DIN 17102 EStE420 special low-temperature fine-grain steel plate, P420NL2, SHH STEEL

DIN 17102 EStE420 Steel Plate | EStE420 Fine Grain Steel

DIN 17102 EStE420 / EStE 420 is weldable normalized fine-grain steel for special low-temperature service. Yield is 420 MPa at ≤16 mm. Tensile is typically 530–680 MPa at ≤70 mm. SHH STEEL supplies EStE420 worldwide as a global steel mill sourcing partner, with 3.1 or 3.2 certificates.
Keywords
DIN 17102 EStE420, EStE420, EStE 420, ESTE420, DIN17102 EStE420, P420NL2, special low temperature fine grain steel, EStE420 supplier
Equivalent Grades:
DIN 17102 EStE420 / EN 10025-3 S420NL (special low-temp) / EN 10028-3 P420NL2 (near) / GB Q420E (near) — Material Specification: DIN 17102 (withdrawn) — Delivery: Normalized (N), lower-temp impact (-60℃ class)
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
How StE / WStE / TStE / EStE Differ at 420
Material Comparison
Special Low-Temperature Fine-Grain Service at 420 MPa
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Equivalent Material Grades
Applications
Global Delivery & Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is DIN 17102 EStE420 Steel?

DIN 17102 EStE420, also written EStE 420, ESTE420, DIN17102 EStE420 and EStE420 steel plate, is a weldable normalized fine-grain structural steel under DIN 17102. The E prefix is the special low-temperature quality — colder and cleaner than TStE420. Yield in the thin band is still 420 MPa. Tensile at ≤70 mm is still typically 530–680 MPa. This is the DIN 17102 special-low-temp line that conversion tables map to P420NL2. It is not EStE380 and not EStE460. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) for this grade. Plate is produced to DIN 17102 and shipped to buyers in the USA, Europe, Middle East and Southeast Asia.

A purchase order that only says “420 NL2 fine grain” is incomplete if the drawing still names DIN. Write DIN 17102 EStE420 and the impact temperature. Do not ship StE420, WStE420 or TStE420 against an EStE420 drawing. Do not ship EStE355 or EStE460 because the yield step is wrong.

DIN 17102 is a legacy specification. New European pressure work usually names P420NL2. Replacement projects still name EStE420 when an old German calculation or mill qualification stays on DIN.

This page is not DIN 17100 St52-3. It is not SA516 Gr.70. It is not nickel plate like SA203 Gr.A or SA203 Gr.D. It is not ASTM A36 steel plate. It is not QT alloy under ASME SA387 or ASME SA543.

Company scope: global steel mill sourcing partner – SHH STEEL.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Grade DIN 17102 EStE420 / EStE 420 Confirmed
Product Specification DIN 17102 Applied
Quality letter E = special low temperature Confirmed
Steel type Killed, weldable, fine grain Confirmed
Usual delivery Normalized Confirmed
Yield idea 420 MPa at ≤16 mm Confirmed
Related modern name P420NL2 Confirm on order
Supply role Global steel mill sourcing partner SHH STEEL
Markets USA, Europe, Middle East, Southeast Asia FOB / CIF as ordered
Certification EN 10204 3.1 or 3.2 / third-party As ordered

This plate sits in structural steel plates, high strength low alloy plates and next to pressure vessel steel plates. ASME carbon comparisons belong on ASME SA516 and ASME SA662, not as automatic substitutes.

Chemical Composition

DIN 17102 EStE420 / EStE 420 is the cleanest 420 column in this book. Product analysis is slightly wider than heat analysis.

Heat Analysis and Product Analysis — DIN 17102 EStE420 (typical limits)

Element Heat Analysis (%) Product Analysis (%)
Carbon (C), max 0.16 0.18
Silicon (Si) 0.10 – 0.50 0.10 – 0.55
Manganese (Mn) 1.00 – 1.70 0.95 – 1.75
Phosphorus (P), max 0.025 0.030
Sulfur (S), max 0.015 0.020
Nitrogen (N), max 0.020 0.022
Aluminium (Al), min (total, when used for grain) 0.020 0.018
Chromium (Cr), max 0.30 0.35
Copper (Cu), max 0.20 0.25
Molybdenum (Mo), max 0.10 0.12
Nickel (Ni), max 0.80 0.85
Niobium (Nb), max 0.05 0.06
Vanadium (V), max 0.20 0.22
Nb + Ti + V, max 0.22 0.24

Compare the 420 family:

Grade C max (heat) P max (heat) S max (heat)
StE420 / WStE420 0.20 0.035 0.030
TStE420 0.18 0.030 0.025
EStE420 0.16 0.025 0.015

Do not ship a TStE420 heat as EStE420. If the order dual-names P420NL2, residuals must also fit EN 10028-3 of the named edition. SHH STEEL reports heat analysis on every certificate and product analysis when the order names it.

Mechanical Properties

Room-temperature yield and tensile follow the 420 family. Special low-temperature impact is why the E letter exists.

Room-temperature properties — DIN 17102 EStE420 (typical published bands)

Thickness (mm) Yield ReH min (MPa) Tensile Rm (MPa)
≤16 420 530 – 680 (≤70 mm band)
16 – 35 410 530 – 680
35 – 50 400 530 – 680
50 – 70 390 530 – 680
70 – 100 380 520 – 670
100 – 150 370 510 – 660
Density 7.85 g/cm³ 7.85 g/cm³

Do not quote 420 MPa yield on an 80 mm plate. Do not treat 530–680 MPa tensile as permission to stamp SA516 Gr.70, SA662 Gr.A or SA285 Gr.A.

Impact for EStE420 is the special low-temperature package. P420NL2 comparison is commonly −50 °C with the tighter NL2 chemistry idea. Write the test temperature, orientation and energy on the order. Do not assume a TStE420 coupon covers EStE420.

How StE / WStE / TStE / EStE Differ at 420

Grade Quality idea Typical modern comparison
StE420 Basic / room-temperature fine grain P420N / S420N
WStE420 Elevated temperature (Warm) P420NH
TStE420 Low temperature (Tief) P420NL1 / S420NL
EStE420 Special low temperature P420NL2

Same 420 MPa yield idea. E is not a marketing letter on TStE420. E has lower carbon, lower P and S, and a colder quality idea. SHH STEEL will not ship TStE420 against an EStE420 purchase order without a written change.

Material Comparison

Grade Route Strength / service idea Swap?
DIN 17102 EStE355 Normalized fine grain 355 / 490–630, special low-temp No
DIN 17102 EStE380 Normalized fine grain 380 / ~510–650, special low-temp No
DIN 17102 StE420 Normalized fine grain 420 / ~530–680, basic quality No
DIN 17102 TStE420 Normalized fine grain 420 / ~530–680, low-temp quality No
DIN 17102 EStE420 Normalized fine grain 420 / ~530–680, special low-temp This page
P420NL2 EN 10028-3 Closest vessel replacement Comparison only
SA516 Gr.70 Carbon vessel 260 / 485–620 No
SA662 Gr.B C-Mn-Si low-temp vessel Different book No
SA203 Gr.E 3.5Ni vessel Nickel toughness, not EStE No

SA285 Gr.C, SA299 Gr.B and SA737 Gr.C are also vessel or HSLA plates. None of them is EStE420

Special Low-Temperature Fine-Grain Service at 420 MPa

DIN 17102 EStE420 / EStE 420 is selected for welded structures and pressure equipment that need the coldest fine-grain package at the 420 MPa yield step: low-temperature tanks, cold-climate steelwork and other work still calculated to the old German book. It is the practical DIN counterpart to P420NL2. It is not automatically an ASME Section VIII plate. If the vessel is ASME, the drawing should name an ASME or ASTM grade such as SA516 Gr.70, SA662 Gr.C or SA537 Cl.1.

SHH STEEL supplies this plate to fabricators in the United States, Europe, the Middle East and Southeast Asia. It is not nickel low-temp plate like SA203 Gr.B or SA203 Gr.F. Those grades use nickel. EStE420 uses fine grain, low residuals and normalize. It is not QT Ni-Cr-Mo like SA543 Type B Cl.3. It is not Cr-Mo like SA387 Gr.22 Cl.2 or SA387 Gr.11 Cl.2. Stainless inquiries belong on ASME SA240 or ASTM A240.

Weldability

EStE420 is killed fine-grain C-Mn-microalloy steel with the lowest C / P / S in the 420 family. Welding is production welding, and Code welding when the equipment is a vessel.

Qualify procedures to the applicable code. For ASME work that happens to use a dual-named plate, use ASME Section IX. Consumables should match the 530–680 MPa tensile band, not a SA387 Gr.12 Cl.2 Cr-Mo procedure and not a QT procedure from SA517 Gr.Q. Preheat follows thickness and hydrogen control. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL is normalized DIN 17102 EStE420 / EStE 420 plate. Fine-grain practice and normalize are the product idea. As-rolled shipment is a special agreement and is a poor fit for a special low-temperature quality.

If the vessel or structure will see PWHT, test coupons shall follow a simulated cycle when the order names it. This is not the QT route used on SA738 Gr.B or SA737 Gr.B. Special heat treatment, extra simulation or third-party hold points add time. Plan about two months when those extras are on the order.

The certificate lists DIN 17102 EStE420 (and EStE 420 if requested); heat number; heat analysis including the tighter C / P / S; product analysis when ordered; tensile results to the correct thickness column; normalize statement; impact at the named temperature. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to P420NL2 is available only when chemistry, tensile and impact all fit the named EN edition.

Dimensions

Usual supply range from SHH STEEL for EStE420 fine grain steel:

  • Thickness: commonly 6 mm – 150 mm. Confirm any request above 150 mm against mill capability
  • Width: 1500 mm – 4000 mm
  • Length: 3000 mm – 12000 mm
  • Cut-to-length plates and nest sizes inside those limits

Ship plate inquiries belong on shipbuilding steel plates or BV Rules. Weathering plate belongs on EN 10025-5 or Corten A/B. TMCP fine-grain structural belongs on EN 10025-4. QT structural belongs on EN 10025-6. Ordinary structural belongs on EN 10025-2 or JIS G3106.

Tolerances

Dimensional limits follow the mill rolling standard named on the order, commonly EN 10029 for plate when the buyer is in Europe. Do not apply ASTM A36/A36M structural tolerances to a DIN fine-grain plate without writing them. UT to EN 10160 or ASTM A435 / A577 / A578 is added when the order names it.

Supplementary Requirements

Most export DIN 17102 EStE420 / EStE 420 orders add extras. SHH STEEL does not assume them.

Charpy details. Temperature, energy, location and orientation. This is the reason EStE420 exists. Write the temperature explicitly.

Product analysis. Add this when the destination file wants finished-plate chemistry, not only ladle chemistry.

Simulated PWHT. When the equipment will be stress-relieved.

NDE. UT per the named method.

Z-direction / through-thickness testing. When the drawing names Z15 / Z25 / Z35.

Restricted residuals. Some European files copy EN 10028-3 NL2 options onto EStE420. Write those options on the order.

Third-party. EN 10204 3.2, with inspectors arranged for US, European or Middle East documentation packages.

Equivalent Material Grades

These names are project-comparison grades. They are not automatic substitutes.

Designation Standard / region Notes
DIN 17102 EStE420 / EStE 420 DIN 17102 Name on this page
P420NL2 EN 10028-3 Closest modern vessel comparison
TStE420 DIN 17102 Low-temperature sister ≈ P420NL1 / S420NL
EStE380 DIN 17102 Lower E step
EStE460 DIN 17102 Higher E step ≈ P460NL2
StE420 DIN 17102 Basic quality ≈ P420N / S420N
SA516 Gr.70 SA-516 Vessel carbon, different book
SA662 Gr.A SA-662 Related low-temp carbon vessel
ASTM A516 A516 family Related vessel family
ASTM A285 A285 family Related low-strength vessel family

ASME SA515 is not EStE420.

Applications

Industry Typical components
Special low-temperature fine-grain equipment DIN 17102 EStE420 shells and EStE 420 plates
Cold-service tanks and process steelwork ESTE420 courses
Dual-certified export EStE420 / P420NL2 plate from SHH STEEL when chemistry fits
Fabrication EStE420 cut to nest sizes

Stainless inquiries belong on stainless steel products, JIS G4305 or AISI stainless. Other vessel comparisons: SA302 Gr.A, SA204 Gr.B, A516 Grade 70, SA533 Type C Cl.1, SA517 Gr.P, SA738 Gr.C.

Global Delivery & Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN and JIS steel to the USA, Europe, Middle East and Southeast Asia. Origin is mill-direct, China origin. We do not treat DIN 17102 EStE420 as an Asia-only stock item. Inquiry packages are written for fabricators and EPC buyers in Houston, Rotterdam, Antwerp, Jebel Ali, Dammam, Singapore and surrounding ports.

Typical trade terms:

  • FOB Shanghai
  • CIF Houston
  • CIF Rotterdam
  • CIF Jebel Ali
  • Other CIF / CFR ports on request (Los Angeles, New York, Hamburg, Genoa, Jeddah, Mundra, Ho Chi Minh)

Typical lead time for DIN 17102 EStE420 / EStE 420:

  • Ex-stock / ready plate: about 5–7 days after order confirmation, subject to actual warehouse size and cutting
  • Mill rolling, standard normalize: about 45 days
  • Special heat treatment, simulated PWHT, 3.2 hold or extra NDE: about 2 months

Documents travel with the cargo: mill certificate, packing list, commercial invoice, bill of lading, and EN 10204 3.1 or 3.2 as ordered. Third-party inspection can be arranged before loading for US, European or Middle East projects. Packing is seaworthy, with edge protection and marking in English as specified on the order.

If the buyer needs dual P420NL2 marking for a European file, say so on the inquiry. If the buyer needs a PED / 3.2 file, say so on the inquiry. Do not assume a domestic Chinese certificate format will pass at destination.

Why Choose SHH STEEL

SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We supply ASTM / ASME / EN / DIN / JIS steel to the USA, Europe, the Middle East and Southeast Asia. On DIN 17102 EStE420 / EStE 420 that means mill pricing, EStE420 chemistry with tight C / P / S reported as heat analysis and as product analysis when ordered, recorded normalize, tensile results to the correct thickness column, impact at the named special low temperature, 3.1 as standard and 3.2 when specified. Trade terms include FOB Shanghai and CIF Houston / Rotterdam / Jebel Ali.

We keep the prefix and the number on the order. EStE420 is not TStE420. EStE420 is not StE420. EStE420 is not WStE420. EStE420 is not EStE380. EStE420 is not EStE460. DIN 17102 is not DIN 17100. EStE420 is not SA516 Gr.70. EStE420 is not SA387 Gr.22 Cl.2. If the drawing names TStE420, we will not ship EStE420 and call the grades the same just because yield is 420 MPa.

Company scope: global steel mill sourcing partner – SHH STEEL.

FAQ

What is EStE420 steel plate?
EStE420 is a DIN 17102 weldable normalized fine-grain steel with the special low-temperature quality letter. Yield is 420 MPa at ≤16 mm and tensile is typically 530–680 MPa at ≤70 mm. Buyers also write EStE 420, ESTE420 and DIN17102 EStE420. SHH STEEL supplies this plate as a global steel mill sourcing partner.
What is the equivalent of EStE420?
The usual modern comparison is P420NL2. TStE420 maps to P420NL1 / S420NL. StE420 maps to P420N / S420N. Dual marking is possible only when chemistry, tensile and impact all fit the named EN edition.
What is the difference between EStE420 and TStE420?
Yield and tensile look the same. EStE420 has lower carbon, lower phosphorus and lower sulfur, and a colder quality idea. TStE420 is the Tief package. Do not ship TStE420 against an EStE420 drawing.
EStE420 vs SA203 Grade D — which one for low temperature?
Different books. SA203 Grade D is 3.5Ni pressure-vessel plate. EStE420 is fine-grain C-Mn-microalloy steel with a special low-temperature letter. Use the grade named on the drawing.
What is the chemical composition of EStE420?
Typical heat limits are C 0.16 max, Si 0.10–0.50, Mn 1.00–1.70, P 0.025 max, S 0.015 max. Product analysis is slightly wider. SHH STEEL reports heat analysis on every certificate and product analysis when ordered.
What Charpy temperature should I specify for EStE420?
Write the temperature, energy, location and orientation. P420NL2 comparison is commonly −50 °C. Do not write only “impact tested” and do not assume a TStE420 coupon covers EStE420.
Can EStE420 be used for pressure vessels?
Yes, when the project still names DIN 17102 or accepts P420NL2 dual marking. It is not an automatic ASME Section VIII grade.
How do you weld EStE420?
Treat it as killed fine-grain C-Mn-microalloy steel with low residuals. Match consumables to the 530–680 MPa tensile band, control hydrogen, and qualify the WPS to the applicable code.
Is EStE420 normalized or quenched and tempered?
Normalized. Fine-grain practice plus normalize is the product idea. QT plates belong on other books.
What thickness of EStE420 plate can SHH STEEL supply?
Common supply is 6–150 mm thick, 1500–4000 mm wide and 3000–12000 mm long. Confirm anything above 150 mm against mill capability.
Where can I buy EStE420 steel plate?
SHH STEEL supplies DIN 17102 EStE420 to the USA, Europe, the Middle East and Southeast Asia on FOB Shanghai or CIF Houston / Rotterdam / Jebel Ali. Ask for mill rolling, stock, dual P420NL2 marking when eligible, or EN 10204 3.2.
Do I need EN 10204 3.1 or 3.2 for EStE420?
EN 10204 3.1 is standard. EN 10204 3.2 is arranged when the destination file or PED package requires third-party inspection. Write 3.2 on the purchase order if you need it.
What is the delivery time for EStE420?
Ex-stock about 5–7 days, subject to warehouse size and cutting. Standard mill normalize about 45 days. Special heat treatment, simulated PWHT or 3.2 inspection about 2 months.
What is the density of EStE 420?
7.85 g/cm³.

Conclusion

DIN 17102 EStE420 Steel Plate, also searched as EStE 420, ESTE420 and DIN17102 EStE420, is weldable normalized fine-grain steel under DIN 17102 for special low-temperature service at the 420 MPa yield step, typically 530–680 MPa tensile at ≤70 mm, with the tightest C / P / S in the 420 family, and the usual DIN counterpart to P420NL2. Whether the inquiry says DIN 17102 EStE420, EStE 420 or EStE420 steel plate, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with EStE420 chemistry, recorded normalize, named impact temperature, and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies DIN 17102 EStE420 / EStE420 Fine Grain Steel to the USA, Europe, the Middle East and Southeast Asia for work that actually names this grade. FOB Shanghai / CIF Houston / Rotterdam / Jebel Ali.

Contact SHH STEEL for mill rolling, stock inquiry, dual P420NL2 marking when eligible, impact testing, 3.2 inspection or a quotation.

DIN 17102 EStE420 Steel Plate, EStE 420, ESTE420, DIN17102 EStE420, P420NL2, special low temperature fine grain steel, EStE420 supplier, global steel mill sourcing partner SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X