone. Duty thread: low-carbon 18-8 austenitic HX tube selected when as-welded corrosion resistance matters more than a hot-strength carbon floor. Document the medium, design temperature, and weld map beside the SUS304LTB line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Keep the SUS304LTB caution visible here: Rm and proof floors sit below SUS304TB — do not swap L stock into a drawing that needs the higher tensile table without engineer sign-off.
Inside this JIS G3463 series, compare SUS304TB, SUS316LTB, SUS321TB, SUS347TB. Hub: JIS G3463. ASTM/ASME related product pages (not interchangeable by default): A213 TP304L, A269 TP304, ASTM A213.
Chemical Composition of JIS G3463 SUS304LTB
Table 3 sets the melt limits for SUS304LTB. Highlight band: C ≤0.030, Si ≤1.00, Mn ≤2.00, P ≤0.040, S ≤0.030, Ni 9.00–13.00, Cr 18.00–20.00. Product analysis, when ordered, applies JIS G 0321 stainless product tolerances on top of Table 3. Alias note: 304L / UNS S30403. Every ladle analysis for SUS304LTB is checked against those windows before the heat is released to piercing, welding, or finishing, and the same numbers reappear on the inspection document. Keep the SUS304LTB caution visible here: Rm and proof floors sit below SUS304TB — do not swap L stock into a drawing that needs the higher tensile table without engineer sign-off.
The composition table below is the cast window SHH STEEL quotes against for SUS304LTB. Edition framing is JIS G3463. Use thread: chemical coolers, food CIP exchangers, pharmaceutical utilities, desalination brine heaters, and U-bend bundles where post-weld anneal is impractical. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 3, SHH STEEL will confirm melt feasibility for SUS304LTB before the order is acknowledged. Weld-shop note tied to SUS304LTB: 308L fillers; keep interpass temperatures moderate and skip unnecessary carbon-steel contamination on the OD.
| Grade | C | Si | Mn | P | S | Ni | Cr |
|---|---|---|---|---|---|---|---|
| SUS304LTB | ≤0.030 | ≤1.00 | ≤2.00 | ≤0.040 | ≤0.030 | 9.00–13.00 | 18.00–20.00 |
Mechanical Properties of JIS G3463 SUS304LTB
Table 4 mechanical acceptance for SUS304LTB: Rm min 481 N/mm², proof stress min 177 N/mm², elongation min 35% (OD ≥20 mm, No.11/12). Elongation rules change for walls under 8 mm and are not mandatory below 40 mm OD (record only unless agreed). Delivery framing: solution annealed. Tensile sampling follows tensile sampling clauses for the ordered test unit of SUS304LTB, and retests follow retest clauses when a result sits under the Table 4 floor. Weld-shop note tied to SUS304LTB: 308L fillers; keep interpass temperatures moderate and skip unnecessary carbon-steel contamination on the OD.
| Grade | Rm min (N/mm²) | Proof stress min (N/mm²) | A OD≥20 mm No.11/12 min (%) | A 10≤OD<20 mm No.11 min (%) | A OD<10 mm No.11 min (%) |
|---|---|---|---|---|---|
| SUS304LTB | 481 | 177 | 35 | 30 | 27 |
Ambient values from JIS G3463 Table 4 for SUS304LTB. Heat treatment (Table 2): 1010 °C min, rapid cool. Elongation reductions apply for walls under 8 mm on No.12 pieces. For heat-exchanger tube the purchaser may designate an upper tensile limit (Table 4 min + 200 N/mm²) when necessary.
Manufacture of JIS G3463 SUS304LTB Tube (Seamless and Welded)
For SUS304LTB, the mill path is not “seamless only.” Table 1 explicitly pairs austenitic, duplex, and ferritic marks with seamless or A/L/E welded process symbols and S-H/S-C/A/A-C/E-C finishes. Order the combination that matches hydrostatic or NDT preference, not a habit from ASTM A213 alone. Seamless and welded options remain available for SUS304LTB; the acknowledgement repeats the Table 1 symbols so production cannot silently change route after the PO is firm. Corrosion framing beside SUS304LTB: low carbon sharply cuts weld-zone sensitisation risk versus standard 304; chloride pitting still tracks the Mo-free 18-8 family.
After forming, SUS304LTB receives Table 2 treatment — 1010 °C min, rapid cool. Austenitic heats take solution annealing with rapid cooling; hot-finished seamless may omit separate solution treatment when hot-worked and rapidly cooled in-line under the Table 2 note, unless the purchaser forbids it. Use thread: chemical coolers, food CIP exchangers, pharmaceutical utilities, desalination brine heaters, and U-bend bundles where post-weld anneal is impractical.
Marking carries the grade symbol SUS304LTB, process/finish marks, manufacturer ID, and other marking-clause items. Size hint: welded A/E routes dominate commodity HX diameters; seamless S for higher-pressure or thicker-wall RFQs. Weld thread: 308L fillers; keep interpass temperatures moderate and skip unnecessary carbon-steel contamination on the OD. Hydrostatic pressure or NDT class for SUS304LTB is frozen with the size list so quality planners can book the correct benches before the tube is cut to length. Application context for SUS304LTB stays chemical coolers, food CIP exchangers, pharmaceutical utilities, desalination brine heaters, and U-bend bundles where post-weld anneal is impractical.
Dimensions and Tolerances for JIS G3463 SUS304LTB
Dimensional order lines for SUS304LTB should state OD × wall (or OD×wall HX gauges; schedule 5S/10S/20S/40/80/…), length type, and end finish. Tolerances follow dimensional tolerance clauses by process route. Use: chemical coolers, food CIP exchangers, pharmaceutical utilities, desalination brine heaters, and U-bend bundles where post-weld anneal is impractical. Tolerance class follows the process route ordered for SUS304LTB, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Corrosion framing beside SUS304LTB: low carbon sharply cuts weld-zone sensitisation risk versus standard 304; chloride pitting still tracks the Mo-free 18-8 family.
OD and wall tolerances differ for hot-finished seamless versus cold-finished / welded routes — quote the process symbol with the size. Caution: Rm and proof floors sit below SUS304TB — do not swap L stock into a drawing that needs the higher tensile table without engineer sign-off. Fixed lengths and multiple cut lengths for SUS304LTB are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Corrosion framing beside SUS304LTB: low carbon sharply cuts weld-zone sensitisation risk versus standard 304; chloride pitting still tracks the Mo-free 18-8 family.
Equivalent Grades for JIS G3463 SUS304LTB
SUS304LTB is the JIS G3463 designation. Alias 304L / UNS S30403 appears only as a cross-walk. Compare sisters SUS304TB, SUS316LTB, SUS321TB, SUS347TB when the medium or temperature outgrows this mark. Hook: lock SUS304LTB on the PO. When a dual-cert path is required, list both JIS G3463 SUS304LTB and the ASTM mark with separate test scopes instead of assuming one chemistry line clears both files. Application context for SUS304LTB stays chemical coolers, food CIP exchangers, pharmaceutical utilities, desalination brine heaters, and U-bend bundles where post-weld anneal is impractical.
Heat Treatment and Delivery Condition for JIS G3463 SUS304LTB
Mill heat treatment for SUS304LTB: 1010 °C min, rapid cool. Bright annealing may omit pickling when the surface is scale-free. Delivery label: solution annealed. Recorded furnace charts for SUS304LTB should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Size practice for SUS304LTB remains welded A/E routes dominate commodity HX diameters; seamless S for higher-pressure or thicker-wall RFQs.
Certificate wording for SUS304LTB should show the heat-treatment condition actually performed, not a generic “annealed” stamp that hides temperature. Use: chemical coolers, food CIP exchangers, pharmaceutical utilities, desalination brine heaters, and U-bend bundles where post-weld anneal is impractical. Field heat treatment of SUS304LTB after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Size practice for SUS304LTB remains welded A/E routes dominate commodity HX diameters; seamless S for higher-pressure or thicker-wall RFQs.
Corrosion Resistance of JIS G3463 SUS304LTB
low carbon sharply cuts weld-zone sensitisation risk versus standard 304; chloride pitting still tracks the Mo-free 18-8 family Special quality annex tests are available by agreement; they are not a blanket warranty for every process medium. Family filing: austenitic. Coupon orientation, weld condition, and surface finish for SUS304LTB belong in the corrosion test order so annex results can be compared to the installed bundle honestly. Weld-shop note tied to SUS304LTB: 308L fillers; keep interpass temperatures moderate and skip unnecessary carbon-steel contamination on the OD.
Do not market invented PREN digits. Bring medium chemistry and SHH STEEL will map SUS304LTB honestly against SUS304TB, SUS316LTB, SUS321TB, SUS347TB. Role: low-carbon 18-8 austenitic HX tube selected when as-welded corrosion resistance matters more than a hot-strength carbon floor. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for SUS304LTB rather than relying on schedule thickness alone. Size practice for SUS304LTB remains welded A/E routes dominate commodity HX diameters; seamless S for higher-pressure or thicker-wall RFQs.
Applications of JIS G3463 SUS304LTB Tube
Typical BOM language pairs JIS G3463 SUS304LTB with OD × wall (or schedule), manufacture/finish symbols, and heat-treatment condition. Primary sketch: chemical coolers, food CIP exchangers, pharmaceutical utilities, desalination brine heaters, and U-bend bundles where post-weld anneal is impractical. Spool fabricators should copy SUS304LTB onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. This paragraph is locked to SUS304LTB duty: low-carbon 18-8 austenitic HX tube selected when as-welded corrosion resistance matters more than a hot-strength carbon floor.
Spell SUS304LTB on tube-sheet drawings and bundle lists, bundle sheets and tubesheet specs alike. Sister options when the medium hardens: SUS304TB, SUS316LTB, SUS321TB, SUS347TB. Commissioning teams benefit when the as-built dossier repeats SUS304LTB beside heat numbers, linking isometric revisions to the same mill certificates. Weld-shop note tied to SUS304LTB: 308L fillers; keep interpass temperatures moderate and skip unnecessary carbon-steel contamination on the OD.
Weldability of JIS G3463 SUS304LTB
Weldability of SUS304LTB follows austenitic practice. Filler/shop note: 308L fillers; keep interpass temperatures moderate and skip unnecessary carbon-steel contamination on the OD. Caution: Rm and proof floors sit below SUS304TB — do not swap L stock into a drawing that needs the higher tensile table without engineer sign-off. Procedure qualification for SUS304LTB should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. Application context for SUS304LTB stays chemical coolers, food CIP exchangers, pharmaceutical utilities, desalination brine heaters, and U-bend bundles where post-weld anneal is impractical.
For welded G3463 tube, confirm whether as-welded or cold-finished welded finish is acceptable to the corrosion owner. Shop note: 308L fillers; keep interpass temperatures moderate and skip unnecessary carbon-steel contamination on the OD. Consumable lot control and shielding-gas notes for SUS304LTB stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Corrosion framing beside SUS304LTB: low carbon sharply cuts weld-zone sensitisation risk versus standard 304; chloride pitting still tracks the Mo-free 18-8 family.
Surface Finishes for JIS G3463 SUS304LTB
Pickled mill finish covers most HX tube RFQs for SUS304LTB. Bright anneal, grind, or polish only when the enquiry writes a measurable target. Use: chemical coolers, food CIP exchangers, pharmaceutical utilities, desalination brine heaters, and U-bend bundles where post-weld anneal is impractical. Roughness or polish callouts for SUS304LTB must name OD, ID, or both; ambiguous “bright tube” language is clarified before finishing slots are booked. This paragraph is locked to SUS304LTB duty: low-carbon 18-8 austenitic HX tube selected when as-welded corrosion resistance matters more than a hot-strength carbon floor.
Sanitary-lean duties may add ID polish; chemical lines may prefer a clean pickle only. State the need on the SUS304LTB order. Final visual standards for SUS304LTB reject grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed. Application context for SUS304LTB stays chemical coolers, food CIP exchangers, pharmaceutical utilities, desalination brine heaters, and U-bend bundles where post-weld anneal is impractical.
Inspection and Testing for JIS G3463 SUS304LTB
SHH STEEL reports the tests actually performed for SUS304LTB — no surrogate NDT lines. Hydrostatic vs eddy-current/ultrasonic choice belongs on the PO. Caution: Rm and proof floors sit below SUS304TB — do not swap L stock into a drawing that needs the higher tensile table without engineer sign-off. Sampling plans for SUS304LTB keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Weld-shop note tied to SUS304LTB: 308L fillers; keep interpass temperatures moderate and skip unnecessary carbon-steel contamination on the OD.
NDT sensitivity levels and hydrostatic pressures follow the standard tables unless the purchaser specifies higher. Size context: welded A/E routes dominate commodity HX diameters; seamless S for higher-pressure or thicker-wall RFQs. Non-conforming SUS304LTB lengths are segregated and retested or rejected under retest clauses rather than reworked into unmarked stock. Keep the SUS304LTB caution visible here: Rm and proof floors sit below SUS304TB — do not swap L stock into a drawing that needs the higher tensile table without engineer sign-off.
Packaging and Shipping for JIS G3463 SUS304LTB
Export packing for JIS G3463 SUS304LTB is built around rust prevention and transit abrasion control. Bundle tickets repeat the grade symbol and heat number. Duty: low-carbon 18-8 austenitic HX tube selected when as-welded corrosion resistance matters more than a hot-strength carbon floor. Bundle tickets for SUS304LTB repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Corrosion framing beside SUS304LTB: low carbon sharply cuts weld-zone sensitisation risk versus standard 304; chloride pitting still tracks the Mo-free 18-8 family.
Marking paint and ink stickers stay chloride-lean. Heat numbers on tags match the MTC for SUS304LTB. Desiccant and wrap choices for SUS304LTB follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Size practice for SUS304LTB remains welded A/E routes dominate commodity HX diameters; seamless S for higher-pressure or thicker-wall RFQs.
Photographic packing records are available on request for project QA files on SUS304LTB. Claims handling for SUS304LTB starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. This paragraph is locked to SUS304LTB duty: low-carbon 18-8 austenitic HX tube selected when as-welded corrosion resistance matters more than a hot-strength carbon floor.
Why Choose SHH STEEL
SHH STEEL can produce and supply JIS G3463 SUS304LTB. Buyers choose SHH STEEL for SUS304LTB because the paperwork matches the stencil: Table 3 chemistry, Table 4 tensile, Table 2 heat treatment, and honest seamless or A/L/E welded marking. Application fit: chemical coolers, food CIP exchangers, pharmaceutical utilities, desalination brine heaters, and U-bend bundles where post-weld anneal is impractical.
SHH STEEL will not invent PREN posters or warehouse tonnages. Bring OD × wall, medium notes, and test scope — we will quote SUS304LTB cleanly. Ask for a written acknowledgement that names SUS304LTB, the manufacture process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS304LTB to that written scope.
Supply Capability
Supply capability for SUS304LTB covers manufacture/finish symbols in Table 1, heat treatment in Table 2, and mechanical acceptance in Table 4. SHH STEEL can make the sizes on your list when the mill slot fits. Role: low-carbon 18-8 austenitic HX tube selected when as-welded corrosion resistance matters more than a hot-strength carbon floor.
| Item | Capability |
|---|---|
| Standard | JIS G3463 stainless steel tubes for boilers and heat exchangers |
| Grade symbol | SUS304LTB |
| Product form | Seamless (S) and welded (A / L / E) tube; finishes S-H / S-C / A / A-C / E-C as marked |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered) |
| Typical OD practice | 15.9–139.8 mm per standard Note 1; other by agreement |
| Wall / gauge | OD × wall / BWG-class HX gauges within Attached Tables; other by agreement |
Stock / Available sizes
Stock / Available sizes for SUS304LTB: common A-number bores with schedule or measured wall as the project uses. Seamless and welded availability varies by diameter — confirm route with the RFQ. Hint: welded A/E routes dominate commodity HX diameters; seamless S for higher-pressure or thicker-wall RFQs. SHH STEEL can supply alternate schedules and measured walls for SUS304LTB once the design pressure and corrosion allowance are clear.
Mill certificates, packing photos, and third-party witness can be bundled into the SUS304LTB supply scope when the PO says so. Use: chemical coolers, food CIP exchangers, pharmaceutical utilities, desalination brine heaters, and U-bend bundles where post-weld anneal is impractical. SHH STEEL can produce trial lengths of SUS304LTB for procedure qualification before the bulk release when the project calendar needs it.
FAQ
-
What is JIS G3463 SUS304LTB stainless steel tube used for?
- JIS G3463 SUS304LTB is stainless tube for boiler and heat-exchanger service (superheater, HX, condenser, catalyser) — chemical coolers, food CIP exchangers, pharmaceutical utilities, desalination brine heaters, and U-bend bundles where post-weld anneal is impractical. Role summary: low-carbon 18-8 austenitic HX tube selected when as-welded corrosion resistance matters more than a hot-strength carbon floor. It is a Japanese boiler/HX tube product standard mark, not an automatic ASTM A213 certificate.
-
Does JIS G3463 SUS304LTB cover seamless and welded tube?
- Yes. Manufacture allows seamless and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish marks such as S-H, S-C, A-C, or E-C. SHH STEEL can produce and supply either route for SUS304LTB when the mill can meet the ordered size and tests. The title omits Seamless/Welded because JIS G3463 covers both manufacture routes — the PO must still name the process mark.
-
What heat treatment applies to SUS304LTB?
- SUS304LTB is delivered solution annealed under JIS G3463. Table 2 reference: 1010 °C min, rapid cool. Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
-
How does SUS304LTB compare with sister grades SUS304TB, SUS316LTB, SUS321TB?
- SUS304LTB is filed as austenitic. Typical sisters on the same RFQ are SUS304TB, SUS316LTB, SUS321TB. Design caution: Rm and proof floors sit below SUS304TB — do not swap L stock into a drawing that needs the higher tensile table without engineer sign-off Pick the sister when the medium or strength floor outgrows this symbol rather than stretching wall alone.
-
What tests appear on the mill certificate for SUS304LTB?
- Expect cast analysis (Table 3), room-temperature tensile results (Table 4), flattening/flaring as applicable, dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
-
Is 304L / UNS S30403 the same as ordering SUS304LTB?
- No. 304L / UNS S30403 is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3463 and SUS304LTB so cast limits, heat treatment, and process marks are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for JIS G3463 SUS304LTB?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS304LTB within the typical 15.9–139.8 mm OD practice, with measured walls by agreement. Size context: welded A/E routes dominate commodity HX diameters; seamless S for higher-pressure or thicker-wall RFQs. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
How should SUS304LTB be welded?
- Shop guidance: 308L fillers; keep interpass temperatures moderate and skip unnecessary carbon-steel contamination on the OD. Mill heat treatment of seamless or welded tube does not replace a qualified WPS on fabricator joints or tube-to-tubesheet welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: Rm and proof floors sit below SUS304TB — do not swap L stock into a drawing that needs the higher tensile table without engineer sign-off
-
When should I choose a duplex or higher-Mo grade instead of SUS304LTB?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: Rm and proof floors sit below SUS304TB — do not swap L stock into a drawing that needs the higher tensile table without engineer sign-off Sister pointers: SUS304TB, SUS316LTB, SUS321TB. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify JIS G3463 SUS304LTB with ASTM A213 or ASME SA213?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3463 SUS304LTB does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What surface finishes are available for SUS304LTB?
- Pickled after heat treatment is the usual HX tube supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS304LTB when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
JIS G3463 SUS304LTB is stainless steel tube for boiler and heat-exchanger service — low-carbon 18-8 austenitic HX tube selected when as-welded corrosion resistance matters more than a hot-strength carbon floor. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS304TB, SUS316LTB, SUS321TB. Related ASTM A213 pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process mark, and medium notes to start the quote.