DIN 17102 Carbon Steel Plates
SHH STEEL supplies DIN 17102 weldable normalized fine grain structural steel plates as China steel mill-Direct Supply. The standard covers plate, strip, wide flats, sections and bars in grades such as StE255, StE285, StE355, StE380, StE420, StE460 and StE500, plus WStE, TStE and EStE qualities for elevated-temperature or low-temperature service. Steels are fine-grain, readily weldable and commonly supplied normalized. Closely related current grades include EN 10025-3 S355N / S355NL / S460N / S460NL. Competitive mill price, cut-to-size service, fast delivery and full MTCs.
-
DIN 17102 EStE380 Steel Plate | EStE380 Fine Grain Steel
DIN 17102 EStE380 / EStE 380 is weldable normalized fine-grain steel for special low-temperature service. Yield is 380 MPa at ≤16 mm. Tensile is typically 510–650 MPa at ≤70 mm. SHH STEEL supplies EStE380 worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.View More -
DIN 17102 TStE380 Steel Plate | TStE380 Fine Grain Steel
DIN 17102 TStE380 / TStE 380 is weldable normalized fine-grain steel for low-temperature service. Yield is 380 MPa at ≤16 mm. Tensile is typically 510–650 MPa at ≤70 mm. SHH STEEL supplies TStE380 worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.View More -
DIN 17102 WStE380 Steel Plate | WStE380 Fine Grain Steel
DIN 17102 WStE380 / WStE 380 is weldable normalized fine-grain steel for elevated-temperature service. Yield is 380 MPa at ≤16 mm. Tensile is typically 510–650 MPa at ≤70 mm. SHH STEEL supplies WStE380 worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.View More -
DIN 17102 StE380 Steel Plate | StE380 Fine Grain Steel
DIN 17102 StE380 / StE 380 is weldable normalized fine-grain steel plate. Yield is 380 MPa at ≤16 mm. Tensile is typically 510–650 MPa at ≤70 mm. SHH STEEL supplies StE380 worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.View More -
DIN 17102 EStE315 Steel Plate | EStE315 Fine Grain Steel
DIN 17102 EStE315 / EStE 315 is weldable normalized fine-grain steel for special low-temperature service. Yield is 315 MPa at ≤16 mm. Tensile is typically 440–590 MPa at ≤70 mm. SHH STEEL supplies EStE315 worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.View More -
DIN 17102 TStE315 Steel Plate | TStE315 Fine Grain Steel
DIN 17102 TStE315 / TStE 315 is weldable normalized fine-grain steel for low-temperature service. Yield is 315 MPa at ≤16 mm. Tensile is typically 440–590 MPa at ≤70 mm. SHH STEEL supplies TStE315 worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.View More -
DIN 17102 WStE315 Steel Plate | WStE315 Fine Grain Steel supplier
DIN 17102 WStE315 / WStE 315 is weldable normalized fine-grain steel for elevated-temperature service. Yield is 315 MPa at ≤16 mm. Tensile is typically 440–590 MPa at ≤70 mm. SHH STEEL supplies WStE315 worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.View More -
DIN 17102 StE315 Steel Plate | StE315 Fine Grain Steel
DIN 17102 StE315 / StE 315 is weldable normalized fine-grain steel plate. Yield is 315 MPa at ≤16 mm. Tensile is typically 440–590 MPa at ≤70 mm. SHH STEEL supplies StE315 worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.View More -
DIN 17102 EStE285 Steel Plate | EStE285 Fine Grain Steel Supplier
DIN 17102 EStE285 / EStE 285 is weldable normalized fine-grain steel for special low-temperature service. Yield is 285 MPa at ≤16 mm. Tensile is typically 390–510 MPa. SHH STEEL supplies EStE285 worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.View More -
DIN 17102 TStE285 Steel Plate | TStE285 Fine Grain Steel supplier
DIN 17102 TStE285 / TStE 285 is weldable normalized fine-grain steel for low-temperature service. Yield is 285 MPa at ≤16 mm. Tensile is typically 390–510 MPa. SHH STEEL supplies TStE285 worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.View More -
DIN 17102 WStE285 Steel Plate | WStE285 Fine Grain Steel supplier
DIN 17102 WStE285 / WStE 285 is weldable normalized fine-grain steel for elevated-temperature service. Yield is 285 MPa at ≤16 mm. Tensile is typically 390–510 MPa. SHH STEEL supplies WStE285 worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.View More -
DIN 17102 StE285 Steel Plate | StE285 Fine Grain Steel supplier
DIN 17102 StE285 / StE 285 is weldable normalized fine-grain steel plate. Yield is 285 MPa at ≤16 mm. Tensile is typically 390–510 MPa. SHH STEEL supplies StE285 worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.View More
DIN 17102 Carbon Steel Plates
Boiler & Pressure Vessel Steel Plates
SHH STEEL, a trusted Pressure Vessel Steel Plates exporter, produces and exports pressure vessel steel plates for boilers, tanks, and petrochemical applications. Our plates, like ASTM A516 Grade 70, offer high tensile strength and toughness, meeting ASME standards. With a 5,000-ton inventory, we ensure 3–5 day delivery for in-stock items, supported by SGS/TUV inspections and mill certificates. Rely on SHH STEEL for boiler steel plates and custom high-pressure solutions.
Boiler & Pressure Vessel Steel Plates
ASME SA-36/SA-36M
JIS G4109
JIS G3119
JIS G3120
ASME SA302
JIS G3126
ASTM A302
JIS G3127
ASME SA225
BS 1501
ASTM A225
DIN 17155
ASME SA455
EN 10120
ASME SA562
GB 6654
ASTM A455
GB/T 6653
ASTM A562
JIS G 3116
ASME SA841
ASME SA553
GB/T 713.3-2023
ASTM A553
GB/T 713.4-2023
GB/T 713.5-2023
ASME SA516
GOST 5520
ASTM A516/516M
GB/T 3077
GB/T 3274
DIN 17102
GB/T 24511
GB/T 24512
GB/T 3077
ASTM A285
ASME SA285
ASTM A515
ASME SA515
ASTM A299
ASTM A517/A517M
ASME SA299
ASTM A204
ASME SA517/SA517M
ASME SA204
ASTM A203
ASME SA203
ASTM A353
ASME SA353
ASTM A387
ASME SA387
ASTM A537
ASME SA537
JIS G3115
GB/T 713.2-2023
GB/T 19189
GB/T 3531
EN 10028-2
EN 10028-3
EN 10028-4
EN 10028-5
EN 10028-6
JIS G3103
ISO 9328-2
X