JIS G3463 SUS309TB Stainless Steel Tube
What is JIS G3463 SUS309TB Stainless Steel Tube
JIS G3463 is the Japanese Industrial Standard for stainless steel tubes used in boiler and heat-exchanger service (superheater, HX, condenser, catalyser). Grade symbol SUS309TB sits in the austenitic set of Table 1. JIS G3463 SUS309TB is the heat-facing step up from 304 when chromium alone — not molybdenum — is the missing alloying lever on the tube.
SHH STEEL can produce and supply JIS G3463 SUS309TB as seamless or welded tube across the enquiry OD×wall band, solution-annealed or annealed as Table 2 requires, pickled or bright-finished, and documented on mill test certificates tied to cast analysis and tensile results. Duty focus: higher Cr-Ni austenitic tube for heat-facing and oxidation-lean HX duties that outgrow 18-8 chromium.
Shop language may still say “309 tube,” yet that commercial alias does not select Japanese cast limits, process symbols, or hydraulic/NDT rules. The purchase order has to name JIS G3463 and SUS309TB so the mill applies the correct analysis, heat treatment, mechanical floors, and marking. Design caution: carbon may reach 0.15% — treat as-welded aqueous corrosion as a separate review; many buyers actually need SUS309STB.
Scope discipline: SUS309TB is HX tube product under JIS G3463, not a piping product under JIS G3459 and not an ASTM A213 order by default. Sister marks often compared on the same RFQ include SUS309STB, SUS310TB, SUS310STB, SUS304TB. Role reminder: higher Cr-Ni austenitic tube for heat-facing and oxidation-lean HX duties that outgrow 18-8 chromium.
Inside this JIS G3463 series, compare SUS309STB, SUS310TB, SUS310STB, SUS304TB. Hub: JIS G3463. ASTM/ASME related product pages (not interchangeable by default): ASTM A213.
Chemical Composition of JIS G3463 SUS309TB
Cast analysis for JIS G3463 SUS309TB follows Table 3. Key windows on a typical certificate include C ≤0.15, Si ≤1.00, Mn ≤2.00, P ≤0.040, S ≤0.030, Ni 12.00–15.00, Cr 22.00–24.00. SHH STEEL ties the heat number on the tube marking to the same cast line on the MTC. Commercial alias 309 / UNS S30900 class is body text only. Corrosion thread: oxide scale resistance improves with the 22–24% Cr / 12–15% Ni balance; aqueous chloride ranking is not why you buy 309 tube.
Chemical limits for SUS309TB under JIS G3463 appear in the table underneath. Source priority is the 2021 Table 3 extract cross-checked to public Nikko / supplier tables. If your client specification cites a different edition footnote, send it before the heat is melted. Duty thread: higher Cr-Ni austenitic tube for heat-facing and oxidation-lean HX duties that outgrow 18-8 chromium.
| Grade | C | Si | Mn | P | S | Ni | Cr |
|---|---|---|---|---|---|---|---|
| SUS309TB | ≤0.15 | ≤1.00 | ≤2.00 | ≤0.040 | ≤0.030 | 12.00–15.00 | 22.00–24.00 |
Mechanical Properties of JIS G3463 SUS309TB
Ambient tensile floors for SUS309TB come from JIS G3463 Table 4: Rm min 520 N/mm², proof stress min 206 N/mm², elongation min 35% (OD ≥20 mm, No.11/12). These are delivery-condition values at room temperature, not elevated-temperature design allowables. SHH STEEL reports actual tensile results on the mill document for the ordered test unit. Family: austenitic. Caution: carbon may reach 0.15% — treat as-welded aqueous corrosion as a separate review; many buyers actually need SUS309STB.
| Grade | Rm min (N/mm²) | Proof stress min (N/mm²) | A OD≥20 mm No.11/12 min (%) | A 10≤OD<20 mm No.11 min (%) | A OD<10 mm No.11 min (%) |
|---|---|---|---|---|---|
| SUS309TB | 520 | 206 | 35 | 30 | 27 |
Ambient values from JIS G3463 Table 4 for SUS309TB. Heat treatment (Table 2): 1030 °C min, rapid cool. Elongation reductions apply for walls under 8 mm on No.12 pieces. For heat-exchanger tube the purchaser may designate an upper tensile limit (Table 4 min + 200 N/mm²) when necessary.
Manufacture of JIS G3463 SUS309TB Tube (Seamless and Welded)
SHH STEEL can produce SUS309TB as seamless S or as A/L/E welded tube, then heat-treat and pickle (or bright-anneal) per Table 2. Bevel ends are available by agreement; plain ends are the default when the PO is silent. Seamless and welded options remain available for SUS309TB; the acknowledgement repeats the Table 1 symbols so production cannot silently change route after the PO is firm. Application context for SUS309TB stays hot-gas coolers, thermal oxidiser exchangers, kiln waste-heat bundles, and high-temperature flue-gas HX stubs.
Austenitic heats take solution annealing with rapid cooling; hot-finished seamless may omit separate solution treatment when hot-worked and rapidly cooled in-line under the Table 2 note, unless the purchaser forbids it. Heat-treatment reference for SUS309TB: 1030 °C min, rapid cool. Pickling follows unless bright heat treatment leaves a scale-free surface. Duty thread: higher Cr-Ni austenitic tube for heat-facing and oxidation-lean HX duties that outgrow 18-8 chromium.
When dual documentation against ASTM A213 is requested for a related chemistry, each standard’s mechanical and test regime still has to be satisfied on its own terms — SHH STEEL will not pretend one MTC covers both without the tests. Size context for SUS309TB: hot-finished seamless for thick heat-service walls; welded routes for large-OD HX shellside stubs when the design allows.
Dimensions and Tolerances for JIS G3463 SUS309TB
SHH STEEL aligns nominal diameter (A/B), outside diameter, schedule or wall, and length tolerance for SUS309TB before the mill slot is locked. Standard Note 1 frames typical OD from 15.9 mm to 139.8 mm (standard Note 1 general practice). Size hint: hot-finished seamless for thick heat-service walls; welded routes for large-OD HX shellside stubs when the design allows.
Length supply may be mill random, fixed, or multiple cut lengths. Bundle make-up and end protection are confirmed against the packaging clause so pickled or polished finishes are not iron-stained in transit. Duty thread: higher Cr-Ni austenitic tube for heat-facing and oxidation-lean HX duties that outgrow 18-8 chromium. Fixed lengths and multiple cut lengths for SUS309TB are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Size practice for SUS309TB remains hot-finished seamless for thick heat-service walls; welded routes for large-OD HX shellside stubs when the design allows.
Equivalent Grades for JIS G3463 SUS309TB
Equivalence talk for SUS309TB starts with 309 / UNS S30900 class: that commercial / UNS framing is useful in body text and dual-cert discussions, but the H1 and order line stay on JIS G3463 SUS309TB. ASTM A213 / A269 pages that share related chemistry are different product standards with different wall bases, mechanical tables, and tests. Sisters: SUS309STB, SUS310TB, SUS310STB, SUS304TB. Caution: carbon may reach 0.15% — treat as-welded aqueous corrosion as a separate review; many buyers actually need SUS309STB.
Heat Treatment and Delivery Condition for JIS G3463 SUS309TB
SUS309TB is delivered solution annealed under JIS G3463. Table 2 reference: 1030 °C min, rapid cool. Fabricator heat treatment after hot bending should chase the same family practice. Weld thread: 309/309L-class fillers; manage dilution when buttering carbon steel; aqueous IGC still wants the S or L sister. Recorded furnace charts for SUS309TB should support the Table 2 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Weld-shop note tied to SUS309TB: 309/309L-class fillers; manage dilution when buttering carbon steel; aqueous IGC still wants the S or L sister.
Cooling type matters — austenitic and duplex need rapid cool after solution treatment; ferritic anneal practice allows rapid or slow cool per Table 2. Duty thread: higher Cr-Ni austenitic tube for heat-facing and oxidation-lean HX duties that outgrow 18-8 chromium. Field heat treatment of SUS309TB after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Corrosion framing beside SUS309TB: oxide scale resistance improves with the 22–24% Cr / 12–15% Ni balance; aqueous chloride ranking is not why you buy 309 tube.
Corrosion Resistance of JIS G3463 SUS309TB
Corrosion behaviour of JIS G3463 SUS309TB tracks its austenitic balance: oxide scale resistance improves with the 22–24% Cr / 12–15% Ni balance; aqueous chloride ranking is not why you buy 309 tube. Optional annex corrosion tests (oxalic, Strauss, Huey, etc.) are special quality items — order them when the duty needs coupon evidence. Design caution: carbon may reach 0.15% — treat as-welded aqueous corrosion as a separate review; many buyers actually need SUS309STB.
For heat-facing austenitics, oxidation resistance may dominate over aqueous IGC talk; for duplex and Mo austenitics, chlorides dominate; for ferritics, mild aqueous and weld practice dominate. SUS309TB is filed as austenitic. Caution: carbon may reach 0.15% — treat as-welded aqueous corrosion as a separate review; many buyers actually need SUS309STB. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for SUS309TB rather than relying on schedule thickness alone. Application context for SUS309TB stays hot-gas coolers, thermal oxidiser exchangers, kiln waste-heat bundles, and high-temperature flue-gas HX stubs.
Applications of JIS G3463 SUS309TB Tube
Applications of JIS G3463 SUS309TB tube centre on hot-gas coolers, thermal oxidiser exchangers, kiln waste-heat bundles, and high-temperature flue-gas HX stubs. Role summary: higher Cr-Ni austenitic tube for heat-facing and oxidation-lean HX duties that outgrow 18-8 chromium. When a related chemistry is required under ASTM A213 or A269, open those sister pages — acceptance text is not automatic.
Downstream fabricators should inherit the same grade symbol on cut lists so informal alias substitutions do not creep in. Primary application sketch: hot-gas coolers, thermal oxidiser exchangers, kiln waste-heat bundles, and high-temperature flue-gas HX stubs. Duty thread: higher Cr-Ni austenitic tube for heat-facing and oxidation-lean HX duties that outgrow 18-8 chromium. Commissioning teams benefit when the as-built dossier repeats SUS309TB beside heat numbers, linking isometric revisions to the same mill certificates. Corrosion framing beside SUS309TB: oxide scale resistance improves with the 22–24% Cr / 12–15% Ni balance; aqueous chloride ranking is not why you buy 309 tube.
Weldability of JIS G3463 SUS309TB
SUS309TB is welded both as a mill product (A/L/E routes) and as fabricator joints on bundles. Shop guidance: 309/309L-class fillers; manage dilution when buttering carbon steel; aqueous IGC still wants the S or L sister. Mill heat treatment of the tube does not replace qualified welding procedures on site joints. Procedure qualification for SUS309TB should use the same product form and wall class as production, including any bead-worked or as-welded finish that will ship. Application context for SUS309TB stays hot-gas coolers, thermal oxidiser exchangers, kiln waste-heat bundles, and high-temperature flue-gas HX stubs.
Filler selection should match or over-alloy the base chemistry as the WPS demands. Heat input, interpass temperature, and shielding follow the family — austenitic, duplex, or ferritic — not a single shop habit. Caution: carbon may reach 0.15% — treat as-welded aqueous corrosion as a separate review; many buyers actually need SUS309STB.
Surface Finishes for JIS G3463 SUS309TB
Surface supply for SUS309TB is typically pickled after heat treatment, or bright-annealed when scale-free OD/ID is ordered. Polished or special roughness finishes are by agreement and must state which surface (OD, ID, or both) is in scope. Duty: higher Cr-Ni austenitic tube for heat-facing and oxidation-lean HX duties that outgrow 18-8 chromium.
Passivation treatments, when ordered, follow agreed ASTM A967 / JIS practice analogues — they are not a substitute for correct heat treatment. Caution: carbon may reach 0.15% — treat as-welded aqueous corrosion as a separate review; many buyers actually need SUS309STB. Final visual standards for SUS309TB reject grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed. Weld-shop note tied to SUS309TB: 309/309L-class fillers; manage dilution when buttering carbon steel; aqueous IGC still wants the S or L sister.
Inspection and Testing for JIS G3463 SUS309TB
Inspection for JIS G3463 SUS309TB covers cast analysis, tensile tests, flattening or weld bend as applicable, hydrostatic test or NDT, dimensions, and appearance. Special quality annex items (IGC, grain size, etc.) apply only when ordered. Documents follow JIS G 0415 / purchaser-specified EN 10204 styles. Sampling plans for SUS309TB keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Application context for SUS309TB stays hot-gas coolers, thermal oxidiser exchangers, kiln waste-heat bundles, and high-temperature flue-gas HX stubs.
Marking includes SUS309TB, manufacture/finish symbols, manufacturer, and other mandatory marking-clause data. Traceability from stencil to MTC is part of supply, not an upgrade. Use: hot-gas coolers, thermal oxidiser exchangers, kiln waste-heat bundles, and high-temperature flue-gas HX stubs. Non-conforming SUS309TB lengths are segregated and retested or rejected under retest clauses rather than reworked into unmarked stock. Corrosion framing beside SUS309TB: oxide scale resistance improves with the 22–24% Cr / 12–15% Ni balance; aqueous chloride ranking is not why you buy 309 tube.
Packaging and Shipping for JIS G3463 SUS309TB
Packaging for SUS309TB uses wooden boxes, plywood cases, or bundled frames with waterproof wrapping as the OD and finish demand. Soft separators protect pickled and polished surfaces. Ends receive caps or bevel protectors when ordered. Bundle tickets for SUS309TB repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Application context for SUS309TB stays hot-gas coolers, thermal oxidiser exchangers, kiln waste-heat bundles, and high-temperature flue-gas HX stubs.
Carbon-steel strapping never contacts the stainless OD without a barrier. Mixed-grade bundles are forbidden when chemistry integrity matters. Caution: carbon may reach 0.15% — treat as-welded aqueous corrosion as a separate review; many buyers actually need SUS309STB. Desiccant and wrap choices for SUS309TB follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Corrosion framing beside SUS309TB: oxide scale resistance improves with the 22–24% Cr / 12–15% Ni balance; aqueous chloride ranking is not why you buy 309 tube.
Shipping documents list JIS G3463, SUS309TB, sizes, quantities, heat numbers, and certificate type. SHH STEEL coordinates inland trucking and FOB/CIF packing scopes as the order states. Role: higher Cr-Ni austenitic tube for heat-facing and oxidation-lean HX duties that outgrow 18-8 chromium. Claims handling for SUS309TB starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Size practice for SUS309TB remains hot-finished seamless for thick heat-service walls; welded routes for large-OD HX shellside stubs when the design allows.
Why Choose SHH STEEL
SHH STEEL can produce and supply JIS G3463 SUS309TB with the process route, heat treatment, and tests named on your enquiry — not a bait-and-switch alias. Mill partners run stainless tube capacity that covers seamless and welded Table 1 symbols for this mark. Duty focus: higher Cr-Ni austenitic tube for heat-facing and oxidation-lean HX duties that outgrow 18-8 chromium.
Technical sales can map SUS309TB against sisters SUS309STB, SUS310TB, SUS310STB, SUS304TB and live ASTM pages without pretending standards are identical. Inspection coordination and export packing are in-house habits, not afterthoughts. Ask for a written acknowledgement that names SUS309TB, the manufacture process/finish marks, and the Table 2 heat-treatment condition before melt. SHH STEEL can make SUS309TB to that written scope.
Supply Capability
SHH STEEL can produce and supply JIS G3463 SUS309TB across enquiry-oriented OD × wall bands, in seamless or welded routes, with certificates and optional annex tests as ordered. Summary capability follows in the table; stock language below is an RFQ map, not a frozen tonnage catalogue. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for SUS309TB when the mill schedule allows.
| Item | Capability |
|---|---|
| Standard | JIS G3463 stainless steel tubes for boilers and heat exchangers |
| Grade symbol | SUS309TB |
| Product form | Seamless (S) and welded (A / L / E) tube; finishes S-H / S-C / A / A-C / E-C as marked |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (JIS G 0415 / EN 10204 3.1 style as ordered) |
| Typical OD practice | 15.9–139.8 mm per standard Note 1; other by agreement |
| Wall / gauge | OD × wall / BWG-class HX gauges within Attached Tables; other by agreement |
Stock / Available sizes
SHH STEEL can produce and supply JIS G3463 SUS309TB. Stock / Available sizes: enquiry band typically aligns with 15.9–139.8 mm OD practice under G3463 Note 1, with OD×wall HX gauges; schedule 5S–80 (and heavier by agreement) depending on grade family. For SUS309TB, practical fast-track sizes often sit in mid-bore process and utility ranges — send the OD × wall list for a firm acknowledgement. Context: hot-finished seamless for thick heat-service walls; welded routes for large-OD HX shellside stubs when the design allows.
Cut lengths, bevels, special NDT, and IGC annex tests add lead time — call them early. Sisters often quoted alongside: SUS309STB, SUS310TB, SUS310STB, SUS304TB. Email the size list to start. SHH STEEL can produce trial lengths of SUS309TB for procedure qualification before the bulk release when the project calendar needs it. SHH STEEL can produce trial lengths of SUS309TB for procedure qualification before bulk release when the project calendar needs it. Keep the SUS309TB caution visible here: carbon may reach 0.15% — treat as-welded aqueous corrosion as a separate review; many buyers actually need SUS309STB.
FAQ
-
What is JIS G3463 SUS309TB stainless steel tube used for?
- JIS G3463 SUS309TB is stainless tube for boiler and heat-exchanger service (superheater, HX, condenser, catalyser) — hot-gas coolers, thermal oxidiser exchangers, kiln waste-heat bundles, and high-temperature flue-gas HX stubs. Role summary: higher Cr-Ni austenitic tube for heat-facing and oxidation-lean HX duties that outgrow 18-8 chromium. It is a Japanese boiler/HX tube product standard mark, not an automatic ASTM A213 certificate.
-
Does JIS G3463 SUS309TB cover seamless and welded tube?
- Yes. Manufacture allows seamless and welded automatic-arc (A), laser (L), or electric-resistance (E) routes with finish marks such as S-H, S-C, A-C, or E-C. SHH STEEL can produce and supply either route for SUS309TB when the mill can meet the ordered size and tests. The title omits Seamless/Welded because JIS G3463 covers both manufacture routes — the PO must still name the process mark.
-
What heat treatment applies to SUS309TB?
- SUS309TB is delivered solution annealed under JIS G3463. Table 2 reference: 1030 °C min, rapid cool. Stabilisation or other purchaser options, where allowed, must be written on the order. Certificate wording should match the treatment actually performed.
-
How does SUS309TB compare with sister grades SUS309STB, SUS310TB, SUS310STB?
- SUS309TB is filed as austenitic. Typical sisters on the same RFQ are SUS309STB, SUS310TB, SUS310STB. Design caution: carbon may reach 0.15% — treat as-welded aqueous corrosion as a separate review; many buyers actually need SUS309STB Pick the sister when the medium or strength floor outgrows this symbol rather than stretching wall alone.
-
What tests appear on the mill certificate for SUS309TB?
- Expect cast analysis (Table 3), room-temperature tensile results (Table 4), flattening/flaring as applicable, dimensions, hydrostatic or NDT as ordered, and every special annex test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow JIS G 0415 or EN 10204 3.1 style when specified.
-
Is 309 / UNS S30900 class the same as ordering SUS309TB?
- No. 309 / UNS S30900 class is a commercial / UNS cross-walk for body text. The purchase order should lock JIS G3463 and SUS309TB so cast limits, heat treatment, and process marks are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for JIS G3463 SUS309TB?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for SUS309TB within the typical 15.9–139.8 mm OD practice, with measured walls by agreement. Size context: hot-finished seamless for thick heat-service walls; welded routes for large-OD HX shellside stubs when the design allows. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
How should SUS309TB be welded?
- Shop guidance: 309/309L-class fillers; manage dilution when buttering carbon steel; aqueous IGC still wants the S or L sister. Mill heat treatment of seamless or welded tube does not replace a qualified WPS on fabricator joints or tube-to-tubesheet welds. For corrosive as-welded duty, confirm low-carbon, stabilisation, duplex ferrite control, or anneal practice as applicable. Caution: carbon may reach 0.15% — treat as-welded aqueous corrosion as a separate review; many buyers actually need SUS309STB
-
When should I choose a duplex or higher-Mo grade instead of SUS309TB?
- Move when chloride pitting, crevice attack, or SCC risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: carbon may reach 0.15% — treat as-welded aqueous corrosion as a separate review; many buyers actually need SUS309STB Sister pointers: SUS309STB, SUS310TB, SUS310STB. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify JIS G3463 SUS309TB with ASTM A213 or ASME SA213?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites JIS G3463 SUS309TB does not clear ASTM A213 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What surface finishes are available for SUS309TB?
- Pickled after heat treatment is the usual HX tube supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for SUS309TB when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
JIS G3463 SUS309TB is stainless steel tube for boiler and heat-exchanger service — higher Cr-Ni austenitic tube for heat-facing and oxidation-lean HX duties that outgrow 18-8 chromium. SHH STEEL can produce and supply it in seamless or welded routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include SUS309STB, SUS310TB, SUS310STB. Related ASTM A213 pages share chemistry families but not Japanese acceptance text. Email admin@steelspecs.com with OD × wall, process mark, and medium notes to start the quote.