DIN 17102 StE315 normalized fine-grain steel plate, 315 MPa yield class, SHH STEEL

DIN 17102 StE315 Steel Plate | StE315 Fine Grain Steel

DIN 17102 StE315 / StE 315 is weldable normalized fine-grain steel plate. Yield is 315 MPa at ≤16 mm. Tensile is typically 440–590 MPa at ≤70 mm. SHH STEEL supplies StE315 worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.
Keywords
DIN 17102 StE315, StE315, StE 315, STE315, DIN17102 StE315, fine grain structural steel, StE315 supplier, StE315 equivalent
Equivalent Grades:
EN 10025-3 S315N (non-standard EN; use S355N downgrade) / EN 10028-3 P315N (rare) / ASTM A515 Gr 60 (near) / JIS G3115 SPV315 / GB Q315R (near, not common) — Material Specification: DIN 17102 (withdrawn) — Delivery: Normalized (N) or Normalized-rolled
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
How StE / WStE / TStE / EStE Differ at 315
Material Comparison
Fine-Grain Structural Service at 315 MPa
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Equivalent Material Grades
Applications
Global Delivery & Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is DIN 17102 StE315 Steel?

DIN 17102 StE315, also written StE 315, STE315, DIN17102 StE315 and StE315 steel plate, is a weldable normalized fine-grain structural steel under DIN 17102. StE means the basic / room-temperature quality. Yield in the thin band is 315 MPa. Tensile at ≤70 mm is typically 440–590 MPa. This grade sits between StE285 and StE355. It is not the P275N line and not the P355N line. Buyers still name it when an old German drawing kept the 315 step instead of jumping to 355. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) for this grade. Plate is produced to DIN 17102 and shipped to buyers in the USA, Europe, Middle East and Southeast Asia.

A purchase order that only says “315 fine grain” is incomplete. Write DIN 17102 StE315. Do not ship StE285 against a StE315 drawing. Do not ship StE355 against a StE315 drawing and call 40 MPa extra yield a free upgrade. The calculation used 315 MPa, not 355 MPa.

DIN 17102 is a legacy specification. New European work usually picks S275N / P275N or S355N / P355N under EN 10025-3. There is no single EN name as clean as StE285 → P275N or StE355 → P355N. Replacement projects still name StE315 when the original German file stays on that number.

This page is not DIN 17100 St52-3. DIN 17100 is ordinary structural steel. DIN 17102 is fine-grain, killed, normally normalized. This page is not SA516 Gr.70. Grade 70 is ASME carbon vessel plate at 260 MPa yield. StE315 is 315 MPa yield fine-grain plate. It is not ASTM A36 steel plate. It is not QT alloy under ASME SA387 or ASME SA543.

Company scope: global steel mill sourcing partner – SHH STEEL.

Material Specification

Specification ElementRequirementSHH STEEL Compliance
GradeDIN 17102 StE315 / StE 315Confirmed
Product SpecificationDIN 17102Applied
Quality letterStE = basic / room temperatureConfirmed
Steel typeKilled, weldable, fine grainConfirmed
Usual deliveryNormalizedConfirmed
Yield idea315 MPa at ≤16 mmConfirmed
Strength positionBetween StE285 and StE355Confirmed
Supply roleGlobal steel mill sourcing partnerSHH STEEL
MarketsUSA, Europe, Middle East, Southeast AsiaFOB / CIF as ordered
CertificationEN 10204 3.1 or 3.2 / third-partyAs ordered

This plate sits in structural steel plates and high strength low alloy plates. Vessel comparisons belong next to pressure vessel steel plates and ASME SA516, not as automatic substitutes.

Chemical Composition

DIN 17102 StE315 / StE 315 uses a manganese band between the 285 and 355 families.

Heat Analysis — DIN 17102 StE315 (typical cast / ladle limits)

ElementHeat Analysis (%)
Carbon (C), max0.18
Silicon (Si), max0.40
Manganese (Mn)0.70 – 1.50
Phosphorus (P), max0.035
Sulfur (S), max0.030
Nitrogen (N), max0.020
Aluminium (Al), min (total, when used for grain)0.020
Chromium (Cr), max0.30
Copper (Cu), max0.20
Molybdenum (Mo), max0.08
Nickel (Ni), max0.30
Niobium (Nb), max0.05
Nb + Ti + V, max0.12

StE285 manganese is 0.60–1.40. StE355 manganese is 0.90–1.65. Do not ship a 355 heat as StE315 because a coupon came in low. TStE315 and EStE315 tighten P and S. SHH STEEL reports heat analysis on every certificate and product analysis when the order names it. If a Houston, Rotterdam or Jebel Ali specification tightens P and S, write that on the order.

Mechanical Properties

Yield starts at 315 MPa at ≤16 mm and falls as thickness rises.

Tensile and Yield — DIN 17102 StE315 (typical published bands)

Thickness (mm)Yield ReH min (MPa)Tensile Rm (MPa)
≤16315440 – 590 (≤70 mm band)
16 – 35305440 – 590
35 – 50295440 – 590
50 – 70285440 – 590
70 – 100275430 – 580
100 – 150265410 – 570
Density7.85 g/cm³7.85 g/cm³

Do not quote 315 MPa yield on a 80 mm plate. Do not treat 440–590 MPa tensile as permission to stamp SA516 Gr.70, SA612 steel plate or SA737 Gr.B.

Impact is the reason buyers pick DIN 17102 instead of DIN 17100. StE315 is the basic quality. If the drawing names −20 °C or −50 °C, the order may actually need TStE315 or EStE315. Write the test temperature, orientation and energy on the purchase order.

How StE / WStE / TStE / EStE Differ at 315

GradeQuality ideaNotes
StE315Basic / room-temperature fine grainThis page
WStE315Elevated temperature (Warm)Same yield idea, warm service
TStE315Low temperature (Tief)Same yield idea, colder impact
EStE315Special low temperatureTightest C / P / S in the 315 family

Same 315 MPa yield idea. Different impact and, on T/E, tighter residuals. SHH STEEL will not ship StE315 against a TStE315 impact temperature without a written change.

Material Comparison

Material Comparison

GradeRouteStrength ideaSwap?
DIN 17102 StE285Normalized fine grain285 / ~390–510No
DIN 17102 StE315Normalized fine grain315 / ~440–590This page
DIN 17102 StE355Normalized fine grain355 / 490–630No
P275N / S275NEN 10028-3 / EN 10025-3Maps to StE285No
P355N / S355NEN 10028-3 / EN 10025-3Maps to StE355No
SA516 Gr.70Carbon vessel260 / 485–620No
SA662 Gr.CC-Mn-Si low-temp vesselDifferent bookNo
ASTM A36 steel plateStructural carbonNot fine-grain DIN 17102No

SA203 Gr.A, SA285 Gr.C and SA299 Gr.A are vessel plates. None of them is StE315.

Fine-Grain Structural Service at 315 MPa

DIN 17102 StE315 / StE 315 is selected when the drawing wants fine-grain, weldable, normalized plate at the intermediate 315 MPa step: frames, tanks, machinery and other work still calculated to the old German book. It is not a free substitute for StE355. It is not automatically a Section VIII plate. If the vessel is ASME, the drawing should name an ASME or ASTM grade such as SA516 Gr.70, SA537 Cl.1 or SA662 Gr.B.

SHH STEEL supplies this plate to fabricators in the United States, Europe, the Middle East and Southeast Asia. It is not nickel low-temp plate like SA203 Gr.D or SA203 Gr.E. It is not QT Ni-Cr-Mo like SA543 Type B Cl.1. It is not Cr-Mo like SA387 Gr.22 Cl.2. Stainless inquiries belong on ASME SA240 or ASTM A240.

Weldability

StE315 is killed fine-grain C-Mn steel. Welding is production welding, and Code welding when the equipment is a vessel.

Qualify procedures to the applicable code. For ASME work that happens to use a dual-named plate, use ASME Section IX. Consumables should match the 440–590 MPa tensile band, not a SA387 Gr.12 Cl.2 Cr-Mo procedure and not a QT procedure from SA517 Gr.F. Preheat follows thickness and hydrogen control. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL is normalized DIN 17102 StE315 / StE 315 plate. Fine-grain practice and normalize are the product idea. As-rolled shipment is a special agreement.

If the vessel or structure will see PWHT, test coupons shall follow a simulated cycle when the order names it. This is not the QT route used on SA738 Gr.A or SA737 Gr.C. Special heat treatment, extra simulation or third-party hold points add time. Plan about two months when those extras are on the order.

The certificate lists DIN 17102 StE315 (and StE 315 if requested); heat number; heat analysis; product analysis when ordered; tensile results to the correct thickness column; normalize statement; impact when ordered. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to an EN name is available only when chemistry, tensile and impact all fit that EN edition. Do not assume P355N dual marking; that name sits on StE355.

Dimensions

Usual supply range from SHH STEEL for StE315 fine grain steel:

  • Thickness: commonly 6 mm – 150 mm. Confirm any request above 150 mm against mill capability
  • Width: 1500 mm – 4000 mm
  • Length: 3000 mm – 12000 mm
  • Cut-to-length plates and nest sizes inside those limits

Ship plate inquiries belong on shipbuilding steel plates or BV Rules. Weathering plate belongs on EN 10025-5 or Corten A/B. TMCP fine-grain structural belongs on EN 10025-4. QT structural belongs on EN 10025-6. Ordinary structural belongs on EN 10025-2 or JIS G3106.

Tolerances

Dimensional limits follow the mill rolling standard named on the order, commonly EN 10029 for plate when the buyer is in Europe. Do not apply ASTM A36/A36M structural tolerances to a DIN fine-grain plate without writing them. UT to EN 10160 or ASTM A435 / A577 / A578 is added when the order names it.

Supplementary Requirements

Most export DIN 17102 StE315 / StE 315 orders add extras. SHH STEEL does not assume them.

Charpy details. Temperature, energy, location and orientation. If the temperature is −40 °C or −50 °C, confirm whether the grade should be TStE315 or EStE315.

Simulated PWHT. When the equipment will be stress-relieved.

NDE. UT per the named method.

Z-direction / through-thickness testing. When the drawing names Z15 / Z25 / Z35.

Third-party. EN 10204 3.2, with inspectors arranged for US, European or Middle East documentation packages.

Equivalent Material Grades

These names are project-comparison grades. They are not automatic substitutes.

DesignationStandard / regionNotes
DIN 17102 StE315 / StE 315DIN 17102Name on this page
StE285DIN 17102Lower step ≈ P275N / S275N
StE355DIN 17102Higher step ≈ P355N / S355N
WStE315DIN 17102Elevated-temperature sister
TStE315DIN 17102Low-temperature sister
EStE315DIN 17102Special low-temperature sister
SA516 Gr.70SA-516Vessel carbon, different book
ASTM A516A516 familyRelated vessel family
ASTM A572 Gr.50Structural HSLANot DIN 17102

ASME SA515 and ASME SA662 are not StE315.

Applications

IndustryTypical components
Intermediate-strength fine-grain structuresDIN 17102 StE315 frames and StE 315 plates
Tanks and process steelworkSTE315 courses
Dual-certified exportStE315 plate from SHH STEEL when the drawing keeps the DIN name
FabricationStE315 cut to nest sizes

Stainless inquiries belong on stainless steel products, JIS G4305 or AISI stainless. Other vessel comparisons: SA203 Gr.B, SA302 Gr.B, A516 Grade 70, SA533 Type C Cl.2, SA517 Gr.P, SA738 Gr.C.

Global Delivery & Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN and JIS steel to the USA, Europe, Middle East and Southeast Asia. Origin is mill-direct, China origin. We do not treat DIN 17102 StE315 as an Asia-only stock item. Inquiry packages are written for fabricators and EPC buyers in Houston, Rotterdam, Antwerp, Jebel Ali, Dammam, Singapore and surrounding ports.

Typical trade terms:

  • FOB Shanghai
  • CIF Houston
  • CIF Rotterdam
  • CIF Jebel Ali
  • Other CIF / CFR ports on request (Los Angeles, New York, Hamburg, Genoa, Jeddah, Mundra, Ho Chi Minh)

Typical lead time for DIN 17102 StE315 / StE 315:

  • Ex-stock / ready plate: about 5–7 days after order confirmation, subject to actual warehouse size and cutting
  • Mill rolling, standard normalize: about 45 days
  • Special heat treatment, simulated PWHT, 3.2 hold or extra NDE: about 2 months

Documents travel with the cargo: mill certificate, packing list, commercial invoice, bill of lading, and EN 10204 3.1 or 3.2 as ordered. Third-party inspection can be arranged before loading for US, European or Middle East projects. Packing is seaworthy, with edge protection and marking in English as specified on the order.

If the buyer actually needs StE355 / P355N, say so on the inquiry. Do not assume a domestic Chinese certificate format will pass at destination.

Why Choose SHH STEEL

SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We supply ASTM / ASME / EN / DIN / JIS steel to the USA, Europe, the Middle East and Southeast Asia. On DIN 17102 StE315 / StE 315 that means mill pricing, StE315 chemistry reported, recorded normalize, tensile results to the correct thickness column, 315 MPa yield in the thin band, 3.1 as standard and 3.2 when specified. Trade terms include FOB Shanghai and CIF Houston / Rotterdam / Jebel Ali.

We keep the grade on the order. StE315 is not StE285. StE315 is not StE355. StE315 is not TStE315. DIN 17102 is not DIN 17100. StE315 is not SA516 Gr.70. StE315 is not SA387 Gr.22 Cl.2. If the drawing names 355 MPa, we will not ship StE315 and call it close.

Company scope: global steel mill sourcing partner – SHH STEEL.

FAQ

What names are used for DIN 17102 StE315?
Buyers write DIN 17102 StE315, StE 315, STE315, DIN17102 StE315 and StE315 steel plate. SHH STEEL prints the wording on the purchase order.
What is the yield strength of StE315?
315 MPa minimum at ≤16 mm. Yield drops as thickness increases. Tensile is typically 440–590 MPa at ≤70 mm.
Is StE315 the same as P355N or P275N?
No. P275N maps to StE285. P355N maps to StE355. StE315 is the intermediate 315 MPa step and has no equally clean single EN name.
How is StE315 different from StE285 and StE355?
StE285 yield is 285 MPa in the thin band. StE355 yield is 355 MPa. StE315 is 315 MPa. Tensile and manganese bands sit between those two grades.
Is StE315 the same as SA516 Grade 70?
No. Different book, different yield and impact rules.
Can SHH STEEL ship DIN 17102 StE315 outside Asia?
es. SHH STEEL is a global steel mill sourcing partner. We supply this plate to the USA, Europe, the Middle East and Southeast Asia on FOB Shanghai or CIF Houston / Rotterdam / Jebel Ali.
What is the delivery time for StE315?
Ex-stock about 5–7 days. Standard mill normalize about 45 days. Special heat treatment, simulated PWHT or 3.2 inspection about 2 months.

Conclusion

DIN 17102 StE315 Steel Plate, also searched as StE 315, STE315 and DIN17102 StE315, is weldable normalized fine-grain steel under DIN 17102 at the intermediate 315 MPa yield step, typically 440–590 MPa tensile at ≤70 mm. Whether the inquiry says DIN 17102 StE315, StE 315 or StE315 steel plate, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with StE315 chemistry, recorded normalize, and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies DIN 17102 StE315 / StE315 Fine Grain Steel to the USA, Europe, the Middle East and Southeast Asia for work that actually names this grade. FOB Shanghai / CIF Houston / Rotterdam / Jebel Ali.

Contact SHH STEEL for mill rolling, stock inquiry, impact testing, 3.2 inspection or a quotation.

DIN 17102 StE315 Steel Plate, StE 315, STE315, DIN17102 StE315, fine grain structural steel, StE315 supplier, global steel mill sourcing partner SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response